• 제목/요약/키워드: butt joint

검색결과 269건 처리시간 0.027초

자기장 센서를 이용한 갭간격이 없는 박판 맞대기 용접부의 용접선 추적 장치 (Joint tracking system for butt joint welding process using eddy current sensors with the condition of no gap distance)

  • 김영선;조형석
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 1997년도 한국자동제어학술회의논문집; 한국전력공사 서울연수원; 17-18 Oct. 1997
    • /
    • pp.836-839
    • /
    • 1997
  • In recent years, much progress has been made in the automation of welding coped with a variety of highly flexible sensors. Among these sensors, only the eddy current sensor can detect the center location of the butt joint whose gap distance is zero. Thus, in this study the eddy current sensor is used to develop a robust and useful joint tracking system. The developed system is tested to qualify the performance of the system and seam tracking algorithm is proposed and two simulation are executed to show the performance of the proposed tracking algorithm.

  • PDF

마찰교반용접된 겹치기 및 맞대기 용접부 특성에 대한 실험 (Experimental Behaviors of Weld Zone Property of the Butt and the Lap Jointed Specimen Friction-Stir-Welded with 2mmt 1050 Aluminum Alloy Sheet)

  • 전정일;장석기
    • 대한기계학회논문집A
    • /
    • 제30권2호
    • /
    • pp.187-193
    • /
    • 2006
  • The butt and the lap welding by friction stir welding performs with $2mm^t$ 1050 aluminum alloy sheet. This paper shows behaviors of property such as vickers hardness, yielding and ultimate stresses, and macro structures for weld zone cross section of the butt and the lap jointed specimens. It is also carried out making comparison with maximum loads, stress-strain diagrams, and deformation after the guided bending test and fracture behaviors between the butt and the lap jointed specimens. It is found that the weldability of the butt jointed specimen is better than that of the lap jointed specimen.

의치수리(義齒修理)에 있어 파절접합부(破折接合部)의 조작형태(造作形態)가 의치(義齒)의 결합력(結合力)에 미치는 영향(影響)에 관(關)한 연구(硏究) (A STUDY REPAIRED JOINT STRENGTH OF COMPLETE DENTURE)

  • 이우현;허성주;조인호
    • 대한치과보철학회지
    • /
    • 제29권3호
    • /
    • pp.101-110
    • /
    • 1991
  • The purpose of this study was to compare the repaired joint strength among several edge profiles after denture repair. For this study, eight edge profiles were used for repair methods and five self-curing resin brands were used for repair materials. Break away loads were tested after 1 hr., 24 hrs. and 1 week. Instron was used for testing the transverse strength of repaired specimen. The results were as follows. 1. Repaired joint strength was about 35-65% of that of original specimen. 2. Joint strengths of round, inverse knife, inverse rabbit, lap ogee joint were higher tnan that of traditional simple butt joint 3. Joint strength of the simple butt joint was low significant. 4. Joint strengths after 1 hr. specimen were lower than those of 24 hrs. and 1 week specimens in joint strengths. 5. There were no significant differences between 24 hrs. and 1 week specimens in joint strengths. 6. It look more than 24 hours to gain satisfactory physical property after repairing the fractured denture base when self-curing resin was used for repair.

  • PDF

리기다소나무 판재(板材)의 접착조건(接着條件)이 집성재(集成材)의 접착성능(接着性能)에 미치는 영향(影響) (Effects of Adhesion Conditions on Bonding Strength of Pitch Pine Woods for Glued-Laminated Wood)

