• 제목/요약/키워드: Extrados

검색결과 35건 처리시간 0.032초

대변형 효과를 고려한 원주방향 관통균열 엘보우의 닫힘굽힘 한계하중에 미치는 내압 영향 평가 (Effect of Internal Pressure on Plastic Limit Loads for Elbows with Circumferential Through-wall Crack under Closing Bending Incorporating Large Geometry Change Effects)

  • 홍석표;김윤재
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.1778-1782
    • /
    • 2007
  • Based on three-dimensional (3-D) FE limit analyses, this paper estimates effect of internal pressure on plastic limit loads for elbows with circumferential through-wall crack under in-plane bending incorporating large geometry change effects. Circumferential through-wall crack in extrados is considered. The FE limit analyses using the large geometry change option provide plastic collapse loads (using the twice-elastic-slope method). For the bending mode, closing bending is considered. Other relevant variables affecting plastic limit loads are systematically varied, related to pipe bend geometry (the mean radius, thickness and bend curvature) and defect geometry (the length of circumferential through-wall crack).

  • PDF

엘보우의 붕괴모멘트에 미치는 감육결함의 영향 (Effect of Wall Thinning Defect on the Collapse Moment of Elbow)

  • 김진원;김태순;박치용
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.622-628
    • /
    • 2003
  • The purpose of this study is to evaluate the effect of local wall thinning on the collapse of elbow subjected to internal pressure and bending moment. Thus, the nonlinear 3D finite element analyses were performed to obtained collapse moment of elbow containing various wall thinning defects under two loading; modes (closing and opening modes) and defect locations (intrados and extrados). From the results of analyses, the influence of wall thinning defect on the global moment-rotation behavior of elbow was discussed, and the dependance of collapse moment of elbow on wall thinning depth, length, and circumferential angle was investigated under different loading mode and defect location.

  • PDF

관통균열이 존재하는 증기발생기 전열관의 파열압력 평가 (Burst Pressure Evaluation for Through-Wall Cracked Tubes in the Steam Generator)

  • 김현수;김종성;진태은;김홍덕;정한섭
    • 대한기계학회논문집A
    • /
    • 제28권7호
    • /
    • pp.1006-1013
    • /
    • 2004
  • Operating experience of steam generators shows that the tubes are degraded by stress corrosion cracking, fretting wear and so on. These defected tubes could stay in service if it is proved that the tubes have sufficient structural margin to preclude the risk of tube bursting. This paper provides detailed plastic limit pressure solutions for through-wall cracks in the steam generator tubes. These are developed based on three dimensional(3D) finite element analyses assuming elastic-perfectly plastic material behavior. Both axial and circumferential through-wall cracks in free span and in u-bend regions are considered. The resulting limit pressure solutions are given in a polynomial form, and thus can be simply used in practical integrity assessment of the steam generator tubes.

유한요소해석에 기초한 감육곡관 손상압력 평가 모델 개발 (Development of Failure Pressure Evaluation Model for Local Wall-Thinned Elbows Based on Finite Element Analysis)

  • 김진원;박종선
    • 대한기계학회논문집A
    • /
    • 제32권12호
    • /
    • pp.1063-1071
    • /
    • 2008
  • This paper provides a failure pressure evaluation model for local wall-thinned elbows. In this study, parametric finite element analyses are performed on the elbows containing local wall-thinning defect at their intrados and extrados, and the failure pressures are obtained from the analysis results by applying a local failure criterion that was validated by real-scale pipe tests. An evaluation model including the effects of thinning depth, length, circumferential angle, thinning location, and elbow geometries on the failure pressure is derived based on the evaluated failure pressures. The proposed model agrees well with the results of finite element analyses and reasonably estimates the dependence of failure pressure on the wall-thinning dimensions and elbow geometries. Also, the comparison with experimental data demonstrates that the proposed evaluation model can accurately predict the failure pressure of local wall-thinned elbows.

In-plane 굽힘 조건에서 감육엘보우 거동에 미치는 내압의 영향 (Effect of Internal Pressure on the Behavior of Wall Thinned Elbow under In-Plane Bending)

  • 김진원;김태순;박치용
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.268-273
    • /
    • 2004
  • This study is conducted to clarify the effect of internal pressure on the deformation and collapse behaviors of wall thinned elbow under in-plane bending moment. Thus the nonlinear three-dmensional finite element analyses were performed to obtain the moment-rotation curve of elbow contatining various wall thinning defects located at intrados and extrados under in-plane bending (closing and opening modes) with internal pressure of $0{\sim}15MPa.$ From the results of analysis, the effect of internal of collapse moment of elbow on the global deformation behavior of wall thinned elbow was discussed, and the dependence of collapse moment of elbow on the magnitude of internal pressure was investigated under different loading mode, defect location, and defect shape.

  • PDF

얇은 두께로 된 U 전열관의 잔류응력 및 부하응력 해석 (Analysis of Residual and Applied Stresses of Thin-walled U tubes)

  • 김우곤;김대환;류우석;국일현;김성청
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1999년도 춘계학술대회 논문집
    • /
    • pp.163-169
    • /
    • 1999
  • Residual stresses causing stress corrosion cracking (SCC) of thin-walled steam generator U tubes were investigated. The residual stresses were measured by hole drilling methods, and the applied stresses resulting from the internal pressure and the temperature gradient in the steam generator were estimated theoretically. In U-bent regions, the residual stresses at extrados were induced with compressive stress(-), and its maximum value reached -319MPa in axial direction at $\phi$= $0^{\circ}$ in position. Maximum tensile residual stress of 170MPa was found to be at the flank side at position of $\phi$= $90^{\circ}$, i.e., at apex region. Hoop stress due to the pressure and temperature differences between primary and secondary side were analyzed to be 76 MPa and 45 MPa, respectively.

