• 제목/요약/키워드: superconducting elements

검색결과 140건 처리시간 0.025초

Quench characteristics of YBCO thin films using magnetic field source for superconducting fault current limiters

  • Lee, B.W.;Park, K.B.;Kang, J.S.;Oh, I.S.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권2호
    • /
    • pp.11-14
    • /
    • 2004
  • YBCO thin films have good characteristics for current limiting materials due to compact size and high current carrying capability. But the irregularities and the extreme thin thickness of YBCO films cause some difficulties in simultaneous quench and thermal shock protection. In order to solve these problems, vertical magnetic field generated from solenoid coil was applied to the YBCO element. And also to minimize the inductance caused by the serial connection of magnetic field source with superconducting elements, magnetic field source was separated from the power lines adapting protective current transformer. In this study, electric field-current (E-I) and quench characteristics of YBCO films were analyzed both by electrical measuring method and observations of bubble propagation. From the experiment results, it was revealed that the magnetic fields generated by surrounding coil could induce the uniform quench distribution for all stripes of current limiting units and finally simultaneous quenches were realized in all serial connection of YBCO elements. In addition, the separation of magnetic field source form electrical network could be good solution for simultaneous quench of YBCO films without any unnecessary effect caused by serial connection.

플라즈마 용사법에 의해 제조된 YBa2Cu$\chi$O7-y(X=3, 3.5, 4) 고온초전도체 후막층의 결정상 및 초전도 특성 (Crystalline Phases and Superconductor Characteristics of the Plasma Sprayed YBa2Cu$\chi$O7-y High Tc Superconductor Thick Film)

  • 한명섭;서동수
    • 한국세라믹학회지
    • /
    • 제29권2호
    • /
    • pp.152-160
    • /
    • 1992
  • High-Tc superconductor thick films of YBa2Cu$\chi$O7-y (X=3, 3.5, 4) of which thickness varies from 100 $\mu\textrm{m}$ to 200 $\mu\textrm{m}$ were successfully prepared by plasma spraying method, and the characteristics of thick film depending on copper content and heat treatment conditions were investigated. Regardless of heat-treated temperature, the specimens with X=3 were composed of YBa2Cu$\chi$O7-y, Y2BaCuO5 and BaCuO3 phases. The specimens with X=4, however, were composed of YBa2Cu$\chi$O7-y phase at all heat treatment conditions. The specimens with X=4 composition showed the best superconducting characteristics after heat treatment at 925$^{\circ}C$, and the superconducting transition temperature with zero resistivity (Tc,zero) was 87K. The thick film lost superconductivity when the specimens were heat-treated at 950$^{\circ}C$ because of interdiffusion between superconductor elements and bond coating elements and Y2BaCuO5 phase was found was found to be main phase at the interface.

  • PDF

초전도 전류제한기의 패턴형상별 특성 (Characteristics of superconducting fault current limiters with various pattern shape)

  • 최효상;정헌상;최창주;이상일;정수복;오금곤;임성훈;한병성;정동철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.529-532
    • /
    • 2003
  • Quench behavior of resistive superconducting fault current limiters (SFCLs) with various pattern shapes was investigated. The pattern shapes employed were meander, bi-spiral, and spiral shapes of identical line width, gap and margin. SFCLs were fabricated from YBCO thin films grown on two-inch diameter $Al_2O_3$ substrates under the same conditions. Resistance rise of current limiting elements was low at a spiral shape before the whole quench completion, which may act as a disadvantage for simultaneous quench in serial connection between current limiting elements, but the temperature tended to have similar values at higher voltages. On the other hand, bi-spiral shape was severe at insulation level between current limiting lines. When these aspects were considered, we concluded that a meander shape was appropriate to design for a resistive SFCL based on thin films except the concentration of electric field at edge areas of strip lines.

