Search Result 94, Processing Time 0.022 seconds

Performance Evaluation for Bending Strength and Tensile Type Shear Strength of GFRP Reinforced Laminated Wooden Pin (GFRP보강적층목재핀의 휨강도 및 인장형 전단내력 성능평가)

  • Song, Yo-Jin;Jung, Hong-Ju;Kim, Dae-Gil;Kim, Sang-Il;Hong, Soon-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.3
    • /
    • pp.258-265
    • /
    • 2014
  • By replacing the previous metal connector on the joints of timber structure, the GFRP reinforced laminated wooden pin was produced using a wooden material and Glass fiber reinforced plastic(GFRP) composite laminate. In addition, using the reinforced wooden pin, the tensile type shear strength test was conducted. Based on the result of the bending strength test of the reinforced laminated wooden pin according to the GFRP arrangement, a specimen(Type-A) with a single insertion of GFRP for each layer have shown the most favorable performance. Also, it was verified that densified specimen hot pressed for an hour at the temperature of $150^{\circ}C$ and with the oppression pressure $1.96N/mm^2$ have shown the improved performance of 1.57 times than the specimen without the densification. And in the bending strength test considering the load direction, edgewise have shown a higher performance of 3.51 times than the flatwise. A shear strength test was conducted using the Type-A reinforced laminated wooden pin which have shown a moderate performance on the test. Based on the test conducted by differentiating the type of the joint plate and the connector, compared to the specimen(Type-DS) applied with the drift pin and steel plate, the specimen( Type-WL) applied with the GFRP reinforced laminated wooden pin and GFRP reinforced wooden laminated plate have shown 1.12 times higher shear strength and also have shown an excellent toughness even after the maximum load.

Adhesive Performance and Fracture Toughness Evaluation of FRP-Reinforced Laminated Plate (FRP 보강적층판의 접착성능 및 파괴인성평가)

  • Jung, Hong-Ju;Hong, Soon-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • v.43 no.6
    • /
    • pp.868-875
    • /
    • 2015
  • In order to replace existing slit type steel plate on the wooden structure joint, the FRP-reinforced laminated plates were produced. Four types of FRP-reinforced laminated plates were produced according to the type of reinforcement and adhesive, and before applying to the joint, the adhesion performance test according to KSF 3021 and KSF 2160 and the Compact Tension (CT) type fracture toughness test specified in ASTM D5045-99 were carried out. As a result of adhesion performance test, all GFRP textile, GFRP sheet, and GFRP Textile-Sheet type FRP-reinforced laminated plates satisfied the requirement of soaking delamination percentage with smaller than 5% based on KS standard. However, aramid type specimen satisfied the standard as the soaking delamination percentage of 4.8% but it did not satisfied the standard as the water proof soaking delamination percentage of 70%. As a result of fracture toughness test, the volume ratio of reinforcement to timber became 23% so that the strength of FRP-reinforced laminated plates increased by two to four times in comparison to the control specimen. It was confirmed that the GFRP Textile-Sheet type specimen was most resistant to the fracture most since the ratio of stress intensity factor compared with that of the control increased to 61% owing to the parallel arrangement of glass fiber to the load. As a result of tensile shear strength test using FRP-reinforced laminated plates and nonmetal dowels, it is about 12% lower than metal connectors.

Challenges in High-rise Wooden Structures and the Seismic Design in Japan

  • Hiroyasu, Sakata;Yoshihiro, Yamazaki
    • International Journal of High-Rise Buildings
    • /
    • v.11 no.3
    • /
    • pp.171-180
    • /
    • 2022
  • Research and development on high-rise or large-scale wooden buildings have been actively conducted both domestically and internationally. The trend of high-rise wooden buildings is driven by increasing awareness of environmental issues. To utilize wooden materials in buildings is believed to lead to the reduction of the environmental impact. On the other hand, Japan is one of the most earthquake-prone countries in the world, and many wooden detached houses have been damaged in past major earthquakes. This paper summarizes the issues that arise in the realization of medium- and high-rise wooden buildings in Japan, and introduces the initiatives that have been seen so far.

