• Title/Summary/Keyword: recycled aggregate concrete (RCA)

Search Result 67, Processing Time 0.021 seconds

Mechanical Properties and Predictions of Strength of Concrete Containing Recycled Coarse Aggregates (순환굵은골재를 포함하는 콘크리트의 역학적 특성 및 강도 예측)

  • Yang, In-Hwan;Kim, Kyoung-Chul
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.2
    • /
    • pp.49-59
    • /
    • 2016
  • According to KS and Standard Specifications for Concrete, the compressive strength of concrete containing recycled aggregate is limited to 27 MPa and thereafter there are little research on concrete containing recycled aggregate of its compressive strength of greater than 27 MPa. Therefore, to expand the applicability of concrete recycled coarse aggregate(RCA), this paper concerns the mechanical properties of concrete containing RCA with compressive strength ranging from 30 to 60 MPa. The experimental parameters were water-cement ratio and replacement ratio of RCA. Water-cement ratio(w/c) was 0.36, 0.46 and 0.53, and replacement ratio of RCA was 30, 50, 70 and 100%. The experimental results were discussed about compressive strength, elastic modulus, split tensile strength and modulus of rupture. Test results of elastic modulus were compared to the design code predictions. Experimental elastic modulus for concrete with w/c=0.53 decreased by greater than 10% compared with that for concrete with w/c=0.36. The design code predictions for elastic modulus overestimated the experimental results. Whereas, the design code predictions for modulus of rupture underestimated the measured values.

Behavior of self-compacting recycled concrete filled aluminum tubular columns under concentric compressive load

  • Yasin Onuralp Ozkilic;Emrah Madenci;Walid Mansour;I.A. Sharaky;Sabry Fayed
    • Steel and Composite Structures
    • /
    • v.51 no.3
    • /
    • pp.243-260
    • /
    • 2024
  • Thirteen self-compacting recycled concrete filled aluminium tubular (SCRCFAT) columns were tested under concentric compression loads. The effects of the replacement ratio of the recycled concrete aggregate (RCA) and steel fibre (SF) reinforcement on the structural performance of the SCRCFAT columns were studied. A control specimen (C000) was cast with normal concrete without SF to be reference for comparison. Twelve columns were cast using RCA, six columns were cast using concrete incorporating 2% SF while the rest of columns were cast without SF. Failure mode, ductility, ultimate load capacity, axial deformation, ultimate strains, stress-strain response, and stiffness of the SCRCFAT columns were studied. The results showed that, the peak load of tested SCRCFAT columns incorporating 5-100 % RCA without SF reduced by 2.33-11.28 % compared to that of C000. Conversely, the peak load of tested SCRCFAT columns incorporating 5-100% RCA in addition to 2% SF increased by 21.1-40.25%, compared to C000. Consequently, the ultimate axial deformation (Δ) of column C100 (RCA=100% and SF 0%) increased by about 118.9 % compared to C000. The addition of 2% SF to the concrete mix decreased the axial deformation of SCRCFAT columns compared to those cast with 0% SF. Moreover, the stiffness of the columns cast without SF decreased as the RCA % increased. In contrast, the columns stiffness cast with 2% SF increased by 26.28-89.7 % over that of C000. Finally, a theoretical model was proposed to predict the ultimate loads tested SCRCFAT columns and the obtained theoretical results agreed well with the experimental results.

The Bond Characteristics of Deformed Bars in Recycled Coarse Aggregates Concrete (RCAC) (순환골재 콘크리트와 이형철근의 부착 특성)

