• Title/Summary/Keyword: 혼입효과

Search Result 451, Processing Time 0.032 seconds

Mechanical Properties of Early Strength Mortar with Ground Granulated Blast Furnace Slag and Expansive Additive (고로슬래그미분말 및 팽창재를 혼입한 조강형 모르타르의 역학적 특성)

  • Koo, Kyung-Mo;Choi, Jae-Won;You, Byeong-Know;Cha, Wan-Ho;Kang, Bong-Hee
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.2
    • /
    • pp.177-184
    • /
    • 2021
  • In this study, the effects of ground granulated blast furnace slag(GGBFS) and expansive additive(EA) on early strength mortar were examined for the purpose of reducing carbon and improving cement performance. As a result, ealry strength Portland cement(EPC) tended to decrease in flow compared to ordinary Portland cement(OPC), but binder with EPC and GGBFS was possible to obtain higher liquidity than OPC. EPC showed higher compressive strength and shrinkage than OPC. The compressive strength of specimen with EPC and GGBFS was reduced proportionally to the replacement ratio of GGBFS. The replacement ratio of GGBFS above the compressive strength equivalent to OPC was higher under low temperature conditions. The use of GGBFS resulted in high shrinkage compared to OPC, and this characteristic was even greater under low temperature conditions. The shrinkage of specimen with EA was decreased in early ages, but was higher than the OPC in long-term ages.

Characteristics of Concrete Using Ready-Mixed Concrete Recycled Water Mixed with Industrial By-Product Desulfurization Gypsum (산업부산물 탈황석고 혼입 레디믹스트콘크리트 회수수를 이용한 콘크리트의 특성)

  • Kim, Young-Yeop;Lee, Han-Seung
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.4
    • /
    • pp.395-403
    • /
    • 2020
  • CaO-based by-product, which consist of CaO, SO3, Al2O3 and so on, has being used to raw materials of CaO compound. When It was applied to recycling water of remicon, concrete performance can be enhanced because hydration reaction of powder material is accelerated. In this study, activated-sludge, which was putted desulfurization gypsum of CaO-based in recycling water, was manufactured to verify effect of them, and then they was investigated by characteristics of redy-mixde concrete. As a result of concrete tests, it was confirmed that there is no problem of strength or drying shrinkage while ensuring workability. Therefore, the possibility of specific application using activated sludge was confirmed.

Effect of hydroxybutyric-acid on lipid bilayers with respect to layer phase

  • Lee, Gaeul;Park, Jin-Won
    • Journal of the Korean Applied Science and Technology
    • /
    • v.39 no.5
    • /
    • pp.720-726
    • /
    • 2022
  • The behavior changes of the lipid bilayer, induced by the hydroxybutyric-acid incorporation, were investigated with respect to each phase of the layer using fluorescence intensity change. Spherical phospholipid bilayers, called vesicles, were prepared using an emulsion technique. Only in the aqueous inside of the vesicles was encapsulated 8-Aminonaphthalene-1,3,6-trisulfonic-acid-disodium-salt(ANTS). p-Xylene-bis-N-pyridinium-bromide(DPX) was included as a quencher only outside of the vesicles. The fluorescence scale was calibrated with the ANTS-encapsulated vesicles in DPX-dispersed-buffer taken as 100% and the mixture of ANTS and DPX in the buffer as 0%. Hydroxybutyric-acid addition into the vesicle solution led the change in the bilayer. The change was found to be related to the phase of each layer according to the ratio of hydroxybutyric-acid to lipid. These results seem to depend on the stability of the vesicles, due to the osmotic and volumetric effects on the arrangement in both head-group and tail-group.

Comparative Analysis of Conductive Paste in Electroencephalography: Evaluation of Artifact and Satisfaction (뇌파검사에서 전도성 접착제의 비교분석: 인공산물과 만족도 평가)

  • Jae-Hwan SONG;Sung-Hee KIM;Dae-Hyun KIM
    • Korean Journal of Clinical Laboratory Science
    • /
    • v.56 no.1
    • /
    • pp.85-88
    • /
    • 2024
  • Electroencephalography (EEG) is a test that diagnoses epilepsy and measures brain function. During EEG, the space between the electrode and the skin is filled with a conductive paste to reduce the impedance between the electrode and the scalp, which helps measure the EEG signals. This study compared the artifacts of the two representative conductive pastes (Ten20 and Elefix). The artifacts, noise, and satisfaction were surveyed after using the two conductive pastes. The two conductive pastes had similar artifacts and noise, but the survey results showed that the Elefix conductive paste had better satisfaction and adhesion. This result may be explained by the imprinting effect according to the experience of using the Elefix conductive paste first in the EEG class. Hence, further research is needed.

