• 제목/요약/키워드: pore ratio

검색결과 779건 처리시간 0.028초

Hebei Spirit호 유류유출 사고 이후 태안 양식어장에서 잔존유류의 농도 변화 (Variation in the Residual Oils in the Culture Grounds on the Taean Coast, Korea after the Hebei Spirit Oil Spill)

  • 김형철;이완석;황운기;최용석
    • 한국수산과학회지
    • /
    • 제43권6호
    • /
    • pp.705-714
    • /
    • 2010
  • The residual oil concentrations in seawater and sediments were investigated along the Taean coast of Korea, following the Hebei Spirit oil spill, which occurred on 7 December 2007. The oil concentration in seawater ranged from 0.059 to $0.866\;{\mu}g/L$ for the tidal flat culture grounds and from 0.016 to $0.943\;{\mu}g/L$ in the fish cage areas in 2008. These were dominated by the seawater temperature relationship. Polycyclic aromatic hydrocarbons (PAHs) in sediments were also analyzed and the concentrations ranged from 3.4 to 509.7 ng/g dry weight. The average PAH level was higher in seawater from the Sinduri area than the Padori area, while the average PAH level in sediments was higher in Padori. The diagnostic ratio of PAHs was investigated to determine the origins of the PAHs. The PAHs in the Seongam area, which was not affected by the oil spill, are of pyrolytic origin, while the PAHs in Padori and Sinduri were of petrogenic origin. The residual oils in the areas affected by the oil spill tended to decrease over time, except in summer. The oils in pore water remained 6- to 16-fold higher, as compared to the seawater overlying the tidal flat, implying that residual oils will continue to influence the affected region for the foreseeable future.

슬래그 미분말 혼합 콘크리트의 공극구조와 염화물 확산계수와의 관계에 대한 실험적 연구 (An Experimental Study on Relation between Chloride Diffusivity and Microstructural Characteristics for GGBS Concrete)

  • 김태상;정상화;최영철;송하원
    • 콘크리트학회논문집
    • /
    • 제21권5호
    • /
    • pp.639-647
    • /
    • 2009
  • 바닷물에 의한 염해와 동결융해 환경에 노출된 철근 콘크리트구조물의 내구성을 평가하기 위해서는 콘크리트의 미세구조적 특성 및 염화물 침투성에 대한 콘크리트의 확산 저항성을 동시에 분석하는 것이 중요하다. 이 연구에서는 고로슬래그 미분말(GGBS)을 혼합한 콘크리트에 대하여 수은압입법(MIP)에 의해 얻어진 콘크리트의 미세공극 구조와 장기 및 단기 재령의 염화물 확산성과의 상관성에 대하여 연구하였다. 물시멘트비는 40, 45, 50%로 변화시키고, 단위시멘트량을 300, 350, 400, 450 kg/$m^3$으로 변화시킨 OPC 및 GGBS 콘크리트 시편에 대하여 동결융해에 의해 손상된 GGBS 콘크리트에서의 확산성과 미세구조의 변화를 관찰하였다.

Closed chamber를 이용한 토양 N2O 배출량과 주요 토양 인자들과의 상관성 (The Relevance of Soil N2O Emissions Measured by a Closed Chamber Technique on the Physico-chemical Soil Parameters)

