Interfacial Structure of Inconel/$Si_3N_4$ Joint Using Ag-Cu-Ti Brazing Metal (Ag-Cu-Ti Brazing 금속을 이용한 Inconel/$Si_3N_4$ 접합의 계면구조)

  • 정창주;장복기;문종하;강경인
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.12
    • /
    • pp.1421-1425
    • /
    • 1996
  • Sintered Si3N4 and Inconel composed of Ni(58-63%) Cr(21-25%) Al(1-17%) Mn(<1%) fe(balance) were pressurelessly joined by using Ag-Cu-Ti brazing filler metal at 950℃ and 1200℃ under N2 gas atmosphere of 1atm and their interfacial structures were investigated. In case that the reaction temperature was low as 950℃ its interfacial structure was "Inconel metal/Ti-rich phase layer/brazing filler metal layer/Si3N4 " Ti used as reactive metal existed in between inconel steel and brazing metal and moved to the interface of between brazing filler metal nd Si3N4 according as reaction temperature increased up to 1200℃. The interfacial structure of inconel steel-Si3N4 reacted at 1200℃ was ' inconel metal/Ni-rich phase layer containing of Fe. Cr and Si/Cu-rich phase layer containing of Mn and Si/Si3N4 " Cr Mn, Ni and Fe diffused to the interface of between brazing filler metal and Si3N4 and reacted with Si3N4 The most reactive components of ingredients of inconel metal were Cr and Mn. On the other hand Ti added as reactive components to Ag-Cu eutectic segregated into Ni-rich phase layer,.

  • PDF

Synthesis and Compaction of Al-based Nanopowders by Pulsed Discharge Method

  • Rhee, Chang-Kyu;Lee, Geun-Hee;Kim, Whung-Whoe
    • Journal of Powder Materials
    • /
    • v.9 no.6
    • /
    • pp.433-440
    • /
    • 2002
  • Synthesis and compaction of Al-base nano powders by pulsed discharge method were investigated. The aluminum based powders with 50 to 200 nm of diameter were produced by pulsed wire evaporation method. The powders were covered with very thin oxide layer. The perspective process for the compaction and sintering of nanostructured metal-based materials stable in a wide temperature range can be seen in the densification of nano-sized metal powders with uniformly distributed hard ceramic particles. The promising approach lies in utilization of natural uniform mixtures of metal and ceramic phases, e.g. partially oxidized metal powders as fabricated in our synthesis method. Their particles consist of metal grains coated with oxide films. To construct a metal-matrix material from such powder, it is necessary to destroy the hard oxide coatings of particles during the compaction process. This goal was realized in our experiments with intensive magnetic pulsed compaction of aluminum nanopowders passivated in air.

Characteristic Analysis of a SCR System using a Metal Foam in Diesel Engines (디젤 엔진에서 금속 폼을 적용한 SCR 촉매의 특성 분석)

  • Kim, Yongrae;Choi, Kyonam
    • Journal of ILASS-Korea
    • /
    • v.18 no.4
    • /
    • pp.196-201
    • /
    • 2013
  • SCR(Selective Catalytic Reduction) is a major after-treatment solution to reduce NOx emission in recent diesel engines. In this study, a metal foam is applied as an alternative SCR substrate and tested in a commercial diesel engine to compared with a conventional ceramic SCR system. Basic engine test from ND-13 mode shows that a metal foam catalyst has lower NOx conversion efficiency than a ceramic catalyst especially over $350^{\circ}C$. A metal foam catalyst has characteristics of high exhaust gas pressure before a SCR catalyst and high heat transfer rate due to its material and structure. NOx conversion efficiency of a metal foam catalyst shows an increasing tendency along with the increase of exhaust gas temperature by $500^{\circ}C$. The effect of urea injection quantity variation is also remarkable only at high exhaust gas temperature.

Variations of Form Accuracy in the Process of Metal Cast Prototyping using Rapid prototype, Vacuum casting and Ceramic Mold (쾌속조형과 진공주형 및 세라믹 몰드를 이용한 금속 주조 시제품 제작 공정에서의 형상정밀도 변화)

  • Kim, Gi-Dae
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.24 no.6
    • /
    • pp.131-137
    • /
    • 2007
  • In metal casting process, it is very difficult to predict the form accuracy of cast part and reduce repeatability error. In this study, the variations of form accuracy were measured in the process of metal cast prototyping, where RP part is manufactured from CAD model in the first, and then, wax part is cast in the vacuum environment using the RP part as master model, and finally metal prototype is cast using ceramic mold and the wax part as pattern. To investigate the variations of form accuracy, the averages and standard deviations of error distribution of the parts measured by 3D scanner were compared. It was observed that the biggest shrinkage is generated during the extraction of wax part in the second step and the biggest deterioration of form accuracy is generated during the metal part casting in the last step.