Characteristics of Cement Matrix/Mortar with CaO-based Activated-sludge (CaO원 활성슬러지를 혼입한 시멘트 경화체 및 모르타르의 특성)

  • Lee, Yong-Soo;Ryu, Seong-Lyong;Shin, Kwang-Ho;Chu, Yong-Sik;Kim, Young-Yup
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.4
    • /
    • pp.399-406
    • /
    • 2017
  • CaO-based by-product, which consist of CaO, $SO_3$, $Al_2O_3$ and so on, has being used to raw materials of CaO compound. When It was applied to recycling water of remicon, concrete performance can be enhanced because hydration reaction of powder material is accelerated. In this study, activated-sludge, which was putted desulfurization gypsum of CaO-based in recycling water, was manufactured to verify effect of them, and then they was investigated by characteristics of cement matrix and mortar. As a results, they indicated reduction of setting time and high soundness in cement matrix, and acceleration of hydration reaction can be verified by XRD analysis. Also, it can be maintained good workability if water content by usage of desulfurization gypsum, which used for production of activated-sludge, was adjusted. In addition, it can be verified strength development by activated-sludge although cement content by usage of desulfurization gypsum was reduced.

Estimation of Bond Performance Improvement by Surface Treatment Equipments and Polymer Content by Boned Concrete Overlays (접착식 콘크리트 덧씌우기 경계면 처리 방식 및 폴리머 혼입률에 따른 부착성능 평가)

  • Jung, Won Kyong;Kim, Hyun Seok;Kwon, Oh Seon;Kim, Hyung Bae
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.36 no.1
    • /
    • pp.39-47
    • /
    • 2016
  • Repair methods of aging concrete pavement are generally used composite structure pavements, such a composite structure is subjected to a large impact on the mechanical behavior and ensure long-term commonality integrated under vehicle loads, environmental loads of the public in accordance with the bond strength between old and new concrete. A common of bonded concrete overlays that are currently available is Interface arrangements using a variety of equipment to ensure the excellent bond strength between old and new concrete than standard concrete, mixed with a material such as a polymer in order to improve the adhesion with the material itself. However, these method of constructions are being applied, depending on the developer site presents no special specifications apply when a specific application criteria objectively, this is due to the situation of each individual method, which is based on the difficulty in quality control of the site manager. In this study by performing a field test for polymer content via the variables that contribute most significantly to ensure bond strength and the field element core of the interface processing method and materials to ensure bond strength between the old and the new concrete, it was to derive the construction site construction method that can improve the performance of the bond strength through a review of the construction around the correlations and the bond strength according to the effective performance analysis of the conventional surface treatment process and variation of polymer volume fraction.

Properties on the Shrinkage of High Performance Concrete Using Expansive Additive and Shrinkage Reducing Agent (팽창재 및 수축저감제를 이용한 고성능 콘크리트의 수축특성)

  • Han, Cheon-Goo;Kim, Sung-Wook;Koh, Kyoung-Taek;Pei, Zheng-Lie
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.6
    • /
    • pp.785-793
    • /
    • 2003
  • This study is intended to analyze the effectiveness of expansive additive, shrinkage reducing agent and combination of the two to reduce the autogenous and drying shrinkage of high performance concrete using mineral admixture such as fly ash, blast furnace slag powder and silica fume. According to results, when expansive additive and shrinkage reducing agent are mixed within an appropriate mixing ratio, fluidity and air content are not influenced, and the enhancement of compressive strength is favorable at the age of 91 and 180days. At the mixing ratio of expansive additive of 5% and 10%, the autogenous and drying shrinkage is reduced by 32∼68% and 25∼49% respectively in comparison with plain concrete. And they are reduced by 18∼34% and 16∼26% respectively at the mixing ratio of shrinkage reducing agent of 0.5% and 1.0%, compared with plain concrete. The mixture of EA-SR combined with expansive additive and shrinkage reducing agent is most effective for reduction of shrinkage. Therefore, it is considered that the using method in combination with expansive additive and shrinkage reducing agent is effective to reduce the shrinkage of high performance concrete using mineral admixture such as fly ash, blast slag powder and silica fume.