  • 박상범;공영토;조재명
    • Journal of the Korean Wood Science and Technology
    • /
    • 제16권4호
    • /
    • pp.48-53
    • /
    • 1988
  • 본(本) 연구(硏究)는 리기다소나무판재(板材)를 이용(利用)하여 집성재(集成材)를 제조(製造)할 경우(境遇), 압체시간(壓締時間) 및 접착제도포량(接着劑塗布量), 목재(木材)의 함수율(含水率), Butt-joint의 틈새간격(間隔) 및 접착제(接着劑)의 종류(種類) 등(等)이 접착강도(接着强度)에 미치는 영향(影響)을 알아보기 위해 수행(遂行)되었다. 1. 리기다소나무집성재(集成材)의 제조(製造)에 수성(水性)비닐우레탄접착제(接着劑)를 사용(使用)한 결과(結果), 접착제도포량(接着劑塗布量) 200g/$m^2$, 압체압력(壓締壓力) 10kg/$cm^2$에서 12시간(時間) 압체(壓締)하면 기준강도(基準强度)(50kg/$cm^2$)이상(以上)에 달(達)하였다. 2. 판재(板材)의 함수율(含水率)의 접착력(接着力)을 크게 감소(減少)시켰으나, 고함수시(高含水時) 접착(接着)한 후(後) 기건(氣乾)하여 접착력(接着力)을 측정(測定)한 결과(結果), 100kg/$cm^2$)이상(以上)의 블록전단강도(剪斷强度)를 나타내었다. 3. 판재(板材)의 Butt joint 부분(部分)의 틈새간격(間隔)이 0.5mm이하(以下)인 경우(境遇), 강도(强度)값은 영향(影響)하지 않았고, 하중방향(荷重方向)이 접착력(接着力)과 수치(垂値)일 때가 수평(水平)일 때보다 강도성태(强度性能)이 양호(良好)하였다. 4. 시험(試驗)에 사용(使用)된 5종(種)의 접착제(接着劑) 중(中) 수성(水性)비닐우레탄수지접착제(樹脂接着劑)가 상태(常態) 및 내수접착력면(耐水接着力面)에서 가장 양호(良好)하였다.

  • PDF

조선해양 구조물 주판의 Butt welding joint 수축에 관한 연구 (A Study on the compensation margin on butt welding joint of large steel plates in shipyards)

  • 김정태;이대철;정효민;정한식
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제37권5호
    • /
    • pp.461-466
    • /
    • 2013
  • 본 논문은 조선해양 구조물 주판의 맞대기용접 수축에 대한 특성을 연구하였다. 주판의 맞대기 용접은 입 열과 냉각과정에서 수축 변형이 일어나 최종 완성된 모재의 치수와 설계 치수가 다르게 된다. 이는 선박의 블록 생산 품질 불량으로서 교정 작업이 필요하며 생산성 향상의 저해요인이다. 이에 대형 구조물 주판의 맞대기용접 수축 변형에 관한 실험을 통하여 I, Y, V 형상의 용접잔류응력 수축 변형 데이터를 확보하고 두께 11 t ~ 21.5 t 범위에서는 1 ~ 2 mm의 한정된 범위의 수축 량이 균일하게 나타나는 특징과 용접부의 열전달 영향이 Seam Line 한쪽을 기준으로 최대 약 1000 mm 이내에 국한되어 모재의 자중이 수축 량에 미치는 영향은 크지 않았고 또한 수축 변형을 최소화하기 위해 설계단계에서 Groove 형상에 따라 수축마진을 다르게 적용해야 함을 알 수 있었다.

EFFECT OF FLASHING AND UPSETTING PARAMETERS ON THE FLASH BUTT WELDING OF HIGH STRENGTH STEEL

  • Kim, Young-Sub;Kang, Moon-Jin
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.384-389
    • /
    • 2002
  • This study was aimed to evaluate the weldability and optimize the welding conditions for flash butt welding of 780MPa grade steel applied to the automotive bumper reinforcement. And then the relationship between the welding conditions and the joint performance relating specifically to coil-joining steel would be established. The effect of welding conditions between flashing and upsetting process was elucidated. Microstructure observation of the joint indicated that the decarburized band was mainly changed with upsetting process. Width of HAZ was also related to the upsetting conditions rather than the flashing conditions. Generally maximum hardness at HAZ was correlated with $C_{eq}$ of steel and the empirical relationship was obtained to estimate the HAZ properties. Tensile elongation at the joint was usually decreased with increasing the initial clamping distance. Investigation of fracture surface after tensile and bending tests reveal that the origin of cracking at the joint was oxide inclusions composed of $SiO_2$, MnO, $Al_2$ $O_3$, and/or FeO. The amount of inclusions was dependent on the composition ratio of Mn/Si in steel. If this ratio was above 4, the amount of inclusions was low and then the resistance to cracking at the joint was enough to maintain the joint performance. It was obtained that the flashing process influenced the conditions for the energy input to establish uniform or non-uniform molten layer, while the upsetting conditions influenced the joint strength. Heat input variable during flashing process was also discussed with the joint properties.

