• Title/Summary/Keyword: High rate dry etching

Search Result 63, Processing Time 0.026 seconds

Dry etching properties of SBT thin films using $Cl_2/Ar$ inductively coupled plasma ($Cl_2/Ar$ 유도결합 플라즈마를 이용한 SBT 박막의 건식 식각 특성)

  • Yeo, Ji-Won;Kim, Kyoung-Tae;Kim, Dong-Pyo;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07a
    • /
    • pp.404-407
    • /
    • 2003
  • Among the ferroeletric thin films that have been widely investigated for ferroelectric random access memory (FRAM) applications, the $SrBi_2Ta_2O_9$ (SBT) thin film is appropriate as a memory capacitor material due to its excellent fatigue endurance. SBT thin films were etched in high-density $Cl_2/Ar$ in inductively coupled plasma. The maximum etch rate of SBT film is $1834\;{\AA}/min$ under $Cl_2/(Cl_2+Ar)$ of 30 %, rf power of 700 W, dc-bias voltage of -250 V, chamber pressure of 11 mTorr and gas flow rate of 20 sccm.

  • PDF

Improvement of Etch Rate and Profile by SF6, C4F8, O2 Gas Modulation (SF6, C4F8, O2 가스 변화에 따른 실리콘 식각율과 식각 형태 개선)

  • Kwon, Soon-Il;Yang, Kea-Joon;Song, Woo-Chang;Lim, Dong-Gun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.4
    • /
    • pp.305-310
    • /
    • 2008
  • Deep trench etching of silicon was investigated as a function of RF source power, DC bias voltage, $C_4F_8$ gas flow rate, and $O_2$ gas addition. On increasing the RF source power from 300 W to 700 W, the etch rate was increased from $3.52{\mu}m/min$ to $7.07{\mu}m/min$. The addition of $O_2$ gas improved the etch rate and the selectivity. The highest etch rate is achieved at the $O_2$ gas addition of 12 %, The selectivity to PR was 65.75 with $O_2$ gas addition of 24 %. At DC bias voltage of -40 V and $C_4F_8$ gas flow rate of 30 seem, We were able to achieve etch rate as high as $5.25{\mu}m/min$ with good etch profile.

Investiagtions on the Etching of Platinum Film using High Density Inductively Coupled Ar/Cl$_2$ HBr Plasmas

  • Kim, Nam-Hoon;Chang-Il kim;Chang, Eui-Goo;Kwon, Kwang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.1 no.3
    • /
    • pp.14-17
    • /
    • 2000
  • Giga bit dynamic random access memory(DRAM) requires the capacitor of high dielectric films. Some metal oxides films have been proposed as the dielectric material . And Pt is one of the most promising electrode materials. However very little has been done in developing the etching technologoy Pt film. Therefore, it is the first priority to develop the technology for plasma etching of Pt film. In this study, the dry etching of Pt film was investigated in Inductively Coupled Plasma(ICP) etching system with Cl$_2$/Ar and HBr/Cl$_2$/Ar gas mixing. X-ray photoelectron spectroscopy (XPS) was used in analysis of sidewall residues for the understanding of etching mechanism. We found the etch residues on the pattern sidewall is mainly Pt-Pt, Pt-Cl and Pt-Br compounds, Etch profile was observed by Scanning Electron Spectroscopy(SEM) . The etch rate of Pt film at 10%, Cl$_2$/90% Ar gas mixing ration was higher than at 100%. Ar. Addition of HBr to Cl$_2$/Ar as an etching gas led to generally higher selectivity to SiO$_2$. And the etch residues were reduced at 5% HBr/5% Cl$_2$/90% Ar gas mixing ration. These pages provide you with an examples of the layout and style which we wish you to adopt during the preparation of your paper, Make the width of abstract to be 14cm.

