Fabrication of Bi-2223 high-Tc superconducting current lead (Bi-2223 고온초전도 전류리드의 제조)

  • Ha, D.W.;Oh, S.S.;Ryu, K.S.;Chang, H.M.
    • Proceedings of the KIEE Conference
    • /
    • 1996.07c
    • /
    • pp.1660-1662
    • /
    • 1996
  • Superconducting current lead is one of the promising applications of the oxide high-Tc superconductors, because they have the advantage of decreasing heat conduction to low temperature region, comparing with a conventional cooper alloy lead. High critical current density is a key factor for the applications such as current lead. $(Bi,Pb)_{2}Sr_{2}Ca_{2}Cu_{3}O_{x}$ high Tc superconductor hase been investigated in terms of critical current density. Bi-2223 superconducting current lead made by CIP and solid state sintering process. Bi-2223 current lead that heat treated at $836\;^{\circ}C$ for 240 h in 1/13 $PO_2$ had over $500\;A/cm^2$ of critical current density at 77K. We knew that the superconducting properties of tube type current leads were better than rods type of them. And we investigated the relation of Bi-2223 formation and heat treatment condition by XRD and SEM analysis.

  • PDF

Influence of Ag Precoating of $Bi_{2212}$ Superconductor-In Base Solder Soldering ($Bi_{2212}$ 초전도체와 In 계열 solder의 soldering에서 Ag precoating의 영향)

  • Jang Ji-Hoon;Kim Sang-Hyun;Shin Seung-Yong;Lee Yong-Chul;Kim Chan-Joong;Hyun Ok-Bae;Park Hae-Woong
    • Journal of the Korean institute of surface engineering
    • /
    • v.39 no.2
    • /
    • pp.57-63
    • /
    • 2006
  • In this study, In-base solder was applied to the interface between $Bi_2Sr_2Ca_1Cu_2O_x(Bi_{2212})$ superconductor and Cu-Ni shunt metal at the temperature lower than $150^{\circ}C$. Most of the cases, $Bi_{2212}$ superconductor was precoated with Ag by electroplating in order to improve the contact properties of the solder layer. When the superconductor was directly soldered on to the superconductor, the solder was easily separated without external force. The shear strength of the contact between superconductor and shunt metal increased from 69.2 kgf to 74.4 kgf and 80.1 kgf, as the current density of the Ag electroplating was changed from 63 mA to 96 mA and 126 mA, respectively. The contact strength also increased to 49.9 kgf and 69.2 kgf when thickness of the electroplated Ag layer increased to $5{\mu}m$ and $10{\mu}m$, reapectively.

Applicability of plate tectonics to the post-late Cretaceous igneous activities and mineralization in the southern part of South Korea( I ) (한국남부(韓國南部)의 백악기말(白堊紀末) 이후(以後)의 화성활동(火成活動)과 광화작용(鑛化作用)에 대(對)한 판구조론(板構造論)의 적용성(適用性) 연구(硏究)( I ))

