• 제목/요약/키워드: powder metallurgy process

검색결과 1,207건 처리시간 0.038초

선택적 레이저 조형된 AlSi10Mg합금의 후열처리에 따른 Si-rich상 형상변화가 기계적 특성에 미치는 영향 (Influence of Si-rich Phase Morphologies on Mechanical Properties of AlSi10Mg Alloys processed by Selective Laser Melting and Post-Heat Treatment)

  • 남정우;엄영성;김경태;손인준
    • 한국분말재료학회지
    • /
    • 제28권2호
    • /
    • pp.134-142
    • /
    • 2021
  • In this study, AlSi10Mg powders with average diameters of 44 ㎛ are additively manufactured into bulk samples using a selective laser melting (SLM) process. Post-heat treatment to reduce residual stress in the as-synthesized sample is performed at different temperatures. From the results of a tensile test, as the heat-treatment temperature increases from 270 to 320℃, strength decreases while elongation significantly increases up to 13% at 320℃. The microstructures and tensile properties of the two heat-treated samples at 290 and 320℃, respectively, are characterized and compared to those of the as-synthesized samples. Interestingly, the Si-rich phases that network in the as-synthesized state are discontinuously separated, and the size of the particle-shaped Si phases becomes large and spherical as the heat-treatment temperature increases. Due to these morphological changes of Si-rich phases, the reduction in tensile strengths and increase in elongations, respectively, can be obtained by the post-heat treatment process. These results provide fundamental information for the practical applications of AlSi10Mg parts fabricated by SLM.

Atmospheric plasma spray 공정으로 제조된 Y2O3 코팅층의 미세조직 및 기계적 특성에 미치는 분사 각도의 영향 (Effect of Spray Angle the on Microstructure and Mechanical Properties of Y2O3 Coating Layer Manufactured by Atmospheric Plasma Spray Process)

  • 황유진;김경욱;이호영;권식철;이기안
    • 한국분말재료학회지
    • /
    • 제28권4호
    • /
    • pp.310-316
    • /
    • 2021
  • The effects of different spray angles (90°, 85°, 80°) on the microstructure and mechanical properties of a Y2O3 coating layer prepared using the atmospheric plasma spray (APS) process were studied. The powders employed in this study had a spherical shape and included a cubic Y2O3 phase. The APS coating layer exhibited the same phase as the powders. Thickness values of the coating layers were 90°: 203.7 ± 8.5 ㎛, 85°: 196.4 ± 9.6 ㎛, and 80°: 208.8 ± 10.2 ㎛, and it was confirmed that the effect of the spray angle on the thickness was insignificant. The porosities were measured as 90°: 3.9 ± 0.85%, 85°: 11.4 ± 2.3%, and 80°: 12.7 ± 0.5%, and the surface roughness values were 90°: 5.9 ± 0.3 ㎛, 85°: 8.5 ± 1.1 ㎛, and 80°: 8.5 ± 0.4 ㎛. As the spray angle decreased, the porosity increased, but the surface roughness did not show a significant difference. Vickers hardness measurements revealed values of 90°: 369.2 ± 22.3, 85°: 315.8 ± 31.4, and 80°: 267.1 ± 45.1 HV. It was found that under the condition of a 90° angle with the lowest porosity exhibited the best hardness value. Based on the aforementioned results, an improved method for the APS Y2O3 coating layer was also discussed.

Direct energy deposition 공정을 이용한 Fe-Mn-Al-C계 저망간 경량철강 제조 (Manufacturing of Fe-Mn-Al-C Based Low Mn Lightweight Steel Via Direct Energy Deposition)

  • 고광규;손한솔;정차희;배효주;박은혜;김정기;최현주;설재복
    • 한국분말재료학회지
    • /
    • 제29권4호
    • /
    • pp.320-324
    • /
    • 2022
  • Lightweight steel is a crucial material that is being actively studied because of increased carbon emissions, tightening regulations regarding fuel efficiency, and the emergence of UAM, all of which have been recently labeled as global issues. Hence, new strategies concerning the thickness and size reduction of steel are required. In this study, we manufacture lightweight steel of the Fe-Mn-Al-C system, which has been recently studied using the DED process. By using 2.8 wt.% low-Mn lightweight steel, we attempt to solve the challenge of joining steel parts with a large amount of Mn. Among the various process variables, the laser scan power is set at 600 and 800 W, and the laser scan speed is fixed at 16.67 mm/s before the experiments. Several pores and cracks are observed under both conditions, and negligibly small pores of approximately 0.5 ㎛ are observed.