  • Jeon, Su-Man;Yun, Hyun-Do;Choi, Ki-Sun;You, Young-Chan;Kim, Keung-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.2
    • /
    • pp.165-173
    • /
    • 2008
  • One of the most important requirements for reinforced concrete constructions is the bond behavior between concrete and reinforcement. For practical application, it is very important to study bond behavior of reinforcing bars in recycled aggregate concrete (RAC). Thirty six pull-out tests were carried out in order to investigate the bond behaviour between recycled coarse aggregate concrete (RCAC) and deformed bars. RCA replacement ratios (i.e., 0%, 30%, 60% and 100%) and positions of deformed bar (i.e., vertical and horizontal position) were considered as variables in this paper. Each specimen was in the form of a cube, with edges of 150 mm in length and for the pull-out tests, a deformed bar, 13 mm in diameter, was embedded in the center of each specimen. Based on the test results, the bond strength between the RCAC and deformed bars were influenced by both RCA replacement ratios and positions of deformed bars. It was found that under the equivalent mix proportion (i.e., the mix proportions are the same, except for different RCA replacement ratios), the bond strength between the RCAC and the ribbed bar has no obvious relation with the RCA replacement ratio, whereas the positions of deformed bars have a significant effect on the bond behavior between the RCAC and deformed bars. Under the condition of same RCA replacement ratio, the specimen of horizontal reinforcement at upper position (HU type) appear considerably low bond stress.

Behaviour of recycled aggregate concrete beam-column connections in presence of PET fibers at the joint region

  • Marthong, Comingstarful
    • Computers and Concrete
    • /
    • v.21 no.6
    • /
    • pp.669-679
    • /
    • 2018
  • In this paper the behavior of reinforced concrete (RC) beam-column connections under cyclic loading was analyzed. The specimens, manufactured in a reduced-scale were made of (a) recycled aggregate concrete (RAC) by replacing 30% of natural coarse aggregate (NCA) with recycled coarse aggregate (RCA) and (b) RAC incorporating Polyethylene terephthalate (PET) fiber i.e., PET fiber-reinforced concrete (PFRC) at the joint region. PET fiber (aspect ratio=25) of 0.5% by weight of concrete used in the PFRC mix was obtained by hand cutting of post-consumer PET bottles. A reference specimen was also prepared using 100% of NCA and subjected to similar loading sequence. Comparing the results the structural behavior under cyclic loading of RAC specimens are quite similar to the reference specimens. Damage tolerance, load resisting capacity, stiffness degradation, ductility, and energy dissipation of the RAC specimens enhanced due to addition of PET fibers at the joint region. PFRC specimens also presented a lower damage indices and higher principal tensile stresses as compared to the RAC specimens. The results obtained gave experimental evidence on the feasibility of RAC for structural use. Using PET fibers as a discrete reinforcement is recommended for improving the seismic performance of RAC specimens.

Carbonation Properties of Recycled Aggregate Concrete by Specified Concrete Strength (설계기준 강도별 순환골재 콘크리트의 탄산화 특성)

  • Lee, Jun;Lee, Bong-Chun;Cho, Young-Keun;Park, Kwang-Min;Jung, Sang-Hwa
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.1
    • /
    • pp.85-93
    • /
    • 2017
  • This paper presents mechanical properties and carbonation behavior of the recycled aggregate concretes(RAC) in which natural aggregate was replaced by recycled coarse aggregate and fine aggregate by specified concrete strength levels(21, 35, 50MPa). A total of 18 RAC were produced and classified into six series, each of which included three mixes designed with three specified concrete strength levels of 21MPa, 35MPa and 50MPa and three recycled aggregate replacement ratios of 0, 50 and 100%. Physical and mechanical properties of RAC were tested for slump test, compressive strength, and carbonation depth. The test results indicated that the slump of RAC could be improved or same by recycled coarse aggregate replacement ratios, when compared with natural aggregate. But slump of RAC was decreased as the recycled fine aggregate replacement ratios increase. Also, the test results showed that the compressive strength was decreased as the recycled aggregate replacement ratios increased and it had a conspicuous tendency to decrease when the content of the recycled aggregate exceeded 50%. Furthermore, the result indicated that the measured carbonation depth increases by 40% with the increase of the recycled aggregate replacement. In the case of the concrete having low level compressive strength, the increase of carbonation depth tends to be higher when using the RCA. However, the trend of carbonation resistivity in high level compressive strength concrete is similar to that obtained in natural aggregate concrete. Therefore, an advance on the admixture application and mix ratio control are required to improve the carbonation resistivity when using the recycled aggregate in large scale.

