Preparation and Characterization of Glass-ceramics in MgO-${Al_2}{O_3}$-$SiO_2$ Glass (MgO-${Al_2}{O_3}$-$SiO_2$계 결정화유리의 제조 및 물성평가)

  • 손성범;최세영
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.6
    • /
    • pp.604-611
    • /
    • 2000
  • Glass-ceramics containing a cordierite (2MgO-2Al2O3-5SiO2) as a main crystal phase was prepared from MgO-Al2O3-SiO2 system glass through a controlled 2-step heat treatment for the application to magnetic memory disk substrate for higher storage capacity. Parent glasses prepared with addition of CeO2 as a fulx and TiO2 as a nucleating agent were crystallized by a 2-step heat treatment i.e. nucleation and crystal grwoth. Then the maximum nucleation and crystal growth rates were investigated and several properties such as bending strength, surface hardness and surface roughness were also studied for heat treated glass. As a result, only a $\alpha$-cordierite was precipitated as a main crystal phase for all heat treatment conditions and the maximum nucleation and crystal growth rates were 2.4$\times$109/㎣.hr at 80$0^{\circ}C$ and 0.3${\mu}{\textrm}{m}$/hr at 915$^{\circ}C$ respectively. After being nucleated at 80$0^{\circ}C$ for 5 hours and then crystallized at 915$^{\circ}C$ for 1 hour, the heat treated glass had a crystal volume fraction of 17.6% and crystal size fo 0.3${\mu}{\textrm}{m}$, and showed the optimum properties for the application to magnetic memory disk substrates as follows. ; Bending strength of 192 MPa, Vidkers hardness of 642.1kgf/$\textrm{mm}^2$, and surface roughness of 27$\AA$.

  • PDF

Deposition of Solar Selective Coatings for High Temperature Applications (고온용 태양 선택흡수막의 제작)

  • Lee, Kil-Dong
    • Journal of the Korean Solar Energy Society
    • /
    • v.28 no.1
    • /
    • pp.33-42
    • /
    • 2008
  • Zr-O ($Zr-ZrO_2$) cermets solar selective coatings with a double cermets layer film structure were prepared using a DC (direct current) magnetron sputtering method. The typical film structure from surface to bottom substrate were an $Al_2O_3$ anti-reflection layer on a double Zr-O cermets layer on an Al metal infrared reflection layer. Optical properties of optimized Zr-O cermets solar selective coating had an absorptance of ${\alpha}\;=\;0.95$ and thermal omittance of ${\epsilon}\;=\;0.10\;(100^{\circ}C)$. The absorbing layer of Zr-O cermets coatings on glass and silicon substrate was identified as being amorphous by using XRD. AFM showed that ZF-O cermets layers were very smooth and their surface roughness were approximately $0.1{\sim}0.2 nm$. The chemical analysis of the cermets coatings were determined by using XPS. Chemical shift of photoelectron binding energy was occurred due to the change of Zr-O cermets coating structure deposited with increase in oxygen flow rate. The result of thermal stability test showed that the Zr-O cermets solar selective coating was stable for use at temperature below $350^{\circ}C$.

Effect of Titanium Sulfate Addition on Crystal Growth of the Flaky α-Al2O3 (황산티타늄의 첨가가 판상 α-Al2O3의 결정성장에 미치는 영향)

  • Park, Byung-Ki;Cho, Sun-Mi;Lee, Jung-Min
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.5 s.276
    • /
    • pp.338-345
    • /
    • 2005
  • To prepare the complex gel of flux and pseudo-boehmite used in precursor of the flaky ${\alpha}-A1_2O_3$ crystal, aqueous solution of the mixture of sodium carbonate and sodium phosphate was added with stirring in aqueous solution of the mixture of sodium sulfate, potassium sulfate and titanium sulfate. The complex gel was dried at $110^{\circ}C$ and was crystallized above $1,050^{\circ}C$, and then the effect of the amount of titanium sulfate on size, morphology, thickness and crystal size distribution of the flaky ${\alpha}-A1_2O_3$ crystal was investigated. Addition of titanium sulfate was prevented the aggregation and generation of twin crystal, and had an effect on the crystal size and the thickness during crystal growth. When the amount of titanium sulfate was more than 6 g, particle size was decreased but was free from crystal twining and aggregation. On the other hand, when the amount of titanium sulfate was lower than 6 g, crystal size was increased but crystal twinning and aggregation were noticed.