카본 코팅된 니켈-코발트 황화물의 요크쉘 입자 제조 및 소듐 이온 배터리의 음극 소재 적용 (Synthesis of Carbon Coated Nickel Cobalt Sulfide Yolk-shell Microsphere and Their Application as Anode Materials for Sodium Ion Batteries )

  • 서효영;박기대
    • 한국분말재료학회지
    • /
    • 제30권5호
    • /
    • pp.387-393
    • /
    • 2023
  • Transition metal chalcogenides are promising cathode materials for next-generation battery systems, particularly sodium-ion batteries. Ni3Co6S8-pitch-derived carbon composite microspheres with a yolk-shell structure (Ni3Co6S8@C-YS) were synthesized through a three-step process: spray pyrolysis, pitch coating, and post-heat treatment process. Ni3Co6S8@C-YS exhibited an impressive reversible capacity of 525.2 mA h g-1 at a current density of 0.5 A g-1 over 50 cycles when employed as an anode material for sodium-ion batteries. However, Ni3Co6S8 yolk shell nanopowder (Ni3Co6S8-YS) without pitch-derived carbon demonstrated a continuous decrease in capacity during charging and discharging. The superior sodium-ion storage properties of Ni3Co6S8@C-YS were attributed to the pitch-derived carbon, which effectively adjusted the size and distribution of nanocrystals. The carbon-coated yolk-shell microspheres proposed here hold potential for various metal chalcogenide compounds and can be applied to various fields, including the energy storage field.

가압소결로 제조된 YSZ-30 vol.% WC 복합체 세라믹스의 상형성 거동과 기계적 특성 (Phase Formation and Mechanical Property of YSZ-30 vol.% WC Composite Ceramics Fabricated by Hot Pressing)

  • 김진권;최재형;남산;류성수;김성원
    • 한국분말재료학회지
    • /
    • 제30권5호
    • /
    • pp.409-414
    • /
    • 2023
  • YSZ (Y2O3-stabilized zirconia)-based ceramics have excellent mechanical properties, such as high strength and wear resistance. In the application, YSZ is utilized in the bead mill, a fine-grinding process. YSZ-based parts, such as the rotor and pin, can be easily damaged by continuous application with high rpm in the bead mill process. In that case, adding WC particles improves the tribological and mechanical properties. YSZ-30 vol.% WC composite ceramics are manufactured via hot pressing under different pressures (10/30/60 MPa). The hot-pressed composite ceramics measure the physical properties, such as porosity and bulk density values. In addition, the phase formation of these composite ceramics is analyzed and discussed with those of physical properties. For the increased applied pressure of hot pressing, the tetragonality of YSZ and the crystallinity of WC are enhanced. The mechanical properties indicate an improved tendency with the increase in the applied pressure of hot pressing.

에너지 밀도 및 분말 증착 밀도를 고려한 직접 에너지 증착법 기반 Ti-6Al-4V 합금의 적층공정 최적화 (Additive Manufacturing Optimization of Directed Energy Deposition-Processed Ti-6Al-4V Alloy using Energy Density and Powder Deposition Density)

  • 이유경;김은성;천세호;설재복;성효경;오정석;김형섭;이태경;남태현;김정기
    • 한국분말재료학회지
    • /
    • 제28권6호
    • /
    • pp.491-496
    • /
    • 2021
  • The process optimization of directed energy deposition (DED) has become imperative in the manufacture of reliable products. However, an energy-density-based approach without a sufficient powder feed rate hinders the attainment of an appropriate processing window for DED-processed materials. Optimizing the processing of DED-processed Ti-6Al- 4V alloys using energy per unit area (Eeff) and powder deposition density (PDDeff) as parameters helps overcome this problem in the present work. The experimental results show a lack of fusion, complete melting, and overmelting regions, which can be differentiated using energy per unit mass as a measure. Moreover, the optimized processing window (Eeff = 44~47 J/mm2 and PDDeff = 0.002~0.0025 g/mm2) is located within the complete melting region. This result shows that the Eeff and PDDeff-based processing optimization methodology is effective for estimating the properties of DED-processed materials.

