• Title/Summary/Keyword: 입열량 변화

Search Result 38, Processing Time 0.02 seconds

A Study on the Residual Stress in the Welded Joints with Different Details (용접상세의 변화에 따른 용접이음부의 잔류응력에 관한 연구)

  • Lim, Cheong Kweon;Park, Moon Ho
    • Journal of Korean Society of Steel Construction
    • /
    • v.10 no.4 s.37
    • /
    • pp.709-720
    • /
    • 1998
  • In order to study the distribution of welding residual stress through the plate thickness. experiment and analysis of fillet welding details were carried out. Especially, a residual stress in the weld root part of T-joint fillet weld whose measurement was difficult up to now was measured. By using the heat input and the number of the weld layers as parameters, the distribution of the 3-dimensional residual stress was investigated. As a result, we can say that with increasing the heat input, the residual stress in the weld toe and weld root barely changes. But, the area of the tensile residual stress became wide. Then, comparing a single pass with multi-pass weld method, it was found that the residual stress decreased more in multi-pass than in single pass. Moreover, it was found the thing that the area of tensile residual stress by multi-pass is lower than that by single-pass in the near weld part.

  • PDF

Welding Characteristics on Heat input Changing of Laser Dissimilar Metals Welding (레이저 이종용접에서의 입열량 변화에 대한 용접특성)

  • Mo Yang-Woo;Shin Byung-Heon;Shin Ho-Jun;Yoo Young-Tae
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.15 no.2
    • /
    • pp.51-58
    • /
    • 2006
  • Laser welding of dissimilar metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research works is to investigate the influence of the process parameters, such as the welding for SM45C and STS304 with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding quality of the cut section, stain-stress behavior and the hardness of the welded part are investigated. From the results of the investigation, it has been shown that the optimal welding condition without defects in the vicinity of the welded area and with a good welding qualify is 1600W of the laser power, 0.85m/min of welding speed and $4{\ell}/min$ of pressure for shielding gas.

Comparison of Welding Characteristics on Heat input Changing of Laser Dissimilar Metals Welding (레이저 이종용접에서의 입열량 변화에 대한 용접특성 비교)

  • Shin H.J.;Yoo Y.T.;Shin B.H.;Ahn D.G.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.997-1003
    • /
    • 2005
  • Laser welding of dissimilar metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research works is to investigate the influence of the process parameters, such as the welding for SM45C and STS304 with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding qualify of the cut section, stain-stress behavior and the hardness of the welded part are investigated. From the results of the investigation, it has been shown that the optimal welding condition without defects in the vicinity of the welded area and with a good welding quality is 1600W of the laser power, 0.85m/min of welding speed and 4m/min of pressure for shielding gas.

  • PDF

Performance Analysis of a 5 RT Air-Cooled $NH_3-H_2O$ Absorption Chiller with the Variations of Heat Input and Ambient Temperature (5 RT 공랭형 $NH_3-H_2O$ 흡수식 냉동기의 발생기 입력 열량과 외기온도 변화에 따른 성능분석)

  • 윤희정;김성수;강용태
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.16 no.5
    • /
    • pp.438-443
    • /
    • 2004
  • The objective of this paper is to study the effects of the input gas flow rate and the ambient temperature variation on the absorption cycle performance. An air-cooled NH$_3$-$H_2O$ absorption chiller is tested in the present study. The nominal cooling capacity of the single effect maching is 17.6 ㎾ (5.0 USRT). The cooling capacity, coefficient of performance, burner efficiency, and each state point are measured with the variations of the heat input and the ambient temperature. It is found that the COP and cooling capacity increase with increasing the generator exit temperature up to a certain temperature and then decrease. It is also found that the COP and the cooling capacity decrease with increasing the ambient temperature. The maximum COP of 0.51 is obtained from the present experiment.

