$Cl_{2}$/$CF_{4}$/Ar gas chemistry에 의한 $SrBi_2Ta_2O_{9}$ 박막의 식각 특성 (Etching Kinetics Of $SrBi_2Ta_2O_{9}$ Thin Film in $Cl_{2}$/$CF_{4}$/Ar gas Chemistry)

  • 김동표;김창일;이원재;유병곤;김태형;장의구
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.62-65
    • /
    • 2001
  • $SrBi_2Ta_2O_{9}$ thin films were etched in inductively coupled $Cl_{2}$/$CF_{4}$/Ar plasma. The maximum etch rate was 1060 $\AA\textrm{m}$/min in $Cl_{2}$/$CF_{4}$/Ar (80). The chemical reactions on the etched surface were studied with x-ray photoelectron spectroscopy. The etching of SBT thin films in $Cl_{2}$/$CF_{4}$/Ar were etched by chemically assisted reactive ion etching. The small addition of $Cl_2$ into $CF_4$(20)/Ar(80) plasma will decrease the fluorine radicals and the increase Cl radical.

  • PDF

Ar/CF4/Cl2 플라즈마에 의한 CeO2 박막의 식각 특성 연구 (A Study on Etch Characteristics of CeO2 Thin Film in An Ar/CF4/Cl2 Plasma)

  • 장윤성;김동표;김창일;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제15권5호
    • /
    • pp.388-392
    • /
    • 2002
  • In this work, the etching of $CeO_2$ thin films has been performed in an inductively coupled $Ar/CF_4/Cl_2$ plasma. The highest etch rate of the $CeO_2$ thin film ws 250 ${\AA}/min$ and the selectivity of CeO$_2$to SBT was 0.4 at a 10% additive $Cl_2$ into Ar/($Ar+CF_4$)gas mixing ratio of 0.8. From result of X-ray photoelectron spectroscopy (XPS) analysis, there are Ce-Cl and Ce-F bonding by chemical reaction between Cl, F and Ce. During the etching of $CeO_2$ thin films in $Ar/CF_4/Cl_2$ plama, Ce-Cl and Ce-F bond is formed, and these prodcuts can be removed by the physical bombardment of Ar ions. The 10% additive $Cl_2$ into the Ar/($Ar+CF_4$)gas mixing ratio of 0.8 could enhance the reaction between Cl, F and Ce.

$Ar/CF_{4}/Cl_{2}$ 유도결합 플라즈마에 의한 SBT 박막의 표면 손상 (The Surface Damage of SBT Thin Film Etched in $Ar/CF_{4}/Cl_{2}$ Plasma)

  • 김동표;김창일;이철인;김태형;이원재;유병곤
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.26-29
    • /
    • 2001
  • $SrBi_2Ta_2O_{9}$ thin films were etched at high-density $Cl_2/CF_4/Ar$ in inductively coupled plasma system. The etching of SBT thin films in $Cl_2/CF_4/Ar$ were chemically assisted reactive ion etching. The maximum etch rate was 1300 $\AA$/min at 900W in $Cl_2(20)/CF_4(20)/Ar(80)$. As rf power increase, radicals (F, Cl) and ion(Ar) increase. The influence of plasma induced damage during etching process was investigated in terms of the surface morphology and th phase of X-ray diffraction. The chemical residue was investigated with secondary ion mass sperometry.

  • PDF

$Ar/CF_{4}/Cl_{2}$ 유도결합 플라즈마에 의한 SBT 박막의 표면 손상 (The Surface Damage of SBT Thin Film Etched in $Ar/CF_{4}/Cl_{2}$ Plasma)

  • 김동표;김창일;이철인;김태형;이원재;유병곤
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.26-29
    • /
    • 2001
  • SrBi$_2$Ta$_2$$O_{9}$ thin films were etched at high-density C1$_2$/CF$_{4}$/Ar in inductively coupled plasma system. The etching of SBT thin films in C1$_2$/CF$_{4}$/Ar were chemically assisted reactive ion etching. The maximum etch rate was 1300 $\AA$/min at 900W in Cl$_2$(20)/CF$_4$(20)/Ar(80). As f power increase, radicals (F, Cl) and ion(Ar) increase. The influence of plasma induced damage during etching process was investigated in terms of the surface morphology and th phase of X-ray diffraction. The chemical residue was investigated with secondary ion mass spectrometry.y.