소결분위기 제어에 의한 Al2O3/Fe-Ni 나노복합재료의 제조 및 특성 (Fabrication of Al2O3/Fe-Ni Nanocomposites by Atmosphere-controlled Sintering and their Properties)

  • 이홍재;정영근;오승탁;이재성
    • 한국세라믹학회지
    • /
    • 제39권2호
    • /
    • pp.199-203
    • /
    • 2002
  • 소결 분위기가 금속입자분산 세라믹스기 복합체의 미세 조직 및 물성에 미치는 영향에 대하여 조사하고자 화학적 방법으로 합성한 $Al_2O_3$/Fe-Ni 나노복합분말을 수소 및 아르곤 가스 분위기, 또한 소결온도 등으로 제어하여 열간가압 소결하였다. 수소분위기에서 소결한 복합체는 아르곤분위기의 경우보다 반응상 $FeAl_2O_4$의 형성이 억제되었으며, 증가된 파괴강도 및 인성 값을 나타내었다. 또한, 소결 온도를 낮추었을 경우 기지상 및 금속 분산상의 미세화와 향상된 기계적 성질을 얻을 수 있었다. 소결 조건에 따른 기계적 특성의 변화는 주로 반응상의 형성과 관련된 미세조직 특성에 의존하는 것으로 해석하였다.

급속응고된 N-type $Bi_2Te_{2.75}Se_{0.15}$ 열전재료의 미세조직과 열전특성에 미치는 압출비의 영향 (The Influence of Extrusion Ratio on Microstructure and Thermoelectric Properties of Rapidly Solidified N-type $Bi_2Te_{2.75}Se_{0.15}$)

  • 이상일;홍순직;손현택;천병선;이윤석
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2001년도 추계학술강연 및 발표대회
    • /
    • pp.30-30
    • /
    • 2001
  • $Bi_2Te_3$계 열전재료는 200~400K 정도의 저온에서 네어지 변환효율이 가장 높은 재료로써 열전냉각, 바런재로 등에 응요하기 위하여ㅠ 제조법 및 특서에 관한 많은 연구가 진행되어 왔다. $Bi_2Te_3$계 화합물은 rhombohedral의 결정 구조를 가지는 층상 화 ;물로 결정대칭성으로 인해 연전기적으로 큰 이방성을 나타낸다. 현재는 일반향용고법에 의해서 입자를 a축 방향으로 성장시켜 큰 결정립을 가진 다결정재료를 사용하고 있으나, c면이 매우 취약하기 때문에 가공서이 나쁘다. 따라서 이와같은 단점을 개선하기 위하여 기계적 강도를 높일 수 있는 가공공정 및 합금설계에 대한 연구가 활발히 진행되고 있다. 측히 열간 압출법으로 제조된 열전재료는 결정립의 미세화와 높은 이방성으로 성능지수와 기계적 강도를 향상시킬 수 있다는 연구결과가 보고되고 있다 또한 Schultz드의 연구결과에 의하면 $Bi_2Te_3$ 계 열전재료는 소성변형에 의하여 발생한 점결함에 의하여 캐리어 농도가 변화되며 이로 인하여 재료의 전기적 성질이 결정된다고 하였다. 따라서 상당히 큰 소성가공량과 열전측성과의 관계를 규명하는 것은 매우 중요하다. 이에 본 연구에서는 압출변수 중 소성가공량에 중요한 변수로 작요아는 압출비를 변화시켜 최적의 열간 소성가공량을 검토하고, 이에 따른 열전측성과 압출비와의 상관관계에 대하여 연구하는 것을 목적으로 하였다. 연구에 사용된 N형의 조성은$Bi_2Te_{2.75}Se_{0.15}$로서 순도 99.99를 사용하였고, dopant로 0.1wt%의 $SbI_3$를 사용하였다. $Bi_2Te_{2.75}Se_{0.15}$ 분말은 가스분사법(Gas atomization Process)를 이용하여, 용탕제조시 아르곤가스로 산화를 방지하였고, 냉매로는 질소가스를 이용하였다. 제조된 분말을 기ㅖ적 분급법을 이용하여 분급하였고, 냉매로는 질소가스를 이용하였다. 제조된 분말을 기계적 분급ㅂ법을 이용하여 분급하였고, 압출에 이용된 분말은 250$\mu\textrm{m}$이하의 크기를 사용하였다. 또한 분말제조과정 중 형성되는 표면산화층을 제거하기 위하여 36$0^{\circ}C$에서 4시간동안 수소 환원처리를 행하였다. 제조된 분말은 열간 압출을 위하여 Aㅣcan에 넣고 냉간성형체를 만들고, 진공처리를 한 후 밀봉하여 탈가스처리를 하였다. 압출다이는 압출비가 각각 28:1과 16:1인 평다이(9$0^{\circ}C$)를 사용하여 각각 내경이 9, 12cm이고, 길이가 50, 30cm인 압출재를 제조하였다. 열간압출한 후의 미세조직을 광학현미경으로 압출방향에 평행한 방향과 수직방향으로 관찰하였고, 열간 압출재 이방성을 검토하기 위하여 X선 회절분석을 실실하여 결정방위를 확인하였다. 전기 비저항 및 Seebeck 계수 측정을 위하여 각각 2$\times$2$\times$10$mm^3$ 그리고 5$\times$5$\times$10$mm^3$ 크기의 시편을 준비하였다.준비하였다.

