• Title/Summary/Keyword: 유리섬유 강화플라스틱

Search Result 104, Processing Time 0.022 seconds

Study on the Qualitative Defects Detection in Composites by Optical Infrared Thermography (적외선 열화상 기술을 이용한 복합재료의 결함 검출 정량화 연구)

  • Park, Hee-Sang;Choi, Man-Yong;Park, Jeong-Hak;Kim, Won-Tae;Choi, Won-Jong
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.31 no.2
    • /
    • pp.150-156
    • /
    • 2011
  • In this paper, infrared thermography measurement technique has been used to develop standard measurement technique for nondestructive testing of composite materials which is widely used in aerospace industries. To increase the defect detection rate, the related experiment used the lock-in IR-thermographiy method. Therefore it is of considerable interest in the field of non-destructive testing for fast discontinuity detection by using ultrasonic lock-in infrared thermography. The result also shows that as the investigation period of light source is lengthened according to the thickness of specimen, the possibility of detecting defects gets higher as well. However, the reason why the result values were not favorable when less than 50 mHz of light source was provided is because it was difficult to detect defects as the defect parts became a state of thermal equilibrium in general when thermal diffusivity affects the entire materials.

A Study on Properties of the Glass Fiber Reinforced PPS Composites for Automotive Headlight Source Module (자동차 전조등 광원 모듈용 유리섬유강화 PPS 복합재료 특성 연구)

  • Heo, Kwang-Yeol;Park, Sung-Min;Lee, Eun-Soo;Kim, Myung-Soon;Sim, Ji-Hyun;Bae, Jin-Seok
    • Composites Research
    • /
    • v.29 no.5
    • /
    • pp.293-298
    • /
    • 2016
  • In this paper, Glass Fiber Reinforced Thermoplastic (GFRTP) for automotive headlight source module was fabricated by compounding and injection molding using PPS (Poly Phenylene Sulfide) resin with glass fiber which has three cross section (round type, cocoon type, flat type). Tensile, flexural, impact properties were investigated on effect of cross section, glass fiber contents. And it was observed flatness, dimensional stability, fluidity depending on glass fiber cross section. As a result, flat glass fiber reinforced thermoplastic's mechanical properties were most excellent. Also, dimensional stability and flatness showed better results when using flat glass fiber.

Effect of Textile Pattern on Mechanical and Impregnation Properties of Glass Fiber/Thermoplastic Composite (유리 섬유/열가소성 복합 재료의 기계적 및 함침 특성에 대한 직물 패턴의 영향)

  • Kim, Neul-Sae-Rom;Lee, Eun-Soo;Jang, Yeong-Jin;Kwon, Dong-Jun;Yang, Seong Baek;Yeom, Jung-Hyun
    • Composites Research
    • /
    • v.31 no.6
    • /
    • pp.317-322
    • /
    • 2018
  • In various industry, the composite is tried to be applied to products and thermoplastic based composite is in the spotlight because this composite can be recycled. The use of continuous fiber thermoplastic (CFT) method increased gradually than long fiber thermoplastic (LFT). In this study, tensile, flexural, and impact test of different array types of glass fiber (GF)/thermoplastic composites were performed to compare with GF array. Impregnation property between GF mat and thermoplastic was determined using computed tomography (CT). At CFT method, thermoplastic film is not wet into GF roving and many voids are appeared into composite. This phenomenon affects to decrease mechanical properties. Plain pattern GF mat was the best mechanical and impregnation properties that distance between two roving was set closely to $100{\mu}m$.

