The changes of resistant starch (RS) contents of cooked rice with soybean and coconut oils under different storage conditions were investigated and RS contents were compared between the rice and cooker types. The japonica (Hopyeong) and the indica (Thailand) type rice were cooked (washed rice: water = 100: 130) using an electric cooker and a saucepan. The coconut oil and soybean oil (3%, based on rice, w/w) were added into cooking water before heating. The RS contents of freeze-dried cooked rice powders (newly-cooked rice, stored for 12 h in the refrigerator, microwave heating after storage for 12 h in the refrigerator) were measured by the AOAC method. The RS contents of cooked rice using a saucepan were higher than those using an electric cooker. The indica type cooked rice had a higher RS content than the japonica type cooked rice, regardless of storage conditions. However, addition of oil before cooking rice resulted in increased RS content on storage in the refrigerator. The highest RS content of the cooked indica type rice with soybean oil ($5.89{\pm}0.22%$) that was stored for 12 h in the refrigerator was analyzed. The results suggested that the cooked rice formed retrograded (RS3) and amylose-lipid complex (RS5) type RS; furthermore, the RS content is affected by storage conditions, rice, cooker and oil types.
최근 전자기기의 소형화, 다기능화 등으로 인한 전자부품 실장 영역의 한계치를 극복하고 플라스틱 사출물에 직접 회로를 인쇄하고 소자 및 부품을 실장하는 molded interconnect device (MID) 형태의 패키징 기법이 도입되고 있다. 다만 열 안정성이 낮은 플라스틱 사출물을 사용하는 경우, 종래의 리플로우 공정을 통한 부품 실장에 어려움이 있다. 본 연구에서는 특정 부위 혹은 소재만을 가열할 수 있는 유도가열 현상을 이용하여 플라스틱에 어떠한 열 데미지 없이 솔더를 용융시켜 실장하는 공정을 개발하였다. 가열하고자 하는 부위에 자속을 집중시킬 수 있는 유도가열용 Cu 코일 형상을 설계하고, 유한요소해석을 통해 패드부 자속 집중 및 가열 정도를 검증하였다. Polycarbonate 기판 위에 실장공정 검증을 위한 LED, capacitor, resistor, connector를 각각 유도가열을 통해 실장하고 작동여부를 확인하였다. 본 연구를 통해 리플로우 공법의 한계를 극복가능한 자기유도를 통한 선택적 가열 공정의 적용 가능성을 제시하였다.
전분의 가열, 호화과정에서 ohmic heater를 이용하여 가열속도를 변화시키면서 가열속도가 전분현탁액의 팽윤특성 및 물성에 미치는 영향을 고찰하였다. 3% 옥수수 전분현탁액을 가열속도를 변화시키면서 $90^{\circ}C$까지 가열한 후 냉각시키고 현미경 관찰과 입도분포를 측정한 결과 생옥수수 전분입자의 평균 직경은 $13.7{\mu}m$이었으며 $0.6^{\circ}C/min$의 가열속도로 가열했을 경우 $30.97{\mu}m$, $16.4^{\circ}C/min$로 가열한 경우는 $37.88\;{\mu}m$로 평균직경이 급속히 증가하였으나 $16.4^{\circ}C/min$ 이상의 가열속도에서는 완만히 증가하여 $45.5^{\circ}C/min$일 때는 $41.56\;{\mu}m$로 증가하였다. 즉, 가열속도는 전분입자의 팽윤에 영향을 주며, 가열속도의 증가는 전분입자의 팽윤을 촉진하는 것으로 나타났다. $7.5^{\circ}C/min$ 이하의 낯은 속도로 가열한 3% 옥수수 전분현탁액은 Newtonian fluid에 가까운 유동곡선 특성을 보였다. 그러나 가열속도 $16.4^{\circ}C/min$ 이상에서는 전분현탁액이 pseudoplastic fluid의 거동을 나타내었으며, yield stress가 현저히 증가되었다. 또한 겉보기 점도는 가열속도가 증가함에 따라 선형적으로 증가하였다. 15%의 옥수수전분현탁액을 각각 다른 가열속도로 $90^{\circ}C$까지 가열한 후, 전분겔을 조제하여 가열속도에 따른 전분겔의 견고성(hardness)을 측정한 결과, 완만 가열하여 제조한 전분겔의 견고성은 높은 값을 나타내었으며, 가열속도가 증가함에 따라 차츰 감소하다가 가열속도 $9.4-23.2^{\circ}C/min$의 범위에서는 거의 일정한 값을 나타내었다. 그러나 이후에는 가열속도가 증가함에 따라 전분겔의 견고성이 다시 증가하였다.