  • PDF

서스펜션 플라즈마 스프레이 코팅법으로 제조된 Ytterbium Silicate 환경차폐코팅의 상형성 및 구조에 미치는 증착인자 및 원료혼합 공정의 영향 (Effect of Deposition Parameter and Mixing Process of Raw Materials on the Phase and Structure of Ytterbium Silicate Environmental Barrier Coatings by Suspension Plasma Spray Method)

  • 류호림;최선아;이성민;한윤수;최균;남산;오윤석
    • 한국분말재료학회지
    • /
    • 제24권6호
    • /
    • pp.437-443
    • /
    • 2017
  • SiC-based composite materials with light weight, high durability, and high-temperature stability have been actively studied for use in aerospace and defense applications. Moreover, environmental barrier coating (EBC) technologies using oxide-based ceramic materials have been studied to prevent chemical deterioration at a high temperature of $1300^{\circ}C$ or higher. In this study, an ytterbium silicate material, which has recently been actively studied as an environmental barrier coating because of its high-temperature chemical stability, is fabricated on a sintered SiC substrate. $Yb_2O_3$ and $SiO_2$ are used as the raw starting materials to form ytterbium disilicate ($Yb_2Si_2O_7$). Suspension plasma spraying is applied as the coating method. The effect of the mixing method on the particle size and distribution, which affect the coating formation behavior, is investigated using a scanning electron microscope (SEM), an energy dispersive spectrometer (EDS), and X-ray diffraction (XRD) analysis. It is found that the originally designed compounds are not effectively formed because of the refinement and vaporization of the raw material particles, i.e., $SiO_2$, and the formation of a porous coating structure. By changing the coating parameters such as the deposition distance, it is found that a denser coating structure can be formed at a closer deposition distance.

기계적 합금화 공정으로 제조된 Fe-14Cr Ferritic 산화물 분산 강화(ODS) 합금 강의 고온 산화 거동 (High Temperature Oxidation Behavior of Fe-14Cr Ferritic Oxide Dispersion Strengthened Steels Manufactured by Mechanical Alloying Process)

  • 김영균;박종관;김휘준;공만식;이기안
    • 한국분말재료학회지
    • /
    • 제24권2호
    • /
    • pp.133-140
    • /
    • 2017
  • This study investigates the oxidation properties of Fe-14Cr ferritic oxide-dispersion-strengthened (ODS) steel at various high temperatures (900, 1000, and $1100^{\circ}C$ for 24 h). The initial microstructure shows that no clear structural change occurs even under high-temperature heat treatment, and the average measured grain size is 0.4 and $1.1{\mu}m$ for the as-fabricated and heat-treated specimens, respectively. Y-Ti-O nanoclusters 10-50 nm in size are observed. High-temperature oxidation results show that the weight increases by 0.27 and $0.29mg/cm^2$ for the as-fabricated and heat-treated ($900^{\circ}C$) specimens, and by 0.47 and $0.50mg/cm^2$ for the as-fabricated and heat-treated ($1000^{\circ}C$) specimens, respectively. Further, after 24 h oxidation tests, the weight increases by 56.50 and $100.60mg/cm^2$ for the as-fabricated and heat-treated ($1100^{\circ}C$) specimens, respectively; the latter increase is approximately 100 times higher than that at $1000^{\circ}C$. Observation of the surface after the oxidation test shows that $Cr_2O_3$ is the main oxide on a specimen tested at $1000^{\circ}C$, whereas $Fe_2O_3$ and $Fe_3O_4$ phases also form on a specimen tested at $1100^{\circ}C$, where the weight increases rapidly. The high-temperature oxidation behavior of Fe-14Cr ODS steel is confirmed to be dominated by changes in the $Cr_2O_3$ layer and generation of Fe-based oxides through evaporation.