  • 김득수;오진만
    • 한국대기환경학회지
    • /
    • 제20권6호
    • /
    • pp.749-758
    • /
    • 2004
  • Nitrous oxide ($N_2$O) has been known as an important trace gas due to the greenhouse gas and the major source of stratospheric oxide of nitrogen (NO). Soil is the major source of $N_2$O in nature. The physicochemical characteristics of soils affect the emission of $N_2$O from soil. These physicochemical parameters are soil moisture, soil temperature, and soil N content. Since these parameters are correlated to the flux of $N_2$O from soil individually and compositely, there still remain many unknowns in the mechanism to produce $N_2$O in soil and the roles of such physicochemical parameters which affect the soil $N_2$O emission. Soil $N_2$O fluxes were measured at different levels in water filled pore space (WFPS), soil temperature and soil N contents from the same amounts of soils which were sampled from agriculturally managed upland field in a depth of ~30 cm at Kunsan. The soil $N_2$O flux measurements were conducted in a laboratory with a closed flux chamber system. The optimum soil moisture and soil temperature were observed at 60% of WFPS and ~13$^{\circ}C$. The soil $N_2$O flux increased as soil N contents increases during the whole experimental hours (up to 48 hours). However, average $N_2$O flux decreased after ~30 hours when organic carbon was mixed with nitrogen in the sample soils. It is suggested that organic carbon could be important for the emission of $N_2$O, and that the ratio of N to C needs to be identified in the process of $N_2$O soil emission.

유기용제 측정용 흡착관 개발을 위한 AC 및 ACF의 흡착특성 (Desorption characteristics of Activated Carbon and Activated Carbon Fiber by Development of Sorbent Tube for Measurement of Organic Solvent)

  • 원정일;김기환;신창섭
    • 환경위생공학
    • /
    • 제17권3호
    • /
    • pp.99-109
    • /
    • 2002
  • Charcoal $tube/CS_2$ method are more popularly used than any other in the measurement of the working environment for the exposure evaluation of organic solvent, but it is some weak points that the lower accuracy can be obtained on the polar materials and within the range of the low concentration. Thus solvent desorption method has been developed to make accuracy higher and to overcome some weak points. However, because of high price of adsorption tube for thermal desorption and the short of study on its application to the working environment, it is not popularly used in the domestic industrial hygiene fields. This dissertation aims to develop thermal desorption and adsorption tubes for measuring organic solvents in the working environment, by comparing and analyzing breakthrough condition and adsorption capacity with ACF. Specific surface area of ACF used in this study is wider than the one of AC and micropore of ACF related with adsorption has been developed, and adsorption velocity and adsorption amount are very excellent by linking a pore of surface and an inside well into micropore. 1. Result of analysis on physical characteristics of adsorbent, the specific surface area of ACF was 1.3 times higher than that of AC. Distribution ratio of micropore related to adsorption was 94% on ACF and AC. Result of SEM, micropore of the AC is opened to the surface. In contrast, ACF shows that extremely fast adsorption speed. Because of micropore are exposed on the surface and penetrate through each other. 2. Breakthrough characteristics of adsorbents was not different from slop of breakthrough curve. The effluent concentration reaches 10% of initial concentration($C_{out}/C_{in}=0.1$, break point) of ACF was 30~316min longer than that of AC. Therefore, the adsorption capacities of ACF was 1.1~4.6 times higher than that of AC. ACF can be used as a proper adsorbent for measurement of organic solvent.

침질침탄시 화합물층의 성장에 따른 표면조도 변화에 관한 연구 (Studies on the Evolution of the Surface Roughness with Development of Surface Compound Layer in Salt Bath Nitrocarburising (Tufftride))

  • 송경석;문경일;김성완
    • 열처리공학회지
    • /
    • 제16권5호
    • /
    • pp.253-259
    • /
    • 2003
  • In this study, to find out the reason of deterioration in surface roughness of steel and cast iron after Tufftride, it has been investigated on the relation between the surface roughness and various factors such as the evolution of compound layer, surface morphology, and surface hardness, and change of pore ratio in the compound layer during Tufftride at $580^{\circ}C$. It is found that the surface roughness was increased with the evolution of compound layer during Tufftride of steel and cast iron. The change of surface roughness after Tufftride was reduced with decreasing tho content of carbon and cementite ($Fe_3C$) in the materials. in the cast irons, the various shaped graphites that was exposed to the surface should induce the discontinuous growth of the compound layer, and this resulted in the incoherent interfaces between matrix and compound layer and the deterioration of surface roughness. In the steels, the existence of cementites in the matrix resulted in the incoherent interfaces between matrix and compound layer. It is considered that during Tufftride the surface roughness must be mainly influenced by the formation of the incoherent interface between compound layer and matrix that is affected by some factors such as the microstructure, the composition, and the hardness of the matrix.