  • Min, Kyung Duck;Kim, Ok Joon;Yun, Suckew;Lee, Dai Sung;Joo, Sung Whan
    • Economic and Environmental Geology
    • /
    • v.15 no.3
    • /
    • pp.123-154
    • /
    • 1982
  • Petrochemical, K-Ar dating, Sand Rb/Sr isotopes, metallogenic zoning, paleomagnetic and geotectonic studies of the Gyongsang basin were carried out to examine applicability of plate tectonics to the post-late Cretaceous igneous activity and metallogeny in the southeastern part of Korean Peninsula. The results obtained are as follows: 1. Bulgugsa granitic rocks range from granite to adamellite, whose Q-Ab-Or triangular diagram indicates that the depth and pressure at which the magma consolidated increase from coast to inland varying from 6 km, 0.5-3.3 kb in the coastal area to 17 km, 0.5-10 kb in the inland area. 2. The volcanic rocks in Gyongsang basin range from andesitic to basaltic rocks, and the basaltic rocks are generally tholeiitic in the coastal area and alkali basalt in the inland area. 3. The volcanic rocks of the area have the initial ratio of Sr^{87}/Sr^{86} varying from 0.706 to 0.707 which suggests a continental origin; the ratio of Rb/Sr changing from 0.079-0.157 in the coastal area to 0.021-0.034 in the inland area suggests that the volcanism is getting younger toward coastal side, which may indicate a retreat in stage of differentiation if they were derived from a same magma. The K_2O/SiO_2 (60%) increases from about 1.0 in the coastal area to about 3.0 in the inland area, which may suggest an increase indepth of the Benioff zone, if existed, toward inland side. 4. The K-Ar ages of volcanic rocks were measured to be 79.4 m.y. near Daegu, and 61.7 m.y. near Busan indicating a southeastward decrease in age. The ages of plutonic rocks also decrease toward the same direction with 73 m.y. near Daegu, and 58 m.y. near Busan, so that the volcanism predated the plutonism by 6 m.y. in the continental interior and 4 m.y. along the coast. Such igneous activities provide a positive evidence for an applicability of plate tectonics to this area. 5. Sulfur isotope analyses of sulfide minerals from 8 mines revealed that these deposits were genetically connected with the spacially associated ingeous rocks showing relatively narrow range of ${\delta}^{34}S$ values (-0.9‰ to +7.5‰ except for +13.3 from Mulgum Mine). A sequence of metallogenic zones from the coast to the inland is delineated to be in the order of Fe-Cu zone, Cu-Pb-Zn zone, and W-Mo zone. A few porphyry type copper deposits are found in the Fe-Cu zone. These two facts enable the sequence to be comparable with that of Andean type in South America. 6. The VGP's of Cretaceous and post Cretaceous rocks from Korea are located near the ones($71^{\circ}N$, $180^{\circ}E$ and $90^{\circ}N$, $110^{\circ}E$) obtained from continents of northern hemisphere. This suggests that the Korean peninsula has been stable tectonically since Cretaceous, belonging to the Eurasian continent. 7. Different polar wandering path between Korean peninsula and Japanese islands delineates that there has been some relative movement between them. 8. The variational feature of declination of NRM toward northwestern inland side from southeastern extremity of Korean peninsula suggests that the age of rocks becomes older toward inland side. 9. The geological structure(mainly faults) and trends of lineaments interpreted from the Landsat imagery reveal that NNE-, NWW- and NEE-trends are predominant in the decreasing order of intensity. 10. The NNE-trending structures were originated by tensional and/or compressional forces, the directions of which were parallel and perpendicular respectively to the subduction boundary of the Kula plate during about 90 m.y. B.P. The NWW-trending structures were originated as shear fractures by the same compressional forces. The NEE-trending structures are considered to be priginated as tension fractures parallel to the subduction boundary of the Kula plate during about 70 m.y. B.P. when Japanese islands had drifted toward southeast leaving the Sea of Japan behind. It was clearly demonstrated by many authors that the drifting of Japanese islands was accompanied with a rotational movement of a clock-wise direction, so that it is inferred that subduction boundary had changed from NNE- to NEE-direction. A number of facts and features mentioned above provide a suite of positive evidences enabling application of plate tectonics to the late Cretaceous-early Tertiary igneous activity and metallogeny in the area. Synthesizing these facts, an arc-trench system of continental margin-type is adopted by reconstructing paleogeographic models for the evolution of Korean peninsula and Japan islands. The models involve an extention mechanism behind the are(proto-Japan), by which proto-Japan as of northeastern continuation of Gyongsang zone has been drifted rotationally toward southeast. The zone of igneous activity has also been migrated from the inland in late-Cretaceous to the peninsula margin and southwestern Japan in Tertiary.

  • PDF

Josephson Vortex Dynamics in Tilted Magnetic Fields (경사 자기장 하에서의 조셉슨 볼텍스 동역학)

  • Jin, Yong-Duk;Ki, Dong-Keun;Lee, Hu-Jong
    • Progress in Superconductivity
    • /
    • v.9 no.2
    • /
    • pp.140-145
    • /
    • 2008
  • We report on the Josephson vortex dynamics in $Bi_2Sr_2CaCuO_{8+\delta}$ natural Josephson junctions by c-axis tunneling measurements. Beside the quasiparticle branches in the current-voltage characteristics, a new set of multiple branches, referred to as Josephson-vortex-flow branches (JVFBs), are observed. The JVFBs emerge in an in-plane magnetic field above $H_0\;=\;{\Phi}_0/{\gamma}s^2$ and show highly hysteretic behavior, which can be explained in terms of the recently proposed dynamic-phase-separation model. In this work we examined the effect on the JVFBs by the presence of pancake vortices generated as the external magnetic field was applied slightly tilted from the in-plane direction. JVFBs were found to become larger and prominent with increasing pancake vortex density as the tilt angle increased, which were presumably caused by slowing down of a Josephson vortex lattice in the presence of pancake vortices.

