• 제목/요약/키워드: Ti-6A1-4V

검색결과 377건 처리시간 0.031초

RAINBOW 압전 액츄에이터의 제조와 물성 (Processing and Properties of RAINBOW Piezoelectric Actuator)

  • 백종후;임은경;김창일;이미재;지미정;최병현;김세기
    • 한국전기전자재료학회논문지
    • /
    • 제19권3호
    • /
    • pp.222-227
    • /
    • 2006
  • RAINBOW(Reduced And Internally Biased Oxide Wafers) are a new class of high-displacement, piezoelectric actuator produced by selectively removing oxygen from one surface of ceramic using a high-temperature chemical reduction process. In this paper, RAINBOW actuator materials of $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_{x}Ti_{1-x})O_3$ ceramics were prepared. Its dielectric and piezoelectric properties were investigated in the vicinity of MPB. The piezoelectric properties showed the maximum value of ${\epsilon}r$ = 4871, $d_{33}$ = 610 ($10^{-12}$ m/V), $d_{31}$ = -299 ($10^{-12}$ m/V), $k_{33}$ = $71\%$, Qm = 70, in $0.4Pb(Ni_{1/3}Nb_{2/3})O_{3}-0.6Pb(Zr_{405}Ti_{595})O_3$ composition sintered at $1250^{\circ}C$. The strain - electric field characteristics of RAINBOW actuator were significantly improved comparison with the conventional bulk actuator. The prepared RAINBOW actuator showed about $390\;{\mu}m/100\;V$ displacement.

Ni-MH 2차 전지용 Zr계 수소저장합금전극의 특성에 미치는 치환원소(Co, Cr, Fe)의 영향 (The effect of substitution elements(Co, Cr, Fe) on the properties of Zr-based hydrogen storage alloy electrode for Ni-MH secondary battery)

  • 최승준;정소이;서찬열;최전;박충년
    • 한국수소및신에너지학회논문집
    • /
    • 제10권3호
    • /
    • pp.185-189
    • /
    • 1999
  • Effects of alloy modification with the $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.4}$ alloy for an electrode use have been investigated. For the alloy composition, a part of Mn was substituted by Co, Cr and Fe. The experimental results showed that Co accelerated activation of alloy, and Fe and Cr improved the discharge capacity. These results agree with P-C-T curves of each alloy. But substituting Fe for Mn showed the decrease of the discharge capacity when discharged at high rate (60mA, about 1C rate). Considering both the discharge capacity and the high rate discharge property, $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.3}Cr_{0.1}$ alloy was found to be the best alloy among the alloys subjected to the test.

  • PDF

2중 용체화처리에 따른 Ti-6AI-4V합금의 미세조직과 인장특성 (Microstructures and Tensile Characteristics of Ti-6AI-4V Alloy by Double Solution Treatment)

  • 최형진;이준희
    • 한국재료학회지
    • /
    • 제4권6호
    • /
    • pp.626-637
    • /
    • 1994
  • Ti-6Ai-4V 합금의 미세조직을 용체화처리온도 및 냉각속도만의 변화로서 Widmanstatten 조직과 이중조직을 얻은 후 이들 미세조직과 인장성질고의 비교. 검토를 통해서 최적 열처리 방안을 설정하고자 하였다. 그 결과 Widmanstatten 조직에 있어서는 열처리온도나 냉각속도에 따라 복잡하고 무질서한 dege형상의 $\alpha$상 및 등축화된 $\alpha$상으로변화시킬 수 있었으며, $\alpha$+$\beta$ 영역에서 2중 용체화 처리의 경우 1차 및 2차 용체화처리 온도가 낮을수록 aspect비는 작아짐을 알 수 있었다. 인장성질에 있어서 Widmanstatten 조직은 이중조직에 비해 강도는 감소하고 연성성질 또한 크게 감소하였으며, 파단양상 Widmanstatten 조직의 경우 준벽개와 dimple형 파단양상이 함께 나타나는 반면 이중조직은 연성파괴를 나타내었다. 또한 이중조직의 파단면을 인장축에 수직인 내부균열영역과 45˚ 정도의 전단각을 갖는 shear lip영역으로 나누어 관찰할 수 있었다.