  • PDF

이종두께 강판의 $CO_2$ 레이저 용접 및 성형성 ($CO_2$ Laser Beam Welding and Formability of Steel Plates with Different Thicknesses)

  • 서정;한유희;김정오;이영신
    • Journal of Welding and Joining
    • /
    • 제14권1호
    • /
    • pp.82-91
    • /
    • 1996
  • The maximum butt-joint gap size in $CO_2$ laser beam welding of SAPH steel plates with different thicknesses and its bending formability were studied. In the range of the gap size$\geq$0.1mm, the optimal butt welding speed was faster than that of no gap (air gap) condition. This behaviour was independent on the difference of thickness at any combination. Also, the allowable gap size in steel plates with different thicknesses was larger than with same thicknesses. In the range of $T/T_0$(bead shape) $\geq$ 0.8, good bending formability was obtained at any combination of thickness. The formability was improved by reducing the hardness in weld bead using pre-heating process. Finally, FEM result of the laser beam welded underframe with different thicknesses was compared to that of the conventional spot welded underframe.

  • PDF

피복(被覆) Arc용접(熔接)으로 Butt이음된 사각평판(四角平板)의 용접변형(熔接變形) (Welding Distortions on Rectangular Butt Welded Plate by Shielded Metal Arc Welding Process)

  • 박종은;임상전;윤봉섭
    • 대한조선학회지
    • /
    • 제17권2호
    • /
    • pp.21-32
    • /
    • 1980
  • The welding distortions, transverse shrinkage and angular change, on the butt welded joint made by the process of shielded metal arc welding, were studied on the basic study of bead on plate weld. On the study of bead on plate weld, the temperature distribution on the plane normal to the direction of the weld line was assumed to be parabolic. The form of the distortion formulas of welded joint for transverse shrinkage and angular change were derived theoretically. Also, the experiments were performed about three cases, for changing type, sizes of welding electrodes and types of grooves, welding on mild steel plate, to compare theoretical study and experiments. It was found that the theoretical study was in good agreement with the result of experiment. Also, the optimal welding conditions for reducing weld distortions were suggested.

  • PDF

고강도강 맞대기 용접 시험편의 루트갭 변경에 따른 피로강도 평가 (Fatigue Assessment of High Strength Steel with Butt Welded Joints for the Root Gap Difference)

  • 김호정;강성원;김명현
    • 대한조선학회논문집
    • /
    • 제48권1호
    • /
    • pp.56-61
    • /
    • 2011
  • In this study, a series of fatigue tests was conducted to evaluate fatigue strength for the root gap difference with high strength steel with butt welded joints. A finite element analysis using effective notch stress method was also performed to compare effective notch factors each other with butt welded specimens made by copper backing. The results of fatigue tests were classified according to the root gap difference. Fatigue life of butt welded specimens is presented for determining the root gap of high strength steel with butt welded joints in terms of fatigue strength. Then effective notch stress was applied to interpret fatigue strength of butt welded specimen model which is reflected actual measured dimensions. As a result, fatigue strength of high strength steel with butt welded specimens is increased by root gap gets longer in length.

알루미늄 박판에 대한 AC 펄스 MIG 용접에서 극성가변의 효과 (The effect of variable polarity on AC pulse Welding for sheet Al metal)

  • 공현상;임성룡;김기정;조상명
    • 한국마린엔지니어링학회:학술대회논문집
    • /
    • 한국마린엔지니어링학회 2001년도 추계학술대회 논문집(Proceeding of the KOSME 2001 Autumn Annual Meeting)
    • /
    • pp.88-91
    • /
    • 2001
  • New type of vehicles made from thin aluminum alloy are under rapid development and some product are already on the market, but when welding sheet metal joint of aluminum alloy, the main problem are burn-through by the high heat input. The purpose of this study, it is to prevent the burn-through and to shallow penetration that AC pulse welding has diminish the penetration and to lower the droplet temperature at Al sheet metal welding. In this study, we observed the bead appearance and whether it was appeared burn through or not , as the variation of the root gap in the lap and butt-joint welding process.

  • PDF