수치해석기법을 이용한 초기 인장잔류응력에 대한 레이저 충격 피닝 효과 분석 (Analysis of the Effects of Laser Shock Peening under Initial Tensile Residual Stress Using Numerical Analysis Method)

  • 김주희;이종우;유삼현
    • 한국군사과학기술학회지
    • /
    • 제20권5호
    • /
    • pp.608-619
    • /
    • 2017
  • In this paper, the effects of parameters related to the residual stress induced due to laser shock peening process to determine mitigation of the initial tensile residual stresses are discussed, such as the maximum pressure, pressure pulse duration, laser spot size and number of laser shots. In order to estimate the influence of the initial tensile residual stresses, which is generated by welding in 35CD4 50HRC steel alloy, the initial condition option was employed in the finite element code. It is found that $2{\times}HEL$ maximum pressure and a certain range of the pressure pulse duration time can produce maximum mitigation effects near the surface and depth, regardless of the magnitudes of tensile residual stess. But plastically affected depth increase with increasing maximum pressure and pressure pulse duration time. For the laser spot size, maximum compressive residual stresses have almost constant values. But LSP is more effective with increasing the magnitudes of tensile residual stress. For the multiple LSP, magnitudes of compressive residual stresses and plastically affected depths are found to increase with increasing number of laser shots, but the effect is less pronounced for more laser shots. And to conclude, even though the initial tensile residual stresses such as weld residual stress field are existed, LSP is enough to make the surface and depth reinforcement effects.

1성분형 실리콘계 실리콘의 열 열화에 대한 인장 성능 평가 (Tensile Properties of One-component Silicon Sealants by Heat Deterioration)

  • 이준;미야우치 히로유키;구경모;최경철;윤민호;미야우치 카오리
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 추계 학술논문 발표대회
    • /
    • pp.173-174
    • /
    • 2013
  • In this study, the tensile properties of sealants by heat deterioration were measured and analysed to gather the basic data of sealant because these studies do not have been investigated in Korea. Most general one-component silicone sealants were used and test specimen was I-type. The test parameters are sealant types which have different density and heat deterioration time in 80℃. As a result, the rat of reduction in area by heat deterioration was considerable increased at SR-A compared with SR-B. The tensile properties by heat deterioration decreased at SR-A because the specimen by deterioration occurred adhesive failure before tensile test. However, SR-B specimen was increased at maximum tensile stress but decreased at elongation in maximum tensile stress. Also, Maximum principal stress was measured at the edge of specimen by FEM simulation in order to find out failure points.

  • PDF

구속된 건조수축이 철근콘트리트 인장거동에 미치는 영향 (Tensile Behavior of Reinforced Concrete Member due to Restrained Shrinkage)

  • 안태송;김진철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회 논문집(I)
    • /
    • pp.315-320
    • /
    • 1998
  • The experimental set-up and one-dimensional analytical model have been developed to investigate the tensile behavior of reinforced concrete member due to restrained drying shrinkage. The experimental results have been compared with the analytical prediction of the maximum residual stress of steel and concrete due to restrained shrinkage. The tensile residual stress concrete by one-dimensional bilinear model shows 0.19 and 0.63 of tensile strength for 0.83% and 3.29 of steel ratio. The residual tensile stress of concrete increases as the steel ratio increases. The effect of steel fiber has not influenced the residual stress due to restrained shrinkage of concrete.

  • PDF

Strength properties of lime stabilized and fibre reinforced residual soil

  • Okonta, Felix N.;Nxumalo, Sinenkosi P.
    • Geomechanics and Engineering
    • /
    • 제28권1호
    • /
    • pp.35-48
    • /
    • 2022
  • The effect of discrete polypropylene fibre reinforcement on shear strength parameters, tensile properties and isotropic index of stabilized compacted residual subgrade was investigated. Composites of compacted subgrade were developed from polypropylene fibre dosage of 0%, 1%, 2.5% and 4% and 3% cement binder. Saturated compacted soil benefited from incremental fibre dosage, the mobilized friction coefficient increased to a maximum at 2.5% fibre dosage from 0.41 to 0.58 and the contribution due to further increase in fibre dosage was marginal. Binder stabilization increased the degree of isotropy for unreinforced soil at lower fibre dosage of 1% and then decreased with higher fibre dosage. Saturation of 3% binder stabilized soil decreased the soil friction angle and the degree of isotropy for both unstabilized and binder stabilized soil increased with fibre dosage. The maximum tensile stress of 3% binder stabilized fibre reinforced residual soil was 3-fold that of 3% binder stabilized unreinforced soil. The difference in computed and measured maximum tensile and tangential stress decreased with increase in fibre dosage and degree of stabilization and polypropylene fibre reinforced soil met local and international criteria for road construction subgrade.

Simplified approach for the evaluation of critical stresses in concrete pavement

  • Vishwakarma, Rameshwar J.;Ingle, Ramakant K.
    • Structural Engineering and Mechanics
    • /
    • 제61권3호
    • /
    • pp.389-396
    • /
    • 2017
  • Concrete pavements are subjected to traffic and environmental loadings. Repetitive type of such loading cause fatigue distress which leads to failure by forming cracks in pavement. Fatigue life of concrete pavement is calculated from the stress ratio (i.e. the ratio of applied flexural stress to the flexural strength of concrete). For the correct estimation of fatigue life, it is necessary to determine the maximum flexural tensile stress developed for practical loading conditions. Portland cement association PCA (1984) and Indian road congress IRC 58 (2015) has given charts and tables to determine maximum edge stresses for particular loading and subgrade conditions. It is difficult to determine maximum stresses for intermediate loading and subgrade conditions. The main purpose of this study is to simplify the analysis of rigid pavement without compromising the accuracy. Equations proposed for determination of maximum flexural tensile stress of pavement are verified by finite element analysis.

