• Title/Summary/Keyword: magnetic nano-particle

Search Result 78, Processing Time 0.027 seconds

Crystallographic and Magnetic Properties of Nickel Substituted Manganese Ferrites Synthesized by Sol-gel Method

  • Chae, Kwang Pyo;Choi, Won Oak;Lee, Jae-Gwang;Kang, Byung-Sub;Choi, Seung Han
    • Journal of Magnetics
    • /
    • v.18 no.1
    • /
    • pp.21-25
    • /
    • 2013
  • Nickel substituted manganese ferrites, $Mn_{1-x}Ni_xFe_2O_4$ ($0.0{\leq}x{\leq}0.6$), were fabricated by sol-gel method. The effects of sintering and substitution on their crystallographic and magnetic properties were studied. X-ray diffractometry of $Mn_{0.6}Ni_{0.4}Fe_2O_4$ ferrite sintered above 523 K indicated a spinel structure; particles increased in size with hotter sintering. The M$\ddot{o}$ssbauer spectrum of this ferrite sintered at 523 K could be fitted as a single quadrupole doublet, indicative of a superparamagnetic phase. Sintering at 573 K led to spectrum fitted as the superposition of two Zeeman sextets and a single quadrupole doublet, indicating both ferrimagnetic and paramagnetic phase. Sintering at 673 K and at 773 K led to spectra fitted as two Zeeman sextets due to a ferrimagnetic phase. The saturation magnetization and the coercivity of $Mn_{0.6}Ni_{0.4}Fe_2O_4$ ferrite sintered at 773 K were 53.05 emu/g and 142.08 Oe. In $Mn_{1-x}Ni_xFe_2O_4$ ($0.0{\leq}x{\leq}0.6$) ferrites, sintering of any composition at 773 K led to a single spinel structure. Increased Ni substitution decreased the ferrites' lattice constants and increased their particle sizes. The M$\ddot{o}$ssbauer spectra could be fitted as the superposition of two Zeeman sextets due to the tetrahedral and the octahedral sites of the $Fe^{3+}$ ions. The variations of saturation magnetization and coercivity with changing Ni content could be explained using the changes of particle size.

A Magnetization Study of Prussian-blue Analogue NaxMny[Fe(CN)6]

  • Minh, Nguyen Van;Phu, Phung Kim;Thuan, Nguyen Minh;Yang, In-Sang
    • Journal of Magnetics
    • /
    • v.13 no.4
    • /
    • pp.149-152
    • /
    • 2008
  • In this report, we present the results of a study on the effects of the particle size on the properties of the Prussian blue (PB) analog $Na_xMn_y[Fe(CN){_6}]$. A novel synthesis method of the $Na_xMn_y[Fe(CN){_6}]$ nano-particles using an organic solvent, formamide, is employed. The size of the PB particles is found to be 100-150 nm for the samples prepared in the formamide solvent, which is much smaller than that of the samples prepared using water only. The broadening of the X-ray diffraction peaks of the nano-sized PB samples is attributed to the lattice disorder and a dramatic reduction in the particle size. The compositions of the samples are confirmed by an energy-dispersive X-ray analysis (EDAX), and the result proves that the samples are actually $Na_xMn_y[Fe(CN){_6}]$ Prussian blue. The UV-vis spectra show a broad intervalence charge-transfer (CT) band in the visible region between 400 and 700 nm, and the absorption decreases abruptly in the green region for the nano-sized PB sample. A divergence between the field cooled (FC) and zero field cooled (ZFC) magnetization curves is observed for the nano-sized PB sample at 11 K, indicating that nanoparticles in the sample are single domain superparamagnets with a blocking temperature of 11 K. Our results reveal that the nano-sized PB samples show significantly different optical and magnetic properties than those of the bulk PB samples.

Micromagnetism (미세자기학)

  • Yu, Yong-Jae
    • 한국지구물리탐사학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.107-109
    • /
    • 2009
  • Micromagnetism explores magnetic configurations in nano-scales to visualize the details of magnetic domain structures, and also can produce snapshots of complex remanence or other magnetic states. The particle shape has a profound effect on the magnetic hysteresis. For instance, octahedral magnetite showed higher coercivity and squareness than cubic magnetite.

  • PDF

Effect of annealing on the magnetic behavior and microstructures of spherical NiZn ferrite particle prepared by ultrasonic spray pyrolysis

  • Nam, Joong-Hee
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.1
    • /
    • pp.11-17
    • /
    • 2007
  • The spherical NiZn ferrite particles were prepared by ultrasonic spray pyrolysis with mixed solution of aqueous metal nitrates. The NiZn ferrite particle was observed with nano-sized primary particles of about 10 nm or less before annealing which represented as paramagnetic behavior measured at 77 K and room temperature. The typical abnormal growth of primary particles like polyhedral primary particles was observed by annealing at 1273 K with Zn-concentration dependency. The XRD patterns showed good crystallinity of NiZn ferrite powder after annealing. In annealing process, the intra-particle sintering phenomenon was observed and the spherical particle morphology was collapsed at 1673 K. The saturation magnetization of NiZn ferrite powder for each annealing temperature was decreased with measuring temperature of $77{\sim}$300K.