Recycle of the Glass fiber Obtained from the Roving Cloth of FRP II: Study for the Physical Properties of fiber-reinforced Concrete (폐 FRP 선박의 로빙층에서 분리한 유리섬유의 재활용 II: 섬유강화 콘크리트의 물성에 관한 연구)

  • Kim, Yong-Seop;Lee, Seung-Hee;Yoon, Koo-Young
    • Journal of the Korean Society for Marine Environment & Energy
    • /
    • v.11 no.1
    • /
    • pp.46-49
    • /
    • 2008
  • Recycling glass fiber, 'F-fiber,' was obtained by the separation of the roving layer from waste FRP and the concrete products or structures were considered for its application. Experiment was carried out for the bending strength of aggregate (2.45 of cement) by weight and F-fiber (density of 1.45, volume ratio to all of the aggregate and the cement). Whereas the specimen containing 1% F-fiber showed the bending strength 23% higher than that without F-fiber after curing far 28 days, the one with 0.5% F-fiber did not give any change. It could be found, therefore, that the minimum mixing amount should be larger than 0.5% fur the strength reinforcement. One of the reinforcing concrete product, bench flume, containing 1% F-fiber showed 21% increment of bending strength In contrast to that without F-fiber.

  • PDF

Recycle of the Glass Fiber Obtained from the Roving Cloth of FRP I: Study for the Physical Properties of Fiber-reinforced Mortar (폐 FRP 선박의 로빙층에서 분리한 유리섬유의 재활용 I: 섬유강화 모르타르의 물성에 관한 연구)

  • Yoon, Koo-Young;Kim, Yong-Seop;Lee, Seung-Hee
    • Journal of the Korean Society for Marine Environment & Energy
    • /
    • v.10 no.2
    • /
    • pp.102-106
    • /
    • 2007
  • While the effort has been made in recycling the FRP (Fiber Reinforced Plastic) used for the medium-to-small size ships, researchers try to find out the methods more favorable for the environments and more value-added. In respect to the fact that the FRP consists of two types of layers, roving and mat, differentiated by the 2-dimensional structure, our group was able to separate the layers of FRP instead of grinding it. The roving cloth was cut to the long glass fibers (about 50 mm long; calling it 'F-fiber' afterwards). F-fiber showed increasing tensile strength and chemical-resistance possibly due to the remained resin (about 25% by weight). In this experiment fiber-reinforced mortars are made of the F-fiber as a recycling method of FRP. The mortar containing 2% (v/v) F-fiber results in 34.6% increment of bending strength from the standard after 28 day curing. The resulting strength is similar to that of the mortar with imported polyvinyl fiber P-54. These results imply that F-fiber can be applied to the 'fiber reinforced mortar' and furthermore may be a substitute for the imported fibers.

  • PDF

Tensile Properties of Plain Weave Glass Fabric Reinforced Epoxy Resin Laminates at Low Temperatures (평직유리섬유 강화 에폭시 적층판의 저온 인장 특성)

  • Kim, Yon-Jig
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.9
    • /
    • pp.788-795
    • /
    • 2008
  • To understand the tensile behaviors of GFRP at low temperature, three types of specimen have been used in this study. Tensile properties and fracture mechanisms for three orthogonal orientations of plain weave glass fabric reinforced epoxy resin laminate were investigated at temperature range of about -30 to $15^{\circ}C$. The tensile properties of axial and edge type specimen decrease slightly with decreasing temperature to $-20^{\circ}C$. However, at $-30^{\circ}C$ the decreases in the tensile properties increased considerably. Below $-20^{\circ}C$, thickness type specimen showed a marked decreases in the tensile properties. It was obvious that the fracture manner of thickness type specimen was adhesive failure at above $-10^{\circ}C$ and a mixed adhesive and cohesive failure at below $-20^{\circ}C$.

Mechanical Properties Anisotropy of Plain Weave Glass Fabric Reinforced Epoxy Resin Laminates (평직유리섬유강화 에폭시 적층판의 기계적 특성 이방성)

  • Kim, Yon-Jig
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.17 no.3
    • /
    • pp.15-21
    • /
    • 2009
  • The anisotropic mechanical properties were measured for the three orthogonal orientations of plain weave glass fabric reinforced epoxy resin laminate. In tensile and flexural tests, axial and edge type specimens failed by pull-out of warp and fill yarns, respectively. In contrast, the thickness type specimens failed by adhesive failure process. Longitudinal cracking occurred in several of the edge type specimens during tensile test. That cracking caused pop-in in the stress-strain curve. Defects induced by improper coupon machining caused that cracking.

