• Title/Summary/Keyword: Water-Binder Ratio

Search Result 492, Processing Time 0.026 seconds

Effect of temperature on the behavior of self-compacting concretes and their durability

  • Salhi, M.;Li, A.;Ghrici, M.;Bliard, C.
    • Advances in concrete construction
    • /
    • v.7 no.4
    • /
    • pp.277-288
    • /
    • 2019
  • The formulation of self-compacting concretes (SCC) and the study of their properties at the laboratory level were currently well mastered. The aim of this work is to characterize SCC under hot climatic conditions and their effects on the properties of fresh and hardened SCC. Particularly, the effect of the initial wet curing time on the mechanical behavior such as the compressive strength and the durability of the SCCs (acid and sulfate attack) as well as the microstructure of SCCs mixtures. In this study, we used two types of cement, Portland cement and slag cement, three water/binder (W/B) ratio (0.32, 0.38 and 0.44) and five curing modes. The obtained results shows that the compressive strength is strongly influenced by the curing methods, 7-days of curing in the water and then followed by a maturing in a hot climate was the optimal duration for the development of a better compressive strength, regardless of the type of binder and the W/B ratio.

Effects of Crushed Coal Bottom Ash on the Properties of Mortar with Various Water-to-binder Ratios (다양한 물-결합재비를 갖는 모르타르의 물성에 대한 파쇄 바텀애시의 영향)

  • Tafesse, Million;Kim, Hyeong-Ki
    • Resources Recycling
    • /
    • v.25 no.6
    • /
    • pp.29-40
    • /
    • 2016
  • Effects of crushed coal bottom ash (CBA) with maximum size of 1 mm on the properties of mortar with various water-to-binder ratios (w/b) were evaluated. The present work is a fundamental study to establish a method of mix proportion design for mortar and concrete with CBA. The workability, air contents, and compressive strength of mortar were measured. Efficiency of CBA on the compressive strength at 28 days, which was adopted for mix proportion design, was evaluated based on concepts of 'equivalent strength' in CEN/TR 16637. It was found that the CBA could be contributed as a binder in mortar in some cases, while in other cases act as at aggregates. The efficiency of CBA was influenced by types of CBA and their replacement ratio, and w/b of mortar.

Characteristics of Excess Water Dewatered Concrete Using Permeable Liner (투수시트를 적용하여 잉여수를 탈수한 콘크리트의 강도 특성)

  • Jeon, Kyu-Nam;An, Gi-Hong;Lee, Jong-Suk
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.6
    • /
    • pp.675-682
    • /
    • 2013
  • In this study, to enhance the quality of concrete surface by removing the surplus water, permeable liner attached the euroform was applied for manufacturing concrete specimens. Various kinds of concrete mixtures with different water to binder ratios were applied and the strength properties of the hardened concrete surfaces were evaluated at different heights. Experimental results showed that the rebound values by schmidt hammer test and the compressive strengths on the surfaces of concrete specimens were increased as proportion to the amount of mixture water which is dependent on the water to binder ratio of each concrete mixture, and more enhancements were observed on the middle and lower specimen surfaces than the upper region. SEM analysis also showed that much denser hydrate structures were observed on the specimen surfaces by the application of the permeable liner while similar hydrate formations were occurred regardless of surface treatment conditions. From the MIP test results of the concrete surfaces, it was observed that, by the application of permeable liner, the pore volume below $0.01{\mu}m$ was decreased with a maximum of 50% resulting in the densification of pore structures.

An Experimental Study on the Quality Control of Fresh Porous Concrete (굳지않은 포러스콘크리트의 품질관리를 위한 실험적 연구)

  • 이성일;장종호;김재환;강석표;백용관;김무한
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.705-710
    • /
    • 2002
  • Recently, there has been for a number of reasons growing interest in the use of porous concrete, and it is used as an ecological material. But, because the valuation methods of the quality on the fresh porous concrete aren't established up till now, it is difficult that the harden porous concrete is made sure of its required quality. This study is to present the measurement method of the void ratio on the fresh porous concrete and to analyze the influence of water-cement ratio and vibrating time on the binder content covered a coarse aggregate. Results of this study were shown as follows; The measurement methods of the void ratio and aggregate-binder weight ratio on the fresh porous concrete can be useful as data for the quality control of fresh porous concrete.

  • PDF

A Study on Drying Shrinkage of the High-Strength Concrete using the Garnet (가네트를 활용한 고강도 콘크리트의 건조수축 특성 연구)

  • Jang Ju-Young;Yoon Yo-Hyun;Park Jung-Min;Kim Wha-Jung
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.676-679
    • /
    • 2004
  • In this study, we considered the characteristic of drying shrinkage from age of high strength concrete with garnet minute powder to be industry by-product. The factors of experiment are unit water content$(160kg/m^3)$, water-binder ratio(30, $35\%$), fine aggregate ratio(40, 42, $44\%$), admixture replacement ratio(0, 10, $20\%$), admixture type(garnet minute powder, fly ash, blast-furnace slag). We make a comparative study of shrinkage about concrete with a passage of age(1, 3, 7, 14, 28, 56, 91 days). As a result of experiment, we reach a conclusion as follow. In the same mix condition, as unit water content and fine aggregate ratio go up, the drying shrinkage ratio increase. In the drying shrinkage ratio according to admixture replacement ratio, it goes up when admixture replacement Ratio increase in case of fly ash and blast-furnace slag. But, drying shrinkage ratio decrease when admixture replacement ratio increase in case of garnet minute powder.