  • PDF

$CF_4/Cl_2/Ar$ 고밀도 플라즈마를 이용한 PZT 박막의 식각 특성에 관한 연구 (A Study on Etching Characteristics of PZT thin films in $CF_4/Cl_2/Ar$ High Density Plasma)

  • 강명구;김경태;김태형;김창일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1512-1514
    • /
    • 2001
  • In this work, PZT thin films were etched as a function of $Cl_2$/Ar and additive $CF_4$ into $Cl_2$(80%)/Ar(20%). The etch rates of PZT films were 1600 $\AA$/min at $Cl_2$(80%)/Ar(20%) gas mixing ratio and 1973 $\AA$/min at 30% additive $CF_4$ into $Cl_2$(80%)/Ar(20%). Therefore the etch rate of PZT in $CF_4/Cl_2/Ar$ plasma is faster than in $Cl_2$/Ar. From XPS and SIMS analysis, metal halides and C-O, FCI and $CClF_2$ were detected. The etching of PZT films in Cl-based plasma is primarily chemically assisted ion etching and the remove of nonvolatile etch byproducts is the dominant step. Consequently, we suggest that the increase of Cl radicals and the volatile oxy-compound such as $CO_y$ are made by adding $CF_4$ into $Cl_2$/Ar plasma. Therefore, the etch rate of PZT in $CF_4/Cl_2/Ar$ plasma is faster than in $Cl_2$/Ar. The etched profile of PZT films was obtained above 70$^{\circ}$ by the SEM micrograph.

  • PDF

$CF_4$/Ar 플라즈마 내 $Cl_2$첨가에 의한 $SrBi_{2}Ta_{2}O_{9}$ 박막의 식각 특성 (Etching Characteristics of $SrBi_{2}Ta_{2}O_{9}$ Thin Film with Adding $Cl_2$ into $CF_4$/Ar Plasma)

  • 김동표;김창일;이원재;유병곤;김태형;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제14권9호
    • /
    • pp.714-719
    • /
    • 2001
  • SrBi$_2$Ta$_2$$O_{9}$ thn films were etched in inductively coupled Cl$_2$/CF$_4$/Ar plasma. THe maximum etch rate was 1060 $\AA$/min at a Cl$_2$/(Cl$_2$+CF$_4$+Ar)=0.2. The 20% additive Cl$_2$ into CF$_4$/Ar plasma decreased carbon and fluorine radicals, but increased Cl radicals. Sr was effectively removed by reacting with Cl radical because the boiling point of SrCl$_2$(125$0^{\circ}C$) is lower than that of SrF$_2$(246$0^{\circ}C$). The chemical reactions on the etched surface were studied with x-ray photoelectron spectroscopy and secondary ion mass spectrometry. The etching profile was evaluated by using scanning electron microscopy.y.

  • PDF

$CF_4/Ar$ 플라즈마 내 $Cl_2$첨가에 의한 $SrBi_2Ta_2O_9$ 박막의 식각 특성 (Etching Characteristics of $SrBi_2Ta_2O_9$ Thin Film with adding $Cl_2$ into $CF_4/Ar$ plasma)

  • 김동표;김창일;이원재;유병곤;김태형;장의구
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 반도체재료
    • /
    • pp.67-70
    • /
    • 2001
  • $SrBi_2Ta_2O_9$ thin films were etched at high-density $Cl_2/CF_4/Ar$ in inductively coupled plasma system. The chemical reactions on the etched surface were studied with x-ray photoelectron spectroscopy and secondary ion mass spectrometry. The etching of SBT thin films in $Cl_2/CF_4/Ar$ were chemically assisted reactive ion etching. The maximum etch rate was 1060 Am /min in $Cl_2$(20)/CF_4(20)/Ar(80). The small addition of $Cl_2$ into $CF_4$(20)/Ar(80) plasma will decrease the fluorine radicals and the increase CI radical. The etch profile of SBT thin films in $Cl_2/CF_4/Ar$ plasma is steeper than in $CF_4$/Ar plasma.Ā저會Ā저ﶖ⨀⡌ឫഀĀ᐀會Ā᐀㡆ﶖ⨀쁌ឫഀĀ᐀會Ā᐀遆ﶖ⨀郞ග堂瀀ꀏ會Āﶖ⨀〲岒ऀĀ᐀會Ā᐀䁇ﶖ⨀젲岒Ā㰀會Ā㰀顇ﶖ⨀끩Ā㈀會Ā㈀ﶖ⨀䡪Ā᐀會Ā᐀䡈ﶖ⨀Ā᐀會Ā᐀ꁈﶖ⨀硫Ā저會Ā저ﶖ⨀샟ගကĀ저會Ā저偉ﶖ⨀栰岒ఀĀ저會Ā저ꡉﶖ⨀1岒Ā저會Ā저Jﶖ⨀惝ග؀Ā؀會Ā؀塊ﶖ⨀ග㼀Ā切會Ā切끊ﶖ⨀⣟ගఀĀ搀會Ā搀ࡋﶖ⨀큭킢Ā저會Ā저