Recycling of Sintered Nd-Fe-B Magnets Doped with PrNd Nanoparticles

  • Zhang, Xuefeng;Liu, Fei;Liu, Yanli;Ma, Qiang;Li, Yongfeng;Zhao, Qian;Wang, Gaofeng;Li, Zhubai
    • Journal of Magnetics
    • /
    • v.20 no.2
    • /
    • pp.97-102
    • /
    • 2015
  • The waste of sintered Nd-Fe-B magnets was recycled using the method of dopingPrNd nanoparticles. The effect of PrNd nanoparticle doping on the magnetic properties of the regenerated magnets has been studied. As the content of the PrNd nanoparticles increases, the coercivity increases monotonically, whereas both the remanence and the maximum energy products reach the maximum values for 4 wt% PrNd doping. Microstructural observation reveals that the appropriate addition of PrNd nanoparticles improves the magnetic properties and refines the grain. Domain investigation shows that the self-pinning effect of the rare earth (Re)-rich phase is enhanced by PrNd nano-particle doping. Compared to the magnet with 4 wt% PrNd alloy prepared using the dual-alloy method, the regenerated magnet doped with the same number of PrNd nanoparticles exhibits better magnetic properties and a more homogeneous microstructure. Therefore, it is concluded that PrNd nanoparticle doping is an efficient method for recycling the leftover scraps of Nd-Fe-B magnets.

Effect of Disk Rotational Speed on Contamination Nano Particles Generated in a Hard Disk Drive (하드 디스크 드라이브 회전수 변화가 드라이브 내 나노 오염 입자 발생에 미치는 영향)

  • Lee, Dae-Young;Hwang, Jung-Ho;Bae, Gwi-Nam
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.28 no.8 s.227
    • /
    • pp.976-983
    • /
    • 2004
  • In high-density hard disk drives, the slider should be made to fly close to the magnetic recording disk to generate better signal resolution and at an increasingly high velocity to achieve better data rate. The slider disk interaction in CSS (contact-start-stop) mode is an important source of particle generation. Contamination particles in the hard disk drive can cause serious problems including slider crash and thermal asperities. We investigated the number and the sizes of particles generated in the hard disk drive, operating at increasing disk rotational speeds, in the CSS mode. CNC (condensation nucleus counter) and PSS (particle size selector) were used for this investigation. In addition, we examined the particle components by using SEM (scanning electron microscopes), AES (auger electron spectroscopy), and TOF-SIMS (time of flight-secondary ions mass spectrometry). The increasing disk rotational speed directly affected the particle generation by slider disk interaction. The number of particles that were generated increased with the disk rotational speed. The particle generation rate increased rapidly at motor speeds above 8000 rpm. This increase may be due to the increased slider disk interaction. Particle sizes ranged from 14 to 200 nm. The particles generated by slider disk interaction came from the lubricant on the disk, coating layer of the disk, and also slider surface.

The Variation of Packing Density According to Powder Size Distribution and Epoxy Resin in Soft Magnetic Composite (연자성 복합체에서 파우더 크기 분포와 Epoxy Resin에 따른 Packing Density 변화)

  • Lee, Chang Hyun;Oh, Sea Moon;Shin, Hyo Soon;Yeo, Dong Hun;Kim, Jin Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.12
    • /
    • pp.782-787
    • /
    • 2017
  • There is growing interest in power inductors in which metal soft magnetic powder and epoxy resin are combined. In this field, the process technology for increasing the packing density of magnetic particles in an injection molding process is very important. However, little research has been reported in this regard. In order to improve the packing density, we investigated and compared the sedimentation heights of pastes for three types of soft magnetic alloy powders as a function of the mixing ratios and the type of resin used. Experimental results showed that the packing density was the highest (71.74%) when the mixing ratio was 80 : 16 : 4 (Sendust : Fe-S : CIP) according to the particle size using an SE-4125 resin. In addition, the packing density was found to be inversely related to the layer separation distance. As a result, it was confirmed that the dispersion of solid particles in the paste was important for curing; however, the duration of the curing process can greatly affect the packing density of the final composite.