  • PDF

The Dry Etching Properties of TaN Thin Film Using Inductively Coupled Plasma

  • Woo, Jong-Chang;Joo, Young-Hee;Kim, Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • v.13 no.6
    • /
    • pp.287-291
    • /
    • 2012
  • We investigated the etching characteristics of TaN thin films in an $O_2/BCl_3/Cl_2/Ar$ gas using a high density plasma (HDP) system. A maximum etch rate of the TaN thin films and the selectivity of TaN to $SiO_2$ were obtained as 172.7 nm/min and 6.27 in the $O_2/BCl_3/Cl_2/Ar$ (3:2:18:10 sccm) gas mixture, respectively. At the same time, the etch rate was measured as a function of the etching parameters, such as the RF power, DC-bias voltage, and process pressure. The chemical states on the surface of the etched TaN thin films were investigated using X-ray photoelectron spectroscopy. Auger electron spectroscopy was used for elemental analysis on the surface of the etched TaN thin films. These surface analyses confirm that the surface of the etched TaN thin film is formed with the nonvolatile by-product.

Dry Etching Properties of HfAlO3 Thin Film with Addition O2 gas Using a High Density Plasma

  • Woo, Jong-Chang;Lee, Yong-Bong;Kim, Jeong-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.15 no.3
    • /
    • pp.164-169
    • /
    • 2014
  • We investigated the etching characteristics of $HfAlO_3$ thin films in $O_2/Cl_2/Ar$ and $O_2/BCl_3/Ar$ gas, using a high-density plasma (HDP) system. The etch rates of the $HfAlO_3$ thin film obtained were 30.1 nm/min and 36 nm/min in the $O_2/Cl_2/Ar$ (3:4:16 sccm) and $O_2/BCl_3/Ar$ (3:4:16 sccm) gas mixtures, respectively. At the same time, the etch rate was measured as a function of the etching parameter, namely as the process pressure. The chemical states on the surface of the etched $HfAlO_3$ thin films were investigated by X-ray photoelectron spectroscopy. Auger electron spectroscopy was used for elemental analysis on the surface of the etched $HfAlO_3$ thin films. These surface analyses confirm that the surface of the etched $HfAlO_3$ thin film is formed with nonvolatile by-product. Also, Cl-O can protect the sidewall due to additional $O_2$.

High density plasma etching of single crystalline $La_3Ga_5SiO_{14}$ for wide band high temperature SAW filter devices (광대역 고온용 SAW filter 소자용 $La_3Ga_5SiO_{14}$ 단결정의 고밀도 플라즈마 식각)

  • Cho, Hyun
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.6
    • /
    • pp.234-238
    • /
    • 2005
  • Effects of plasma composition, ion flux and ion energy on the etch rate, surface morphology and near surface stoichiometry of a single crystalline $La_3Ga_5SiO_{14}$ wafer have been examined in $Cl_2/Ar$ inductively coupled plasma (ICP) discharges. Maximum etch rate ${\sim}1600{\AA}/min$ was achieved either at relatively high source power $({\sim}1000W)$ or high $Cl_2$ content conditions in $Cl_2/Ar$ discharges. The etched surfaces showed similar or better RMS roughness values than those of the unetched control sample and the near surface stoichiometry was found not to be affected by ICP etching.

F Ion-Assisted Effect on Dry Etching of GaAs over AlGaAs and InGaP (GaAs/AlGaAs와 GaAs/InGaP의 건식 식각 시 Flourine 이온의 효과)

  • Jang, Soo-Ouk;Park, Min-Young;Choi, Chung-Ki;Yoo, Seung-Ryul;Lee, Je-Won;Song, Han-Jung;Jeon, Min-Hyon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.164-165
    • /
    • 2005
  • The dry etch characteristics of GaAs over both AlGaAs and InGaP in planar inductively coupled $BCl_3$-based plasmas(ICP) with additions of $SF_6$ or $CF_4$ were studied. The additions of flourine gases provided enhanced etch selectivities of GaAs/AlGaAs and GaAs/InGaP. The etch stop reaction involving formation of involatile $AlF_3$ and $InF_3$ (boiling points of etch products: $AlF_3\sim1300^{\circ}C$, $InF_3$ > $1200^{\circ}C$ at atmosphere) were found to be effective under high density inductively coupled plasma condition. Decrease of etch rates of all materials was probably due to strong increase of flourine atoms in the discharge, which blocked the surface of the material against chlorine neutral adsorption. The process parameters were ICP source power (0 - 500 W), RF chuck power (0 - 30 W) and variable gas composition. The process results were characterized in terms of etch rate, selectivities of GaAs over AlGaAs and InGaP, surface morphology, surface roughness and residues after etching.