Stiffness Comparison with Design of GFRP Roof Panels Prepared by RTM Method (RTM 성형 GFRP 차체 설계에 따른 강성연구)

  • 유용문;윤의박;윤여성;이순홍
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.6 no.4
    • /
    • pp.32-38
    • /
    • 1998
  • In order to investigate the relationship between the stiffness and structure of the automotive roof panels, two kinds of glass fiber reinforced plastic(GFRP) roof panels without and with insert material were fabricated by resin transfer molding(RTM) method. The stiffness test was performed at the same condition as it of actual driving. The structural design and material selection for improving the recyclability of GFRP roof panels were also covered.

  • PDF

Hull Strength Evaluation of Dissemination 12ft Bass Fishing Boat Using FEA (보급형 12피트 배스 낚시보트의 유한요소해석을 통한 선체강도평가)

  • Oh, Young-Cheol;Ko, Jae-Yong;Chung, Se-Yun;Choi, Jeong-Hwan;Kim, Hyeon-Jin
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • 2012.06a
    • /
    • pp.225-226
    • /
    • 2012
  • Recently, In the domestic is used mainly fiberglass reinforced plastic(GRP) and is built for maritime leisure vessel & structures. but it less attention is insufficient for ship of structural strength assessment of maritime leisure vessel. Therefore, The structural strength evaluation suitable for the domestic situation formulate and is applied to domestic regulations of "Guidance for Recreational Crafts" of Korea register of shipping(KR) & "Reinforced plastic line structure standards" of Ministry of Land, Transport and Maritime Affairs. the structural design and finite element analysis(FEA) to ensure the reliability.

  • PDF

Exposure to Styrene in the Lamination Processes with Fiberglass-Reinforced Plastics: Health Diagnosis Case Report (유리섬유강화 플라스틱을 이용한 적층공정 근로자들의 스티렌 노출 평가: 보건진단 사례)

  • Choi, Sangjun;Jeong, Yeonhee
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.25 no.2
    • /
    • pp.126-133
    • /
    • 2015
  • 연구목적: 이 연구는 노동부의 보건진단 명령에 의해 유리섬유 강화플라스틱(FRP)을 이용한 이중벽 탱크 제조 사업장의 적층 공정 근로자들을 대상으로 스티렌 노출 특성을 평가하기 위해 수행되었다. 연구방법: 스티렌의 주요발생원 파악을 위해 불포화 폴리에스테르 수지(UPR), 경화제, 조색제, 세척액 등의 원료 내 스티렌 함유량을 가스크로마토그래피 질량분석기(GC-MS)를 이용하여 분석하였다. FRP 적층 공정에 근무하는 작업자들을 대상으로 NIOSH 1501 공정시험법에 의해 공기 중 스티렌 노출 농도에 대한 개인노출 평가를 실시하였고, 생물학적 노출 지표로 뇨 중 만델릭산을 채취한 후 고성능액체크로마토그래피(HPLC)로 분석하였다. 또한 각 직무 특성과 단위작업 중심으로 스티렌에 대한 단시간 노출평가를 수행하였다. 연구결과: 스티렌의 함유량이 가장 많은 주요 원료는 중량비율로37%의 스티렌이 함유된 UPR이었다. 적층 공정의 FRP분무 작업자와 보조 작업자들 모두 스티렌의 8시간 가중평균 노출기준(20 ppm)을 초과하였다. 단시간 노출평가 결과 FRP분무 작업자의 경우 45.9 ppm에서 86.1 ppm 수준으로 FRP를 사용하지 않는 작업보다 통계적으로 유의하게 높은 수준이었다(P<0.01). 가장 높은 수준의 스티렌에 노출되는 단위작업은 FRP를 이용하여 1차 코팅 하는 작업으로 특별한 관리가 필요하였다. 결론: 보건진단을 위해 실시한 이중벽 탱크 제조 사업장의FRP 적층 공정 작업자의 스티렌 노출수준은 노출기준을 초과할 정도로 높은 수준이었다. 그러나 탱크를 천장에 매달고 돌리면서 적층작업을 수행하기 때문에 적절한 국소환기 시스템을 구축하는데 어려움이 있다. 따라서 적절한 방독마스크 착용으로 스티렌 노출 예방이 필요하였다.