봉파쇄기로 제조한 재생 굵은골재의 품질특성 (Quality Properties of Recycled Coarse Aggregate Manufactured by the Bar-Crusher)

  • 백대현;한동엽;유명열;이건철;한천구
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.509-512
    • /
    • 2006
  • In this study, the quality properties of recycled coarse aggregate, manufactured by the barcrusher, were compared to that of aggregate, manufactured by conservative systems. Test showed that recycled coarse aggregate, manufactured by the bar-crusher, had higher density and shape index, and exhibited lower absorption and abrasion ratios, compared with a con-crusher and an impact-crusher. This is due to the peeling-off effect of mortar, attached on recycled aggregate and the improved round shape of that.

  • PDF

쇄석 골재의 광물학적 특성 및 알칼리-골재 반응성 (The Petrographic Properties and Alkali-Aggregate Reaction of Crushed Stones)

  • 전쌍순;박현재;이효민;황진연;진치섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.249-254
    • /
    • 2002
  • In Korea, due to the shortcomings of natural aggregates and increasing needs of crushed stones, it is necessary to examine the alkali-aggregate reaction of the crushed stones. The purpose of this study is to analyze petrographic properties and alkali-aggregate reaction of crushed stones This study was peformed to investigate the alkali-aggregate reaction of crushed stones using chemical analysis, physical properties, XRD, XRF and mortar-bar method.

  • PDF

국내 쇄석골재의 화학반응성 분석 (An Analysis on the Reaction of Crushed Aggregates)

  • 이장화;김성욱;최일섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1993년도 가을 학술발표회 논문집
    • /
    • pp.97-102
    • /
    • 1993
  • In the country, due to short comings of natural aggregates of good quality, it is common to use crushed stones. However, the investigation has not been done on the chemical reaction of crushed stones. This study tested and analyzed the aggregate chemical reaction by Petrographic Examination(ASTM C 295),Chemical Metho(ASTM C 289) and Mortar-Bar Method (ASTM C 227). As a result, most of test aggregates didn't show any reaction but many have common deleterious mineral. Therefore, there exists the possibility of chemical reaction in petrographic point of view.

  • PDF

해수침지-건조 환경에 노출된 모르타르속 철근의 부식속도 평가 (Corrosion Monitoring of Reinforcing Bars in Cement Mortar Exposed to Seawater Immersion-and-dry Cycles)

  • 김제경;기성훈;이정재
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제22권4호
    • /
    • pp.10-18
    • /
    • 2018
  • 본 연구는 시멘트 모르타르속에 매입된 철근주위가 건조될 때 불안정한 전류분포의 영향을 측정하고, 교류 임피던스 특성변화에 대한 영향을 고찰하는 것을 목적으로 한다. 건조과정중 철근의 전기화학적 반응을 측정하기 위해, 두 개의 철근이 매입된 3개의 시멘트 모르타르가 실험을 위해 준비되었다. 주요 변수는 20mm 모르타르 두께를 동일하게 가지도록 하여, 두 철근사이의 간격이 10, 20과 30mm가 되도록 하였다. 해양환경에서 콘크리트 구조물속의 철근 부식속도를 가정하기 위해서, 3개의 모르타르 시험체는 15 사이클의 침지-건조환경(해수에서 24시간 침지와 48시간 실온 건조)에 노출되었다. 부식전위의 변화는 건조중에 용존산소의 확산속도 증가로 인해 귀한 방향으로 이동하는 것이 관찰되었다. 침지-건조환경에서 교류 임피던스는 100kHz에서 1mHz까지 측정되었다. 철근과 모르타르사이의 계면상태를 설명하기 위해 이론적 모델이 제안되었으며, 그것은 용액저항, 전하이동저항과 CPE로 구성된 등가회로를 사용하였다. 철근의 부식이 진행됨에 따라, 저주파수 영역에서 확산 임피던스가 나타났다. 침지-건조 환경중 건조과정에서 이송차가 $45^{\circ}$에 가까워지는 현상으로써 전류분포가 불균일해지는 경향을 보였다.