  • PDF

Development of joining process of the BSCCO(2223)/Ag multi-filament tapes (BSCCO(2223)/Ag 다심 초전도선재의 접합공정 개발)

  • Kim, Kyu-Tae;Kim, Jung-Ho;An, Hyuck;Jang, Seok-Hern;Joo, Jin-Ho
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.02a
    • /
    • pp.120-122
    • /
    • 2003
  • We jointed Bi(Pb)-Sr-Ca-Cu-O multifilament tapes and evaluated their electrical properties. In order to improve connectivity of multifilarnents, single-filament tape was inserted between two multifilament tapes or multifilament was stepped by mechanical remove. The critical current ratio (CCR) and n-value of the jointed tapes were evaluated as a function of uniaxial pressure. It was observed that CCR and n-value were 24.8-29.0% and 2.5-2.8 for lap-jointed tape. On the other hand, the corresponding values were improved to 51.8-61.9% and 2.9-5.1 for three stepped jointed tape, and 63.4-67.9% and 3.4-4.2 for double MSM lap-jointed tape, respectively. These improvements are to be due to better interconnection between filaments of two tapes.

  • PDF

High-$T_c$ 2nd-order SQUID Gradiometer for Use in Unshielded Environments (비차폐 환경에서의 고온초전도 SQUID 2차 미분기의 특성연구)

  • 박승문;강찬석;이순걸;유권규;김인선;박용기
    • Progress in Superconductivity
    • /
    • v.5 no.1
    • /
    • pp.50-54
    • /
    • 2003
  • We have fabricated $∂^2$$B_{z}$ /$∂x^2$ type planar gradiometers and studied their properties in operation under various field conditions. $YBa_2$$Cu_3$$O_{7}$ film was deposited on $SrTiO_3$ (100) substrate by a pulsed laser deposition (PLD) system and patterned into a device by the photolithography with ion milling technique. The device consists of 3 pickup loops designed symmetrically Inner dimension and the width of the square side loops are 3.6 mm and 1.2 mm, respectively, and the corresponding dimensions of the center loop are 2.0 mm and 1.13 mm. The length of baseline gradiometer is 5.8 mm. Step-edge junction width is 3.0 $\mu\textrm{m}$ and the hole size of the SQUID loop is 3 $\mu\textrm{m}$ ${\times}$ 52 $\mu\textrm{m}$. The SQUID inductance is estimated to be 35 pH. The device was formed on a 20 mm ${\times}$ 10 mm substrate. We have tested the behavior of the device in various field conditions. The unshielded gradiometer was stable under extremely hostile conditions on a laboratory bench. Noise level 0.45 pT/$\textrm{cm}^2$/(equation omitted)Hz and 0.84 pT/$\textrm{cm}^2$/(equation omitted)Hz at 1 Hz for the shielded and the unshielded cases, which correspond to equivalent field noises of 150 fT/(equation omitted)Hz and 280 fT/(equation omitted)Hz, respectively. In spite of the short baseline of 5.8 mm, the high common-mode-rejection-ratio of the gradiometer, $10^3$, allowed us to successfully record magnetocardiogram of a human subject, which demonstrates the feasibility of the design in biomagnetic studies.

  • PDF

Influence of Milling Condition on the Phase Formation and Jc of Ag/Bi 2223 Superconducting Tapes (분말의 분쇄조건이 Ag/Bi-2223 초전도 선재의 상전이와 임계전류 밀도에 미치는 영향)

  • Kim, Won-Ju;Yu, Jae;Lee, Hui-Gyun;Hong, Gye-Won
    • Korean Journal of Materials Research
    • /
    • v.7 no.2
    • /
    • pp.140-144
    • /
    • 1997
  • The effects of the particle size of precursor powder on the microstructure and Jc of Ag-sheathed Ri-2223 tapes were investigated. The calcined powder with overall composition of $Bi_{1-89}Pb_{0-41}Sr_{2-01}Ca_{2-23}Cu_{3-03}O_{y}$ was milled for various times using planetary ball mill. The transport property of the tapes were found to depend strongly on the particle size of the precursor powder Enhanced reactivity of the milled powder facilitated the formation of 2223 phase and resulted in an increase of Jc. Excessive milling, however, led to the amorphisation of the powder and degraded the electrical property of the tapes.