Charactrerization of microstructure, hardness and oxidation behavior of carbon steels hot dipped in Al and Al-1% Si molten baths (Al과 Al-1% Si 용융조에서 용융 도금된 탄소강의 경도, 산화 및 미세조직의 특성)

  • Hwang, Yeon-Sang;Won, Seong-Bin;Chunyu, Xu;Lee, Dong-Bok
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2013.05a
    • /
    • pp.109-110
    • /
    • 2013
  • Medium carbon steel was aluminized by hot dipping into molten Al or Al-1%Si baths. After hot-dipping in these baths, a thin Al-rich topcoat and a thick alloy layer rich in $Al_5Fe_2$ formed on the surface. A small a mount of FeAl and $Al_3Fe$ was incorporated in the alloy layer. Silicon from the Al-1%Si bath was uniformly distributed throughout the entire coating. The hot dipping increased the microhardness of the steel by about 8 times. Heating at $700-1000^{\circ}C$ however decreased the microhardness through interdiffusion between the coating and the substrate. The oxidation at $700-1000^{\circ}C$ in air formed a thin protective ${\alpha}-Al_2O_3$ layer, which provided good oxidation resistance. Silicon was oxidized to amorphous silica, exhibiting a glassy oxide surface.

  • PDF

Influence of the Duty Cycle on the Characteristics of Al2O3 Coatings Formed on the Al-1050 by Plasma Electrolytic Oxidation (Al-1050 위에 플라즈마 전해 산화법으로 형성된 Al2O3 피막 특성에 미치는 듀티사이클의 영향)

  • Nam, Kyung-Su;Moon, Jung-In;Kongsy, Phimmavong;Song, Jeong-Hwan;Lim, Dae-Young
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.2
    • /
    • pp.108-115
    • /
    • 2013
  • Oxide coatings were prepared on Al-1050 substrates by an environment-friendly plasma electrolytic oxidation (PEO) process using an electrolytic solution of $Na_2SiO_3$ (8 g/L) and NaOH (3 g/L). The effects of three different duty cycles (20%, 40%, and 60%) and frequencies (50 Hz, 200 Hz, and 800 Hz) on the structure and micro-hardness of the oxide coatings were investigated. XRD analysis revealed that the oxides were mainly composed of ${\alpha}-Al_2O_3$, ${\gamma}-Al_2O_3$, and mullite. The proportion of each crystalline phase depended on various electrical parameters, such as duty cycle and frequency. SEM images indicated that the oxide coatings formed at a 60% duty cycle exhibited relatively coarser surfaces with larger pore sizes and sintering particles. However, the oxides prepared at a 20% duty cycle showed relatively smooth surfaces. The PEO treatment also resulted in a strong adhesion between the oxide coating and the substrate. The oxide coatings were found to improve the micro-hardness with the increase of duty cycle. The structural and physical properties of the oxide coatings were affected by the duty cycles.

Characterization of Defects in a Synthesized Crystal of Sapphire $({\alpha}-Al_2O_3)$ by TEM (투과전자현미경 조사에 의한 사파이어 $({\alpha}-Al_2O_3)$합성 결정내의 결함특성 분석)

  • Kim, Hwang-Su;Song, Se-Ahn
    • Applied Microscopy
    • /
    • v.36 no.3
    • /
    • pp.155-163
    • /
    • 2006
  • The defects in a synthesized crystal of ${\alpha}-Al_2O_3$ used as substrate for growing of semi-conductor materials such as GaN were examined by the conventional transmission electron microscopy (TEM), Large Angle CBED and High-Angle Annular Dark Field (HAADF) STEM methods. The dominant defects found in the specimen are basal microtwins with the thickness of ${\sim}2\;to\;32 nm$ and the associated strong strain field at the interface of microtwin/matrix, basal dislocations and complex dislocations in the one of {$2\bar{1}\bar{1}3$} pyramidal slip plane. All these basal and pyramidal dislocations seem to be strong related to basal microtwins. It was also found that the density of defects is very uneven. In the certain area with the dimension of a few fm, the dislocation density is quite high as an order of ${/sim}10^{10}/cm^2, but the average density is roughly estimated to be less than ${\sim}10^5/cm^2, as is usually expected in general synthesized crystals.