몰타르 시험편(W/C:0.4) 내부철근의 분극특성에 미치는 재령년수의 영향 (The Effect of Passing Aged Years to the Polarization Characteristics of Embedded Steel Bar of Mortar Specimen(W/C:0.4))

  • 문경만;원종필;박동현;이성열;정진아;이명훈;백태실
    • Corrosion Science and Technology
    • /
    • 제13권1호
    • /
    • pp.20-27
    • /
    • 2014
  • The structures of reinforced concrete has been extensively increased with rapid development of industrial society. Futhermore, these reinforced concretes are easy to expose to severe corrosive environments such as sea water, contaminated water, acid rain and seashore etc.. Thus, corrosion problem of inner steel bar embedded in concrete is very important in terms of safety and economical point of view. In this study, multiple mortar test specimen(W/C:0.4) with six types having different cover thickness each other was prepared and was immerged in seawater solution for five years to evaluate the effect of cover thickness and immersion years to corrosion property of embedded steel bar. And the polarization characteristics of these embedded steel bars was investigated using electrochemical methods such as measuring corrosion potential, cathodic polarization curve, and cyclic voltammogram. At the beginning of immersion, the corrosion potentials exhibited increasingly nobler values with increasing cover thickness. However, after immersed for 5 years, the thicker cover of thickness, the corrosion potentials shifted in the negative direction, and the relationship between corrosion potential and cover thickness was not in good agreement with each other. Therefore, it is considered that the thinner cover of thickness, corrosive products deposited on the surface of the embedded steel bar plays the role as a resistance polarization which is resulted in decreasing the corrosion rate as well as shifting the corrosion potential in the positive direction. As a result, it seemed that the evaluation which corrosion possibility of the reinforced steel would be estimated by only measuring the corrosion potential may not be a completely desirable method. Therefore, it is suggested that we should take into account various parameters, including cover thickness, passed aged years as well as corrosion potential for more accurate assessment of corrosion possibility of reinforced steel which is exposed to partially or fully in marine environment for long years.

촉진시험법을 이용한 하천골재의 알칼리 반응성 판정 (Identification of Alkali Reactivity of Natural Aggregates by Application of a Rapid Method)

  • 양동윤;이창범
    • 자원환경지질
    • /
    • 제30권2호
    • /
    • pp.175-183
    • /
    • 1997
  • The concrete structure can be easily damaged due to alkali-aggregates reaction. There are several methods to identify alkali reactivity of aggregates. The most reliable method is mortar-bar test, but it takes 3 to 12 months for whole test. The authors applied "rapid method" which takes only 7 days for this test. The result of this rapid method follows; expansion ratio of mortar bar for natural aggregates taken at the Youngsan River ranges from 0.197 to 0.489%, but that from Changseong Lake has low expansion ratio of 0.147%, which is below the limit of allowance, 0.168%. Those from the Seomjin River range from 0.173 to 0.22%, and those from the Keum River range from 0.078% to 0.111%. In the case of higher expansion ratio than 0.168%, aggregates must be used with cement containing low alkali content or adding material consuming the alkali content of cement, for example, fly ash and silica fume, etc.. Most of natural aggregates in Cheolla area have no problem in physical properties, particularly the abrasion ratio is below 40%, the limit of allowance. The natural aggregate from Cheolla area consists mostly of gneiss, granite and volcanic rocks. The major alkali reactive materials are quartz mineral with undulatory extinction in gneiss and granite, and amorphous silica in volcanic rocks. Even if a certain aggregate consists of the same kind of rocks and has similar rock composition each other, content of alkali reactivity material can be various, because rock formation is locally different according to temperature and pressure. Therefore every rock type must be physically and chemically identified before using for aggregates.

  • PDF

콘크리트를 위한 매화천 A, B 지역 골재의 암석기재학적 시험 (ASTM C 295) (Petrographic Examination of Aggregates for Concrete from Maewhacheon A, B area (ASTM C 295))

  • 정지곤
    • 한국광물학회지
    • /
    • 제14권2호
    • /
    • pp.85-98
    • /
    • 2001
  • 콘크리트 구조물에 사용되는 골재의 화학적 안전성을 진단하는 방법 중의 하나인 암석기재학적 시험(ASTM C 295)에 관한 연구로서, 이 연구를 위하여 골재의 입도 분석, 피막 검사, 풍화 ·오염상태, 암석학적 기재, 그리고 알칼리-골재 반응성 광물 및 암석의 정성·정량적 분석을 실시하였다. 경남 울진군 매화천 유역 A, B 지역의 하천 골재에 대하여 암석기재학적 방법으로 검사한 결과 풍화상태는 F(신선) 등급과 WS(약간 풍화) 등급이며 골재의 피막과 오염 상태는 우려할 정도는 아니다. 알칼리-골재 반응 광물이나 구조적으로 취약한 암석이 함유된 골재는 매화천 A 지역 골재 전체의 26 wt.%, B 지역은 19 wt.%로 집계되는데 이는 양호한 골재로 볼 수 없기 때문에 화학적 방법과 몰탈바 방법으로 더욱 정밀한 시험을 거쳐 안전성이 확인되어야 한다.