On Probability Distribution of Chloride Diffusion Coefficient for Recycled Aggregate Concrete

  • Ying, Jingwei;Xiao, Jianzhuang;Meng, Qiujiang
    • International Journal of Concrete Structures and Materials
    • /
    • v.10 no.1
    • /
    • pp.61-73
    • /
    • 2016
  • In predicating the probability distribution of chloride diffusion coefficient of recycled aggregate concrete ($D_{RAC}$), the morphological characteristics of three phases, i.e., the old attached mortar, the natural aggregate and the new mortar, should all be taken into account. The present paper attempts to develop a probability density evolution method (PDEM) to achieve this. After verifying the derived PDEM results with experimental results, the effects of old attached mortar to the $D_{RAC}$ are examined in a quantitative manner. It is found that (1) the variation of the attached mortar content is much sensitive to $D_{RAC}$; (2) given the probability distribution of the content and chloride diffusion coefficient of old mortar, the probability distribution of DRAC can be analysed based on the PDEM; and (3) the critical chloride diffusion coefficient at a certain assurance rate can be obtained by the PDEM. The analysis results of this investigation will be valuable to the durability design for RAC.

Effect of Replacement of 5~13mm Recycled Coarse Aggregates on Field Applicability of the Concrete through Mock-up Test (목업 시험을 통한 5~13mm 순환 굵은골재 치환 사용이 콘크리트의 현장적용성에 미치는 영향 고찰)

  • Han, Min-Cheol;Song, Young-Woo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.1
    • /
    • pp.59-67
    • /
    • 2017
  • The objective of this paper is to investigate experimentally the effect of replacement of recycled coarse aggregates with 5~13mm in size on a field applicability of concretes through Mock-up test. Seven different mock-up specimens were prepared with the size of $1200{\times}800{\times}800mm$ simulating column and wall. For the concrete mixtures, 24MPa, 27MPa and 40MPa of nominal strength were adopted with 30% and 70%(only for 24MPa) of 5~13mm recycled coarse aggregate (RCA) replacement and without 5~13mm RCA(Plain). For test items, slump, slump flow, compressive strength with different curing conditions, core drilling, rebound numbers and drying shrinkage were measured. Test results indicated that 30% of 5~13 mm RCA replacement resulted in increase in slump, slump flow and resistance against segregation, while air contents decreased compared to those of plain mixture. Compressive strength of concrete with 30% of 5~13mm RCA was shown to be higher than that of plain mixture due to optimum packing effect associated with presence of well graded aggregates. Rebound number of the mock-up specimen with 30% of 5~13mm RCA had lower fluctuation according to hitting location than that of plain mock-up specimen. It is believed from the results of the study that replacement of 30% of 5~13mm RCA brings desirable improvement in various aspect of concrete performance due to associated dense packing effect.

Mechanical behaviour of composite columns composed of RAC-filled square steel tube and profile steel under eccentric compression loads

  • Ma, Hui;Xi, Jiacheng;Zhao, Yaoli;Dong, Jikun
    • Steel and Composite Structures
    • /
    • v.38 no.1
    • /
    • pp.103-120
    • /
    • 2021
  • This research examines the eccentric compression performance of composite columns composed of recycled aggregate concrete (RAC)-filled square steel tube and profile steel. A total of 17 specimens on the composite columns with different recycled coarse aggregate (RCA) replacement percentage, RAC strength, width to thickness ratio of square steel tube, profile steel ratio, eccentricity and slenderness ratio were subjected to eccentric compression tests. The failure process and characteristic of specimens under eccentric compression loading were observed in detail. The load-lateral deflection curves, load-train curves and strain distribution on the cross section of the composite columns were also obtained and described on the basis of test data. Results corroborate that the failure characteristics and modes of the specimens with different design parameters were basically similar under eccentric compression loads. The compression side of square steel tube yields first, followed by the compression side of profile steel. Finally, the RAC in the columns was crushed and the apparent local bulging of square steel tube was also observed, which meant that the composite column was damaged and failed. The composite columns under eccentric compression loading suffered from typical bending failure. Moreover, the eccentric bearing capacity and deformation of the specimens decreased as the RCA replacement percentage and width to thickness ratio of square steel tube increased, respectively. Slenderness ratio and eccentricity had a significantly adverse effect on the eccentric compression performance of composite columns. But overall, the composite columns generally had high-bearing capacity and good deformation. Meanwhile, the mechanism of the composite columns under eccentric compression loads was also analysed in detail, and the calculation formulas on the eccentric compression capacity of composite columns were proposed via the limit equilibrium analysis method. The calculation results of the eccentric compression capacity of columns are consistent with the test results, which verify the validity of the formulas, and the conclusions can serve as references for the engineering application of this kind of composite columns.

