Property of the Nano-Thick TiO2 Films Using an ALD at Low Temperature (저온 ALD로 제조된 TiO2 나노 박막 물성 연구)

  • Yoon, Ki-Jeong;Song, Oh-Sung
    • Korean Journal of Materials Research
    • /
    • v.18 no.10
    • /
    • pp.515-520
    • /
    • 2008
  • We fabricated 10 nm-$TiO_2$ thin films for DSSC (dye sensitized solar cell) electrode application using ALD (atomic layer deposition) method at the low temperatures of $150^{\circ}\;and\;250^{\circ}$. We characterized the crosssectional microstructure, phase, chemical binding energy, and absorption of the $TiO_2$ using TEM, HRXRD, XPS, and UV-VIS-NIR, respectively. TEM analysis showed a 10 nm-thick flat and uniform $TiO_2$ thin film regardless of the deposition temperatures. Through XPS analysis, it was found that the stoichiometric $TiO_2$ phase was formed and confirmed by measuring main characteristic peaks of Ti $2p^1$, Ti $2p^3$, and O 1s indicating the binding energy status. Through UV-VIS-NIR analysis, ALD-$TiO_2$ thin films were found to have a band gap of 3.4 eV resulting in the absorption edges at 360 nm, while the conventional $TiO_2$ films had a band gap of 3.0 eV (rutile)${\sim}$3.2 eV (anatase) with the absorption edges at 380 nm and 410 nm. Our results implied that the newly proposed nano-thick $TiO_2$ film using an ALD process at $150^{\circ}$ had almost the same properties as thsose of film at $250^{\circ}$. Therefore, we confirmed that the ALD-processed $TiO_2$ thin film with nano-thickness formed at low temperatures might be suitable for the electrode process of flexible devices.

Characteristics of Nano-Size Au Fine Particles Doped TiO2 Thin Films by Sol-Gel Method (졸-겔법에 의한 나노크기 Au 미립자 분산 TiO2 박막의 특성)

  • Park, Min-Jung;Koo, Se-Na;Lee, Kyoung-Seok;Mun, Chong-Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.2 s.285
    • /
    • pp.114-120
    • /
    • 2006
  • Nano-size Au particle doped $TiO_2$ films were prepared with $Ti(OC_3H_7^i)_4$, polyvinylpyrrolidone(PVP), $HAuCl_4$ and $C_3H_7OH$ etc. by sol-gel method. $TiO_2$ gel films were obtained by the dip-coating method on the $SiO_2$ glass substrates, and then heat-treated at $700^{\circ}C$ for 10 min. The thickness of $TiO_2$ films were $0.7\~1.8\;{\mu}m$. It was found that the thickness of films prepared from PVP containing solution was about $2\~8$ times higher values than that of thin films without PVP. The size of Au particles doped in the films were about $350\~750\;nm$. Nano-size Au particle dispersed $TiO_2$ films showed high absorption peak at visible region 450nm, which made them good candidates for non-linear optical materials and photo-catalytic materials. The contact angle of $TiO_2$ film for water was $12.5^{\circ}$, and therefore it is clear that $TiO_2$ films have very high hydrophilic properties and the self-cleaning effects.

UV Absorption of Nano-thick $TiO_2$ Prepared Using an ALD (ALD 방법으로 제조된 나노급 $TiO_2$에 의한 자외선 차단효과 연구)

  • Han, Jeung-Jo;Song, Oh-Sung;Ryu, Ji-Ho;Yoon, Ki-Jeong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.8 no.4
    • /
    • pp.726-732
    • /
    • 2007
  • We fabricated UV absorption functional $10{\sim}50nm-TiO_{2-x}/quartz$ structures layer using ALD (atomic layer deposition) method. We deposited $10nm-TiO_{2-x}$ layer on quartz substrate using ALD, and film thickness was determined by an ellipsometer. The others specimen thickness was controlled by ALD time lineally. We characterized controlling phase UV and visible optical property using an X-ray difractometer, a UV-VIS-IR spectrometer and a digital camera. $ALD-TiO_{2-x}$ layers were non-stoichiometric $TiO_{2-x}$ form and amorphous phases comparing with bulk $TiO_2$. While the conventional bulk $TiO_2$ had band gap of $3.0{\sim}3.2eV$ resulting in absorption edges at 380 nm and 415 nm, $ALD-TiO_{2-x}$ layers showed absorption edges at 197 nm and 250 nm. Therefore, our nano-thick $ALD-TiO_{2-x}$ was able to absorb shorter UV region and showed excellent transmittance in visible region. Our result implies that our newly proposed nano-thick $TiO_{2-x}$ using ALD process may improve transmittance in visible rays and be able to absorb shorter UV light effectively.