  • PDF

The electrical and structual characteristics of BSCCO film by MOD method (MOD법을 제작된 BSCCO 고온초전도체의 구조적 전기적 특성)

  • Kim, Sun-Mi;Yoon, Soon-Il;Park, Mi-Hwa;Lee, Kie-Jin;Cha, Deok-Joon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07a
    • /
    • pp.553-556
    • /
    • 2003
  • 금속유기물 용액 증착법(MOD)법은 금속유기물 용액을 스핀 코팅하여 고온 열처리를 통해 대면적의 고온 초전도 박막을 만들 수 있으며, 고가의 진공 시스템이 필요하지 않기 때문에 매우 경제적인 박막 증착 방법이다. 본 연구에서는 MOD법을 이용해서 고온초전도체 마이크로파 필터나 터널접합 소자와 같은 전자 소자 응용 연구를 위해 요구되는 높은 임계전류 특성을 갖도록 박막 성장 조건을 변화시켜서 제작된 고온 초전도체 Bi2Sr2CaCu2O8+d (BSCCO2212) 박막을 제작하였다. 박막 특성은 x-ray diffraction (XRD), scanning electron microscope (SEM)으로 표면적, 구조적 특성을 관찰하고 저항-온도 (R-T) 변화 및 전류-전압 (I-V) 특성 측정을 통해 전기적 특성을 연구하여 임계전류를 향상 시킬 수 있는 박막제작 조건에 관해 논의하였다.

  • PDF

Superconducting Joint of Multi-filament BSCCO(2223) Tapes by using Single-filament Tape (BSCCO(2223) 단심 초전도 선재를 이용한 다심 초전도 선재의 접합공정 연구)

  • 김규태;김정호;장석헌;주진호;강형구;고태국;하홍수;오상수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.10
    • /
    • pp.923-930
    • /
    • 2003
  • We jointed Bi(Pb)-Sr-Ca-Cu-O multifilament tapes and evaluated their electrical and mechanical properties. In order to improve connectivity of multifilaments, one or two single-filament tape was inserted between two multifilament tapes. The critical current ratio(CCR) and n-value of the jointed tapes were evaluated as a function of uniaxial pressure. It was observed that critical current ratio and n-value were 24.8-29.0% and 2.5-2.8 for MM lap-jointed tape. On the other hand, the corresponding values were improved to 24.7-53.9% and 3.1-4.2 for MSM jointed tape, and 63.4-76.0% and 3.4-5.1 for double MS:vr lap-jointed tape, respectively. The highest electrical properties of double MSM lap-jointed tape are considered to be owing to the presence of single core, causing better interconnections of multifilaments between the two tapes. The mechanical property of jointed tape was evaluated and correlated to the microstructural evolution. The strength of jointed tapes was 44-64% less than that of the unjoined tape. The strain tolerance of jointed tape was also reduced compared to that of the unjoined tape. These lower mechanical properties of jointed tape are probably due to the induced nonuniform microstructure such as the existence of cracks and Ag-intrusion in the joined region.

A Study on the Fabrication of Superconductor Using Pyrolysis Methods for Electric power Machinery (열분해법에 의한 전력기기용 초전도 합성 기술에 관한 연구)

  • Lee, Sang-Heon;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.11a
    • /
    • pp.153-154
    • /
    • 2005
  • A high Tc superconducting with a nominal composition of $Bi_2Sr_2Ca_2Cu_3O_Y$ was prepared by the citarte method. The solid precursor produced by the dehydration of the gel at 120$^{\circ}C$ for 12h is not in the amorphous state as expected but in a crystalline state. X-ray diffraction peaks of nearly the same angular position as the peaks of high Tc phase were observed in the precursor. After pyrolysis at 400$^{\circ}C$ and calcination at 840$^{\circ}C$ for 4h, the (001)peak of the high Tc phase was cleary observed. Experimental results suggest that the intermediate phase formed before the formation of the superconducting phase may be the most important factro in determining whether it is easy to form the high Tc phase or not, because the nucleation barriers of the two superconducting phase may be altered by the variation of the crystal structures of those intermediate phase.