Compressive performance of RAC filled GFRP tube-profile steel composite columns under axial loads

  • Ma, Hui;Bai, Hengyu;Zhao, Yanli;Liu, Yunhe;Zhang, Peng
    • Advances in concrete construction
    • /
    • v.8 no.4
    • /
    • pp.335-349
    • /
    • 2019
  • To investigate the axial compressive performance of the recycled aggregate concrete (RAC) filled glass fiber reinforced polymer (GFRP) tube and profile steel composite columns, static loading tests were carried out on 18 specimens under axial loads in this study, including 7 RAC filled GFRP tube columns and 11 RAC filled GFRP tube-profile steel composite columns. The design parameters include recycled coarse aggregate (RCA) replacement percentage, profile steel ratio, slenderness ratio and RAC strength. The failure process, failure modes, axial stress-strain curves, strain development and axial bearing capacity of all specimens were mainly analyzed in detail. The experimental results show that the GFRP tube had strong restraint ability to RAC material and the profile steel could improve the axial compressive performance of the columns. The failure modes of the columns can be summarized as follow: the profile steel in the composite columns yielded first, then the internal RAC material was crushed, and finally the fiberglass of the external GFRP tube was seriously torn, resulting in the final failure of columns. The axial bearing capacity of the columns decreased with the increase of RCA replacement percentage and the maximum decreasing amplitude was 11.10%. In addition, the slenderness ratio had an adverse effect on the axial bearing capacity of the columns. However, the strength of the RAC material could effectively improve the axial bearing capacity of the columns, but their deformability decreased. In addition, the increasing profile steel ratio contributed to the axial compressive capacity of the composite columns. Based on the above analysis, a formula for calculating the bearing capacity of composite columns under axial compression load is proposed, and the adverse effects of slenderness ratio and RCA replacement percentage are considered.

Analysis of axial compression performance of BFRRAC-filled square steel tubular column

  • Xianggang Zhang;Jixiang Niu;Wenlong Shen;Dapeng Deng;Yajun Huang
    • Steel and Composite Structures
    • /
    • v.49 no.4
    • /
    • pp.457-471
    • /
    • 2023
  • To make up for the performance weaknesses of recycled aggregate concrete (RAC), expand the application range of RAC, and alleviate the environmental problems caused by excessive exploitation of natural coarse aggregates (NCA), this study proposes a basalt fiber-reinforced recycled aggregate concrete (BFRRAC)-filled square steel tubular columns that combines two modification methods of steel tube and fiber, which may greatly enhance the mechanical properties of RAC. The axial compression performance for BFRRAC-filled square steel tubular columns was reported during this study. Seven specimens with different replacement ratios of recycled coarse aggregate (RCA), length-diameter ratios, along with basalt fiber (BF) contents were designed as well as fabricated for performing axial compression test. For each specimen, the whole failure process as well as mode of specimen were discovered, subsequently the load-axial displacement curve has obtained, after which the mechanical properties was explained. A finite element analysis model for specimens under axial compression was then established. Subsequently, based on this model, the factors affecting axial compression performance for BFRRAC-filled square steel tubes were extended and analyzed, after which the corresponding design suggestion was proposed. The results show that in the columns with length-diameter ratios of 5 and 8, bulging failure was presented, and the RAC was severely crushed at the bulging area of the specimen. The replacement ratio of RCA as well as BF content little affected specimen's peak load (less than 5%). As the content of BF enhanced from 0 kg/m3 to 4 kg/m3, the dissipation factor and ductility coefficients increased by 10.2% and 5.6%, respectively, with a wide range.