A study on the Fracture Mechanical Strength Evaluation in Joint Interface of Ceramics and Metal (세라믹스/금속 접합계면에서의 파괴력학적 강도평가에 관한 연구)

  • 최병기
    • Journal of the Korean Society of Safety
    • /
    • v.11 no.3
    • /
    • pp.20-24
    • /
    • 1996
  • Indentation fracture method and 4-point bending test are carried out to measure the residual stresses and the bending strength, and to investigate the mechanism of fracture mechanics in the bonded interface of ceramic and metal. The results obtained are as follows ; 1) The fracture patterns of bonded materials shows that the delamlnatlon fracture of Interfaces is stablely developed from the interfaces of ceramic/active metallic bonded materials at the specimen center, and the fracture is unstablely generated through a refraction on the middle ceramic. 2) Distribution of residual stresses is quantitatively investigated on the ceramic side of bonded materials. 3) It Is found that the residual stresses of interface vertical direction are concentrated on the bonded interface at the ceramic side.

  • PDF

Metal/$Al_2O_3-SiO_2$ System Interface Investigations

  • Korobova, N.;Soh, Deawha
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2004.05a
    • /
    • pp.70-73
    • /
    • 2004
  • The packaging of the integrated circuits requires knowledge of ceramics and metals to accommodate the fabrication of modules that are used to construct subsystems and entire systems from extremely small components. Composite ceramics (Al$_2$O$_3$-SiO$_2$) were tested for substrates. A stress analysis was conducted for a linear work-hardening metal cylinder embedded in an infinite ceramic matrix. The bond between the metal and ceramic was established at high temperature and stresses developed during cooling to room temperature. The calculations showed that the stresses depend on the mismatch in thermal expansion, the elastic properties, and the yield strength and work hardening rate of the metal. Experimental measurements of the surface stresses have also been made on a Cu/Al$_2$O$_3$-SiO$_2$ceramic system, using an indentation technique. A comparison revealed that the calculated stresses were appreciably larger than the measured surface stresses, indicating an important difference between the bulk and surface residual stresses. However, it was also shown that porosity in the metal could plastically expand and permit substantial dilatational relaxation of the residual stresses. Conversely it was noted that pore clusters were capable of initiating ductile rupture, by means of a plastic instability, in the presence of appreciable tri-axiality. The role of ceramics for packaging of microelectronics will continue to be extremely challenging.

  • PDF

Variation of Dielectric Constant with Various Particle Size and Packing Density on Inkjet Printed Hybrid $BaTiO_3$ Films

  • Lim, Jong-Woo;Kim, Ji-Hoon;Yoon, Young-Joon;Yoon, Ho-Gyu;Kim, Jong-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2010.06a
    • /
    • pp.271-271
    • /
    • 2010
  • $BaTiO_3$(BT) has high permittivity so that has been applied to dielectric and insulator materials in 3D system-level package integration. In order to achieve excellent performance of device, the BT layer should be highly dense. In this study, BT thick films were prepared by the inkjet printing method. And these films were cured at $280^{\circ}C$ after infiltration of polymer resin. As a result, we have successfully fabricated not only the inkjet-printed hybrid BT film but also metal-insulator-metal(MIM) capacitor without sintering process. Changes in the dielectric constant of BT hybrid film with particle size and packing density were investigated. The dielectric constant was increased with increasing packing density and particle size. Further, the BT hybrid film using two different size particles had even higher packing density and dielectric constant.

  • PDF

The comparative study on the marginal fit of a metal-ceramic alloy, IPS - Empress and a zirconia($ZrO_2$) ceramic used for fabrication of dental restoration (치과보철물 제작에 사용되는 금속-도재용 합금, IPS - Empress, 지르코니아($ZrO_2$) 세라믹의 변연적합도에 관한 비교평가)

  • Kim, Chul-Soo
    • Journal of Technologic Dentistry
    • /
    • v.33 no.1
    • /
    • pp.7-14
    • /
    • 2011
  • Purpose: As the demand and importance of aesthetic aspects in dental treatment become higher, much attention is paid to materials used for dental prostheses. Thus, the marginal fidelity of most-commonly used alloy, IPS - Empress and ZrO2 ceramic is compared. Methods: The alloy core made by casting, IPS - Empress core made by pressing and ZrO2 ceramic core made by CAD/CAM are used to make 10 samples respectively. For each core, three points were measures and the optical microscope (Axio Imager.Alm,Zeiss co., Oberkochen, Germany) was used to observe the cores with a magnification of 100. Results: As for alloy, IPS - Empress and ZrO2 ceramic, the average and deviation of their marginal distance are $29.91\;{\pm}11.93{\mu}m$ for alloy, $33.45\;{\pm}8.61{\mu}m$ for IPS - Empress, and $31.55\;{\pm}9.85{\mu}m$ for ZrO2. The one-way ANOVA test was conducted to compare them. However, there was no statistically significant difference among them. Conclusion: The study on marginal fidelity of alloy, IPS - Empress, and ZrO2 ceramic shows they have no marginal fidelity problem clinically. Therefore, if a system is selected based on the patient's condition or treatment method, there will be no problem.