  • The surface region of a sheet metal may have different characteristics from the inner region because the surface region is less restricted than the interior. In addition, the grains on the free surface are less hardened because of surface adsorption of the dislocations, rather than piling up. In the case of bulk or thick sheet metals, this effect is negligible because the fraction of the surface region is much smaller than that of the inner region. However, this surface effect is important in the case of ultra-thin sheet metals. In order to evaluate the surface effect, tensile and bending tests were performed for the SS304 stainless steel with a thickness of 0.39 mm. The bending force predicted using the tensile behavior is higher than the measurement because of the surface effect. To account for the surface effect, the surface layer model was developed by dividing the sheet section into surface and inner layers. The mechanical behaviors of the two regions were calibrated using the tensile and bending properties. The surface layer model reproduced the bending behavior of the ultra-thin sheet metal.

가공식품 설비의 재질별 베이스 프레임에 관한 변형 및 하중 구조해석 (Structural Analysis of Deformation and Force on Base Frame by Materials of Processed Food Equipment)

  • 김기홍;김석호;최원식
    • 한국산업융합학회 논문집
    • /
    • 제25권5호
    • /
    • pp.741-746
    • /
    • 2022
  • In this paper, structural analysis was conducted on the base frame for materials of the conveyor system that automatically produces nurungji. The materials of the base frame were selected as SS400, STS304, Al6063-5. Structural analysis performed Von-Mises stress and maximum displacement for 38 hot plates in real situation, and performed weight of distribution force for yield strength, and calculated safety factor. SS400 and STS304 have little displacement, but Al6063-5 is deformed to 0.149mm, which is 2.6 times greater than other materials. However, since the safety factor was calculated as 8.5, it can be applied to the applicable food processing equipment. The weight of the distributed force for the yield strength of the materials was 17.7kN for SS400, 14.7kN for STS304, and 10.2kN for Al6063-T5. When manufacturing other processed foods with a base frame of the same size, a material suitable for the corresponding weight should be selected.

Fractal Approach to Passivated Surface of Stainless Steel

  • Heo, Jung-Ho;Lee, Yong-Heon;Shin, Heon-Cheol
    • 한국표면공학회지
    • /
    • 제43권1호
    • /
    • pp.12-16
    • /
    • 2010
  • The morphology of the passivated surface of stainless steel (SS) was quantitatively characterized based on fractal geometry. In particular, the surface irregularities of the passivated 304 and 439 SSs were comparatively analyzed in terms of their self-similar fractal dimensions. The passivated surface of 439 SS in an acid-based electrolyte proved to have a higher fractal dimension, as compared to that of 304 SS, esp. at a scale of several tens of nanometers, strongly indicating the higher irregularity of the passivated surface. It is anticipated that the fractal approach suggested herein might be effectively utilized to analyze the irregularity of the steel surface and/or the compactness of the oxide film.

염분분사환경에서 냉연 304 스테인레스강의 부식거동 (The Corrosion Behavior of Cold-Rolled 304 Stainless Steel In Salt Spray Environments)

  • Chiang, M.F.;Young, M.C.;Huang, J.Y.
    • 방사성폐기물학회지
    • /
    • 제9권2호
    • /
    • pp.93-98
    • /
    • 2011
  • 염분분위기에서의 부식은 사용후핵연료의 중간저장 기간동안 304 스테인레스 강재 건식저장용기의 주 열화기구들 중 하나다. 본 연구에서는 감소정도가 서로 다른 냉연 304 스테인레스 강 시편들에 0.5wt.%의 염화나트륨 연무를 분사시키면서 느린 변형속도시험(SSRT)과 중성염 분사시험(NSS)을 $85^{\circ}C$$200^{\circ}C$ 에서 수행하였다. $85^{\circ}C$에서 2000 시간 동안 시험한 NSS시편의 무게 변화는 $200^{\circ}C$에서 시험한 시편의 무게 변화와 크게 달랐다. NSS 시편의 $85^{\circ}C$에서 무게 감량은 미미하였지만, 냉연 감소율이 증가함에 따라서 무게 변화는 점진적으로 감소하였다. $85^{\circ}C$$200^{\circ}C$에서 그리고 염분분사 환경에서 가볍게 냉연 가공된 시편의 SSRT 시험으로부터 얻은 항복강도와 극한 인장응력의 값은 공기 중의 값보다 약간 낮았다. 그러나 염분 분위기에서 부식으로 인한 20% 감소 냉연시편의 강도는 더 이상 변화하지 않았다. 예비결과는 냉연 304 스테인레스 강의 질과 성능이 건식저장용기의 제작을 위한 조건에 맞는다는 것을 증명하였다. 그러나 냉연 스테인레스 강의 장기적인 성능을 더 잘 이해하기 위해서는 염분분위기에서 이 재질의 부식거동에 관한 더 많은 연구가 필요하다.