침엽수 구조재인 S.P.F 수종을 마이크로파로 단시간에 급속 건조시켜 액상의 인산염계 방염약제에 시간별로 침지시킨 후 2차 마이크로파 가열을 한 다음 3.8cm의 두께에서 1cm를 압축시켜 방염 후 처리물품 시험과 내구성 시험을 실시한 결과 1차 마이크로파 적정 가열시간은 5kW에서 7분 동안 가열할 경우 목표 함수율(4~5%)을 만족하는 것으로 나타났다. 인산염계 방염약제에 침지, 건조 후 3kW로 9분 동안 가열시켜 연화된 상태에서 압축된 목재의 함수율 측정결과 시험편 모두 외부용 목재의 적정 함수율인 12~14%의 범위를 만족하는 것으로 나타났다 또한 압축된 목재의 방염후 처리물품 시험을 통한 방염성능은 방염약제에 30분간 침지된 시험편이 가장 우수한 것으로 나타났으며 압축된 목재의 성능 시험 결과 경도, 못뽑기 저항, 압축, 휨강도, 전단 강도 모두 약 2~3배 이상 역학적 특성이 향상되었다.
In this study, the effects of the pouring temperature, preheating temperature, surface condition and fraction of the wear resistant part on the production of duo-castings were investigated using a high Cr white cast iron with excellent abrasion resistance and a low Cr alloy steel with good toughness. The constituent materials of the duo-castings were designed to have high hardness, fracture toughness and abrasive wear resistance for the replacement of high Mn alloy steels with low abrasive wear resistance. In particular, the amount of abrasive wear of 17% Cr white cast iron was about 1/20 of that of high Mn alloy steel. There was an intermediate area of about 3mm due to local melting at the bonding interface of the duo-castings. These intermediate regions were different from those of the constituent materials in chemical composition and microstructure. This region led to fracture within the wear resistant part rather than at the bonding interface in the bending strength test. The bending fracture strengths were 516-824 MPa, which were equivalent to the bending proof strength of high Mn steel. The effects of various casting conditions on the duo-cast behavior were studied by simple pouring of low Cr alloy steel melt, but the results proved practically impossible to manufacture duo-castings with a sound bonding interface. However, the external heating method was suitable for the production of duo-castings with a sound bonding interface.
Strong winds according to global warming cause the increase of the frequency and the repair cost of damaged roofs. In the United States, Factory Mutual Insurance Company(FMIC) promotes the roofing design that resists heavy wind-load, as the means of strict criteria. This fact reveals that more durable roofing system will be also required in Korea. Therefore, this study aims at developing such a system with high wind-resistance performance using Thermoplastic polyolefin(TPO) and Electromagnetic induction technology(EIT) than the previous systems. The system presented in this study consists of 4 main devices as follow; 1) a disc to fix sheets for TPO & EIT method, which can conduct structural design according to site condition, such as region, building height, and wind load. 2) a nail to have about 30% stronger lifting-up capacity than that of the previous nail. 3) a disc to fix sheets, which has triangle protuberance not to damage sheets in the repeatable wind load, and 4) a electromagnetic induction device to combine a disc and a sheet by heating uniformly and quickly adhesive agent on the disc. The results of mock-up test illustrate that the system provides wind-resistant performance to achieve satisfactorily the structural design criteria of FMIC. In addition, the system is faster, chipper, and easier than the existing system, and is expected that this roofing system can be applied to the rehabilitations of an existing as well as a new building.
