The sintering behavior of $BaFe_{12}O_{19}$ with the addition of one and three weight % of $CuWO_4$ as a liquid phase sintering aid is studied. Samples are sintered in the temperature range $900-1250^{\circ}C$ and the effect of $CuWO_4$ addition on density, microstructure, phase composition and magnetic properties is examined. Compared to $BaFe_{12}O_{19}$ with no sintering aid addition, addition of 1 wt % $CuWO_4$ retards densification. Addition of 3 wt % $CuWO_4$ promotes densification at lower sintering temperatures but retards densification at temperatures > $1050^{\circ}C$. Three wt % $CuWO_4$ addition induces the formation of $BaWO_4$ and $Ba_3WFe_2O_9$ secondary phases at temperatures ${\geq}1100^{\circ}C$. Addition of $CuWO_4$ causes a decrease in saturation magnetization, remanent magnetization and coercivity.
Hard shaped bodies are made by sintering a cold-pressed compact of a boron carbide compound which contains a densification aid. Titanium diboride and carbon were used as a densification aid in a range of 1% to 10% by weight. The effects of sintering temperature and additives on linear shrinkage porosity hardness bend strength and microstructure were examined. The initial partical size dependence on the sintered density was also discussed.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.21
no.10
/
pp.906-910
/
2008
$(K_{0.5}Na_{0.5})NbO_3$ (NKN) ceramics doped with $Li_{2}CO_3$ as sintering aids were manufactured in order to develop the low temperature sintering ceramics for piezoelectric device. The sintering aids were proved to lower the sintering temperature of doped NKN ceramics due to the effect of $Na_{2}CO_{3}-Li_{2}CO_3$ liquid phase. All the specimens showed the orthorhombic phase without secondary phase. And also, the piezoelectric properties of specimens were improved with increasing $Li_{2}CO_3$ contents. At sintering temperature of $930^{\circ}C$, the density, electromechanical coupling factor (kp), mechanical quality factor (Qm) and dielectric constant(${\epsilon}_{\gamma}$), piezoelectric constant of 0.3 wt.% $Li_{2}CO_3$ added specimen showed the optimum values of $4.255 g/cm^3$, 0.37, 234, 309, 136 pC/N, respectively.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.29
no.8
/
pp.476-482
/
2016
Convectional PZT based piezoelectric ceramics have to sinter at high temperature about $1,200^{\circ}C$ for their suitable electrical properties. However, some issues: low temperature sintering piezoelectric ceramic composition and reliable internal electrode, have recently attracted a great deal of interest as a highly efficient multi-layered piezoelectric ceramics. In order to optimize low temperature sintering conditions of thick-film PMN-PZ-PT ceramic, it was investigated sintering and piezoelectric properties according to the change of $LiBiO_2$ contents. Thus, the superior piezoelectric properties were found at the pallet type PMN-PZ-PT optimized with low sintering processing at $925^{\circ}C$ including 7 wt% $LiBiO_2$ sintering aid. Consequentially, we successfully manufactured thick-film PMN-PZ-PT ceramics, which had superior piezoelectric and dielectric properties, with 5 wt% of $LiBiO_2$ sintering aid at temperature of $900^{\circ}C$.
A sintering aid, $B_{2}O_{3}$ have been included into a $LiAlO_{2}$ electrolyte support by a tape casting method in order to reinforce mechanical strength of the support for molten carbonate fuel cells [MCFCs). Starting idea originates from the low melting point of $B_{2}O_{3}$ ($450^{\circ}C$), which can provide the low temperature consolidation of ceramic materials. The mechanical properties and the microstructure changes of the $B_{2}O_{3}$-included electrolyte support were examined by scanning electron microscope, mercury porosimetry, X-ray powder diffraction [XRD], high temperature differential scanning calorimeter and three-point bending strength measurement. The mechanical strength was clearly improved by addition of $B_{2}O_{3}$. The increase of mechanical strength results from the neck growth of a new $LiAlO_{2}$ phase between $LiAlO_{2}$ particles by the liquid phase sintering. Average pore size and porosity of the electrolyte support reinforced by addition of the sintering aid, $B_{2}O_{3}$, was $0.24{\mu}m$ and 59%, respectively which were suitable microstructure of a matrix for an application of MCFCs.