  • PDF

Preparation and Electrical Properties of TiO2 Films Prepared by Sputtering for a Pulse Power Capacitor (스퍼터링에 의한 펄스파워 캐패시터용 TiO2 박막의 제조 및 전기적특성)

  • Park, Sang-Shik
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.642-647
    • /
    • 2012
  • $TiO_2$ thin films for a pulse power capacitor were deposited by RF magnetron sputtering. The effects of the deposition gas ratio and thickness on the crystallization and electrical properties of the $TiO_2$ films were investigated. The crystal structure of $TiO_2$ films deposited on Si substrates at room temperature changed to the anatase from the rutile phase with an increase in the oxygen partial pressure. Also, the crystallinity of the $TiO_2$ films was enhanced with an increase in the thickness of the films. However, $TiO_2$ films deposited on a PET substrate showed an amorphous structure, unlike those deposited on a Si substrate. An X-ray photoelectron spectroscopy(XPS) analysis revealed the formation of chemically stable $TiO_2$ films. The dielectric constant of the $TiO_2$ films as a function of the frequency was significantly changed with the thickness of the films. The films showed a dielectric constant of 100~110 at 1 kHz. However, the dissipation factors of the films were relatively high. Films with a thickness of about 1000nm showed a breakdown strength that exceeded 1000 kV/cm.

Fabrication and Characterization of Y2Ti2O7 Powder and Thick Film by Chemical Processing (화학적 공정을 이용한 Y2Ti2O7 분말과 후막 제조 및 특성)

  • Lee, Won-Joon;Choi, Yeon-Bin;Bae, Dong-Sik
    • Korean Journal of Materials Research
    • /
    • v.27 no.5
    • /
    • pp.289-293
    • /
    • 2017
  • $Y_2Ti_2O_7$ nanoparticles (0.3 mol%) have been successfully synthesized by the co-precipitation process. The samples, adjusted to pH7 with ammonia solution as catalyst and calcined at $700{\sim}900^{\circ}C$, exhibit very fine particles with close to spherical shape and average size of 10-30 nm. It was possible to control the size of the synthesized $Y_2Ti_2O_7$ particles by manipulating the conditions. The $Y_2Ti_2O_7$ nanoparticles were coated on a glass substrate by a dipping coating process with inorganic binder. The $Y_2Ti_2O_7$ solution coated on the glass substrate had excellent adhesion of 5B; pencil hardness test results indicated an excellent hardness of 6H. The thickness of the thick film was about $30{\mu}m$. Decomposition of MB on the $Y_2Ti_2O_7$ thin film shows that the photocatalytic properties were excellent.

High-temperature Oxidation of Nano-multilayered TiAlSiN Filems (나노 다층 TiAlSiN 박막의 고온 산화)

  • Lee, Dong-Bok;Kim, Min-Jeong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.189-189
    • /
    • 2016
  • In this study, the Al-rich AlTiSiN thin films that consisted of TiN/AlSiN nano-multilayers were deposited on the steel substrate by magnetron sputtering, and their high-temperature oxidation behavior was investigated, which has not yet been adequately studied to date. Since the oxidation behavior of the films depends sensitively on the deposition method and deposition parameters which affect their crystallinity, composition, stoichiometry, thickness, surface roughness, grain size and orientation, the oxidation studies under various conditions are imperative. AlTiSiN nano-multilayer thin films were deposited on a tool steel substrate, and their oxidation behavior of was investigated between 600 and $1000^{\circ}C$ in air. Since the amount of Al which had a high affinity for oxygen was the largest in the film, an ${\alpha}-Al_2O_3-rich$ scale formed, which provided good oxidation resistance. The outer surface scale consisted of ${\alpha}-Al_2O_3$ incoporated with a small amount of Ti, Si, and Fe. Below this outer surface scale, a thin ($Al_2O_3$, $TiO_2$, $SiO_2$)-intermixed scale formed by the inwardly diffusing oxygen. The film oxidized slower than the $TiO_2-forming$ kinetics and TiN films, but faster than ${\alpha}-Al_2O_3-forming$ kinetics. During oxidation, oxygen from the atmosphere diffused inwardly toward the reaction front, whereas nitrogen and the substrate element of iron diffused outwardly to a certain extent.