A Study on the Block Shear Strength according to the Layer Composition of and Adhesive Type of Ply-Lam CLT (Ply-Lam CLT의 층재 구성 및 접착제 종류에 따른 블록전단강도에 관한 연구)

  • CHOI, Gyu Woong;YANG, Seung Min;LEE, Hyun Jae;KIM, Jun Ho;CHOI, Kwang Hyeon;KANG, Seog Goo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.6
    • /
    • pp.791-806
    • /
    • 2020
  • In this study, a block shear strength test was conducted to compare and analyze the strength and failure mode on the glued laminated timber, CLT, and Ply-lam CLT, which are mainly used for the construction of wood construction as engineering wood. Through this, the Ply-lam CLT manufacturing conditions for optimum production, such as the type of lamina, plywood, adhesive, and layer composition, were investigated. The results are as follow. Through block shear strength test, it showed high strength in the order of glued laminated timber, Ply-lam CLT and CLT. In particular, the shear strength of Ply-lam CLT, which is made of a composite structure of larch plywood and larch lamina, passed 7.1 N/㎟, which is a Korean industrial standards for block shear strength of structural glued laminated timber. In addition, in this study, there was no different in shear strength according to the adhesive type used for glulam, CLT, and Ply-lam CLT adhesion. However, in the case of Ply-lam CLT, the difference in shear strength of Ply-lam CLT was shown according to the type of lamina and plywood. The results showed high strength in the order of Larix kaempferi > Mixed light hardwood ≒ Pinus densiflora, sieb, et, Zucc plywood. The optimal configuration of Ply-lam CLT is when larch plywood and larch lamina are used, and it is decided that the adhesive can be used by selecting PRF and PUR according to the application. The results of block shear strength failure mode by type of wood based materials were analyzed. The failure mode showed shear parallel-to-grain for glulam, rolling shear for CLT, and shear parallel-to-grain and rolling for ply-lam CLT. This is closely related to shear strength results and is decided to indicate higher shear strength in Ply-lam CLT than in CLT due to rolling shear.

Evaluation of Shear Strength by Direction of Wood Grain for Korean Pine Using PRF Adhesive (페놀레조시놀공축합수지로 접착된 국산 잣나무의 목리방향별 전단성능평가)

  • Park, Sun-Hyang;Kim, Kwang-Mo;Pang, Sung-Jun;Kong, Jin Hyuk;Lee, Sang-Joon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.3
    • /
    • pp.243-249
    • /
    • 2017
  • This study was performed to find out the optimum adhesive conditions on manufacturing a cross-laminated timber (hereinafter CLT) with using domestic Korean Pine (Pinus koraiensis). The adhesive conditions including a applied amount of the glue and a Pressure are the one of the most important key factors on establishing CLT production process. The shear strength was examined with differing the adhesive conditions while using Phenol Resorcinol Formaldehyde Resin Adhesive (PRF resin). The optimum adhesive conditions was confirmed to be: glue spread of $250g/m^2$ and Pressure of 0.8 MPa respectively. The grain directions of glued specimens were also considered, perpendicularly bonded and parallelly bonded groups. Shear strength of the former group showed lower values than the latter group which is considered to be the effect of a rolling shear. Meanwhile the shear strength of both group satisfied the Korean Standard (KS F 3021) and the European Standard (EN 14080 and EN 16351). The results derived from this study can be used as the basic data for manufacturing the CLT with domestic Korean Pine. And additional researches for the other species including domestic Korean Larch and Pitch Pine is also now being performed.

Development of Pitch Pine Glued Laminated Timber for Structural Use -Improvement of Bending Capacity of Pitch Pine Glulam by Using Domestic Larch Laminars- (리기다소나무의 구조용 집성재 이용기술 개발 -낙엽송 층재와의 혼합 구성을 통한 집성재의 휨성능 향상-)

  • Kim, Kwang-Mo;Shim, Kug-Bo;Park, Joo-Saeng;Kim, Wun-Sub;Lim, Jin-Ah;Yeo, Hwanmyeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.35 no.6
    • /
    • pp.13-22
    • /
    • 2007
  • This study was carried out to scrutinize possibility of manufacturing pitch pine (Pinus rigida) glued laminated timber in order to add values of pitch pine trees. Also, it was investigated to improve bending performance of pitch pine glulam. Pitch pine was imported as one of major plantation species in Korean peninsula. Machine stress rated grades of pitch pine lumber mostly ranged between E7 and E9. which grades were more or less inferior to producing high quality glulam. However, the adhesive properties between pitch pine and pitch pine, and between pitch pine and Japanese larch (Larix kaempferi Carr.), such as shear bond strength, wood failure rate and de-lamination rate of bonded layer submerged in cold and boiling water, were higher than Korean Standard criteria. These properties are essential for manufacturing glulam with single species or multiple species. The modulus of rupture (MOR) of pitch pine glulam exceeded the criterion of Korean Standard for glulam strength grade but modulus of elasticity (MOE) was lower than the criterion. On the other hand, the bending performances (MOR and MOE) were improved 20 percent by mixing with Japanese larch laminar. It is effective to arrange higher quality Japanese larch laminar at the outer layer of glulam for improving bending performances. In conclusion, it is possible to use low quality pitch pine as laminar of structural glulam for adding values of pitch pine.

