• 제목/요약/키워드: HTS tube

검색결과 48건 처리시간 0.021초

Measurement of outgassing rates of Kevlar and S-Glass materials used in torque tubes of High Tc Superconducting (HTS) Motors

  • Thadela, S.;Muralidhar, BVAS;Kalyani, B;Choudhury, UK;Yadav, SN;Rao, V.V.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제20권4호
    • /
    • pp.11-15
    • /
    • 2018
  • Torque tubes in High Temperature Superconducting (HTS) motor transfer torque from superconducting field winding rotor to the room temperature shaft. It should have minimum heat conduction property for minimizing the load on cryo-refrigerator. Generally, these torque tubes are made with stainless steel material because of high strength, very low outgassing and low thermal contraction properties at cryogenic temperatures and vacuum conditions. With recent developments in composite materials, these torque tubes could be made of composites such as Kevlar and S-Glass, which have the required properties like high strength and low thermal conductivity at cryogenic temperatures, but with a reduced weight. Development and testing of torque tubes made of these composites for HTS motor are taken up at Bharat Heavy Electricals Limited (BHEL), Hyderabad in collaboration with Central Institute of Plastics and Engineering Technology (CIPET), Chennai and Indian Institute of Technology (IIT), Kharagpur. As these materials are subjected to vacuum, it is important to measure their outgassing rates under vacuum conditions before manufacturing prototype torque tubes. The present study focusses on the outgassing characteristics of Kevlar and S-Glass, using an Outgassing Measurement System (OMS), developed at IIT Kharagpur. The OMS facility works under vacuum environment, in which the test samples are exposed to vacuum conditions over a sufficient period of time. The outgassing measurements for the composite samples were obtained using pressure-rise technique. These studies are useful to quantify the outgassing rate of composite materials under vacuum conditions and to suggest them for manufacturing composite torque tubes used in HTS motors.

$SrSO_{4}$의 첨가량이 Bi2212 고온초전도체 튜브에 미치는 영향 (The effect of $SrSO_{4}$ on Bi2212 HTS tube)

  • 정승호;장건익
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 초전도 자성체 연구회
    • /
    • pp.80-83
    • /
    • 2003
  • $SrSO_4$ were systematically added on Bi2212 from 0 to 10wt% to study the effect of Bi2212 superconductor tube characteristics. After mixing, the melted solution of Bi2212 and $SrSO_4$ was initially poured into the cylinder type of steel mold preheated at $550^{\circ}C$ for 30min and rotated at 1000rpm. Following that, tube was annealed at $840^{\circ}C$ for 72hrs. The tube dimension was 60 in diameter, 60mm in length and 2mm in thickness. XRD data suggests that there was no typical segregation phase related with $SrSO_4$. Well textured grain with typical 2212 phase was observed and average size was $20{\mu}m$. The measured critical current and critical current density of Bi2212 tube added by 5% $SrSO_4$ at 77K were 495A and $202A/cm^2$ respectively.

  • PDF

고온 초전도 tape의 임계전류 저하에 따른 교류손실 특성 (AC loss Characteristics under Critical Current Degradation of HTS Tapes)

  • 김해준;조전욱;김재호;심기덕;곽동순;배준한;김해종;성기철
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제7권3호
    • /
    • pp.29-33
    • /
    • 2005
  • Critical current$(I_c)$ degradation of High $T_c$ Superconducting(HTS) tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the $I_c$ degradation affects the AC loss of the wire. We measured the $I_c$ degradation and AC loss under tension and bending of Bi-2223 tapes made by 'Powder-in-Tube' technique at 77K with self-field. Also, we have studied the frequency characteristics on self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between $I_c$ degradation and AC loss are presented.

고온초전도 선재의 Bending횟수에 따른 임계전류의 특성 (Characteristic of Critical Current after Repetitive Bending for High Superconducting Tapes)

  • 김해준;주진홍;김석환;김해종;배준한;조전욱;성기철
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2003년도 하계학술대회 논문집 B
    • /
    • pp.900-902
    • /
    • 2003
  • Critical current($I_c$) degradation of HTS tapes after bending is one of the holiest issues in HTS development and application studies. Many people are measuring $I_c$ degradations for effect of tending radius. However even if the bending radius is larger than the breaking radius a HTS tapes can be damaged by repetitive bending, which is unavoidable in the winding processes. Therefore, We studied the $I_c$ degradation after repetitive bending, at 77K with self-field, of Bi-2223 tapes processed by "Powder-in-Tube" technique, which was made by America Superconductor Corporation(AMSC), Innova Superconductor Technology(InnoST) and Korea Electro-technology Research Institute(KERI). For each specimen $I_c$ degradation was measured various bending radius as function of repetitive bending number.

  • PDF

고온 초전도체의 임계전류 저하에 따른 교류 손실 특성 (Ac Loss Characteristics under Critical Current Degradation of HTS Tapes)

  • 김해준;김재호;심기덕;조전욱;곽동순;김해종;성기철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.286-287
    • /
    • 2005
  • Critical current(Ic) degradation of HTS tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the Ie degradation affects the AC loss of the wire. We measured the Ie degradation and AC loss under tension and bending of Bi-2223 tapes processed by "Powder-in-Tube" technique at 17K with self-field. And we have studied the frequency dependence of self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between Ic degradation and AC loss are presented.