반복 인장 하중을 받는 YP47 극후판 Butt 용접부의 잔류응력 재분포에 관한 연구 (A Study on Evaluation of Residual Stress Redistribution for FCA Butt Weldment of Ultra-Thick YP47 Steel Plate under Tensile Cyclic Load)

  • 강봉국;이동주;신상범
    • Journal of Welding and Joining
    • /
    • 제34권4호
    • /
    • pp.28-33
    • /
    • 2016
  • The purpose of this study is to evaluate the redistribution of transverse residual stress in the multi-pass FCA butt weld of YP47 in the hatch coaming top plate of ultra large size containership under the tensile cyclic load. In order to do it, the configuration of modified H type specimen including restraint length was first designed to simulate the restraint condition of the butt weld in hatch coaming top plate. FE analysis procedure for evaluating the transverse residual stress was verified by comparing the calculated mean and surface residual stresses with the measured results in the test specimen. After that, the effect of the cyclic load on the redistribution of transverse residual stress was evaluated by comprehensive FEA. From the results, it was found that although the maximum transverse residual stress decreased with an increase in the applied maximum load, the effect of the cyclic load on the mean residual stress is small enough to be negligible. It is because the maximum stress of the ship corresponding to the probability of 10E-8 is less than 70% of yield stress of the weld.

고강도강재의 고온인장특성 및 용접시 잔류응력특징에 관한 연구 (A Study on the High Temperature Tensile Property and the Characteristics of Residual Stress in Welds of High Strength Steels)

  • 장경호;이진형;신영의
    • Journal of Welding and Joining
    • /
    • 제22권4호
    • /
    • pp.50-58
    • /
    • 2004
  • In this study, high temperature tensile properties of high strength steels(POSTEN60, POSTEN80) were investigated. The three-dimensional thermal elastic-plastic analyses were conducted to investigate the characteristics of welding residual stresses in welds of high strength steels on the basis of thermal and mechanical properites at high temperature obtained from the experiment. According to the results, high temperature tensile strength of POSTEN60 steel deteriorated slowly to 10$0^{\circ}C$. As the temperature went up, the tensile strength became better because of blue shortness, and it deteriorated radically after reaching to the maximum value around 30$0^{\circ}C$. For the POSTEN80 steel, high temperature tensile strength deteriorated slowly to 20$0^{\circ}C$. As the temperature went up the tensile strength became better and it deteriorated slowly to $600^{\circ}C$ after reached to the maximum value around 30$0^{\circ}C$. Strain of high strength steels at the elevated temperature increased radically after the mercury rose to $600^{\circ}C$. The strain hardening ratio of POSTEN60 steel was larger then that of POSTEN80 steel at the elevated temperature as in the case at the room temperature and it became smaller radically after the mercury rose to 40$0^{\circ}C$. And, in the welding of high strength steels, increasing tensile strength of the steel (POSTEN60

Stress intensity factors for an interface crack between an epoxy and aluminium composite plate

  • Itou, S.
    • Structural Engineering and Mechanics
    • /
    • 제26권1호
    • /
    • pp.99-109
    • /
    • 2007
  • A cracked composite specimen, comprised of an epoxy and an aluminium plate, was fractured under a tensile load. In this paper, two crack configurations were investigated. The first was an artificial center crack positioned in the epoxy plate parallel to the material interface. The other was for two edge cracks in the epoxy plate, again, parallel to the interface. A tensile test was carried out by gradually increasing the applied load and it was verified that the cracks always moved suddenly in an outward direction from the interface. The d/a ratio was gradually reduced to zero, and it was confirmed that the maximum stress intensity factor value for the artificial center crack, $K_{{\theta}{\theta}}^{max}$, approached that of an artificial interface crack,$K_{{\theta}{\theta}}^{ifc\;max}$ (where: 2a is the crack length and d is the offset between the crack and interface). The same phenomenon was also verified for the edge cracks. Specifically, when the offset, d, was reduced to zero, the maximum stress intensity factor value, $K_{{\theta}{\theta}}^{max}$, approached that of an artificial interface edge crack.

PMMA의 동적 인장 거동 (Dynamic tensile behavior of PMMA)

  • 이억섭;김면수;황시원
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.395-400
    • /
    • 2001
  • The Split Hopkinson Pressure Bar(SHPB) technique, a special experimental apparatus, has been used to obtain the material behavior under high strain rate loading condition. In this paper, dynamic deformation behaviors of the PMMA under high strain rate tensile loading are determined using SHPB technique.

  • PDF

Fatigue Strength Evaluation of the Clinch Joints of a Cold Rolled Steel Sheet

  • Kim, Ho-Kyung
    • International Journal of Railway
    • /
    • 제2권4호
    • /
    • pp.131-138
    • /
    • 2009
  • Static tensile and fatigue tests were conducted using tensile-shear specimens to evaluate the fatigue strength of a SPCC sheet clinch joint. The maximum tensile strength of the specimen produced at the optimal punching force was 1750 kN. The fatigue endurance limit (=760 N) approached 43% of the maximum tensile load (=1750 N) at a load ratio of 0.1, suggesting that the fatigue limit is approximately half of the value of the maximum tensile strength. The FEM analysis showed that at the fatigue endurance limit, the maximum von-Mises stress of 373 MPa is very close to the ultimate tensile strength of the SPCC sheet (=382 MPa).

  • PDF