The Strength and Environmental Friendly Characteristics of Non-chemical Accelerating Shotcrete (비약액계 급결성 숏크리트재의 강도특성과 친환경성)

  • Chun, Byungsik;Park, Dukhyum;Kang, Hyoungnam;Do, Jongnam
    • Journal of the Korean GEO-environmental Society
    • /
    • v.9 no.5
    • /
    • pp.29-36
    • /
    • 2008
  • The shotcrete is a NATM technique as a major tunnel support for ground stability after tunnel excavation. Instead of a general concrete lining method, it is a trend for curtail of construction periods and reduction of construction expenses that required to use of the permanent shotcrete lining. This high-strength shotcrete is required to use as a permanent shotcrete lining. This brought out the solution of environmental pollution and harmfulness to human. Accordingly, in this study specimens for strength measurement were made to develop shotcrete possible to develop materials in early with cement mineral accelerator as NATM method construction. It was compared with existing shotcrete material, unconfined compression test, flexural strength test, antiwashout underwater test were experimented. The fish poison test was experimented to evaluate an influence of environment. As a results of the test, unconfined compressive strength and flexural strength were equivalent with 28-curing day strength of existing material. An antiwashout of research subject material was revealed excellently in antiwashout Underwater test. As a results of the fish poison, an evaluation research subject material was founded more environmentally friendly than existing shotcrete.

  • PDF

Excavation of Kim Jeong-gi and Korean Archeology (창산 김정기의 유적조사와 한국고고학)

  • Lee, Ju-heun
    • Korean Journal of Heritage: History & Science
    • /
    • v.50 no.4
    • /
    • pp.4-19
    • /
    • 2017
  • Kim Jeong-gi (pen-name: Changsan, Mar. 31, 1930 - Aug. 26, 2015) made a major breakthrough in the history of cultural property excavation in Korea: In 1959, he began to develop an interest in cultural heritage after starting work as an employee of the National Museum of Korea. For about thirty years until he retired from the National Research Institute of Cultural Heritage in 1987, he devoted his life to the excavation of our country's historical relics and artifacts and compiled countless data about them. He continued striving to identify the unique value and meaning of our cultural heritage in universities and excavation organizations until he passed away in 2015. Changsan spearheaded all of Korea's monumental archeological excavations and research. He is widely known at home and abroad as a scholar of Korean archeology, particularly in the early years of its existence as an academic discipline. As such, he has had a considerable influence on the development of Korean archeology. Although his multiple activities and roles are meaningful in terms of the country's archaeological history, there are limits to his contributions nevertheless. The Deoksugung Palace period (1955-1972), when the National Museum of Korea was situated in Deoksugung Palace, is considered to be a time of great significance for Korean archeology, as relics with diverse characteristics were researched during this period. Changsan actively participated in archeological surveys of prehistoric shell mounds and dwellings, conducted surveys of historical relics, measured many historical sites, and took charge of photographing and drawing such relics. He put to good use all the excavation techniques that he had learned in Japan, while his countrywide archaeological surveys are highly regarded in terms of academic history as well. What particularly sets his perspectives apart in archaeological terms is the fact that he raised the possibility of underwater tombs in ancient times, and also coined the term "Haemi Culture" as part of a theory of local culture aimed at furthering understanding of Bronze Age cultures in Korea. His input was simply breathtaking. In 1969, the National Research Institute of Cultural Heritage (NRICH) was founded and Changsan was appointed as its head. Despite the many difficulties he faced in running the institute with limited financial and human resources, he gave everything he had to research and field studies of the brilliant cultural heritages that Korea has preserved for so long. Changsan succeeded in restoring Bulguksa Temple, and followed this up with the successful excavation of the Cheonmachong Tomb and the Hwangnamdaechong Tomb in Gyeongju. He then explored the Hwangnyongsa Temple site, Bunhwangsa Temple, and the Mireuksa Temple site in order to systematically evaluate the Buddhist culture and structures of the Three Kingdoms Period. We can safely say that the large excavation projects that he organized and carried out at that time not only laid the foundations for Korean archeology but also made significant contributions to studies in related fields. Above all, in terms of the developmental process of Korean archeology, the achievements he generated with his exceptional passion during the period are almost too numerous to mention, but they include his systematization of various excavation methods, cultivation of archaeologists, popularization of archeological excavations, formalization of survey records, and promotion of data disclosure. On the other hand, although this "Excavation King" devoted himself to excavations, kept precise records, and paid keen attention to every detail, he failed to overcome the limitations of his era in the process of defining the nature of cultural remains and interpreting historical sites and structures. Despite his many roles in Korean archeology, the fact that he left behind a controversy over the identity of the occupant of the Hwangnamdaechong Tomb remains a sore spot in his otherwise perfect reputation.