  • PDF

Cl2CF4/Ar 유도결합 플라즈마에 의해 식각된 SBT 박막의 표면 손상 (The Surface Damage of SBT Thin Film Etched in Cl2CF4/Ar Plasma)

  • 김동표;김창일;이철인;김태형;이원재;유병곤
    • 한국전기전자재료학회논문지
    • /
    • 제15권7호
    • /
    • pp.570-575
    • /
    • 2002
  • $SrBi_2Ta_2O_9$ thin films were etched in $Cl_2/CF_4/Ar$ inductively coupled plasma (ICP). The maximum etch rate was 1300 ${\AA}/min$ at 900 W ICP power in Cl$_2$(20%)/$CF_4$(20%)/Ar(60%). As RF source power increased, radicals (F, Cl) and ion ($Ar^+$) increased. The influence of plasma induced damage during etching process was investigated in terms of P-E hysteresis loops, chemical states on the surface, surface morphology and phase of X-ray diffraction. The chemical states on the etched surface were investigated with X-ray spectroscopy and secondary ion mass spectrometry. After annealing $700^{\circ}C$ for 1 h in $O_2$ atmosphere, the decreased P-E hysteresises of the etched SBT thin films in Ar and $Cl_2/CF_4/Ar$ plasma were recovered.

CF4/CI2/Ar유도 결합 플라즈마에 의한 gold 박막의 식각특성 (Etching Characteristics of Gold Thin Films using Inductively Coupled CF4/CI2/Ar Plasma)

  • 김창일;장윤성;김동표;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제16권7호
    • /
    • pp.564-568
    • /
    • 2003
  • The etching of Au thin films have been performed in an inductively coupled CF$_4$/Cl$_2$/Ar plasma. The etch rates were measured as CF$_4$ contents added from 0 to 30 % to Cl$_2$/Ar plasma, of which gas mixing ratio was fixed at 20%. Other parameters were fixed at an rf power of 700 W, a dc bias voltage of 150 V, a chamber pressure of 15 mTorr, and a substrate temperature of 3$0^{\circ}C$. The highest etch rate of the Au thin film was 3700 $\AA$m/min at a 10% additive CF$_4$ into Cl$_2$/Ar plasma. The surface reaction of the etched Au thin films was investigated using x-ray photoelectron spectroscopy (XPS) analysis. XPS analysis indicated that Au reacted with Cl and formed Au-Cl, which is hard to remove on the surface because of its high melting point. The etching products could be sputtered by Ar ion bombardment.

$Ar/CF_{4}/Cl_{2}$ 플라즈마에 의한 $CeO_2$ 박막의 식각 특성 연구 (A study on etch Characteristics of $CeO_2$ thin Film in an $Ar/CF_{4}/Cl_{2}$ Plasma)

  • 장윤성;장의구;김창일;이철인;김태형;엄준철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.217-220
    • /
    • 2001
  • The possibility of cerium dioxide $(CeO_2)$ thin films as insulators of metal erroelectric insulator semiconductor (MFIS) structures have been studied. The etching $CeO_2$ thin films have been perfonned in an inductively coupled $Cl_{2}/CF_{4}/Ar$ plasma. The high etch rate of the $CeO_2$ thin film was $250\AA /m$ at a 10 % addition of $Cl_2$ into the $Ar(80)/CF_{4}(20)$. The surface reaction of the etched $CeO_2$ thin films was investigated using X-ray photoelectron spectroscopy (XPS) analysis. There are Ce-Cl and Ce-F bonding by chemical reaction between Cl, F and Ce. These products can be removed by the physical bombardment of incident Ar ions.

  • PDF