• 제목/요약/키워드: High-strength mortar

검색결과 533건 처리시간 0.021초

섬유복합재봉(FRP ROD)과 고강도 모르터를 이용한 철근 콘크리트 구조물의 휨 보강공법(MFRI) 공법 (Reinforcing System(MFRI) for Concrete Structure using FRP ROD & High-performance Mortar)

  • 배기선;박상훈;이상욱
    • Composites Research
    • /
    • 제18권4호
    • /
    • pp.59-65
    • /
    • 2005
  • This report is on the Reinforcing System(MFRI) for Concrete Structure using FRP ROD & High-Performance Mortar. The main characteristic of this system is as follow. First, the fiber rods in this system have seven times greater tensile strength than general reinforcing steel bars(re-bar) and the weight is a fifth lighter. Camels coated on the fiber rods' surfaces to improve adhesive strength and pull-out strength. Second, high strength shotcrete mortar is has very good workability and low rebound rate. After installing the Fiber Rods, Shotcrete mortar Is applied or sprayed to finish reinforcement. Finally, MFRI system has excellent fire-resisting performance and sogood tolerance against external environment by inserting fiber rods and reinforcing materials into mortar which has high compressive strength. It is applied to bridge slab, utility box and tunnel of civil engineering works, and beam and slab of building structures.

성형직후 건조환경이 시멘트 모르터의 강도에 미치는 영향 (The Effect of Dry Environment on Strength of Cement Mortar Immediately after Casting)

  • 오무영;김준희
    • 한국농공학회지
    • /
    • 제33권2호
    • /
    • pp.61-72
    • /
    • 1991
  • This study was carried out to research the strength drop of concrete in dry environment. The mixing ratio of cement-fine aggregate was 1: 1, 1 : 2, 1: 3 and 1 : 4. The curing was compared standard curing with dry curing immediately after casting. It is analysis of strength change by water-proof mixing. The curing age of cement mortar was 3days, 7days, l4days and 28days. The result obtained from this study are summarized as follows. 1. The compressive and bending strength change by increasing the curing age, dry curing mortar the increasing rate of strength was decreased than standard curing mortar. 2. The compressive and bending strength change in early curing, strength difference between standard curing mortar and dry curing motar was gradually closed by increasing the W/C. 3. The dry curing mortar was decreased than standard curing mortar in decreasing rate of compressive and bending strength by increasing the W/C. 4. The compressive strength of water-proof mortar in early curing, liquid water-proof mortar was shown high strength in dry curing than standard curing. The powder and liquid water-proof mortar have a small effect in dry environment. The liquid water-proof mortar was high strength without relation change of curing age in dry environment than standard curing. 5. The compressive strength of liquid water-proof mortar in poverty mix, dry curing was shown high strength than standard curing. 6. The bending strength was increased than compressive strength by decreasing the volume of cement in early curing. The increasing rate of bending strength was decreased to compressive stength by increasing the curing age.

  • PDF

폴리머 모르터를 이용한 사면보호재의 개발 (Development of Polymer Mortar Defensive Block for Erosion Control Works)

  • 유능환;연규석;김기성;지경용
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 1998년도 학술발표회 발표논문집
    • /
    • pp.107-112
    • /
    • 1998
  • The objective of this study was to develop a polymer mortar defensive block with high strength and durability using unsaturated polyester resin to complement defects of conventional cement mortar defensive block. Physical and mechanical properties of the polymer mortar defensive block were also investigated. Low absorptivity, high impact strength, and great bending strength of the polymer mortar defensive block was compared with those of the conventional cement defensive block. In conclusion, the polymer mortar defensive block is excellent and useful as industrial products for erosion control works.

  • PDF

섬유복합모르터의 뿜칠마감에 의한 고강도콘크리트 기둥부재의 폭렬방지 (Spatting Resistance of High Strength RC Column Covering Spray-on Materials of Fiber Composite Spray Mortar(FCSM))

  • 송용원;한동엽;이건철;고경택;김진수;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.5-8
    • /
    • 2006
  • High strength concrete has been increasingly used in high rue building and it is very obvious re consider fire resistance performance of that. Unlike the normal strength concrete, high strength concrete in sudden elevating temperature at fire is susceptible to spalling with severe explosion and surface split, due to high density of concrete. In order to endure the spalling, inner space temperature of concrete should be control less than certain point. Therefore this study investigated the influence of covering materials on high strength concrete finishing spray-on materials of fiber composite spray mortar(FCSM). Both polypropylene(PP) and polyvinyl alcohol(PVA) fiber were used in this test. Test showed that concrete, covering 18mm mortar containing PVA fiber and confining metal lath 2.3mm thickness, decreased 50% of main bar ambient temperature. compared with control concrete. In addition, concrete covering 18mm mortar without fiber caused falling of covering materials and then it was exposed in elevating temperature. As a result, spatting of the concrete occurred same as control concrete. However, concrete covering spray-on mortar containing PVA or PP fiber resisted spatting occurrence.

