• Title/Summary/Keyword: ferroelectric devices

Search Result 121, Processing Time 0.024 seconds

The Structural and electrical Properties of $BaTiO_3$ Thin Films Deposited on Si/MgO Substrates (Si/MgO 기판에 증착된 BaTiO$_3$ 박막의 구조 및 전기적 특성)

  • 홍경진;김태성
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.12
    • /
    • pp.1108-1114
    • /
    • 1998
  • $BaTiO_3$ thin films preferred c-axis orientation for the potential application of ferroelectric memory devices were deposited on silicon substrates(100) by RF sputtering and annealed at 800 and 900[$^{\circ}C$] in air. The BT(100)/BT(110) peak ratio of the sputtered sample was decreased with post-annealing in air. According to increasing with annealing temperature and time, the peak ratio of BT(100)/BT(110) was decreased and the surface density of thin film was high. Dielectric characteristics of $BaTiO_3$ thin film was measured as a function of annealing temperature and frequency. The dielectric constants were increased with annealing and decreased with frequency by space charge polarization and dipole polarization below 600[kHz]. The remanent polarization and coercive field in P-E hysteresis loop of $BaTiO_3$thin film were increased with the annealing temperature in air. The remanent polarization and coercive filed annealed at 800[$^{\circ}C$] for 1hr were 1.2[$\mu$C/$cm^2$] and 200[kV/cm]

  • PDF

Fabrications and properties of MFIS capacitor using $LiNbO_3$/AIN structure ($LiNbO_3$/AIN 구조를 이용한 MFIS 커패시터의 제작 및 특성)

  • 이남열;정순원;김용성;김진규;정상현;김광호;유병곤;이원재;유인규
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.743-746
    • /
    • 2000
  • Metal-ferroelectric-insulator-semiconductor(MFIS) devices using Pt/$LiNbO_3$/Si structure were successfully fabricated. The dielectric constant of the AIN film calculated from the capacitance in the accumulation region in the capacitance-voltage(C-V) curve was about 8.2. The gate leakage current density of MIS devices using a aluminum electrode showed the least value of 1$\times$$1O^{-8}$A/$cm^2$ order at the electric field of 500kV/cm. The dielectric constant of $LiNbO_3$film on AIN/Si structure was about 23 derived from 1MHz capacitance-voltage (C-V) measurement and the resistivity of the film at the field of 500kV/cm was about 5.6$\times$ $1O^{13}$ $\Omega$.cm.

  • PDF

Review on Atomic Layer Deposition of HfO2-based Ferroelectrics for Semiconductor Devices (반도체 소자용 산화하프늄 기반 강유전체의 원자층 증착법 리뷰)

  • Lee, Younghwan;Kwon, Taegyu;Park, Min Hyuk
    • Journal of the Korean institute of surface engineering
    • /
    • v.55 no.5
    • /
    • pp.247-260
    • /
    • 2022
  • Since the first report on ferroelectricity in Si-doped hafnia (HfO2), this emerging ferroelectrics have been considered promising for the next-generation semiconductor devices with their characteristic nonvolatile data storage. The robust ferroelectricity in the sub-10-nm thickness regime has been proven by numerous research groups. However, extending their scalability below the 5 nm thickness with low temperature processes compatible with the back-end-of-line technology. In this review, therefore, the current status, technical issues, and their potential solutions of atomic layer deposition (ALD) of HfO2-based ferroelectrics are comprehensively reviewed. Several technical issues in the physical scaling of the ferroelectric thin films and potential solutions including advanced ALD techniques including discrete feeding ALD, atomic layer etching, and area selective ALD are introduced.

The etching properties of MgO thin films in $Cl_2/Ar$ gas chemistry (유도 결합 플라즈마를 이용한 MgO 박막의 식각특성)

  • Koo, Seong-Mo;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.734-737
    • /
    • 2004
  • The metal-ferroelectric-semiconductor (MFS) structure is widely studied for nondestructive readout (NDRO) memory devices, but conventional MFS structure has a critical problem. It is difficult to obtain ferroelectric films like PZT on Si substrate without interdiffusion of impurities such as Pb, Ti and other elements. In order to solve these problems, the metal-ferroelectric-insulator-semiconductor (MFIS) structure has been proposed with a buffer layer of high dielectric constant such as MgO, $Y_2O_3$, and $CeO_2$. In this study, the etching characteristics (etch rate, selectivity) of MgO thin films were etched using $Cl_2/Ar$ plasma. The maximum etch rate of 85 nm/min for MgO thin films was obtained at $Cl_2$(30%)/Ar(70%) gas mixing ratio. Also, the etch rate was measured by varying the etching parameters such as ICP rf power, dc-bias voltage, and chamber pressure. Plasma diagnostics was performed by Langmuir probe (LP) and optical emission spectroscopy (OES).

  • PDF

Metal-Organic Chemical Vapor Deposition of $Pb(Zr_xTi_{1-x})O_3$ Thin Films for High-Density Ferroelectric Random Access Memory Application

  • Lee, June-Key;Ku, June-Mo;Cho, Chung-Rae;Lee, Yong-Kyun;Sangmin Shin;Park, Youngsoo
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • v.2 no.3
    • /
    • pp.205-212
    • /
    • 2002
  • The growth characteristics of metal-organic chemical vapor deposition (MOCVD) $Pb(Zr_xTi_{1-x})O_3 (PZT) thin films were investigated for the application of high-density ferroelectric random access memories (FRAM) devices beyond 64Mbit density. The supply control of Pb precursor plays the most critical role in order to achieve a reliable process for PZT thin film deposition. We have monitored the changes in the microstructure and electrical properties of films on increasing the Pb precursor supply into the reaction chamber. Under optimized conditions, $Ir/IrO_2/PZT(100nm)/Ir capacitor shows well-saturated hysteresis loops with a remanent polarization (Pr) of $~28{\mu}C/textrm{cm}^2$ and coercive voltage of 0.8V at 2.5V. Other issues such as step coverage, compositional uniformity and low temperature deposition was discussed in viewpoint of actual device application.

