• 제목/요약/키워드: $Bi_2Sr_2Ca_1Cu_2O_x$ (Bi-2212)

검색결과 33건 처리시간 0.021초

Cu-free 전구체를 이용하여 구리 기판 위에 ${Bi_2}{Sr_2}{CaCu_2}{O_8}$ 초전도 후막의 제조 및 특성 (Fabricatiion and Characterization of ${Bi_2}{Sr_2}{CaCu_2}{O_8}$ Superconductor Thick Films on Cu Substrates using Cu-free Precursors)

  • 한상철;김상준;한영희;성태현;한병성
    • 한국전기전자재료학회논문지
    • /
    • 제13권4호
    • /
    • pp.349-358
    • /
    • 2000
  • Fabrication and Characterization of Bi$_{2}$/Sr$_{2}$/CaCu$_{2}$/O$_{8}$(Bi2212) superconductor thick films were fabricated successfully on C tapes by liquid reaction between Cu-free precursors of Bi$_{x}$/SrCaO/$_{y}$(x=1.2-2) and Cu tapes. Cu-free Bi-Sr-Ca-O powder mixtures were screen-printed on Cu tapes and heat-treated at 850-87$0^{\circ}C$ for several minutes in air oxygen nitrogen and low oxygen pressure. In order to obtain the optimum heat-treatment condition we studied the effect of the precursor composition the printing thickness and the heat-treatment atmosphere on the superconducting properties of Bi2212 films and the reaction mechanism. Microstructures and phases of thick films were analyzed by films and the reaction mechanism. Microstructures and phases of thick films were analyzed by optical microscope and XRD. The electric properties of superonducting films were examined by the four probe method. At heat-treatment temperature the thick films were in a partially molten state by liquid reaction between CuO of the oxidized copper tape and the precursors which were printed on Cu tapes. During the heat-treatment procedure Bi2212 superconducting particle nucleate and grow in preferred orientations.ons.s.

  • PDF

부착율 개선을 위해 증발 법으로 제작한 Bi2Sr2CanCun+1Ox 박막의 부착 특성 (Sticking Characteristics in Bi2Sr2CanCun+1Ox Thin Films Fabricated by using the Evaporation Method to Improve the Sticking Ratio)

  • 천민우;박용필
    • 한국전기전자재료학회논문지
    • /
    • 제16권11호
    • /
    • pp.1029-1034
    • /
    • 2003
  • The Bi$_2$Sr$_2$Ca$_{n}$Cu$_{n+1}$ O$_{x}$, superconducting thin films arc fabricated by using the sputtering and evaporation method. Because we confirmed the sticking ratio of Bi element in the Bi$_2$Sr$_2$Ca$_{n}$Cu$_{n+1}$ O$_{x}$ superconducting thin film fabricated by using the sputtering method was much lower than the expected value, to get the enough number of the flakes of Bi, faraday cup was used to evaporate Bi clement. As a result of the fabrication, Bi 2201 and Bi 2212 single phases could be made by the optima of deposition condition. And we confirmed the sticking coefficient of Bi element was clearly related to the temperature change of the substrate and the generation of Bi22l2 phase

스퍼터링 법과 증발 법으로 제작한 초전도 박막의 비교 (Comparison between Superconducting Thin Films Fabricated by Using the Sputtering and the Evaporation Method)

  • 천민우;박노봉;양승호;박용필;김혜정
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 제6회 학술대회 논문집 일렉트렛트 및 응용기술연구회
    • /
    • pp.39-42
    • /
    • 2004
  • The $Bi_2Sr_2Ca_nCu_{n+1}O_x$ superconducting thin film fabricated by using the sputtering method was compared with the $Bi_2Sr_2Ca_nCu_{n+1}O_x$ superconducting thin film fabricated by using the evaporation method. In doing the ultra-low deposition because each element can exist on the substrate surface, both the sputtering method and the evaporation method could easily fabricate single phase of the Bi2212 phase. Also, it is cofirmed that by optimizing the deposition condition, each single phase of the Bi2201 phase and the Bi2212 phase can be fabricated, the sticking coefficient of Bi element is clearly related to the changing of substrate temperature and the formation of the Bi2212 phase.