  • PDF

플라이애시와 질산리튬을 사용한 시멘트 경화체의 ASTM C 1260 적용성 검토 (Application of ASTM C 1260 for Cement Matrix Mixed with FlyAsh and Lithium Nitrate)

  • 김성권;윤경구;홍승호;강문식
    • 한국도로학회논문집
    • /
    • 제14권3호
    • /
    • pp.1-7
    • /
    • 2012
  • 본 논문에서는 ASTM C 1260을 이용하여 국내산 골재를 대상으로 알칼리-실리카 반응 판정 결과 반응성으로 판정된 골재를 대상으로 알칼리-실리카 반응 억제효과를 고찰하기 위하여 플라이애시와 질산리튬을 사용한 시멘트 경화체의 ASTM C 1260 적용성을 평가하였다. 알칼리-실리카 반응에 의한 팽창현상이 발생하는 지역에서 CaO 함량이 낮은 플라이애시를 시멘트 중량의 10, 20, 30%를 대체하는 경우 ASTM C 1260으로 알칼리-실리카 반응 억제효과를 확인할 수 있었다. 그러나 질산리튬을 사용할 경우는 ASTM C 1260은 시편을 1N NaOH 수용액에 수침하여 $80^{\circ}C$의 온도로 길이변화를 유도하므로 시편내에 혼입된 질산리튬 성분이 외부로 용출될 수 있기 때문에 알칼리-실리카 반응 억제효과를 도출하지 못하였다. 따라서 질산리듐의 ASR 억제효과를 확인하기 위해서는 다른 시험방법을 고려해야 한다.

콘크리트용 KEDO 골재의 암석기재시험 (ASTM C295) (Petrographic Study(ASTM C 295) on the KEDO Concrete Aggregates)

  • 정지곤;김경수;이철우
    • 지질공학
    • /
    • 제17권4호
    • /
    • pp.589-599
    • /
    • 2007
  • 본 연구는 한반도에너지개발기구(KEDO) 골재에 대하여 ASTM C 295를 적용, 암석기재학적 시험을 통하여 콘크리트를 위한 골재의 적합성을 타진하는데 목적이 있다. 시험에는 천연의 자갈골재와 모래골재를 재료로 하여 편광현미경, 실체현미경, XRD를 주로 사용하였다. KEDO의 천연골재 중 자갈골재의 23%, 모래골재의 5.1%가 화학적으로 불안정한 골재에 해당된다. 따라서 콘크리트용 KEDO 골재의 선정에 있어서 가능한 한 편마암과 같은 고변성 작용을 받은 변성암, 산성화산암, 엽리가 발달된 암석, 그리고 모르타르 봉 시험에서 불량한 골재로 확인된 암석은 피하여야 한다. 본 연구결과, 콘크리트용 KEDO 골재의 적합성 여부를 판단하기 위해서는 추가적인 화학적 시험과 모르타르 봉 시험을 거친 후 종합적으로 그 사용 여부를 결정함이 바람직하다.

광학적 시간영역 반사시스템을 이용한 모르타르 보의 균열 탐사 (Crack Detection in Mortar Beams using Optical Time Domain Reflectometry)

  • 임홍철;이경근
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제4권3호
    • /
    • pp.185-195
    • /
    • 2000
  • Detection of cracks in concrete beams using optical fiber sensors is useful for monitoring of concrete structures. In this study, optical time domain reflectometry (OTDR) is used to detect cracks. Resolution of OTDR is the main contributor to detect cracks in concrete structures. The OTDR used in this study can detect cracks with high precision of 0.5 m. Two mortar beams, reinforced with a 19 mm diameter steel bar, are made with the dimensions of 140 mm (width) ${\times}$ 200 mm (depth) ${\times}$ 2.000 mm (length). Two fibers are embedded inside each beam and two fibers are attached under the beams. The application of measurement system which consists of fiber and FC/PC connecter is studied. For this, theory of optics, resolution, crack moment, and size of specimens are investigated. From the measured data, it is verified that fibers which are attached under the beam can detect the crack in beams effectively. However, fibers embedded inside the beam are unable to detect cracks in beams using the OTDR in this study.

  • PDF