  • This article investigated to polymer-clay nanocomposite, especially in interfacial respect clay structure, its dispersion into polymer matrix, and clay modification is studied. The cationic exchange of surfactants with clay gallery results in preparing organo-clay capable of compatiblizing to monomer or polymer and increasing interlayer adhesion energy due to expansion of interlayer spacing. The orientation of surfactant in clay gallery is affected by chemical structure and charge density of clay, and interlayer spacing and volume is increased with alkyl chain length of surfactant, or charge density of clay. Also, the interaction between clay and polymer in preparing polymer-clay nanocomposite is explained thermodynamically. In the future, the study and development of polymer-clay nanocomposite is paid attention to the interfacial adhesion, clay dispersion within polymer, mechanism of clay intercalation or exfoliation.

유기화제 구조가 열가소성 나노복합체의 제조에 미치는 영향 (Effects of Organosilicate Structure on Melt Intercalation of Thermoplastic Polymers)

  • 어태식;김성수;송기국;김준경
    • 폴리머
    • /
    • 제24권6호
    • /
    • pp.794-801
    • /
    • 2000
  • Static 용융 삽입에 의하여 열가소성 고분자의 나노복합체를 제조할 때 유기화 점토에 치환된 유기화제의 길이와 packing 밀도, 그리고 열처리 온도와 시간 등이 고분자의 점토 층간 삽입에 미치는 영향에 대하여 x-ray와 FTIR spectroscopy를 이용하여 조사하였다. 초기 유기화제의 배열형태가 lateral monolayer일 때는 고분자들의 용융 삽입이 일어나지 않았으며 그 외의 경우 유기화제의 종류 및 구조 등에 따라 최종 점토 층간 간격은 큰 변화를 보이지 않았다. 열처리 시간에 따라서 층간 간격은 증가하며 더욱 규칙적으로 변하는 것을 알 수 있었고, 온도가 증가함에 따라서는 점토 층간 간격은 증가하지만 불규칙적으로 배열이 되어가는 것을 관찰하였다.

  • PDF

Controlling interlayer spacing of GO membranes via the insertion of GN for high separation performance

  • Xuan Liu;Zhu Zhou;Hengzhang Dai;Kuang Ma;Yafei Zhang;Bin Li
    • Membrane and Water Treatment
    • /
    • 제14권3호
    • /
    • pp.107-114
    • /
    • 2023
  • Graphene oxide (GO) membranes have attracted extensive attention in water treatment and related fields. However, GO films are unstable and have low permeability, which have hindered their further development. In this paper, a simple and effective method was used in which GO and single-layer graphene (GN) were mixed, and the layer spacing was effectively controlled by accurately controlling the ratio of GO to GN. GO-GN composite membranes have excellent stability, salt rejection (95.4%), and water flux (26 L m-2 h-1 bar-1). This unique design structure can be used for precise and effective regulation of the layer spacing in GO, improving the rejection rate, and increasing water flux via the enhancement of low-friction capillary action. The rational development and use of this unique composite membrane provides a reference for the water treatment field.

Magadiite 주형을 이용한 층상 카본의 합성 (Preparation of Porous Layered Carbon Using Magadiite Template)

  • 최석현;정순용;오성근;권오윤
    • 공업화학
    • /
    • 제16권3호
    • /
    • pp.408-412
    • /
    • 2005
  • Magadiite 주형에 pyrolized fuel oil (PFO)를 층간 삽입, 열처리하여 층간에 탄소 박막을 형성하고 magadiite 주형을 제거함으로서 다공성 층상탄소를 합성하였다. 층상카본은 주형과 유사한 판상 구조이며, d-spacing은 ~0.7 nm로서 일정한 값을 보여주었다. 비표면적은 주형의 형태, 혼합비율, 소성시간에 따라 $147{\sim}385m^2/g$ 크게 다른 값을 나타내었다.

층상 실리케이트 주형을 이용한 층상 카본의 합성 (Preparation of Layered Carbon Using Layered Silicate Template)

  • 정은일;정순용;권오윤
    • 공업화학
    • /
    • 제16권1호
    • /
    • pp.68-73
    • /
    • 2005
  • 층상 실리케이트를 주형으로 이용하여 실리케이트의 층간에 pyrolized fuel oil (PFO)를 삽입하고 열분해시킨 후 실리케이트 골격을 용출 제거함으로써 다공성 층상카본을 제조하였다. 층상카본의 입자모양은 층상실리케이트 주형과 유사한 판상 형태이며, d-spacing은 0.78~0.82 nm로 일정한 값을 나타내었다. 실리케이트와 PFO의 혼합비율과 열처리 온도, 열처리 시간에 따른 비표면적은 $30{\sim}576m^2/g$로 크게 다른 값을 나타내었다.