The eutectic melt of BaO-CuO flux is known to be a potential sintering aid for $Ba(Zr,Y)O_3$ (BZY) electrolyte for proton-conducting ceramic fuel cells (PCFCs). A density of BZY higher than 97% of theoretical density can be achieved via sintering at $1300^{\circ}C$ for 2 h using a flux composed of 28 mol% BaO and 72 mol% CuO. In the present study, chemical and structural evolution of BaO-CuO flux throughout the sintering process was investigated. An intermediate holding step at $1100^{\circ}C$ leads to formation of various impurity compounds such as $BaCuO_{1.977}$, $Ba_{0.92}Cu_{1.06}O_{2.28}$ and $Cu_{16}O_{14.15}$, which exhibit significantly larger unit cell volumes than the matrix. The presence of such secondary compounds with large lattice mismatch can potentially lead to mechanical failure. On the other hand, direct heating to the final sintering temperature produced CuO and $Cu_2O$ as secondary phases, whose unit cell volumes are close to that of the matrix. Therefore, the final composition of the flux is strongly affected by the thermal history, and a proper sintering schedule should be used to obtain the desired properties of the final product.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.8
no.2
/
pp.324-331
/
1998
After the addition of yttrium aluminum garnet of 2, 5, 10 mol% as a sintering aid, $\alpha$-silicon carbides were prepared by a liquid-phase sintering at $1850^{\circ}C$, and the microstructural evolution was investigated during sintering as functions of liquid-phase amount and sintering time. The highest apparent density in each compositions was obtained in specimens sintered for 2 h, and the percentage of weight loss increased with sintering time. By increasing the amount of sintering aid (yttrium aluminum garnet), the rate of grain growth during sintering decreased, but the apparent density of sintered body increased. The phase transformation from 6H-SiC to 4H-SiC was partially observed in specimens sintered for a long time, and so, a few rod-like grains were observed.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.20
no.12
/
pp.1034-1038
/
2007
In order to develop the composition ceramics capable of being sintered at low temperature with high piezoelectric properties for multilayer piezoelectric actuator application, PZW-PMN-PZT system ceramics were manufactured according to sintering aid $Li_2CO_3$ addition and their microstructural, dielectric and piezoelectric properties were investigated. The crystal structure of the specimens showed a perovskite phase and no pyrochlore or other second phase was detected. At the sintering temperature of $900\;^{\circ}C,\;0.2\;wt%Li_2CO_3$ added specimen showed a optimum values of kp = 0.562, $d_{33}\;=\;360\;pC/N$ and Qm = 1184, respectively.
The Transactions of the Korean Institute of Electrical Engineers C
/
v.55
no.11
/
pp.505-513
/
2006
The present study investigated the influence of the content of $Al_2O_3+Y_2O_3$ sintering additives on the microstructure, mechanical and electrical properties of the pressureless-sintered $SiC-ZrB_2$ electroconductive ceramic composites. Phase analysis of composites by XRD revealed mostly of ${\alpha}-SiC(4H),\;ZrB_2,\;{\beta}-SiC(15R)$ and In Situ $YAG(Al_5Y_3O_{12})$. The relative density and the flexural strength showed the highest value of 86.8[%] and 203[Mpa] for $SiC-ZrB_2$ composite with an addition of 8[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid at room temperature respectively. Owing to crack deflection and crack bridging of fracture toughness mechanism, the fracture toughness showed 3.7 and $3.6[MPa{\cdot}m^{1/2}]\;for\;SiC-ZrB_2$ composites with an addition of 8 and 12[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid at room temperature respectively. Abnormal grain growth takes place during phase transformation from ${\beta}-SiC\;into\;{\alpha}-SiC$ was correlated with In Situ YAG phase by reaction between $Al_2O_3\;and\;Y_2O_3$ additives during sintering. The electrical resistivity showed the lowest value of $6.5{\times}10^{-3}[({\Omega}{\cdot}cm]$ for the $SiC-ZrB_2$ composite with an addition of 8[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid at room temperature. The electrical resistivity of the $SiC-ZrB_2$ composites was all positive temperature coefficient(PTCR) in the temperature ranges from $25[^{\circ}C]\;to\;700[^{\circ}C]$. The resistance temperature coefficient showed the highest value of $3.53{\times}10^{-3}/[^{\circ}C]\;for\;SiC-ZrB_2$ composite with an addition of 8[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid in the temperature ranges from $25[^{\circ}C]\;to\;700[^{\circ}C]$. In this paper, it is convinced that ${\beta}-SiC$ based electroconductive ceramic composites for heaters or ignitors can be manufactured by pressureless sintering.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.