Characteristics of Eco-friendly Porous Concrete for Seawater Purification Using By-Products of Steel Industry (철강산업 부산물을 활용한 해수정화용 친환경 다공질콘크리트의 특성)

  • Han, Woonwoo;Lee, Byungjae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.1
    • /
    • pp.1-7
    • /
    • 2020
  • As of 2018, Steel slag was generated approximately 24.23 million tons. Howeve, except blast furnace slag, steel slag is a typical by-product which does not have a clearly defined purpose in recycling. Thus, countries around the world are putting great efforts into developing a purpose for the recycling of steel slag. The vast habitat foundation of marine life has been destroyed due to recent reckless marine development and environment pollution, resulting in intensification of the decline of marine resources, and a solution to this issue is imperative. In order to propose a method to recycle large amounts of by-product slag into a material that can serve as an alternative to natural aggregate, the engineering properties and applicability for each mixing factor of environment friendly porous concrete as a material for the composition of seawater purification were in this study. Regarding the nutrient elution properties, it was clear that the nutrients continuously flowed out up to an immersion time by 8 months in natural seawater; the nitrogenous fertilizer displayed excellent elution properties in this regard.

A study on evaluation of flexural toughness of synthetic fiber reinforced shotcrete (구조용 합성섬유 보강 숏크리트 휨인성 평가에 관한 연구)

  • Moon, Kyoung-Sun;Kim, Seog-Jin;Kim, Yeon-Deok;Min, Byeong-Heon;Kim, Sang-Hwan
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.21 no.3
    • /
    • pp.433-452
    • /
    • 2019
  • This study deals with shotcrete reinforcing performance according to the amount of synthetic fiber (PP fiber) and proper evaluation method. The shotcrete compressive strength, flexural strength and flexural toughness were tested by setting the mixing amounts of steel fiber ($37.0kg/m^3$) and synthetic fiber (PP fiber) as parameters ($5.0kg/m^3$, $7.0kg/m^3$ and $9.0kg/m^3$). Particularly, circular panel flexural toughness test (Road and Traffic Authority, RTA) was performed to evaluate the shotcrete energy absorption capacity. As a result, the compressive strength and the bending strength of the steel fiber reinforced shotcrete were large, but the flexural toughness of the synthetic fibe (PP fiber) reinforced shotcrete was large. Therefore, synthetic fiber (PP fiber) reinforced shotcrete is considered to have a reinforcing effect comparable to that of steel fiber reinforced shotcrete. Analysis of the relationship between the flexural toughness and the energy absorption capacity of synthetic fiber (PP fiber) reinforced shotcrete revealed that the energy absorbing ability is exhibited at a flexural toughness lower than the allowable standard (3.0 MPa). (Class A: 2.55 MPa = 202J, Class B: 2.72 MPa = 282J, Class C: 3.07 MPa = 403J). As a result of this study, it can be concluded that the actual shotcrete support performance can be evaluated by evaluating the support performance of the shotcrete measured at less than the allowable standard (3.0 MPa) at the actual tunnel site.

Strength and Durability Characteristics of Low-alkali Mortar for Artificial Reefs Produced by 3D Printers (인공어초 3D 프린터 출력을 위한 저알칼리 모르타르의 강도와 내구성능)

  • Lee, Byung-Jae;Kim, Bong-Kyun;Kim, Yun-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.26 no.1
    • /
    • pp.67-72
    • /
    • 2022
  • Concrete prevents corrosion of reinforcing bars due to its strong alkalinity. However, in the sea, strong alkali components with a pH of 12 to 13 are eluted, which adversely affects the ecological environment and growth of marine organisms. In this study, the mechanical properties and durability of the low alkali mortar were evaluated for the development of a low alkali mortar for the 3D printed artificial reefs. As a result of evaluation of strength characteristics, the α-35 mixture, which were produced with fly ash, silica fume and α-hemihydrate gypsum, satisfied the strength requirement 27 MPa in terms of compressive strength. As a result of pH measurement, it was found that mixing with alpha-type hemihydrate gypsum resulted in minimizing pH due to the the formation of calcium sulfate instead of calcium hydroxide production. As a result of the chloride ion penetration resistance test, the α-35 mixture exhibited the best performance, 3844C. As a result of measuring the length change over time, the α-35 mixture showed the shrinkage 33.5% less compared to the Plain mix.