Thickness Effects on Electrical Properties of PVDF-TrFE (51/49) Copolymer for Ferroelectric Thin Film Transistor

  • Kim, Joo-Nam;Jeon, Ho-Seung;Han, Hui-Seong;Im, Jong-Hyung;Park, Byung-Eun;Kim, Chul-Ju
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.130-131
    • /
    • 2007
  • In this study, polyvinylidene fluoride/trifluoroethylene (PVDF-TrFE) was investigated. For a metal-ferroelectic-metal (MFM) structure, We obtained that the 70 nm-thick film showed the maximum polarization of $8.24\;{\mu}C/cm^2$, 2Pr of $6\;{\mu}C/cm^2$ and the coercive voltage of ${\pm}3.1\;V$ at 12 V. The 140 nm-thick film showed higher performance. However, the thicker film required a higher voltage. The current density was $10^{-6}{\sim}10^{-7}\;A/cm^2$ under 15 V. We can expect from these results that the electrical properties of the devices particularly ferroelectric thin film transistor using PVDF-TrFE copolymer, be able to be on the trade-off relationship between the remanent polarization and the leakage current.

  • PDF

Deposition and XPS Study of Pb, Zr, and Ti Films

  • Choi, Sujin;Park, Juyun;Jeong, Eunkang;Kim, Beob Jun;Son, Seo Yoon;Lee, Jeong Min;Lee, Jin Seong;Jo, Hee Jin;Park, Jihun;Kang, Yong-Cheol
    • Journal of Integrative Natural Science
    • /
    • v.7 no.3
    • /
    • pp.183-187
    • /
    • 2014
  • Lead zirconate titanate (PZT) is significant material in electrical and optical devices for their ferroelectric, piezoelectric and dielectric properties. In this research, PZT films were fabricated by reactive RF co-sputtering method using Pb, Zr, and Ti targets. From XPS study, lead, zirconium, and titanium are successfully deposited on Si(100) substrate. Thickness of PZT films was measured with a surface profiler and the thickness was decreased as the oxygen gas ratio increased in the sputter gas.

The Effect of Layer Spacing Changes in the SmA Phase on Defects Observed in SSFLC Devices.

  • Wang, Chenhui;Bos, Philip J.;Kumar, Satyendra;Wand, Michael;Handschy, Mark
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2004.08a
    • /
    • pp.193-197
    • /
    • 2004
  • The effect of the temperature dependence of the smectic layer spacing in the smectic-A (SmA) phase on the formation of defects in the ferroelectric smectic-$C^{\ast}$ ($SmC^{\ast}$) phase is investigated with x-ray scattering technique. The study is based on thin parallel-aligned surface stabilized ferroelectric liquid crystal cells with two different alignment conditions, high pretilt $SiO_x$, alignment and low pretilt polyimide films. It is found that defects observed in the $SmC^{\ast}$ phase have much more profound dependence on the layer changes and chevron formation in the SmA phase than in the $SmC^{\ast}$ phase. We find that thermal layer expansion with decreasing temperature in the SmA phase suppresses the formation of defects observed in the SmC phase.

  • PDF

Characteristics of Ferroelectric SrBi2Ta2O9 Thin Films deposited by Plasma-Enhanced Atomic Layer Deposition (플라즈마 원자층증착법에 의해 제조된 강유전체 SrBi2Ta2O9박막의 특성)

  • 신웅철;류상욱;유인규;윤성민;조성목;이남열;유병곤;이원재;최규정
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.03a
    • /
    • pp.35-35
    • /
    • 2003
  • Recent progress in the integration of the ferroelectric random access memories (FRAM) has attracted much interest. Strontium bismuth tantalate(SBT) is one of the most attractive materials for use in nonvolatile-memory applications due to low-voltage operations, low leakage current, and its excellent fatigue-free property. High-density FRAMs operated at a low voltage below 1.5V are applicable to mobile devices operated by battery. SBT films thinner than 0.1 #m can be operated at a low voltage, because the coercive voltage (Vc) decreases as the film thickness is reduced. In addition, the thickness of the SBT film will have to be reduced so it can fit between adjacent storage nodes in a pedestal type capacitor in future FRAMs.

  • PDF

Waveguides Fabrication for Optical Integrated Devices Application on Relaxor-ferroelectric $Pb(Mg_{1/3}Nb_{2/3})O_{3}-PbTiO_3$Single Crystal (완화형 강유전체$Pb(Mg_{1/3}Nb_{2/3})O_{3}-PbTiO_3$ 단결정의 광 집적소자 응용을 위한 도파로 제작)

  • Yang, Woo-Seok;Lee, Sang-Goo;Koo, Kyoung-Hwan;Huh, Hyun;Yoon, Dae-Ho;Lee, Han-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.546-547
    • /
    • 2002
  • Ni thin film on the PMN-PT crystal wafer were deposited by using E-beam evaporator technique. Deposited film was patterned by UV-lithography and etching and was in-diffused at 300~600C. Diffusion profile of Ni ions in PMN-PT was measured by secondary ion mass spectroscopy (SIMS).

  • PDF