Development of Structural Glued Laminated Timber with Domestic Cedar (국산 삼나무를 이용한 구조용 집성재 이용기술)

  • Kim, Kwang-Mo;Shim, Sang-Ro;Shim, Kug-Bo;Park, Joo-Saeng;Kim, Wun-Sub;Kim, Byoung-Nam;Yeo, Hwanmyeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.3
    • /
    • pp.184-191
    • /
    • 2009
  • In the southern part of the Korean Peninsula including Jeju-island, the production amount of domestic cedar has increased gradually. However, their low qualities, expected to be caused by the low density and frequent knots, have restricted their practical utilization as the high value-added products. In this study, it is aimed to look for the new uses of domestic cedar and to examine the applicability for lamination lumbers of structural glued laminated timber (glulam). Above all, machine stress ratings for individual sawn lumbers confirmed that modulus of elasticity (MOE) of cedar lumber was lower than that of other common softwood species in Korea. On the other hand, cedar lumbers have enough stiffness to manufacture the structural glulam in accordance with Korean Industrial Standard (KS). The bonding strength and durability also met the KS limitation. Nevertheless, from the result of bending tests for cedar glulam, it was shown that the modulus of elasticity (MOE) did not meet the KS limitation. Therefore, it was concluded that additional researches were needed for reinforcing the stiffness of cedar glulam.

Design and Manufacturing Characteristics of Eco-Friendly Wood Street Lamp (친환경 목재가로등의 디자인 및 제조특성)

  • Kim, Jong-In;Jung, Su-Young;Won, Kyung-Rok
    • Journal of the Korea Furniture Society
    • /
    • v.25 no.4
    • /
    • pp.345-352
    • /
    • 2014
  • This study was carried out to develop eco-friendly wood street lamp (EFWSL) by using wood resources stacked in the forests after tree tending operations which were mostly abandoned, but economical as renewable wood resources for developing the wood coated street lamps with the effects of cost reduction and their attractive appearances. This study has led to the development of key compact structures of street-lighting wood poles (shaft) using laminated timber. The core technique in this study is related with producing the more stable wood poles (shaft) with the hole inside than wood poles exposed under the natural environment through applicable process to protect the wood from bursting and splitting. We also comprehensively developed the method to conserve the timber durability of wood shaft and connect the wood shaft with groove, race way to be located in the groove, locking ring, current stabilizer connected to the groove and luminaire support arm, base and hand-hole which was partly used in combination with steel materials and wood. Also we increased the utilization of abandoned and stacked woods after thinning in the forests such as Pinus densiflora, Larix leptolepis, and Pinus koraiensis plantations by maximizing the value of these natural wood resources as main materials of eco-friendly street lightings with the effects of cost reduction and attractive appearances and also the expectation of advertising effects of street lightings developed in this study.

  • PDF

A Study on the Fire Resistance Performance of Wood Framed Lightweight Wall which Including a Middle Lintel (중인방을 포함한 목골조 경량벽체의 내화성능에 관한 연구)

  • Yeo, In-Hwan;Cho, Bum-Yean;Min, Byung-Yeol;Yoon, Myung-O
    • Fire Science and Engineering
    • /
    • v.25 no.3
    • /
    • pp.91-98
    • /
    • 2011
  • This study is about fire resistance performance of wood framed lightweight wall including a middle lintel as a traditional wall form in Korea. The target wall is non-loadbearing system which constructed with $38{\times}89$ mm ($2"{\times}4"$) wood frame and fireproof gypsum board covering, including a middle lintel made of $150{\times}150$ mm section glue-laminated timber. As a test results, all specimens have showed fire resistant performance over 90 minutes and tests were maintained until flame occuring on Specimen-l, 2, 3 at 91 min, 97 min and 98 min respectively. Fire resistance of the heat side gypsum board was 45 minutes and charring rate of middle lintel was equivalant with that of usual timber. The wood stud inside wall system showed relatively quick combution characteristic when exposed to high temperature with no temperature rising delaying time caused by moisture evaporation because of the dehydration preceded during the early period of fire side gypsum board resist to heat.

Experimental Study on Pull-out Strength of Glued-in Rods Connection according to Adhesive (접착제에 따른 Glued-in Rod 접합부 인발성능에 관한 실험 연구)

  • Park, Keum-Sung;Oh, Keunyeong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.22 no.2
    • /
    • pp.149-160
    • /
    • 2022
  • In this study, a pull-out test considering the adhesive type, embedded length, and direction of re-bar was conducted to evaluate the pull-out performance of glued-in rod joints using timber and adhesive produced in Korea. In the test, the specimens using liquid adhesive showed better pull-out performance, and the longer the embedded length of the re-bar, the higher the maximum tensile load by inducing the yield of the re-bar first. Through the test results, a glued-in rod joints design, which is advantageous to design the adhesive strength stronger than the yield strength of re-bar, was proposed, and a correction factor of 0.75 for the adhesive strength considering construction error was also suggested.