  • PDF

고강도콘크리트의 제물성 향상을 위한 연구

  • 문한영;김기형;문대중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1994년도 가을 학술발표회 논문집
    • /
    • pp.143-150
    • /
    • 1994
  • To improve the qualities of high strength mortar and concrete with high range water reducing admixture, silica fume and gypsum is applied. The flow loss of mortar is reduced and the compressive strength of mortar and concrete is improved by silica fume. And the silica fume is effective for decreasing the temperature of high strength concrete. In addition to, the strength of high strength concrete is more improved by the gypsum.

  • PDF

시멘트.몰탈의 압축강도 개선을 위한 고강도 혼화재의 제조 및 적용특성 (Manufacture and Application Properties of High Strength Admixture for Improving Compressive Strength of Cement and Mortar)

  • 노재성;김도수;임채영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회 논문집(I)
    • /
    • pp.83-88
    • /
    • 1998
  • II-anhydrite, slag, and fly ash produced as industrial by-product were reutilized for the manufacture of high strength admixtures for cement and concrete. The effects of these admixtures on the compressive strength of cement mortar and concrete were examined with those of domestic admixture. At the condition mortar and concrete. Especially, adding of II-anhydrite was very effective for the increasing of compressive strength. Therefore it is possible that these admixture as a high strength admixture apply to cement and concrete.

  • PDF

식물성 유지류에 의한 고강도 모르터의 자기수축 저감에 관한 기초적 연구 (A Basic Study on Reduction of Autogenous Shrinkage of High Strength Mortar by Plant Edible Oil)

  • 송일범;백대현;최영화;백병훈;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2009년도 춘계 학술논문 발표대회 학계
    • /
    • pp.69-72
    • /
    • 2009
  • This study reviewed the reduction effect of autogenous shrinkage of high strength mortar by plant edible oils based on existing studies, in an effort to find the method of reducing autogenous shrinkage of high strength concrete. To summarize the results, first as characteristics of fresh mortar, substitution of plant edible oil showed slight reduction in liquidity. Compressive strength was reduce at age of 28 days compared to plain mix regardless of type and substitution ratio. Ratio of change in the length of autogenous shrinkage of high strength mortar by plant oils was found to reduce compared to the plain, and the reduction effect was most satisfactorγ in bean oil.

  • PDF

촉진양생에 의한 온도이력이 고강도 모르타르의 강도발현에 미치는 영향 (An Effects of the Strength Development of High Strength Mortar under Temperature History by Steam Curing)

  • 권희성;최응규;임남기;이영도;정상진
    • 한국건축시공학회지
    • /
    • 제8권4호
    • /
    • pp.115-121
    • /
    • 2008
  • The present study performed low-pressure steam curing with mortar specimens in order to examine the temperature profile and strength development of steam curing in high-strength specimens of 100MPa. In addition, as a basic research to utilize PC products, we examined the effects of curing temperature and time in steam curing cycle on strength development resulting from the hydration of cement within the range of high strength by changing four factors affecting the quality of PC displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature - in various patterns, and analyzed the optimal strength development characteristic based on the relation between temperature profile and strength development. With regard to the high-temperature curing characteristic of PC, we performed an experiment on the strength characteristic according to the temperature profile of high-strength mortar, and from the results of the experiment according to curing characteristic, displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature, we drew conclusions as follows.

물이 아닌 액체의 종류 변화에 따른 공강도 모르터의 특성분석 (Investigation of the High Strength Mortar in accordance with various Non-water based liquid types)

  • 한동엽;박병관;백대현;송용원;김태완;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2007년도 추계 학술논문 발표대회
    • /
    • pp.61-64
    • /
    • 2007
  • This study progressed fresh mortar test and hardening mortar test as a characteristic analysis of high strength mortar that is not water but replaced liquid, and the results are summarized as following. As a characteristic of fresh mortar, the flow that is following by the changes of the kind of replaced liquid decreased in order of E, M, A, K, O, L, G, and H, and it is indicated that liquid except H, the flow was better then others. The test show the bending strength of G, L, K, O at and H were more increased then plain as the replaced liquid change on the first day, and on the 28th day, G, L, and K was more increased then plain. The compressive strength of G, K, and O was similar with P(-10) at the first day. On 7th day, the test show G, and L was more increased then P(-10), and other replaced liquid were similar or decreased. On the 28th day, G, K, and A was similar with P(-10) and it is decreased in order of E, L, O, and H.

  • PDF

폴리머 혼입률에 따른 고강도 자기 수평 모르타르의 역학적 성능에 대한 실험적 연구 (An Experimental study on the Mechanical Performance of High-Strength Self-Leveling Mortar according to Polymer Mixing Ratio)

  • 정민구;조인성;김인수;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 가을 학술논문 발표대회
    • /
    • pp.21-22
    • /
    • 2020
  • This study is about high strength self-leveling mortar according to the mixing ratio of polymer. The self-leveling mortar currently released in Korea maintains a compressive strength of 40 Mpa as of 28 days. In addition, the level of bonding strength and flexural strength are kept the same. However, through this study, it is confirmed how the self-leveling mortar with a compressive strength of 60Mpa as of the 28th is shown according to the amount of polymer mixed. Experimental factors were configured according to the amount of polymer mixed, and the types of experiments were to confirm compressive strength, flexural strength, adhesion strength and flow. In addition, by confirming the early strength, a study was conducted to improve the quick workability compared to the self-horizontal mortar in the market.

  • PDF