  • PDF

Bi2-δAuδSr2CaCu2O8+δ(x = 0~0.15) 산화물고온초전도체의 Bi 위치에 Au 혼합효과 (Effect of Au Additive on The Bi Site in The Bi2-δAuδSr2CaCu2O8+δ (x=0~0.15) Superconductors)

  • 이민수;최봉수;이정화;송기영;정성혜;홍병유
    • 한국전기전자재료학회논문지
    • /
    • 제15권4호
    • /
    • pp.308-313
    • /
    • 2002
  • Samples with the norminal composition, $Bi_{2-x}Au_xSr_2CaCu_2O_{8+\delta}$ (x = 0, 0.05. 0.1, 0.15) were prepared by the solid-state reaction method. The superconducting properties, x-ray powder diffraction patterns, critical temperature and microstructure of surface were measured the samples. x-ray patterns show the single phase(2212) nature of the samples. But, the peaks of 2201 at $2\theta=30^{\circ}$ and Au peak at $2\theta=38.31^{\circ}$ are observed in the Au additive samples. The grain sire are enlarged with the increase of x. As the result of enlargement the grain size, the onset and offset critical temperature($T_c^{on}$,$T_c^{zero}$) increased with increase of x.

$Bi_2Sr_2Ca_{n-1}Cu_nO_x$(n=0, 1, 2) 초전도 박막의 혼합상에 대한 고용비 해석 (Analysis of Stacking-Fault Proportion on the Mixed Phase of the $Bi_2Sr_2Ca_{n-1}Cu_nO_x$(n=0, 1, 2) Superconducting Thin Films)

  • 양승호;이호식;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.486-487
    • /
    • 2007
  • $Bi_2Sr_2Ca_{n-1}Cu_nO_x$(n=0, 1, 2) thin films have been fabricated by co-deposition at an ultra-low growth rate using ion beam sputtering(IBS) method. The growth rates of the films was set in the region from 0.17 to 0.27 nm/min. MgO(100) was used as a substrate. In order to appreciate stable existing region of Bi 2212 phase with temperature and ozone pressure, the substrate temperature was between 655 and $820^{\circ}C$ and the highly condensed ozone gas pressure in vacuum chamber was varied between $2{\times}10^{-6}{\sim}4{\times}10^{-5}$ Torr. Bi 2212 phase appeared in the temperature range of 750 and $795^{\circ}C$ and single phase of Bi 2201 existed in the lower region than $785^{\circ}C$. Whereas, $PO_3$ dependance on structural formation was scarcely observed regardless of the pressure variation.

  • PDF

BSCCO 플라즈마 용사피막의 부분용융열처리 후 어닐링 시간에 따른 초전도 특성 (Characteristics of Plasma Sprayed BSCCO Superconductor Coatings with Annealing Time After Partial Melt Process)

  • 박정식;이선홍;박경채
    • 한국재료학회지
    • /
    • 제24권2호
    • /
    • pp.116-122
    • /
    • 2014
  • $Bi_2Sr_2CaCu_2O_x$(Bi-2212) and $Bi_2Sr_2Ca_2Cu_3O_y$(Bi-2223) high-Tc superconductors(HTS) have been manufactured by plasma spraying, partial melt process(PMP) and annealing treatment(AT). A Bi-2212/2223 HTS coating layer was synthesized through the peritectic reaction between a 0212 oxide coating layer and 2001 oxide coating layer by the PMP-AT process. The 2212 HTS layer consists of whiskers grown in the diffusion direction. The Bi-2223 phase and secondary phase in the Bi-2212 layer were observed. The secondary phase was distributed uniformly over the whole layer. As annealing time goes on, the Bi-2212 phase decreases with mis-orientation and irregular shape, but the Bi-2223 phase increases because a new Bi-2223 phase is formed inside the pre-existing Bi-2212 crystals, and because of the nucleation of a Bi-2223 phase at the edge of Bi-2212 crystals by diffusion of Ca and Cu-O bilayers. In this study the spray coated layer showed superconducting transitions with an onset Tc of about both 115 K, and 50 K. There were two steps. Step 1 at 115 K is due to the diamagnetism of the Bi-2223 phase and step 2 at 50 K is due to the diamagnetism of the Bi-2212 phase.

Bi1.84Pb0.34Sr1.91Ca2.03Cu3.06O10+δ(110 K 상)산화물 고온초전도체에 Mg 첨가에 따른 영향 (Effect of Mg Additive in the Bi1.84Pb0.34Sr1.91Ca2.03Cu3.06O10+δ(110 K phase) Superconductors)

  • 이민수
    • 한국전기전자재료학회논문지
    • /
    • 제16권6호
    • /
    • pp.522-531
    • /
    • 2003
  • Samples with the nominal composition, B $i_{1.84}$P $b_{0.34}$S $r_{1.91}$C $a_{2.03}$C $u_{3.06}$ $O_{10+{\delta}}$ high- $T_{c}$ superconductors containing MgO as an additive were fabricated by a solid-state reaction method. Samples with MgO of 5~30 wt% each were sintered at 820~86$0^{\circ}C$ for 24 hours. The structural characteristics, critical temperature, grain size and image of mapping with respect to MgO contents were analyzed by XRD(X-Ray Diffraction), SEM(Scanning Electron Microscope) and EDS(Energy dispersive X-ray spectrometer) respectively. As MgO contents increased, intensity of MgO Peaks and ratio of Bi-2212 phase in superconductors intensified and the proportion of the phase transition from Bi-2223 to Bi-2212 was increased.