Magnetic Properties and Relaxation of Vanadium Monolayer on Pd(001) Surface

  • Landge, Kalpana K.;Bialek, Beata;Lee, Jae-Il
    • Journal of Magnetics
    • /
    • 제15권2호
    • /
    • pp.45-50
    • /
    • 2010
  • We investigated the magnetism of vanadium monolayers on a Pd(001) surface. The electronic structure and the magnetic properties of the V/Pd(001) system were determined with the use of the full-potential linearized augmented plane-wave method within the general gradient approximation. Three magnetic configurations were studied: non-, ferro-, and antiferromagnetic. From the total energy calculations, we found that the V/Pd(001) system is the most stable in the antiferromagnetic configuration. The importance of relaxation on the magnetic properties of the systems was also studied. It was found that the Pd(001) surface covered with a V monolayer undergoes considerable relaxation in which the spacing between Pd layers increases in all three magnetic configurations. Contrary to the Pd interlayer spacing, the distance between the V overlayer and the topmost Pd layer is reduced. The interlayer spacing between the V overlayer and the Pd surface layer is the largest for the antiferromagnetic configuration. In the relaxed antiferromagnetic structure, the magnitude of the calculated magnetic moments on the V atoms was $1.31\;{\mu}_B$. The presence of the vanadium monolayer does not affect the paramagnetic properties of the Pd(001) surface.

Interlamellar Silylation of Montmorillonite with 3-Aminopropyltriethoxysilane

  • Park, Kyeong-Won;Kwon, Oh-Yun
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권7호
    • /
    • pp.965-968
    • /
    • 2004
  • H-montmorillonite was modified by interlayer surface silylation using 3-aminopropyltriethoxysilane and dodecylamine in ethanol without a pre-swelling step. Dodecylamine acts as a gallery expander and silylation catalyst. The evaporation of ethanol from the dispersion yields well-ordered silylated montmorillonites with large basal spacing between 1.50 and 4.20 nm. Solid-state $^29Si$ CP MAS NMR of the silylated samples showed $Q^2\;and\;Q^3$ signals as well as $T^2\;and\;T^3$ signals. The increase in the relative intensity of $Q^3\;for\;Q^2$ and the appearance of $T^2\;and\;T^3$ signals was attributed to the grafting of 3-aminopropyltriethoxysilane to the interlayer surface silanol groups.

Magadiite 주형을 이용한 다공성 흑연제조에 미치는 Co와 Ni 촉매 효과 (Effect of Co and Ni Catalyst on the Preparation of Porous Graphite Using Magadiite Template)

  • 최석현;권오윤
    • 한국재료학회지
    • /
    • 제28권3호
    • /
    • pp.189-194
    • /
    • 2018
  • Porous graphites were synthesized by removing the template in HF after cabothermal conversion for 3 h at $900^{\circ}C$, accompanied by intercalations of pyrolyzed fuel oil (PFO) in the interlayer of Co or Ni loaded magadiite. The X-ray powder diffraction pattern of the porous graphites exhibited 00l reflections corresponding to a basal spacing of 0.7 nm. The particle morphology of the porous graphites was composed of carbon plates intergrown to form spherical nodules resembling rosettes like a magadiite template. TEM shows that the cross section of the porous graphites is composed of layers with very regular spaces. In particular, crystallization of the porous graphite was dependent on the content of Co or Ni loaded in the interlayer. The porous graphite had a surface area of $328-477m^2/g$. This indicates that metals such as Co and Ni act as catalysts that accelerate graphite formation.

엽층리가 발달된 규조토성 규질이암의 강화제에 의한 광물학적 특성변화 (Change in Mineralogical Characteristics of the Laminated Diatomaceous Siliceous Mudstone by the Treatment of Consolidants)

  • 도진영
    • 광물과 암석
    • /
    • 제35권1호
    • /
    • pp.51-64
    • /
    • 2022
  • 포항 금광동층 함식물화석층 암석의 효과적인 보존을 위하여 구성암석의 특징과 보존처리제 적용을 인공풍화시험을 통해 살펴보았다. 화석지 구성암석은 규조토성 규질이암으로 팽윤성 광물인 스멕타이트를 약간 함유하고 있으며, 엽층리가 발달되어 있다. 화석지 암석은 물과 반응 후 팽윤성 광물의 d001 층간간격이 증가하였다. 에틸실리케이트 암석강화제를 적용한 후 시편의 경도는 향상되었으나 팽윤성 광물의 층간간격은 감소하였다. 팽윤저지제를 선처리한 후 강화제를 처리하였을 때 광물 층간간격의 변화는 강화제만을 처리하였을 때와 유사하여 팽윤저지제의 효과는 거의 없었다. 보존약품이 처리된 암석에 수분이 닿았을 경우, 강화제 또는 팽윤저지제를 선처리한 후 강화제를 처리한 암석 모두 엽층리 간격이 확대되었으나, 습기만 접했을 때는 변화가 적었다. 또한 보존처리 후 노천에 그대로 위치하여 풍화를 받게 되면, 약품이 처리되지 않은 암석에 비해 약간 느리게 발생하기는 하지만, 매우 빠른 시간 내에 엽층리면의 분리와 암석의 분말화가 발생하는 결과를 보였다. 화석지 암석의 원활한 보존을 위해서는 보존약품의 처리가 필요하나, 강우를 접하고 동결융해과정을 거치면 그 효과는 매우 빠른 시간에 소멸되기 때문에 약품처리에 상관없이 암석에 직접적인 강우의 접촉을 막는 것이 우선적으로 요구된다.