  • PDF

Dry Sol-Gel법에 의한 $TiO_2$ hybrid 박막의 광학특성 및 유전특성에 관한 연구 (Optical and dielectric Properties of $TiO_2$ hybrid thin films by dry sol-gel processing)

  • 정재훈;조종래;손세모;정수태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.315-318
    • /
    • 2001
  • The optical and dielectric properties of TiO$_2$ thin films prepared with mixtures of Epoxy, bits-(4, 4'-p-toluenesulfonylacidic isoproplylidene)-cyclohexadiol and UVI 6990 in dry sol-gel process were investigated. The absorption peak of the films was showed at 360nm. Photocurrent of the thin films doped with 50 wt% of TiO$_2$was higher than that of nondoped thin films. Energy gap was lowered from 3.6 to 3.3 eV with increasing amount of TiO$_2$. Relative dielectric constants of samples were 1.5 to 3 and showed a characteristics of lower dielectric materials.

  • PDF

급속냉각된 $SmFe_{7+x}M_{x}(M=Mo,\;V,\;Ti)$ 화합물에서 생성된 신 강자성상 (Magnetic Hardening of Rapidly Solidified $SmFe_{7+x}M_{x}(M=Mo,\;V,\;Ti)$ Compounds)

  • Choong-Jin Yang;E. B. Park;S. D. Choi
    • 한국자기학회지
    • /
    • 제4권3호
    • /
    • pp.226-232
    • /
    • 1994
  • 철-희토류 화합물인 Sm-Fe 이원계에서 조성식 $SmFe_{7+x}M_{x}(M=Mo,\;V,\;Ti)$ 화합물을 급속냉각기술로 제조하여 강자성을 나타내는 새로운 자성상인 ${Sm(Fe,\;M)}_{7}$을 합성하였다. Sm-Fe 이원계에 제 2의 천이원소 Mo, V 또는 Ti를 첨가함으로써, ${Sm(Fe,\;M)}_{7}$ 자성상은 큐리온도(Tc)가 $T_{c}=355^{\circ}C$에 달했으며 x=0.8과 1.0 사이에서 $SmFe_{7+x}M_{x}(M=Mo,\;V,\;Ti)$의 고유보자력 ($_{i}H_{c}$)이 3~6 kOe를 갖는 신 자성상을 제조하였다. ${Sm(Fe,\;M)}_{7}$ 상은 급냉응고 된 상태에서나 열처리 후에도 변함없이 안정하였으며 오히려 급냉상태에서 보다 우수한 강자기 특성을 보였다. ${Sm(Fe,\;M)}_{7}$은 육방정계 결정구조를 갖는 능방정계이며 P6/mmm Space Group에 속하는 것으로 판명되었다. ${Sm(Fe,\;M)}_{7}$ 자성상이 고보자력을 나타내는 원천적인 이유는 급속냉각에 의하여 결정입도가 $2000~8000\;{\AA}$의 미립자로 형성되기 때문이며, 높은 규리온도를 보이는 까닭은 급속냉각에 의해 제 2의 천이원소인 Mo, V 또는 Ti의 Fe에 대한 고용도가 평형상태에서 보다 월등히 높아져 자기변환온도를 상승하게 하였기 때문이다.

  • PDF

IEC국제규격을 보급하기 위한 RRR측정장치 제작 (Fabrication of RRR Measuring System for Disseminating IEC International Standard)

  • 이규원;김규태
    • Progress in Superconductivity
    • /
    • 제4권1호
    • /
    • pp.80-85
    • /
    • 2002
  • In order to disseminate the IEC international standard of RRR measurement of Cu/Nb/-Ti composite superconductors, a measuring system was developed at KRISS. The system consisted of helium reservoir, base plate, thermometer, voltmeter and current source. The helium reservoir and base plate provided a stable temperature of a range from 4.2 K to 300 K and the voltmeter measured several order of $mutextrm{V}$ on specimen for obtaining RRR of the Cu/Nb-Ti composite superconductor. Three specimens of the Cu/Nb-Ti composite superconductors were measured using this system for characterizing their RRR. The resistance-temperature curves ortho specimens showed 10/sup -6/ to 10/sup -5/ Ohms near transition temperature and 10/sup -4/ to 10/sup -3/ Ohms at 293 K. The RRR values of the specimens were 145, 71 and 140, respectively.