A Study on the Soluble Salt and Deterioration of Ceramics from Taean Shipwreck (태안 마도 출토 도자기의 염에 의한 손상상태 연구)

  • Jang, Sung-Yoon;Nam, Byeong-Jik;Park, Dae-Woo;Kang, Hyun-Mi;Jung, Yong-Hwa
    • 보존과학연구
    • /
    • s.30
    • /
    • pp.189-202
    • /
    • 2009
  • Ceramics from Taean shipwreck were studied to investigate the deterioration by soluble salts and desalination pattern according to each ceramic characterization. NaCl crystals were found as a crystal growth on the ceramic microstructure and deteriorated to push off the glaze layer of some Puncheong ware sample. As a result of monitoring the desalination pattern of ceramics for 74days, the earthenware sample with big pores and no glaze removed soluble salts so fast, but Puncheong ware and Whiteware samples removed lots of soluble salts slowly and continuously. Generally, it takes long time to remove soluble salts from porcelains, due to small pores and glaze, but the long-term desalination probably can cause the damage on the surface layer such like glaze. As some soluble salts still remains in the ceramic microstructures after desalination, it is very important to control and keep the relative humidity stable through the proper storage. There are various ceramic deterioration patterns by soluble salts. Therefore, it needs to select the desalination method of ceramics from shipwreck, considering the material characteristics and the production techniques.

  • PDF

An analysis of anchor stones on the west and south coasts (서·남해안 출수 닻돌 분석)

  • PARK Seungmin
    • Korean Journal of Heritage: History & Science
    • /
    • v.55 no.4
    • /
    • pp.6-22
    • /
    • 2022
  • In this paper classifies the types of 228 anchor stones discharged from the west and south coasts, assumes a combined method by type, routes through discharge locations, and It attempted to estimate the burial site. Prior to classification of types, the weight, thickness, width, and length of the anchor stone were measured, and the largest Young in the tomb The scent weight was classified into I~V groups, and the shape of the anchor stone was classified into 1-6 types. All of these weight and shape correlations It was classified into 17 types. The combined method by type is 180kg or less depending on the morphological characteristics of the reference value of the extracted anchor stone, and the type An anchor of type 1 or 2 is used in combination with an anchor, and a anchor of type 3 or 6 weighs more than 180kg and is combined with an anchor The dragon was assumed to be an anchor. Along with this, the route and burial site are identified through past records and testimony of local residents It was checked against the data. The route was largely consistent with past records, but the new route was apparent in waters near the island or inland It was also drawn. In the case of burial sites, small and large in Taean Mado Sea and Jindo Byeokpajin Sea, where anchor stones are concentrated, Considering the pattern of the type anchor stones being discharged, it was consistent with the testimony that ships of various sizes were mysterious in the two seas. Based on this type classification, a study on the spatiality of the anchors was conducted. First, a comparison and analysis was done on whether actual real data, such as anchor stones, old ships, and relics, were identified on the Joun-ro route and international trade routes as recorded in the past literature. Where there was no record, the route was estimated based on real data. To this end, routes estimated based on the testimony of local residents and modern ship workers were analyzed as to whether ships traveled there in the past and whether they could actually sail. Next, the location of each seedling was estimated by ship size according to the weight of the anchor stone. In the case of the Taean Mado Sea and Jindo Byeokpajin Sea, both small and large anchor stones were discharged from the coastline and were far away.