단결정 형성을 위한 열역학 분석 (Analysis of Thermodynamics for Single Crystal Formation)

  • 천민우;양승호;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 학술대회 및 기술세미나 논문집 디스플레이 광소자
    • /
    • pp.70-73
    • /
    • 2006
  • High quality $Bi_2Sr_2Ca_nCu_{n+1}O_x$ superconducting thin films fabricated by using the evaporation method at various substrate temperatures, $T_{sub}$, and ozone gas pressures, $pO_3$. The correlation diagrams of the $Bi_2Sr_2Ca_nCu_{n+1}O_x$ phases with $T_{sub}$ and $pO_3$ are established in the 2212 arid 2223 compositional films. In spite of 2212 compositional sputtering, Bi2201 and Bi2223 as well as Bi2212 phases come out as stable phases depending on $T_{sub}$ and $pO_3$. From these results, the thermodynamic evaluation of ${\Delta}H$ and ${\Delta}S$, which are related with Gibbs' free energy change for single Bi2212 or Bi2223 phase, was performed.

  • PDF

$Bi_2Sr_2CaCu_2O_{8+x}$ 단결정 선천성 조셉슨 접합에서의 플럭손 결맞음 운동 (Coherent motion of fluxons in stacked intrinsic Josephson junctions of $Bi_2$$Sr_2$Ca$Cu_2$$O_{8+x}$ single crystals)

  • 도용주;장현식;장동인;이후종;김진희;김규태;이우;최진호
    • Progress in Superconductivity
    • /
    • 제3권1호
    • /
    • pp.28-30
    • /
    • 2001
  • We studied the flux-flow current-voltage characteristics of microwave-generated fluxons formed in serially stacked intrinsic Josephson junctions fabricated on$ HgI_2$-intercalated $Bi_2$$Sr_2$$CaCu_2$O/8+x/(Bi2212) single crystals. With increasing the irradiation power of 73$\square$76 GHz microwave, the supercurrent branch became resistive and split into multiple sub -branches. Each sub-branch represented a specific mode of collective motion of Josephson fluxons. We also observed similar branch splitting In a mesa prepared on an underdoped Bi2212 single crystal in a static magnetic field.

  • PDF

Bi-Sr-Ca-Cu-O계열 초전도체의 초구조 (SUPERSTRUCTURES OF Bi-Sr-Ca-Cu-O SUPERCONDUTORS)

  • 남궁찬;이상윤
    • 한국재료학회지
    • /
    • 제4권3호
    • /
    • pp.268-279
    • /
    • 1994
  • 단일상을 갖는 $Bi_2S_2CaCu_2O_{8+x}$ (2212)의 x-ray 분말 pattern을 a=5.408, c=30.83 $\AA$의 격자상수 및 역격자 벡터 $q^*=0.211b^*-c^*$을 갖는 pseudo tetragonal subcell을 이용하여 모두 index하였다. 임계온도 110K를 갖는 $Bi_2S_2CaCu_2O_{10+x}$ 상은 incommensurate supercell에 속하는 매우 많은 x-ray분말선들을 가지고 있다. Indixing guide로 전자회절사진(electron diffraction photographs)을 이용 x-ray분말 pattern에 대한 지수결정방법을 얻었다.$Bi_2S_2CaCu_2O_{10+x}$(2223)의 단위세표(unit cell)는 기하학적으로 격자상수 a=5.411, b=5.420, c=37.29(2) A을 갖는 orthorhombic subcell이다. Supercell반사 지수들은 subcell의 파 벡터 $\pm q^*=0.211b^*-0.78c^*$을 갖는 k,1지수로부터 영향을 받은 것이다. b 방향으로의 inconnensurate성분 $\delta$는 두 상에 대해 다 같으나, 2212에서 2223 상으로의 변환에 따라 c 방향으로의 초격자성분(superlattic component)은 connensurate($\varepsilon$=1)로부터 incommensurate($\varepsilon$=0.78)로 변한다.

  • PDF