Experimental Study on the Flame Stability and the NOx Emission Characteristics of Low-Btu Coal Gas Fuel (저 발열량 석탄가스 연료의 화염 안정성 및 NOx 발생 특성에 관한 실험적 연구)

  • Lee, Chan;Kim, Yong-Chul
    • Journal of Energy Engineering
    • /
    • v.9 no.2
    • /
    • pp.109-116
    • /
    • 2000
  • 저발열량 석탄가스의 thermal/fuel NOx 생성특성과 화염 안정성을 규명하기 위한 실험적 연구를 수행하였다. 저발열량 합성 연료 가스는 일산화탄소, 수소, 질소 및 암모니아를 천연가스 연료와 동일한 입열량을 가지도록 혼합하여 만들었고 , 합성가스는 평면 화염 버너를 공급하여 태웠다. 특정한 합성가스에 대해 당량비를 변화시켜 가며, 비화 또는 역화에 의한 화염안정성을 규명하였고 안정된 화염 영역을 정의하였다. 저발열향 합성가스의 연소시 발생하는 thermal 및 fuel NOx를 측정하여 천연가스 연소시의 경우와 비교하였다.

  • PDF

Correlation of Microstructure with Mechanical Properties by Welding Conditions of Electric Resistance Welding(ERW) (전기저항용접(ERW)조건에 따른 미세조직과 기계적 특성의 연관성)

  • Lee, Kyung-Min;Lee, Dong-Eon;Kim, Sung-Woong;Yoon, Byung-Hyun;Kang, Hee-Jae;Kang, Nam-Hyun
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.27-27
    • /
    • 2010
  • 청정에너지원의 수요가 증가함에 따라 에너지원의 공급로의 역할을 하는 강관의 수요가 증가하고 있다. 소재가공 기술의 발전과 함께 경량의 고장력 강재의 적용은 공급로의 역할을 하는 강관의 비용절감 및 자원의 효율적 이용 측면에서 지속적으로 연구 개발을 이어왔다. 이러한 추세에 따라 구조용 또는 라인파이프용 강관에서도 고장력 강재의 적용과 함께 고인성 그리고 용접성의 향상을 위한 다양한 라인파이프용 강재의 개발과 이의 적용이 그간 활발히 진행되어왔다. 용도상 반드시 필요한 특성인 고장력, 고인성, 용접성 등 외에도 다양한 강재의 사용에 따른 제조공정상 즉 용접공정에서 발생될 수 있는 용접부의 기계적 특성 변화에 대한 특성 연구 및 기술 연구가 계속 되어왔다. 주로 강관을 생산하는데 쓰이는 ERW (Electric Resistance Welding) 공정에서도 이러한 문제점을 해결하기 위해 많은 연구가 진행되고 있다. ERW는 높은 생산성과 낮은 제조비용의 장점을 가지고 있으나 용접 후 용접부의 기계적 특성 감소로 인한 단점이 있다. 때문에 기계적 특성향상을 위해 최적의 용접조건에 대해 연구해야 할 필요가 있다. 본 연구에서는 4가지 합금강관의 ERW 용접시 용접 입열량의 변화와 용접부의 후열처리를 통한 미세조직의 변화와 기계적 특성에 대해서 고찰하였다. 4강종 시편의 미세조직을 OM, SEM을 통한 분석 이후 인장시험 및 경도시험 등을 통해 기계적 특성을 평가하였다. 대부분의 시편에서 입열량의 증가에 따라 Ferrite 분율이 증가하였고 용접중앙부의 Ferrite 양이 용접경계부 보다 많았다. Ferrite 집중부의 분포가 극명하게 관찰되었던 DP780 (적정) 강종과 미세하게나마 Ferrite 집중부가 존재하였던 K55 (과소, 과대) 강종에서 나란히 경도 하락 현상이 관찰되었다. 이는 강종마다 고유의 Ceq, 합금 중 Mn 농도, 입열량 등에 의한 복합적인 이유 때문으로 판단된다. 탄소가 0.3~0.4 wt% 함유된 중탄소강인 S45C, K55의 경우 용접중앙부와 용접경계부의 페라이트 분율 차이가 큰 것을 알 수 있었다. 이는 용접시 열에 의한 탈탄현상으로 인해 나타나는 현상으로 판단된다.