An optimized condition for corrosion protection of Type 304 Films prepared by unbalanced magnetron sputtering in 3.5% NaCl solution

  • Yoo, Ji-Hong;Ahn, Seung-Ho;Kim, Jung-Gu;Lee, Sang-Yul
    • 한국표면공학회지
    • /
    • 제34권5호
    • /
    • pp.465-474
    • /
    • 2001
  • Type 304SS coatings were performed at 200$\square$ onto AISI 1045 carbon steel substrate using unbalanced magnetron sputtering (UBMS) with an austenitic AISI 304 stainless steel (SS) target of 100mm diameter. The total deposition pressure in the active Ar gas was 2$\times$10$^{-3}$ Torr. Coatings were done at various target power densities and bias voltages. Chemical compositions of metallic elements of the coatings were measured by energy dispersive X-rays spectroscopy (EDS). The structure and the morphology of Type 304SS coatings were investigated by means of X-ray diffraction (XRD) and scanning electron microscopy (SEM). Corrosion properties of the coated specimens were examined using electrochemical polarization measurements and electrochemical impedance spectroscopy in a deaerated 3.5% NaCl solution. The porosity rate was obtained from a comparison of the dc polarization resistance of the uncoated and coated substrates. Scratch adhesion testing was used to compare the critical loads for different coatings. XRD results showed that the sputtered films exhibit a ferritic b.c.c. $\alpha$-phase. Potentiodynamic polarization curves indicated that all samples had much higher corrosion potential and better corrosion resistance than the bare steel substrate. The corrosion performance increased with increasing power density and the adhesion was enhanced at the bias voltage of -50V. An improvement in the corrosion resistance can be obtained with a better coating adhesion. Finally, an optimized deposition condition for corrosion protection was found as $40W/cm^2$ and -50V.

  • PDF

고인장 합금재를 활용한 철근콘크리트 기둥의 내진보강공법 개발에 관한 실험적 연구 (Experimental Study on the Development of a Seismic Reinforcement Method for Reinforced Concrete Columns using High-tensile Alloy Materials)

  • 김도연;장일영
    • 한국재난정보학회 논문집
    • /
    • 제20권2호
    • /
    • pp.411-418
    • /
    • 2024
  • 연구목적: 본 연구에서는고인장 합금재를 활용하여 기존 철근콘크리트 기둥의 내진성능 향상이 가능한 새로운 형식의 볼트 체결식 내진보강재를 개발하고자 한다. 연구방법: 고인장 합금재인 SUS304 및 일반 구조용 강재인 SS275를 이용하여 T형 단면 강판을 제작하고 이를 SCM435의 고장력 볼트로 체결한 내진보강재 실험체를 제작하여 휨 실험을 통해 재료적 특성이 내진 보강성능에 미치는 영향에 대해 비교 분석한다. 연구결과: SUS304를 사용한 실험체가 7% 높은 최대 강도와 22% 높은 항복 강도를 보이며, 360MPa 더 높은 압축응력을 나타낸다. 또한 중립축의 변화도 더 미소하여 더 우수한 내력을 가진 것으로 판단된다. 결론: 동일한 단면에서 SUS304를 사용한 내진보강재가 휨 강도, 항복강도, 인장강도, 중립축 변화, 연성능력 측면에서 더 우수한 것으로 판단되며 추후 연구에서 철근콘크리트 기둥 실물 실험체에 적용함으로써 기둥-보강재간 일체 거동에 대한 실험이 필요하다고 사료된다.