  • PDF

The Effect of $TiO_2$ Thickness on the Performance of Dye-Sensitized Solar Cells ($TiO_2$ 두께에 따른 염료감응형 태양전지의 효율 변화)

  • Kim, Dae-Hyun;Park, Mi-Ju;Lee, Sung-Uk;Choi, Won-Seok;Hong, Byung-You
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.147-148
    • /
    • 2007
  • Dye-sensitized solar cell using conversion of solar energy to electrical energy appeared that which solves a environmental matter. The dye-sensitized solar cell uses nano-crystalline oxide semiconductor for absorbing dye. The $TiO_2$ is used most plentifully. The efficiency of the dye-sensitized solar cell changes consequently in the particle size, morphology, crystallization and surface state of the $TiO_2$. In this paper, we report The effect of titania$(TiO_2)$ thickness on the performance of dye-sensitized solar cells. Using doctor blade method, It produced the thickness of the $TiO_2$ with $7\;{\mu}m,\;10\;{\mu}m,\;13\;{\mu}m$. The efficiency was the best from $10{\mu}m$. It had relatively low efficiency on the thickness from $7\;{\mu}m\;to\;13\;{\mu}m$. The reason why it presents low efficiency on $7\;{\mu}m$ thickness is that excited electrons can not be delivered enough due to thin thickness of $7\;{\mu}m\;TiO_2$. And The reason why it presents low efficiency on $13\;{\mu}m$ thickness is that thick $13\;{\mu}m\;TiO_2$ can not penetrate the sunlight enough.

  • PDF

The Effects of WO3 Nanoparticles Addition to the TiO2 Photoelectrode in Dye-Sensitized Solar Cells

  • Vu, Hong Ha Thi;Hwang, Yoon-Hwae;Kim, Hyung-Kook
    • Current Photovoltaic Research
    • /
    • v.4 no.2
    • /
    • pp.42-47
    • /
    • 2016
  • Increasing the efficiency of dye-sensitized solar cells (DSSCs) by the fabrication of new photoelectrodes (PEs) is an important challenge. This study examined the photovoltaic parameters of DSSCs composed of a $TiO_2$ PE with $WO_3$ nanoparticles (NPs). A number of PEs with the same thickness but different concentrations of $WO_3$ NPs in the $TiO_2PE$ were prepared. The morphology and structural properties of the prepared PEs were examined by field-emission scanning electron microscopy and X-ray diffraction, respectively. The effects of the $WO_3$ NPs mixing concentration on the efficiency of DSSCs were investigated under simulated solar light irradiation.

The Effect of Surface Plasmon on Internal Photoemission Measured on Ag/$TiO_2$ Nanodiodes

  • Lee, Hyosun;Lee, Young Keun;Park, Jeong Young
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.662-662
    • /
    • 2013
  • Over the last several decades, innovative light-harvesting devices have evolved to achieve high efficiency in solar energy transfer. Research on the mechanisms for plasmon resonance is very desirable to overcome the conventional efficiency limits of photovoltaics. The influence of localized surface plasmon resonance on hot electron flow at a metal-semiconductor interface was observed with a Schottky diode composed of a thin silver layer on $TiO_2$. The photocurrent is generated by absorption of photons when electrons have enough energy to travel over the Schottky barrier and into the titanium oxide conduction band. The correlation between the hot electrons and the surface plasmon is confirmed by matching the range of peaks between the incident photons to current conversion efficiency (IPCE, flux of collected electrons per flux of incident photons) and UV-Vis spectra. The photocurrent measured on Ag/$TiO_2$ exhibited surface plasmon peaks; whereas, in contrast to the Au/$TiO_2$, a continuous Au thin film doesn't exhibit surface plasmon peaks. We modified the thickness and morphology of a continuous Ag layer by electron beam evaporation deposition and heating under gas conditions and found that the morphological change and thickness of the Ag film are key factors in controlling the peak position of light absorption.

  • PDF

The Study of Color and Hardness of TiN Thin Film by UBM Sputtering System (UBM Sputtering System에 의한 TiN막의 색상과 경도에 관한 연구)

  • Park, Moon Chan;Lee, Jong Geun;Joo, Kyung Bok
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.14 no.1
    • /
    • pp.57-62
    • /
    • 2009
  • Purpose: TiN films were deposited on sus304 by unbalanced magnetron sputtering system which was designed and developed as unbalancing the strength of the magnets in the magnetron electrode. The color and hardness of deposited TiN films was investigated. Methods: The cross sections of deposited films on silicon wafer were observed by SEM to measure the thickness of the films, the components of the surface of the films were identified by XPS, the components of the inner parts of the films were observed by XPS depth profiling. XPS high resolution scans and curve fittings of deposited films were performed for quantitative chemical analysis, Vickers micro hardness measurements of deposited films were performed with a nano indenter equipment. Results: The colors of deposited films gradually changed from light gold to dark gold, light violet, and indigo color with increasing of the thickness. It could be seen that the color change come from the composite change of three compound,$TiO_{x}N_{y}$, $TiO_2$, TiN. Especially, the composite change of$TiO_{x}N_{y}$ compound was thought to affect the color change with respect to thickness. Conclusions: Deposited films had lower than the value of general TiN film in Vickers hardness, which was caused by mixing three TiN, $TiO_2$,$TiO_{x}N_{y}$ compound in the deposited films. The increasing and decreasing of micro hardness with respect to thickness was thought to have something to do with the composite of TiN in the films.