  • PDF

엘보우의 붕괴모멘트에 미치는 국부 감육결함의 영향 (Effect of Local Wall Thinning Defect on the Collapse Moment of Elbow)

  • 김진원;김태순;박치용
    • 대한기계학회논문집A
    • /
    • 제28권4호
    • /
    • pp.402-409
    • /
    • 2004
  • The purpose of this study is to investigate the effect of local wall thinning on the collapse of elbow subjected to internal pressure and bending moment. Thus, the nonlinear three-dimensional finite element analyses were performed to obtain the collapse moment of elbow containing various wall thinning defects located at intrados and extrados under two loading modes (closing and opening modes) with internal pressure. From the results of analysis, the effect of wall thinning defect on the global moment-rotation behavior of elbow was discussed, and the dependence of collapse moment of elbow on wall thinning depth, length, and circumferential angle was investigated under different loading mode and defect location.

Alloy 690 제1열 시제전열관의 U 굽힘가공에서 치수평가 및 표면잔류응력

  • 김우곤;이창규;장진성;국일현;이동희;주영한
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1997년도 춘계학술발표회논문집(2)
    • /
    • pp.110-117
    • /
    • 1997
  • Alloy 690 제1열 시제 전열관을 U 굽힘 가공할 시 전열관에 도입된 표면 잔류응력 및 굽힘 단면에서 치수변화 (벽두께, 진원도)를 위치별로 측정하여 평가하였다. 외측호(extrados)의 표면 잔류응력은 $\psi$=0$^{\circ}$에서 축 방향 응력이 -319 MPa (압축)로 가장 높았으며, 내측호(intrados)는 $\psi$=0$^{\circ}$, 160$^{\circ}$ 위치인 천이영역 부관에서 응력 변화가 크게 되는 경향을 보였다 측면(flank)은 인장 잔류응력으로 $\psi$=90$^{\circ}$(apex)에서 최대 190 MPa 로 축방향 응력으로 나타났다. 잔류응력치는 벽두께 보다는 진원도 변화와 일치되어 나타났으며, 시제 전열관의 벽두께 및 진원도는 ASTM의 치수 허용치 내에 포함되는 것으로 평가되었다. 잔류응력 측정은 스트레인 게이지를 이용한 구멍뚫기 방법 (Hole-Drilling Method)을 사용하였다.

  • PDF

하이드로포밍 응용을 위한 벤딩튜브의 스프링백 특성 (Springback Characteristics of Bent Tubes for Hydroforming Applications)

  • 이호국;박성호
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 제5회 박판성형 SYMPOSIUM
    • /
    • pp.45-48
    • /
    • 2006
  • Recently, the use of tubular hydroforming technology has seen increased usage and increased consideration for wide range of tubular automotive applications. In manufacturing hydroformed parts, bending and pre-forming operations are often required prior to the hydroforming process. Higher bending quality of bent tubes is crucial for the successful hydroforming operation because most of plastic strains and wall thinning at the extrados of bend area occur in the bending operation. Springback is also observed due to elastic recovery of tube material after bending. Proper correction of springback is required not only to well place the bent tube into a hydroforming die cavity but also to avoid pinching when the upper die is brought down to closing position. Therefore, prediction of springback at early development stage is one of the key factors to produce high quality hydroformed parts. In this study, a variety of bending experiments has been carried out to investigate springback amount under change in bending angle and material boosting. Throughout the experimental approach, springback characteristics of bent tubes are quantified according to the change in various bending parameters, and a mathematical model to predict correction amount of springback to a given bend angle is found.

  • PDF

증기발생기 제1열 전열관의 응력 해석 (Stress Analysis of Steam Generator Row-1 Tubes)

  • 김우곤;류우석;이호진;김성청
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 춘계학술대회논문집A
    • /
    • pp.25-30
    • /
    • 2000
  • Residual stresses induced in U-bending and tube-to-tubesheet joining processes of PWR's steam generator row-1 tube were measured by X-ray method and Hole-Drilling Method(HDM). The stresses resulting from the Internal pressure and the temperature gradient in the steam generator were also estimated theoretically. In U-bent lesions, the residual stresses at extrados were induced with compressive stress(-), and its maximum value reached -319 MPa in axial direction at ${\psi}=0^{\circ}$ in position. Maximum tensile residual stress of 170MPa was found to be at the flank side at Position of${\psi}=90^{\circ}$, i.e., at apex region. In tube-to-tubesheet fouling methods, the residual stresses induced by the explosive joint method were found to be lower than that by the mechanical roll method. The gradient of residual stress along the expanded tube was highest at the. transition region, and the residual stress in circumferential direction was found to be higher than the residual stress in axial direction. Hoop stress due to an internal pressure between primary and secondary side was analyzed to be 76 MPa and thermal stress was 45 MPa.

  • PDF