  • PDF

Characterization of alkali activated geopolymer mortar doped with MWCNT

  • Khater, H.M.;Abd el Gawaad, H.A.
    • Advances in materials Research
    • /
    • v.4 no.1
    • /
    • pp.45-60
    • /
    • 2015
  • This paper aimed to investigate the effect of MWCNTs on properties of slag Geopolymeric mortar. Geopolymeric matrices containing different MWCNTs concentrations (0.0, 0.1, 0.2, 0.3 and 0.4 % by weight of the used binder) were synthesized. The Geopolymer mortar composed of aluminosilicate slag to sand (1:2), while the alumino silicate source binder composed of 50% air cooled slag and 50%water cooled slag both passing a sieve of $90{\mu}m$, while the sand passing a sieve of 1 ml. The materials prepared at water/binder ratios in a range of 0.34-0.39% depending on the added MWCNT, whereas the Gelenium Ace-30 superplasticizer used in the ratio of 1.4-2.2% from the total dry weight for better dispersion of MWCNT under sonication for 15 min. Alkaline activation of the Geopolymer mortar was carried by using of 6% NaOH. Curing was performed under temperature of $40^{\circ}C$ and 100% R.H. Results showed that the addition of MWCNTs enhanced the resulting amorphous geopolymer structure with marked decrease in the drying shrinkage as well as water absorption specially when using 0.1% MWCNT, while further increase in MWCNTs results in agglomeration in MWCNT within the matrix and so hinder the propagation of Geopolymerization reaction and negatively affect the formed geopolymer structure.

Soil stabilization by ground bottom ash and red mud

  • Kim, Youngsang;Dang, My Quoc;Do, Tan Manh;Lee, Joon Kyu
    • Geomechanics and Engineering
    • /
    • v.16 no.1
    • /
    • pp.105-112
    • /
    • 2018
  • This paper presents results of a compressive investigation conducted on weathered soil stabilized with ground bottom ash (GBA) and red mud (RM). The effects of water/binder ratio, RM/GBA ratio, chemical activator (NaOH and $Na_2SiO_3$) and curing time on unconfined compressive strength of stabilized soils were examined. The results show that the water/binder ratio of 1.2 is optimum ratio at which the stabilized soils have the maximum compressive strength. For 28 days of curing, the compressive strength of soils stabilized with alkali-activated GBA and RM varies between 1.5 MPa and 4.1 MPa. The addition of GBA, RM and chemical activators enhanced strength development and the rate of strength improvement was more significant at the later age than at the early age. The potential environmental impacts of stabilized soils were also assessed. The chemical property changes of leachate from stabilized soils were analyzed in terms of pH and concentrations of hazardous elements. The observation revealed that the soil mixture with ground bottom ash and red mud proved environmentally safe.

Pull-Out Behaviour of Hooked End Steel Fibres Embedded in Ultra-high Performance Mortar with Various W/B Ratios

  • Abdallah, Sadoon;Fan, Mizi;Zhou, Xiangming
    • International Journal of Concrete Structures and Materials
    • /
    • v.11 no.2
    • /
    • pp.301-313
    • /
    • 2017
  • This paper presents the fibre-matrix interfacial properties of hooked end steel fibres embedded in ultra-high performance mortars with various water/binder (W/B) ratios. The principle objective was to improve bond behaviour in terms of bond strength by reducing the (W/B) ratio to a minimum. Results show that a decrease in W/B ratio has a significant effect on the bond-slip behaviour of both types of 3D fibres, especially when the W/B ratio was reduced from 0.25 to 0.15. Furthermore, the optimization in maximizing pullout load and total pullout work is found to be more prominent for the 3D fibres with a larger diameter than for fibres with a smaller diameter. On the contrary, increasing the embedded length of the 3D fibres did not result in an improvement on the maximum pullout load, but increase in the total pullout work.

Influence of Curing Condition on Drying Shrinkage of Concrete (초기 양생조건에 따른 콘크리트의 건조수축 특성)

  • 하재담;김태홍;유재상;이종열;배수호;권영호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.277-280
    • /
    • 2003
  • Material, mix proportion, curing condition, temperature, humidity and wind velocity have an influence on drying shrinkage of concrete. In this paper, to evaluate the effect of curing condition at early age on the drying shrinkage of concrete was investigated varying curing age for different binder. The principal conclusions from this research were as follows: 1) In case of 14 days of water curing, the drying shrinkage of concrete is smaller than 7 days of water curing, independence of type of binder. 2) In case of 4 days of water curing, the ratio of increase of drying shrinkage of concrete using fly-ash and slag powder is more remarkable than using portland cement alone, comparing the drying shrinkage of 7 days of water curing.

  • PDF

Using Carboxylmethylated Cellulose as Water-Borne Binder to Enhance the Electrochemical Properties of Li4Ti5O12-Based Anodes

  • Liu, Lili;Cheng, Chongling;Liu, Hongjiang;Shi, Liyi;Wang, Dayang
    • Journal of Powder Materials
    • /
    • v.22 no.5
    • /
    • pp.315-320
    • /
    • 2015
  • The present work reports a systematic study of using carboxymethylated cellulose (CMC) as water-borne binder to produce $Li_4Ti_5O_{12}$-based anodes for manufacture of high rate performance lithium ion batteries. When the LTO-to-CB-to-CMC mass ratio is carefully optimized to be 8:1:0.57, the special capacity of the resulting electrodes is $144mAh{\cdot}g^{-1}$ at 10 C and their capacity retention was 97.7% after 1000 cycles at 1 C and 98.5% after 500 cycles at 5 C, respectively. This rate performance is comparable or even better than that of the electrolytes produced using conventional, organic, polyvinylidene fluoride binder.