  • PDF

100m 급 초전도선재 제조용 EDDC 증착시스템 (EDDC deposition system for 100m long superconducting coated conductor)

  • 김호섭;하홍수;오상수;고락길;양주생;김태형;송규정;하동우;박유미;염도준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.18-19
    • /
    • 2005
  • EDDC(Evaporation using Drum in Dual Chamber) deposition system was manufactured for 100m long superconducting coated conductor. It is composed of reaction chamber, evaporation chamber and differential chamber. The drum is located across the differential and exposed to both of the evaporation chamber and the reaction chamber, and the tape is wound on the drum. The elements of superconducting material are co-evaporated from respective element boats in the evaporation chamber and deposited on the drum and reacted with oxygen in the reaction chamber. This process repeats by rotating the drum. When the total pressure of the reaction chamber was 5 mTorr, that of the evaporation chamber was $5{\sim}10^{-5}$Torr. This atmosphere can be achieved by means of differential pumping. There are four evaporator in the evaporation chamber. One is the radiation heating evaporator and the others are the high frequency induction evaporator. EDDC is one of promising methods for commercialization of superconducting coated conductor.

  • PDF

Enrichment of valuable elements from vanadium slag using superconducting HGMS technology

  • He, Sai;Yang, Chang-qiao;Li, Su-qin;Zhang, Chang-quan
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권1호
    • /
    • pp.17-21
    • /
    • 2017
  • Vanadium slags is a kind of vanadiferous solid waste from steelmaking process. It not only occupies land, pollutes environment, but also leads to waste of resources. Based on the difference of magnetic susceptibility of different particles caused by their chemical and physical properties from vanadium slag, a new technology, superconducting high gradient magnetic separation was investigated for separation and extraction of valuable substances from vanadium slag. The magnetic concentrate was obtained under optimal parameters, i.e., a particle size -200 mesh, a magnetic flux density of 0.8 T, a slurry concentration of 5 g/L, an amount of steel wools of 25 g and a slurry flow velocity of 2 L/min. The content of $Fe_2O_3$ in concentrate could be increased from 39.6% to 55.0% and $V_2O_5$ from 2.5% to 4.0%, respectively. The recovery rate is up to 42.9%, and the vanadium slag has been effectively reused.

고온초전도테이프 제작을 위한 YSZ 박막의 고속증착방법 (High speed deposition technique of YSZ film for the superconducting tape)

  • 김호섭;석동기;정준기;고락길;하홍수;송규정;염도준;박찬
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권3호
    • /
    • pp.27-32
    • /
    • 2004
  • High temperature superconducting coated conductor has a structure of /< superconducting layer>//. The buffer layer consists of multi layer, and the architecture most widely used in RABiTS approach is CeO$_2$(cap layer)/YSZ(diffusion barrier layer)/CeO$_2$(seed layer). Evaporation technique is used for the CeO$_2$ layer and DC reactive sputtering technique is used for the YSZ layer, A chamber was set up specially for DC reactive sputtering, Detailed features are as following. A separator divided the chamber into two halves a sputtering chamber and a reaction chamber. The argon gas for sputtering target elements flows out of the cap of sputtering gun, and water vapor for reaction with depositing species spouts near the substrate. Turbo pump is connected with reaction chamber. High speed deposition of YSZ film could be achieved in the chamber. Detailed deposition conditions (temperature and partial pressure of reaction gas) were investigated for the rapid growth of high quality YSZ film.

Designs of 10 MW Air-core and Iron-core HTS Wind Power Generators

  • Sung, Hae-Jin;Park, Minwon;Yu, In-Keun
    • Journal of Electrical Engineering and Technology
    • /
    • 제10권2호
    • /
    • pp.545-550
    • /
    • 2015
  • High Temperature Superconducting (HTS) synchronous generators can be designed with either an air-core type or iron-core type. The air-core type has higher efficiency under rated rotating speed and load than the iron-core type because of the iron losses which may produce much heat. However, the total length of HTS wire in the air-core type is longer than the iron-core type because the generated magnetic flux density of the air-core type is low. This paper deals with designs of 10 MW air-core and iron-core HTS wind power generators for wind turbines. Fully air-core, partially iron-core, and fully iron-core HTS generators are designed, and various stator winding methods in the three HTS generators are also considered, such as short-pitch concentrated winding, full-pitch concentrated winding, short-pitch distributed winding, and full-pitch distributed winding. These HTS generators are analyzed using a 3D finite elements method program. The analysis results of the HTS generators are discussed in detail, and the results will be effectively utilized for large-scale wind power generation systems.