Nickel Substitution Effects on Nano-sized Co, Mn and MnZn Ferrites Synthesized by Sol-gel Method

  • Choi, Won-Ok;Kwon, Woo Hyun;Chae, Kwang Pyo;Lee, Young Bae
    • Journal of Magnetics
    • /
    • v.21 no.1
    • /
    • pp.40-45
    • /
    • 2016
  • Nickel substituted nano-sized ferrite powders, $Co_{1-x}Ni_xFe_2O_4$, $Mn_{1-x}Ni_xFe_2O_4$ and $Mn_{1-2x}Zn_xNi_xFe_2O_4$ ($0.0{\leq}x{\leq}0.2$), were fabricated using a sol-gel method, and their crystallographic and magnetic properties were subsequently compared. The lattice constants decreased as quantity of nickel substitution increased, while the particle size decreased in $Co_{1-x}Ni_xFe_2O_4$ ferrite but increased for the $Mn_{1-x}Ni_xFe_2O_4$ and $Mn_{1-2x}Zn_xNi_xFe_2O_4$ ferrites. For the $Co_{1-x}Ni_xFe_2O_4$ and $Mn_{1-x}Ni_xFe_2O_4$ ($0.0{\leq}x{\leq}0.2$) ferrite powders, the $M{\ddot{o}}ssbauer$ spectra could be fitted as the superposition of two Zeeman sextets due to the tetrahedral and octahedral sites of the $Fe^{3+}$ ions. However, the $M{\ddot{o}}ssbauer$ spectrum of $Mn_{0.8}Zn_{0.1}Ni_{0.1}Fe_2O_4$ consisted of two Zeeman sextets and one single quadrupole doublet due to the ferrimagnetic and paramagnetic behavior. The area ratio of the $M{\ddot{o}}ssbauer$ spectra could be used to determine the cation distribution equation, and we also explain the variation in the $M{\ddot{o}}ssbauer$ parameters by using this cation distribution equation, the superexchange interaction and the particle size. The saturation magnetization decreased in the $Co_{1-x}Ni_xFe_2O_4$ and $Mn_{1-2x}Zn_xNi_xFe_2O_4$ ferrites but increased in the $Mn_{1-x}Ni_xFe_2O_4$ ferrite with nickel substitution. The coercivity decreased in the $Co_{1-x}Ni_xFe_2O_4$ and $Mn_{1-2x}Zn_xNi_xFe_2O_4$ ferrites but increased in the $Mn_{1-x}Ni_xFe_2O_4$ ferrite with nickel substitution. These variations could thus be explained by using the site distribution equations, particle sizes and spin magnetic moments of the substituted ions.

Densification of $TiO_2$+Ti powder by Magnetic Pulsed Compaction (자기펄스 성형법에 의한 $TiO_2$+Ti 혼합 분말의 치밀화 거동)

  • Park, J.S.;Kim, H.S.;Lee, J.G.;Rhee, C.K.;Hong, S.J.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.394-397
    • /
    • 2008
  • In this research, the fine-structure TiO2+Ti bulks have been fabricated by the combined application of magnetic pulsed compaction (MPC) and subsequent sintering, and their densification behavior was investigated. The obtained density of $TiO_2$+Ti bulk prepared by the combined processes was increased with increasing MPC pressure from 0.7 to 1.7 GPa. Relatively higher density (88%) in the MPCed specimen at 0.7Gpa was attributed to the decreasing of the inter-particle distance of pre-compacted component. High pressure and rapid compaction by Magnetic Pulsed Compaction could reduce shrinkage rate (about 10%) of the sintered bulks compared to that of general processing (about 20%). Mixing conditions of PVA, water, Ti and $TiO_2$ nano powder for compaction of $TiO_2$ nano powder did not affect on density and shrinkage of the sintered bulks due to high pressure of MPC.

  • PDF

Removal of Aqueous Cr(VI) using Magnetite Nanoparticles Synthesized from a Low Grade Iron Ore

  • Do, Thi May;Suh, Yong Jae
    • Particle and aerosol research
    • /
    • v.9 no.4
    • /
    • pp.221-230
    • /
    • 2013
  • We demonstrated the efficacy of magnetic nanoparticles (MNPs) produced from a low grade iron ore as an adsorbent for the removal of Cr(VI), a toxic heavy metal anion present in wastewater. The adsorption of Cr(VI) by these MNPs strongly depended on the dosage of MNPs, the initial concentration of the Cr(VI) solutions, and pH. The highest Cr(VI) adsorption efficiency of 22.0 mg/g was observed at pH 2.5. The adsorption data were best fit with the Langmuir isotherm and corresponded to a pseudo-second-order kinetic model. The used adsorbent was regenerated by eluting in highly alkaline solutions. Sodium bicarbonate showed the highest desorption efficiency of 83.1% among various eluents including NaOH, $Na_2HPO_4$, and $Na_2CO_3$. Due to the high adsorption capacity, the simple magnetic separation, and the high desorption efficiency, this nano-adsorbent produced from inexpensive and abundant resources may attract the attention of the industries to apply for removing various metal anionic contaminants from wastewater.