석회 처리에 의한 오염 퇴적물 내 중금속의 형태 변화 및 용출 가능성 (Chemical Forms and Release Potential of Heavy Metals from the Lime Treated Sediments)

  • 박길옥;전상호
    • 생태와환경
    • /
    • 제41권2호
    • /
    • pp.166-173
    • /
    • 2008
  • 오염물질을 제거하기 위한 방법 중 하나인 석회 처리를 통하여 청초호 표층 퇴적물에 함유된 중금속의 존재 형태 변화와 환경변화시 수층으로의 용출가능성을 알아보았다. 연속추출 방법을 사용하여 중금속의 화학적 형태를 분석하였고 수층으로의 용출 가능성은 흡착된 형태와 공침된 형태의 합으로 하였다. 석회 처리 전의 청초호 퇴적물에 함유된 Cd과 Cu 및 Zn의 존재형태는 호수 바닥과 같은 혐기성 상태에서 안정된 산화성 형태가 많았으나 석회 처리 시료에서는 이 부분의 비율이 줄어든 반면 용출되기 쉬운 부분인 흡착된 형태와 공침된 형태의 비율이 증가하였다. 이는 석회 첨가로 인한 공극수의 pH상승과 대기중에 노출로 인한 산화에 의한 것으로 판단된다. 수층으로 이동 가능한 부분의 비율은 Cd의 경우 석회함량 15%, Pb은 10%, Cu와 Zn은 20%에서 높게 나타나 중금속으로 오염된 퇴적물의 석회 처리는 퇴적물에 함유된 중금속의 용출을 증가시킬 가능성이 있는 것으로 사료된다.

배가스 중 SO2가 V/TiO2 SCR활성에 미치는 영향 (The Effect of SO2 in Flue Gas on the SCR Activity of V/TiO2)

  • 홍성창
    • 공업화학
    • /
    • 제17권5호
    • /
    • pp.490-497
    • /
    • 2006
  • $V_{2}O_{5}$/$TiO_{2}$계 선택적촉매환원법(SCR) 촉매는 $SO_{2}$가 존재하는 조건에서 $SO_{2}$의 산화 및 암모니아의 반응에 의해 형성된 황산암모늄염으로 인해 촉매는 비활성화될 수 있다. 본 연구에 의하면, $SO_{2}$에 의한 촉매의 비활성화는 $SO_{2}$의 흡착이후 $SO_{3}$로의 산화 정도에 의존한다. $SO_{2}$의 산화는 배가스 내의 산소 농도에 약하게 영향을 받으며 바나듐 함량에 영향을 받는다. 또한 미반응 암모니아 역시 황산암모늄염 형성의 원인이므로 SCR 반응에 있어서 암모니아 투입비율에 대한 영향을 도출하였다. 황산암모늄염에 의해 비활성화된 촉매가 낮은 SCR 활성을 갖는 이유를 촉매의 기공부피 변화에서 찾을 수 있다. 이러한 황산암모늄염의 분해 반응도출을 위해 TPD (Temperature Programmed Decomposition) 실험이 수행되었다.

