The Facing Targets Sputtering(FTS) system has several advantages for preparing films over a wide range of working gas pressure on plasma-free substrates. Co-Cr thin films seem to be one of the most promising media for perpendicular magnetic recording system. In this study, the capabillities of the system fordepositing C0-Cr films have been investigated. Under various Ar gas pressure, films with morphologically dense microstructure and good c-axis orientation were deposited, even when the incident angle $\psi_x$ of sputtered part icles to the film plane was below abount $50^{\circ}C$. this may imply that the shadowing effect by obique incidence of particle can be compensated by rapid surface diffusion owing to the high kinetic energy of particles arriving at the growing film. It has been confirmed that the FTS system is very useful for perparing Co-Cr thin films recorging media.
ZnO : Al transparent conductive thin films were prepared by facing targets sputtering system with a DC power supply which can deposit a high quality thin films and control deposition condition in all range of $O_2$ gas ratio using ZnO target containing 8 at% of Al. Sputtering was carried out at a substrate temperature of R T with a DC current of 0.6 A and $O_2$ flow rate of 0 $\sim$ 0.9. The characteristics of ZnO : Al thin films was investigated by $\alpha$-step, four point probe, X-ray diffraction and UV/VIS spectrometer.
We prepared ZnO thin film with Facing Targets Sputtering system that can deposit thin film in plasma-free situation and change the deposition condition in wide range. And prepared thin film's c-axis orientation and grain size were analyzed by XRD(x-ray diffractometer). In the results, we suggest that FTS system is very suitable to preparing high quality ZnO thin film with good c-axis orientation.
Aluminum nitride having a dense hexagonal structure is used as a high-temperature material because of its excellent heat resistance and high mechanical strength; its excellent piezoelectric properties are also attracting attention. The structure and residual stress of AlN thin films formed on glass substrate using TFT sputtering system are examined by XRD. The deposition conditions are nitrogen gas pressures of 1 × 10-2, 6 × 10-3, and 3 × 10-3, substrate temperature of 523 K, and sputtering time of 120 min. The structure of the AlN thin film is columnar, having a c-axis, i.e., a <00·1> orientation, which is the normal direction of the glass substrate. An X-ray stress measurement method for crystalline thin films with orientation properties such as columnar structure is proposed and applied to the residual stress measurement of AlN thin films with orientation <00·1>. Strength of diffraction lines other than 00·2 diffraction is very weak. As a result of stress measurement using AlN powder sample as a comparative standard sample, tensile residual stress is obtained when the nitrogen gas pressure is low, but the gas pressure increases as the residual stress is shifts toward compression. At low gas pressure, the unit cell expands due to the incorporation of excess nitrogen atoms.
Piezoelectric ZnO thin films were deposited on slide glass by Facing Targets Sputtering(FTS). The Facing Targets Sputtering system can deposit thin film in plasma-free situation and change the deposition condition in wide range. The characteristics of zinc oxide thin films on power, working pressure, and substrate temperature were investigated by XRD (x-ray diffractometer), alpha-step (Tencor) and SEM (Scanning Electron Microscopy) analyses. In the results, we suggest that FTS system is very suitable to preparing high quality ZnO thin films with good c-axis orientation.
We prepared Co-Cr thin film for perpendicular magnetic recording media with facing targets sputtering system(FTS system) which can deposit a high quality thin film in plasma-free state and wide range of working pressure. The effect of sputtering conditions(argon gas pressure and substrate temperature) on the magnetic and the crystallographic characteristic of Co-Cr thin film was investigated. And the variation of perpendicular coercivity with the variation of film thickness was studied. As a result we obtained the high perpendicular coercivity of 1900Oe and the good dispersion angle of c-axis($\Delta$$\theta$$_{50}$) of 5$^{\circ}$on the film thickness of 100nm for the promising recording layer of perpendicular magnetic recording media.c recording media.a.
We prepared Co-Cr-Ta and Co-Cr-Ta/Ti thin film for perpendicular magnetic recording media by facing targets sputtering system (FTS system). Ti underlayer effects on crystallographic and magnetic characteristics of Co-Cr-Ta perpendicular magnetic recording media have been investigated. Crystallgraphic and magnetic characteristic of prepared thin films were evaluated by x-ray diffractometry(XRD), vibrating sample magnetometer(VSM) and kerr hysteresis loop measurement. The coercivity and anisotropy field increase by introduced Ti underlayer when substrate temperature is higher than 150$^{\circ}C$. The c-axis dispersion angle and grain size of Co-Cr-Ta/Ti thin film is decrease than Co-Cr-Ta when substrate temperature is higher than 100$^{\circ}C$. Consequently, the use of a Ti underlayer highly orientated can be improved crystallographic and magnetic characteristics of Co-Cr -Ta perpendicular media layer.
In this paper we studied that the effect of substrate temperature on crystallography and electrical properties of ZnO thin films. Facing Targets Sputtering system can deposit thin films in plasma-free situation and change the deposition condition in wide range. And prepared thin film\`s c-axis orientation and grain size were analyzed by XRD(x-ray diffractometer). In the results, we suggest that FTS system is very suitable to preparing high quality ZnO thin film with good c-axis orientation.
Kim, H.W.;Keum, M.J.;Lee, K.S.;Kim, H.K.;Kim, K.H.
한국정보디스플레이학회:학술대회논문집
/
한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
/
pp.1477-1479
/
2005
In this work, the ITO thin films were prepared by FTS (Facing Targets Sputtering) system under different sputtering conditions which were varying $O_2$ gas flow, input current at room temperature. As a function of sputtering conditions, electrical and optical properties of prepared ITO thin films were measured. The electrical, optical characteristics and surface roughness of prepared ITO thin films were measured. In the results, as increasing $O_2$ gas 0.1[sccm] to 0.7[sccm], resistivity of ITO thin film was increased with a decreasing carrier concentration, $O_2$ gas over 0.3[sccm] the carrier mobility have a similarly value. Transmittance of prepared ITO thin films were improved at increasing $O_2$ gas 0.1[sccm] to 0.7[sccm]. And transmittance of all of the prepared ITO thin films was over 80%. We could obtain resistivity $6.19{\times}10^{-4}[{\omega}{\cdot}cm]$, carrier mobility $22.9[cm^2/V{\cdot}sec]$, carrier concentration $4.41{\times}10^{20}[cm^{-3}]$ and transmittance over 80% of ITO thin film prepared at working pressure 1mTorr, input current 0.4A without any substrate heating.
We report on plasma damage free-sputtering technologies for organic light emitting diodes (OLEDs), organic thin film transistor (OTFT) and flexible displays by using a box cathode sputtering (BCS) method. Specially designed BCS system has two facing targets generating high magnetic fields ideally entering and leaving the targets, perpendicularly. This target geometry allows the formation of high-density plasma between targets and enables us to realize plasma damage free sputtering on organic layer without protection layer against plasma. The OLED with Al cathode prepared by BCS shows electrical and optical characteristics comparable to OLED with thermally evaporated Mg-Ag cathode. It was found that OLED with Al cathode layer prepared by BCS has much lower leakage current density ($1{\times}10^{-5}\;mA/cm^2$ at -6 V) than that $(1{\times}10^{-2}{\sim}-10^0\;mA/cm^2)$ of OLED prepared by conventional DC sputtering system. This indicates that BCS technique is a promising electrode deposition method for substituting conventional thermal evaporation and DC/RF sputtering in fabrication process of organic based optoelectronics.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.