  • PDF

Microstructural Evolution and Mechanical Properties of Ti-6Al-4V Alloy through Selective Laser Melting: Comprehensive Study on the Effect of Hot Isostatic Pressing (HIP)

  • Gargi Roy;Raj Narayan Hajra;Woo Hyeok Kim;Jongwon Lee;Sangwoo Kim;Jeoung Han Kim
    • 한국분말재료학회지
    • /
    • 제31권1호
    • /
    • pp.1-7
    • /
    • 2024
  • This study explores the profound impact of varying oxygen content on microstructural and mechanical properties in specimens HO and LO. The higher oxygen concentration in specimen HO is found to significantly influence alpha lath sizes, resulting in a size of 0.5-1 ㎛, contrasting with the 1-1.5 ㎛ size observed in specimen LO. Pore fraction, governed by oxygen concentration, is high in specimen HO, registering a value of 0.11%, whereas specimen LO exhibits a lower pore fraction (0.02%). Varied pore types in each specimen further underscore the role of oxygen concentration in shaping microstructural morphology. Despite these microstructural variations, the average hardness remains consistent at ~370 HV. This study emphasizes the pivotal role of oxygen content in influencing microstructural features, contributing to a comprehensive understanding of the intricate interplay between elemental composition and material properties.

타이타늄 합금 분말의 열적산화를 통한 TiO2 나노와이어의 합성 (Synthesis of TiO2 Nanowires by Thermal Oxidation of Titanium Alloy Powder)

  • 김유영;조권구
    • 한국분말재료학회지
    • /
    • 제25권1호
    • /
    • pp.48-53
    • /
    • 2018
  • One-dimensional rutile $TiO_2$ is an important inorganic compound with applicability in sensors, solar cells, and Li-based batteries. However, conventional synthesis methods for $TiO_2$ nanowires are complicated and entail risks of environmental contamination. In this work, we report the growth of $TiO_2$ nanowires on a Ti alloy powder (Ti-6wt%Al-4wt%V, Ti64) using simple thermal oxidation under a limited supply of $O_2$. The optimum condition for $TiO_2$ nanowire synthesis is studied for variables including temperature, time, and pressure. $TiO_2$ nanowires of ${\sim}5{\mu}m$ in length and 100 nm in thickness are richly synthesized under the optimum condition with single-crystalline rutile phases. The formation of $TiO_2$ nanowires is greatly influenced by synthesis temperature and pressure. The synthesized $TiO_2$ nanowires are characterized using field-emission scanning electron microscopy (FE-SEM), X-ray diffraction (XRD), and high-resolution transmission electron microscopy (HR-TEM).

제조방법에 따른 $MnO_2$ coating 전극의 전기화학적 특성 (Electrochemical Characteristics of $MnO_2$ coated electrodes as a function of manufacturing method)

  • 김현식;이해연;허정섭;안용운;김종령;박혜영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 하계학술대회 논문집 C
    • /
    • pp.1740-1742
    • /
    • 2004
  • 산소 과전압이 낮은 $MnO_2$를 촉매로 사용하여 반도체 산화물계의 산소선택성 전극을 제조하고 산화물 코팅층의 미세구조와 전기화학적 특성을 분석하였다. Ti 기판에 열분해 법을 이용하여 $MnO_2$ 피막을 형성하였고, 또한 binder를 이용한 코팅 방법을 이용하여 Ti, Fb 기판에 $MnO_2$ 피막층을 형성하였다. 450$^{\circ}C$에서 1시간 열분해하여 약 1 ${\mu}m$$MnO_2$ 피막층을 형성 시켰으나 Ti 기판과의 접착력이 약하여 피막자체에 대한 전기화학적 특성은 관찰할 수 없었다. PVDF : $MnO_2$의 함량비가 1:1에서 1:6 까지는 DMF의 함량에 무관하게 전극 특성이 나타나지 않았지만 20:1 이상의 조성에서는 균일한 C-V 특성을 나타냈고, 산소 발생 과전압도 약 1.4V 정도로 감소되었다. 그러나 Ti 기판의 경우 열분해법을 이용하여 제조된 전극과 같이 낮은 기판과의 접착력 때문에 $MnO_2$ 피막층의 촉매효과가 현저하게 감소하였다.

  • PDF

Ti 합금의 기계가공 방법에 따른 경도 변화에 관한 연구 (Hardness of Ti alloys by mechanical processing methods)

  • 반재삼;김규하;정상원;기강호;조규종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.792-795
    • /
    • 2002
  • In previous researches, it is reported that Ti-10Ta-10Nb is robuster than Ti-6A1-4V which is used as a biomaterial in a experiment of cytotoxicity. Ti-10Ta-10Nb has enough hardness to be required as a biomaterial because the change of its hardness can be controlled more than 100% according to heat treatment condition and manufacturing condition. There are many hardness changing condition including Cast Homogenization, Solution treatment. Forging, Rolling in this research. The changing form and amount of new Ti-10Ta-10Nb to be developed in this researches, are measured as quantitative. Specially, the changing hardness amount of the specimen that is manufactured in single phase temperature, i.e. 80$0^{\circ}C$, are measured in case of high temperature rolling and high temperature cast condition.