이중퀜치를 이용한 자속구속형 초전도한류기의 과도전류제한 특성 (Transient Current Limiting Characteristics of Flux-Lock Type SFCL Using Double Quench)

  • 최상재;임성훈
    • 한국전기전자재료학회논문지
    • /
    • 제30권2호
    • /
    • pp.96-100
    • /
    • 2017
  • In this paper, the flux-lock type superconducting fault current limiter (SFCL) using double quench was suggested and its transient current limiting characteristics were analyzed. The suggested flux-lock type SFCL using double quench consists of two magnetically coupled windings and two $high-T_{c}$ superconducting (HTSC) elements connected in series with each winding. To analyze the transient current limiting characteristics of the flux-lock type SFCL using double quench, the short-circuit tests according to the fault angles, which affect the transient component of the fault current right after the fault occurs, were executed. From the comparative analysis for the short-circuit tests at both $0^{\circ}$ and $90^{\circ}$ fault angles, the useful transient current limiting operations of the suggested flux-lock type SFCL through the double or the single quench occurrence were confirmed.

Transient Fault Current Limiting Characteristics of a Transformer Type SFCL Using an Additional Magnetically Coupled Circuit

  • Lim, Seung-Taek;Lim, Sung-Hun
    • Transactions on Electrical and Electronic Materials
    • /
    • 제18권1호
    • /
    • pp.42-45
    • /
    • 2017
  • In this paper, a transformer type SFCL (superconducting fault current limiter) using an additional magnetically coupled circuit was suggested. Its transient fault current limiting characteristics, due to the winding direction of additional coupled circuit, were analyzed through fault current limiting tests. The suggested transformer type SFCL was composed of the primary winding, and one secondary winding wound on the same iron core together with an additional magnetically coupled circuit. That circuit consists of the other secondary winding together with the other SC (superconducting) element connected in parallel with its other secondary winding. As one of the effective design parameters to affect the transient fault current of the SFCL, the fault current limiting tests of the suggested SFCL were carried out considering the winding direction of its additional coupled circuit. It was confirmed that, through the analysis on the fault current tests of the SFCL, the quench sequence of two SC elements comprising the suggested SFCL could be adjusted by the winding direction of the additional coupled circuit.

Quench properties of superconducting fault current limiters connected in parallel

  • Kim, Hye-Rim;Park, Hyo-Sang;Park, Kwon-Bae;Hyun, Ok-Bae;Hwang, Si-Dole
    • Progress in Superconductivity
    • /
    • 제3권2호
    • /
    • pp.224-228
    • /
    • 2002
  • We investigated the quench properties of superconducting fault current limiters (SFCLs) connected in parallel. It was carried out as an effort to scale up the current capacity of SFCL toys texts. SFCLs were based on $YBa_2$$Cu_3$$O_{7}$ films coated in-situ with a gold layer and fabricated by patterning the films into 2 mm wide and 42 cm long meander lines by photolithography. Two SFCLS were connected in parallel and tested with simulated AC fault currents. Initially the current was divided unequally into branches of parallel connection due to unequal resistance of the branches. However, once quench started in the SFCLs, the current oscillated between the branches and then was distributed nearly equally between the branches. In other words, the elements quenched simultaneously. The oscillation amplitude decreased as the source voltage was increased: the oscillation was the most prominent near the quench current. The observed oscillation and the consequent simultaneous quench was understood in terms of quench start and development in the SFCLs.

  • PDF