  • PDF

Dry Etching of $Al_2O_3$ Thin Film in Inductively Coupled Plasma

  • Xue, Yang;Um, Doo-Seung;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.67-67
    • /
    • 2009
  • Due to the scaling down of the dielectrics thickness, the leakage currents arising from electron tunneling through the dielectrics has become the major technical barrier. Thus, much works has focused on the development of high k dielectrics in both cases of memories and CMOS fields. Among the high-k materials, $Al_2O_3$ considered as good candidate has been attracting much attentions, which own some good properties as high dielectric constant k value (~9), a high bandgap (~2eV) and elevated crystallization temperature, etc. Due to the easy control of ion energy and flux, low ownership and simple structure of the inductively coupled plasma (ICP), we chose it for high-density plasma in our study. And the $BCl_3$ was included in the gas due to the effective extraction of oxygen in the form of BClxOy compound. In this study, the etch characteristic of ALD deposited $Al_2O_3$ thin film was investigated in $BCl_3/N_2$ plasma. The experiment were performed by comparing etch rates and selectivity of $Al_2O_3$ over $SiO_2$ as functions of the input plasma parameters such as gas mixing ratio, DC-bias voltage and RF power and process pressure. The maximum etch rate was obtained under 15 mTorr process perssure, 700 W RF power, $BCl_3$(6 sccm)/$N_2$(14 sccm) plasma, and the highest etch selectivity was 1.9. We used the x-ray photoelectron spectroscopy (XPS) to investigate the chemical reactions on the etched surface. The Auger electron spectroscopy (AES) was used for elemental analysis of etched surface.

  • PDF

Plasma Etching Characteristics of Sapphire Substrate using $BCl_3$-based Inductively Coupled Plasma ($BCl_3$ 계열 유도결합 플라즈마를 이용한 사파이어 기판의 식각 특성)

  • Kim, Dong-Pyo;Woo, Jong-Chang;Um, Doo-Seng;Yang, Xue;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.363-363
    • /
    • 2008
  • The development of dry etching process for sapphire wafer with plasma has been key issues for the opto-electric devices. The challenges are increasing control and obtaining low plasma induced-damage because an unwanted scattering of radiation is caused by the spatial disorder of pattern and variation of surface roughness. The plasma-induced damages during plasma etching process can be classified as impurity contamination of residual etch products or bonding disruption in lattice due to charged particle bombardment. Therefor, fine pattern technology with low damaged etching process and high etch rate are urgently needed. Until now, there are a lot of reports on the etching of sapphire wafer with using $Cl_2$/Ar, $BCl_3$/Ar, HBr/Ar and so on [1]. However, the etch behavior of sapphire wafer have investigated with variation of only one parameter while other parameters are fixed. In this study, we investigated the effect of pressure and other parameters on the etch rate and the selectivity. We selected $BCl_3$ as an etch ant because $BCl_3$ plasmas are widely used in etching process of oxide materials. In plasma, the $BCl_3$ molecule can be dissociated into B radical, $B^+$ ion, Cl radical and $Cl^+$ ion. However, the $BCl_3$ molecule can be dissociated into B radical or $B^+$ ion easier than Cl radical or $Cl^+$ ion. First, we evaluated the etch behaviors of sapphire wafer in $BCl_3$/additive gases (Ar, $N_2,Cl_2$) gases. The behavior of etch rate of sapphire substrate was monitored as a function of additive gas ratio to $BCl_3$ based plasma, total flow rate, r.f. power, d.c. bias under different pressures of 5 mTorr, 10 mTorr, 20 mTorr and 30 mTorr. The etch rates of sapphire wafer, $SiO_2$ and PR were measured with using alpha step surface profiler. In order to understand the changes of radicals, volume density of Cl, B radical and BCl molecule were investigated with optical emission spectroscopy (OES). The chemical states of $Al_2O_3$ thin films were studied with energy dispersive X-ray (EDX) and depth profile anlysis of auger electron spectroscopy (AES). The enhancement of sapphire substrate can be explained by the reactive ion etching mechanism with the competition of the formation of volatile $AlCl_3$, $Al_2Cl_6$ or $BOCl_3$ and the sputter effect by energetic ions.

  • PDF