CNT 첨가량에 따른 시멘트의 역학성능 및 미세구조의 영향 (Effects of CNT Additions on Mechanical Properties and Microstructures of Cement)

  • 오성우;오경석;정상화;정원석;유성원
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제21권6호
    • /
    • pp.162-168
    • /
    • 2017
  • 탄소나노튜브는 고강도, 고내구성 콘크리트의 생산을 위한 새로운 재료 중 하나로 여겨지며, 많은 연구자들에 의하여 연구되고 있다. 탁월한 열전도도는 향후 자가발열 콘크리트의 개발에 필수적이며, 이 연구에서는 다양한 목적을 갖는 콘크리트의 개발을 위한 역학적 특성 및 미세구조 분석을 실시하였다. CNT 첨가량은 시멘트 중량대비 0.115, 0.23, 0.46wt%로 하였다. 압축강도/휨강도 시험은 재령 3, 7, 28일에 실시하였으며, 공극률은 MIP 시험을 통해 실시하였다. CNT 분산성 및 수화생성물 분석을 위하여, SEM 분석 및 열분석을 실시하였다. 그 결과, CNT 첨가에 따른 역학성능은 다소 감소하는 경향을 나타내었으나, 0.115wt% 첨가한 경우 플레인 배합과 동등 수준의 결과를 확인할 수 있었다. 향후, 기존 콘크리트와 동일한 역학성능을 보유한 CNT 첨가 배합의 개발을 통한 발열성능 확보가 가능할 것으로 기대된다.

공극구조 및 하중조건에 따른 콘크리트의 초음파 속도 모델링 (Modeling on Ultrasonic Velocity in Concrete Considering Micro Pore Structure and Loading Conditions)

  • 김윤용;오광진;박기태;권성준
    • 한국콘텐츠학회논문지
    • /
    • 제15권3호
    • /
    • pp.415-426
    • /
    • 2015
  • 초음파 속도를 이용한 콘크리트의 건전성 및 강도평가는 오랫동안 사용되어 왔으며, 현장조사에서 필수적이다. 콘크리트 내부의 공극률은 내구성 및 강도를 평가할 수 있는 주요인자이며, 초음파 진행에 방해가 되므로 공극률 변화에 따라 초음파 속도변화가 발생한다. 본 연구에서는 기존의 공극률 모델을 이용하여 콘크리트 내부를 통과하는 초음파 속도 모델링을 수행하였으며 실험값과의 비교하였다. 또한 인장 및 압축 재하 시험과 동시에 초음파 속도를 측정하여 재하 하중비를 이용한 모델링을 수행하였다. 압축영역에서는 하중재하비 50% 수준까지 초음파 속도가 약간 증가하였으며, 최대하중에 근접할수록 급격한 속도의 감소가 발생하였다. 인장영역에서는 압축영역과 다르게 초기부터 초음파 속도가 상당히 변화하였다. 제안된 기법은 콘크리트의 건전부 및 압축영역에서는 합리적인 결과를 보이고 있으며 인장영역에서는 미세균열 및 국소적인 골재치합을 고려한 보완이 필요할 것으로 판단된다.

준설점토 활용 경량혼합토의 연약지반개량공법 수치해석 (Numerical Analysis of Light-weight Air Foamed Soils using Dredged Marine Clay for Soft Ground Improvement Method)

  • 윤길림;김선빈
    • 한국지반환경공학회 논문집
    • /
    • 제15권3호
    • /
    • pp.5-13
    • /
    • 2014
  • 본 논문에서는 준설토를 활용한 경량혼합토(LWFS)의 연약지반개량 적용성에 대해 검토한 내용을 다루었다. 현재까지 제시된 경량혼합토의 공학적 특성에 관한 연구결과를 종합 분석하여 경량혼합토의 물성을 정리하였으며, 그 결과를 토대로 임의의 현장조건을 가정하여 경량혼합토공법과 SCP 공법 및 DCM 공법 적용 시에 대한 3차원 수치해석을 수행하였다. 연약지반개량공법 비교해석 결과, 경량혼합토 공법을 적용하는 경우 SCP 공법을 적용하는 수준 이상의 침하관리가 가능하며, 경량혼합토의 목표성능에 따라 침하발생 수준을 조절할 수 있는 것으로 검토되었다. 또한 DCM 공법과 비교 시 경량혼합토 재료의 경량성으로 과잉간극수압 발생량이 현저히 작아져 잔류침하를 최소화할 수 있는 것으로 검토되었다.