Preparation of Nanoporous Ceramic Membranes by Sol-gel Method and Characterization of Gas Permeation (졸-겔법에 의한 나노기공성 세라믹 막의 제조 및 기체투과 특성)

  • Lee, Yong-Taek;Choi, Ga-Young;Han, Hyuk-Hee
    • Membrane Journal
    • /
    • v.18 no.2
    • /
    • pp.176-184
    • /
    • 2008
  • Nano-porous ceramic membranes was synthesized by the sol-gel method. Gas permeation of hydrogen and nitrogen was determined by single composition gas. Pore size $0.1{\mu}m$ and porosity 32% of flat type ${\alpha}-Al_2O_3$ substrate was manufactured. An intermediate ${\gamma}-Al_2O_3$ layer with pore size of 4 nm was formed by dip-coating. Polymeric silica sol was synthesized by acid catalyzed hydrolysis and condensation of tetra-ethyl-ortho-silicate. Supported membranes on alumina were prepared by dipping and calcining. He, $N_2$ permeation experiments with nanoporous sol-gel modified supported ceramic membranes were peformed to determine the gas transport characteristics. $He/N_2$ permselectivity around $100{\sim}160$ and helium permeation in the order of $10^{-7}mol/m^2{\cdot}s{\cdot}Pa$ were measured in the temperature range of $303{\sim}363K$.

Oxidation Rates of TiAlLaN Thin Films Deposited by Ion Plating (이온플레이팅법으로 제조된 TiAlLaN계 박막의 산화속도)

  • Seo Sung Man;Lee Kee Sun;Lee Kee-Ahn
    • Korean Journal of Materials Research
    • /
    • v.14 no.3
    • /
    • pp.163-167
    • /
    • 2004
  • TiAl(La)N thin films were oxidized in vacuum of about 7 Pa to reduce the oxidation of WC-Co as a substrate. The oxidation rate constants of the thin films were quantified by an assumption of parabolic oxidation. Increasing AI content significantly decreased the parabolic oxidation rate constant. A simultaneous addition of AI and La was more effective to reduce the oxidation rate. The parabolic oxidation rate constant of $Ti_{0.66}$ $Al_{0.32}$ $La_{ 0.02}$N thin film at 1273 K showed about ten times lower than that of TiN. The addition of a small amount of La with Al induced the preferential formation of dense $\alpha$ $-Al_2$$O_3$ film in oxide film, leading to the abrupt reduction of oxidation rate.

Deposition of Cermet Solar Selective Coatings for High Temperature Applications (고온용 서밋 태양선택흡수막의 증착)

  • Lee, Kil-Dong
    • Journal of the Korean Solar Energy Society
    • /
    • v.26 no.1
    • /
    • pp.57-64
    • /
    • 2006
  • Cr-CrO cermet solar selective coatings with a double cermets layer film structure were prepared using a special direct current (dc) magnetron sputtering technology. The typical films structures from surface to bottom substrate were measured to be an $Al_2O_3$ anti-reflection layer on a double Cr-CrO cermet layer on an Al metal infrared reflection layer. Optical properties of optimized Cr-CrO cermet solar selective coating were absorptance (${\alpha}$) = 0.95 and emittance (${\varepsilon}$) = 0.10 ($100^{\circ}C$). Atomic force microscopy (AFM) image showed that Cr-CrO cermet film was very smooth and their grain size was also very small The results of thermal stability test showed that the Cr-CrO cermet solar selective coatings were stable for use at temperature of $400^{\circ}C$.

fabrication of DMMP Thick Film Gas Sensor Based on SnO2 (산화주석을 기반으로 한 DMMP 후막가스센서 제작)

  • 최낙진;반태현;곽준혁;백원우;김재창;허증수;이덕동
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.12S
    • /
    • pp.1217-1223
    • /
    • 2003
  • Nerve gas sensor based on tin oxide was fabricated and its characteristics were examined. Target gas is dimethyl methyl phosphonate(C$_3$ $H_{9}$ $O_3$P, DMMP) that is simulant gas of nerve gas. Sensing materials were Sn $O_2$ added a-Al$_2$ $O_3$ with 0∼20wt.% and were physically mixed each material. They were deposited by screen printing method on alumina substrate. The sensor device was consisted of sensing electrode with interdigit(IDT) type in front and a heater in back side. Total size of device was 7${\times}$10${\times}$0.6㎣. Crystallite size & phase identification and morphology of fabricated Sn $O_2$ powders were analyzed by X-ray diffraction and by a scanning electron microscope, respectively. Fabricated sensor was measured as flow type and resistance change of sensing material was monitored as real time using LabVIEW program. The best sensitivity was 75% at adding 4wt.% $\alpha$-Al$_2$ $O_3$, operating temperature 30$0^{\circ}C$ to DMMP 0.5ppm. Response and recovery time were about 1 and 3min., respectively. Repetition measurement was very good with $\pm$3% in full scale.TEX>$\pm$3% in full scale.