  • PDF

A study on laser welding characteristics of 1500MPa grade ultra high strength steel for automotive application (자동차용 1500MPa급 초고강도강의 레이저 용접 특성에 관한 연구)

  • Choi, Jin-Kang;Kim, Cheol-Hee;Rhee, Se-Hun
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.113-113
    • /
    • 2009
  • 세계적으로 환경문제에 대한 관심이 커짐에 따라 연료 효율 향상과 매연을 줄이기 위해 차량 경량화 요구가 증가하는 동시에 안전 규제가 강화되고 있어 높은 강도를 가지는 소재의 적용이 증가하고 있다. 충돌 시 차량 구조를 유지시켜주는 범퍼나 B-필러와 같은 부품에 1500MPa급의 초고강도강이 적용되고 있으며 레이저 용접이 가지는 장점이 많이 알려지면서 그 사용이 증가하는 추세이다. 따라서 레이저 용접에 의한 초고강도강의 용접 특성에 대한 연구가 필요하다. 본 연구에서는 1500MPa급 초고강도강의 레이저 맞대기 용접을 실시하여 단면, 경도 측정, 인장시험을 통해 용접부 특성을 파악하였다. 파이버 레이저와 디스크 레이저를 사용하여 각각의 레이저빔 직경 변화에 따른 입열량 변화에 따라 용접성에 미치는 영향에 대해 알아보았다.

  • PDF

Control of arc pulse to overcome misalignment and gap variation in root pass welding of pipe butt joint by GMAW (GMAW 초층 이면비드 용접에서 단차와 갭변동 극복을 위한 아크 충격량 제어)

  • Son, Chang-Hui;Kim, Nam-Gyu;Park, Hyo-Hui;Cho, Sang-Myoung
    • Proceedings of the Korean Society of Marine Engineers Conference
    • /
    • 2011.06a
    • /
    • pp.76-76
    • /
    • 2011
  • 선박이나 산업 플랜트에서 파이프 또는 탱크류의 맞대기 용접 시 안정적인 이면비드의 형성은 매우 중요하다. 대부분의 현장에서 파이프 맞대기 초층용접부의 안정적인 이면비드를 형성하기 위해 3mm의 루트갭을 띄우고 루트면이 없는 V-그루브에서 필러를 사용하는 수동 TIG용접을 주로 사용하고 있다. 수동 TIG용접은 고품질의 비드와 우수한 아크안정성, 그리고 용접인자의 제어가 쉽다는 장점이 있다. 그러나 수동 TIG용접은 용접속도가 10cpm정도로 느리기 때문에 GMAW에 비해 생산성이 낮고 작업자의 숙련도에 따라 품질이 변하게 된다. 본 연구에서는 높은 생산성과 기준갭 1.5mm에서 단차의 허용공차를 크게 하기 위해 루트면 3mm를 가지는 U-그루브의 설계를 하였으며, 두꺼운 루트면을 가지는 그루브에서 안정적인 이면비드를 형성시키기 위해 GMAW에서 아크 충격량에 대한 검토를 실시하였다. GMAW의 아크력이 용입에 어떠한 영향을 미치는지 검토하기 위해 수냉되는 동판에 갭을 1.5mm 띄우고 동일한 용착량과 입열량에서 아크력만을 변화시켜 실험하였다. 또한, U-그루브의 루트부를 모델링하여 두께3t의 평판시편을 각각의 갭과 단차 조건에서 실험하였다. 이 때, 기준갭 1.5mm에서 갭에 의해 생기는 단면적을 기준 갭단면적, 갭이 증가함에 따라 증가되는 단면적을 추가 갭단면적, 갭이 감소함에 따라 감소하는 단면적을 감소 갭단면적으로 정의하였다. 용접 중 발생하는 추가, 감소 갭단면적에 대하여 용착량을 50%의 수준으로 증가, 감소 시켰다. 갭에 따라 아크력을 변경하여 실험을 실시하였고 이면비드의 형상을 확인 하였다. 마지막으로 평판 시편의 조건에서 안정적으로 이면비드가 형성된 조건을 pipe U-그루브에 적용하였다. 그 결과 동판에서 용착량과 입열량이 같음에도 불구하고 아크력이 증가함에 따라 용입이 깊어짐을 확인하였다. 또한. 3t 평판시편에서 아크력의 제어를 통해 큰 단차와 갭이 있을 때, 안정적인 이면비드를 얻을 수 있는 조건을 확립하였다. 마지막으로 pipe U-그루브에서 앞선 실험의 용접조건으로 갭과 단차의 변화에 대해 실험을 하였으나, 시험편의 두께차이에 의한 전도 열손실로 인해 이면비드의 형성이 어려웠고, 아크 충격량의 증가를 통해 이러한 문제를 해결하였다.

  • PDF