환원제염조건에서 가압경수로 구조재료의 틈부식 특성 (Crevice Corrosion Properties of PWR Structure Materials Under Reductive Decontamination Conditions)

  • 정준영;박상윤;원휘준;최왕규;문제권;박소진
    • 방사성폐기물학회지
    • /
    • 제12권3호
    • /
    • pp.199-209
    • /
    • 2014
  • 가압경수로의 일차계통 제염을 위해 개발된 HYBRID 제염제의 재료부식 특성을 틈부식 시험방법을 사용하여 수행하였다. 기존 제염제의 부식특성과 비교하기 위하여 상용 제염제인 OA, CITROX 제염제의 부식특성도 함께 평가하였다. 시험재료는 가압경수로의 일차계통의 주 재료인 Alloy 600과 304 SS을 대상으로 시험하였다. 틈부식 시험은 가혹조건의 부식시험으로써 내식성이 강한 원전 구조재료의 건전성을 짧은 시간에 잘 확인할 수 있었다. 시험결과 OA와 CITROX 제염제에서는 crevice 시편 표면에 pitting과 IGA가 나타났으나 HYBRID 제염제에서는 국부부식이 전혀 발생되지 않았다. 무게감소 측정결과 HYBRID 제염조건에서는 $1.3{\times}10^{-3}{\mu}m/h$ 이하의 매우 낮은 부식속도를 나타내었다. 반면에, OA 제염제의 경우 Alloy 600은 $4.0{\times}10^{-2}{\mu}m/h$ 로 비교적 균일한 부식율을 나타내었으나, 304 SS의 경우 pH = 2.0 이하에서 급격한 가속부식을 나타내었다. HYBRID 제염제의 경우 일반부식에서뿐만 아니라 crevice 부식조건에서도 거의 부식이 일어나지 않아 PWR 계통제염 시 산화막 용해 후 제염제가 계통재료에 노출되어도 재료의 건전성이 입증되었다.

정면밀링시 절삭신호측정에 의한 공구마모 검출에 관한 연구 (A Study on Detection of Tool Wear by Cutting Signal Measurements in Multi-insert Face Milling)

  • 김성일
    • 한국생산제조학회지
    • /
    • 제6권4호
    • /
    • pp.124-129
    • /
    • 1997
  • The experimental investigation is mainly focused to detect tool wear by cutting signal measurements in multi-insert face milling SS 41 and STS 304. This research have investigated the effects on the insert number, which has relationship with mean-cutting force. AE(acoustic emission) signal, tool life and surface roughness in machining SS41 and STS 304. The cutting force and AE signal are monitored to analyse the cutting process, The surface roughness of the specimens machined by TiN coated tool with the various insert numbers measured at various cutting speeds, feed rates and depths of cut, The width of flank wear is also observed.

  • PDF

온도분포가 이동하는 액체금속로 원통용기의 열적 라체팅 해석

  • 이형연;김종범;이재한;구경회;유봉;곽대영;임용택
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1996년도 춘계학술발표회논문집(4)
    • /
    • pp.235-240
    • /
    • 1996
  • 본 연구에서는 고온의 천이 열하중을 받는 304 SS 재질의 액체금속로 원통용기에 대하여 진행성 변형기구인 열적 라체팅(thermal ratcheting) 변형거동을 해석하였다. 재료의 반복 소성을 나타내는 구성식으로서 Chaboche모델을 이용하였으며 이 모델의 적용을 위하여 ABAQUS의 사용자 프로그램을 개발하였다. 열천이 과정이 반복되는 동안에 축방향의 온도분포 이동에 따른 탄소성 해석을 수행한 결과 소성변형이 각 싸이클마다 누적되어 점진적 변형이 일어났으며 이 해석결과를 시험치와 비교함으로써 해석의 타당성을 검토하였다. 반복 소성거동에 대한 Chaboche 모델을 이용하면 천이 열하중을 받는 304 SS. 재질의 고온구조물에 대하여 라체팅 거동을 정량적으로 평가 할 수 있는 것으로 나타났다.

  • PDF

구조용 압연강재와 스테인리스 강재의 MIG 용접에 대한 기계적 특성연구 (Characteristic study of mechanical properties of Structural rolled steel and Stainless steel for MIG welding)

  • 임종영;윤명진;김상윤;김태규
    • 한국기계가공학회지
    • /
    • 제13권1호
    • /
    • pp.100-106
    • /
    • 2014
  • It is well known that fatigue failures occur on welded structures in industrial application due to repetitive load force. In order to decrease the incidence of fatigue failure, we analyzed the mechanical properties based on structural aspects in rolled steel(SS 400) welded onto stainless steel (STS 304) by the MIG welding method as well as the structure of rolled steel welded onto itself. We compared the hardness, tensile and fatigue properties with two types of samples which had no defects on the welding parts as observed by X-ray topographic analysis. It was found that the tensile and fatigue strength levels of SS 400 welded onto STS 304 by the MIG welding method were higher than those of STS 304 welded onto itself.