Anaerobic Corrosion Properties of Sangpyeongtongbo Excavated at Bigyeongdo, Seosan (서산 비경도 출수 상평통보의 혐기성 부식 특성)

  • Kim, Kyu Been;Chung, Kwang Yong
    • Journal of Conservation Science
    • /
    • v.33 no.3
    • /
    • pp.167-179
    • /
    • 2017
  • In this study, Sangpyeontongbo excavated at Bigyeongdo, Seosan, were investigated to determine the components of the corrosion products that were formed while they were buried underwater in an anaerobic environment. The causes of corrosion product formation were also determined. Microstructure observation, element mapping, principle component analysis for each year, and the detection of corrosion products were carried out. Results indicate that the concretions of corrosion products on the surface are needle-, hexahedral-, and octahedral-shaped; Pb, Cu, and S were among the elements detected. The Cu-S layer was clearly verified using element mapping. An analysis of major elements for each layer showed that Cu, S, and Pb were present and that most Zn was eliminated. The corrosion products detected were $PbCO_3$ (concretion) and $Cu_{1.96}S$ (metal). Accordingly, the anaerobic corrosion properties of Sangpyeongtongbo are summarized as follows: dezincification, copper sulfide, and lead compound.

Analysis for Temperature and Relative Humidity of Showcase in Exhibition Hall Operated Intermittent Air Conditioning (간헐공조 전시관내 유물 진열장의 온·습도 환경 분석)

  • Lee, Sun Myung;Lim, Bo A;Kim, Seojin
    • Journal of Conservation Science
    • /
    • v.29 no.4
    • /
    • pp.311-320
    • /
    • 2013
  • The showcase has insufficient temperature control, but it has excellent humidity control. The annual average temperature and relative humidity inside the showcase was $18.8^{\circ}C$ and 60.3%, respectively, and the showcase showed lower temperature and higher humidity than the exhibition room. The temperature inside the showcase appeared with high variation according to the seasons, while relative humidity was ranging from 59% to 61% regardless of the seasons. The showcase showed high temperature and humidity likewise the exhibition room in summer. In addition, lowering of temperature was elevated relative humidity according to the operation of air conditioner in summer. A moisture problem occurred because the temperature and humidity differences between the exhibition room and showcase were large according to the operation of air conditioner in winter. PI for temperature and relative humidity inside the showcase is 18.0%, and it means conservation environment for exhibition is unsuitable. In particular, continuous management of temperature and humidity inside the showcase is required because PI in the summer and winter is less than 1.0%.

Chemical Characteristics of Timbers from the Yeongheungdo Shipwreck (영흥도선의 화학적 특성)

  • Cha, Mi Young
    • Journal of Conservation Science
    • /
    • v.33 no.1
    • /
    • pp.35-42
    • /
    • 2017
  • The Yeongheungdo shipwreck was excavated in the sea of Seomeopbeol, Ongjin-gun, Incheon, Korea. Chemical characterization of timbers from the shipwreck occurred via maximum moisture content, chemical composition, FT-IR, solid state $^{13}C$ NMR, and XRD analyses. As maximum moisture content of the outer part of the timbers averaged 623%, a phenomenon in that lignin increased relatively, according to the decrease in cellulose, and the ash content increased, which is typical of waterlogged archaeological wood was shown. The results from the FT-IR and solid state $^{13}C$ NMR analyses showed that the cellulose band of the outer part had disappeared or had remarkably decreased. In addition, the bands assigned to lignin dramatically increased. However, regarding the inner part of the timbers, hemicellulose and some crystalline cellulose and amorphous cellulose bands decreased. Therefore, a large difference exists between the degradation levels of the outer and inner parts of the timbers of the Yeongheungdo shipwreck.