Observations from experiments and real fire indicate that restrained steel beams have better fire-resistant capability than isolated beams. Due to the effects of restraints, a steel beam in fire condition can undergo very large deflections and the run away damage may be avoided. However disgusting damages may occur in the beam-to-column connections, which is considered to be mainly caused by the enormous axial tensile forces in steel beams resulted from temperature decreasing after fire dies out. Over the past ten years, the behaviour of restrained steel beams subjected to fire during heating has been experimentally and theoretically investigated in detail, and some simplified analytical approaches have been proposed. While the performance of restrained steel beams during cooling has not been so deeply studied. For the safety evaluation and repair of steel structures against fire, more detailed investigation on the behaviour of restrained steel beams subjected to fire during cooling is necessary. When the temperature decreases, the elastic modulus and yield strength of steel recover, and the contraction force in restrained steel beams will be produced. In this paper, an incremental method is proposed for analyzing the behaviour of restrained steel beams subjected to cooling. In each temperature decrement, the development of deformation and internal forces of a restrained beam is divided into four steps, in order to consider the effect of the recovery of the elastic modulus and strength of steel and the contraction force generated by temperature decrease in the beam respectively. At last, the proposed approach is validated by FE method.
($Ti_{1-x}$$Cr_{x}$ )N coatings were deposited by an ion-plating method in a reactor with two separate metal sources, Ti and Cr. Ti was evaporated using an electron beam, while Cr evaporation was carried out by resistant heating. The Ti and Cr concentrations in the coatings were controlled by the Ti and Cr evaporation ratio. The coating hardness increased with increasing the Cr content(x) and showed a maximum value of 6,000 HK at around x=0.8. The critical load of the coatings, measured by the scratch test, was around 30 N. The wear resistance properties of the ($Ti_{1-x}$$Cr_{ x}$)N coatings were evaluated using a CSEM pin-on-disk type tribometer. A Cr-steel ball as well as a SiC ball, which had hardness values of 590 HK and 2,600 HK respectively, were used as the pin. After the wear test, the surface morphology, roughness and the concentration of the coatings were investigated, with the main focus being on the effect of wear debris and the transferred layer on the wear behavior.
Inorganic oxide colloids dispersed in alcohol were applied to a stainless steel substrate to produce oxide coatings for the purpose of minimizing emissive thermal transfer. The microstructure, roughness, infrared emissive energy, and surface heat loss of the coated substrate were observed with a variation of the nano oxide sol and coating method. It was found that the indium tin oxide, antimony tin oxide, magnesium oxide, silica, titania sol coatings may reduce surface heat loss of the stainless steel at 300${\circ}C$. It was possible to suppress thermal oxidation of the substrate with the oxide sol coatings during an accelerated thermal durability test at 600${\circ}C$. The silica sol coating was most effective to suppress thermal oxidation at 600${\circ}C$, so that it is useful to prevent the increase of radiative surface heat loss as a heating element. Therefore, the inorganic oxide sol coatings may be applied to improve energy efficiency of the substrate as the heating element.
PMMA와 TBBA의 혼합비를 변화시킨 시료를 질소기류 하에서 비등온 열중량 분석법으로 가열속도 $1-20^{\circ}C/min$, 등온분해온도 $200-300^{\circ}C$로 열분해시킨 시료를 적외선 분광분석한 결과 TBBA의 함량 증가에 따라 활성화에너지 값은 Friedman법으로 28-46 Kcal/mol, Ozawa법으로 28-38 Kcal/mol로 증가 하였다. PMMA에 TBBA의 첨가에 따른 열분해반응은 주쇄 분해반응으로 이루어지며 실제 열중량곡선과 거의 일치되는 최적의 분해반응 모델식을 산출할 수 있었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.