  • PDF

초전도필터 및 적외선검지기 냉각용 극저온냉동기 (Cryocoolers for cooling of HTS RF Filter and IR detector)

  • 홍용주
    • 한국정밀공학회지
    • /
    • 제19권11호
    • /
    • pp.18-23
    • /
    • 2002
  • 고품질의 극저온 환경의 생성 및 유지는 고품질 대용량 정보통신, 의료진단, 초전도 및 고집적반도체 제조공정 등의 차세대 유망 산업 분야에서 필수적인 요소로 자리 잡고 있으며, cryopump, 민수용 및 군수용의 적외선 검지기 및 초전도 RF 필터의 효과적 냉각을 위해 보다 높은 신뢰성과 수명, 고효율의 극저온 냉동기에 대한 수요는 점차 증대될 것으로 기대된다. 스터링 냉동기 및 맥동관 냉동기는 짧은 역사에도 불구하고, 다양한 분야에서 기존의 한제 및 극저온 냉동기를 대치하여 활용될 수 있을 것으로 전망된다.

원심 성형법에 의한 고온초전도체 제조 (Fabrication of Bi2212 superconductor by Centrifugal Forming Process)

  • 정승호;장건익
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.503-506
    • /
    • 2002
  • BSCCO 2212 HTS was fabricated by CFP(centrifugal forming process). The powder was initially ground in the mixing ratio of 2:2::1:2 with 10% of SrSO$_4$. The temperature increased up to 1035$^{\circ}C$ and 1200$^{\circ}C$ for melting. The melt was poured into the preheated and rotating copper mould from 200 to 600$^{\circ}C$. The specimen was not broken by thermal impact when the melting temperature was over 1050$^{\circ}C$ and copper mould was preheated over 400$^{\circ}C$ for 30min. A tube type of specimen was annealed at 840$^{\circ}C$ or 860$^{\circ}C$ in oxygen atmosphere for 24hours. Typical microstructure was analyzed in terms of CFP parameters by XRD, SEM, and EDS and also superconducting characteristics were compared.

  • PDF

Bi-2223 고온초전도 선재의 임계전류 향상에 관한 연구 (A study on Improvement of Critical Current for Bi-2223 HTS Tapes)

  • 하홍수;정종만;이남진;장현만;하동우;오상수;권영길;류강식
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2000년도 KIASC Conference 2000 / 2000년도 학술대회 논문집
    • /
    • pp.3-5
    • /
    • 2000
  • Among the various processing techniques used in HTS wire fabrication, the PIP(Powder In Tube) method is currently one of the most promising for applications on an industrial scale. In this study, we have fabricated Bi-2223/Ag superconducting tapes using the modified PIT process, where several process factors were changed and improved, ie., powder packing, drawing, rolling and heat treatment. We obtained Bi-2223 tape that have high critical current, 46 a at 77.3 K, have high critical current, 46A at 77.3 K, self field although the tape was not pressed but only rolled. The critical current of 100m class long length tape was measured 21.6A at the same criterion. Besides, the critical current of Bi-2223/Ag tape was measured applying magnetic fields with different directions at various temperatures.

  • PDF

고화질소 냉각형 고온초전도마그네트 개발(I) (Development of HTS magnet cooled by solid nitrogen(I))

  • 오상수;하홍수;하동우;권영길;류강식;이해근;;한일용
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2000년도 KIASC Conference 2000 / 2000년도 학술대회 논문집
    • /
    • pp.19-21
    • /
    • 2000
  • We are developing portable type HTS magnet system cooled by solid nitrogen. This system have recooling and recharging capabilities. In this paper, we report preliminary test results obtained from the experimental solid nitrogen system and pancake magnet would with Bi-2223/Ag tapes, respectively. The operation period was sensitively dependent on the vacuum rate n the cryostat, size of SUS tube for flowing N_{2}$, and liquid nitrogen to cool the cryostat. The fabricated coil I_{c}$was 75 A at 20 K in self field.

  • PDF

700A급 고온초전도 전류도입선 제조 (700Amp class of HTS current lead Fabrication)

  • 박승남;박치완;장건익;하동우;성태현
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 추계학술대회 논문집
    • /
    • pp.72-75
    • /
    • 2003
  • HTS tubes were fabricated in terms of various SrSO4 additions by Centrifugal Forming Method. For powder melting by induction, the optimum temperature ranges of melting and preheating were 105$0^{\circ}C$~110$0^{\circ}C$ and 55$0^{\circ}C$ for 30min respectively The mould rotating speed was 1000rpm. A tube was annealed at 84 $0^{\circ}C$ for 72 hours in oxygen atmosphere. The plates like grains more than 20${\mu}{\textrm}{m}$ were well developed along the rotating direction of mould regardless of the amounts of SrSO4 in Bi2212. The measured Ic and Jc at 77K(B = 0T) in Bi2212 with 7% SrSO4 composition were about 680A and 380A/$\textrm{cm}^2$.

  • PDF