Conservation and Analysis of Inner Materials of a Stoneware Bottle from Incheon Ongjingun Yeongheungdo Shipwreck (인천 옹진군 영흥도선 출수 도기병의 보존처리와 내용물 분석)

  • Kim, Hyoyun;Kim, Seojin
    • Journal of Conservation Science
    • /
    • v.32 no.4
    • /
    • pp.449-457
    • /
    • 2016
  • A stoneware bottle was recovered from the Incheon Yeongheungdo Shipwreck in 2013. Primary observations showed that this object had a sealed opening and was covered with a foreign material. After it was cleaned via mechanical and chemical methods, wave patterns were observed on the outer surface of the bottle and a yellowish-brown transparent material was found within. In this paper, the process of conserving the stoneware bottle and the analysis conducted on the unknown material found within is explained. The conservation process included steps such as cleaning, desalination and restoration. After of the missing area located at the rim, the original shape of the bottle was made clear. In addition, the unknown inner material was analyzed using FT-IR and GC-MS. Results showed that the material is similar to golden lacquer. It is speculated that the Yeongheungdo Ship had wrecked during the Unified Silla period while carrying a bottle loaded with golden lacquer.

Chemical Cleaning of Iron Stains on Ceramics (화학세척제를 이용한 도자기의 철산화물 제거 특성 연구)

  • Park, Dae-Woo;Jang, Sung-Yoon;Nam, Byeong-Jik;Ham, Chul-Hee;Lim, Seong-Tae
    • Journal of Conservation Science
    • /
    • v.27 no.4
    • /
    • pp.345-356
    • /
    • 2011
  • To remove metal stains of the ceramics, chemical cleaning is essential case by case. This study investigated the removal characteristics of iron stains by oxalic acid and citric acid including their application methods of soaking and poultice. The soaking method in cleaning agents showed removal process by color difference and released iron contents from iron stains on ceramics. Iron stains were removed successfully from ceramics, which soaked in oxalic acid for 60 hours. However, it is recommendable to soak in 0.25M oxalic acid for one to three hours because most iron stains were disappeared in 3 hours soaking. Citric acid is less effective than oxalic acid in removing iron stains because of heavy molecular weight and low acidity. Poultices (bentonite, sepiolite, activated carbon fiber and celite) with oxalic acid were applied on contaminated ceramics. After ten hours, iron stains on ceramics were removed successfully by poultice. Among them, bentonite and sepiolite have better application. Therefore, sepiolite with 0.25M oxalic acid was applied on the iron stains of whiteware and celadon from Ma Island, and then stains were removed. However, it is judged that the application methods can be varied according to the form and depth of contaminant. In addition, the residues of poultice on the ceramics will be considered for preventing contamination.

Damage Characteristics of Korean Traditional Textiles by Nitrogen Dioxide (NO2) Concentrations (이산화질소(NO2) 농도에 따른 전통직물의 손상 특성)

  • Kim, Myoung Nam;Lim, Bo A;Kim, Seojin;Lee, Sun Myung
    • Journal of Conservation Science
    • /
    • v.29 no.3
    • /
    • pp.197-207
    • /
    • 2013
  • The gas acceleration test was conducted to identify the deterioration of Korean traditional textiles caused by $NO_2$. Total 20 specimens were prepared using 4 different materials (silk, cotton, ramie, hemp) after dyeing with 5 colors (undyed, red, yellow, blue, black). The specimens were exposed to 0.01, 0.1, 1, 10, 100, and 1000 ppm $NO_2$ gas in the test chamber at $20^{\circ}C$, 50% RH for 1 day. Optical, chemical, and physical evaluation was carried out after the exposure. In the case of Korean traditional textile, color difference increased at 1 ppm/day, $NO_3{^-}$ concentration, carbonyl and C-$NO_2$ functional group increased while pH decreased at 10 ppm/day and tensile strength weakened at 100 ppm/day. when it comes to undyed textile, alteration of color difference on silk and hemp cloth, $NO_3{^-}$ concentration and tensile strength on hemp cloth was remarkable. In addition, color difference on blue and yellow textile, $NO_3{^-}$ concentration increase of yellow textile and tensile strength decrease of hemp cloth & ramie cloth were significant. The results suggest that critical $NO_2$ concentration of optical, chemical, and physical damage on Korean traditional textiles are 1ppm/day, 10 ppm/day, 100 ppm/day respectively.