Proceedings of the Korean Institute of Building Construction Conference
/
2002.11a
/
pp.77-86
/
2002
In this study we intended to investigate properties of cement mortar with recycled PET fiber, PE fiber, and PP fiber such as slump flow, compressive strength, tensile strength, and flexural strength. As results of experiment, several properties of specimen with recycled PET fiber were little low comparing those of specimen with PE fiber and PP fiber. But if we see from point of economy and recycle of industrial wastes, it has enough reason to be used. Compressive strength of specimen with recycled PET fiber at 56 days was about 10% higher, but tensile strength and flexural strength were lower than that of no-fiber.
Kim, Sang-Woo;Hong, Sang-Hee;Kim, Gi-Cheol;Ryu, Hyun-Ki;Han, Cheon-Goo
Proceedings of the Korea Concrete Institute Conference
/
2000.04a
/
pp.169-172
/
2000
In this paper applicabilities of coolant wastes are an admixture, which are produced from cooling line of the cars and industrial engines, to concrete under cold climate are investigated. According to the test results, as the contents f coolant wastes increase, setting time of cement mortar is shown to be delayed. However, when coolants wastes are overadded, it appears to be fast. In case of compressive strength, It tends to decline as the contents of coolant waste increase. Under low curing temperature, compressive strength of cement mortar containing coolant wasted with the increase of the contents of coolants wastes.
Proceedings of the Korea Concrete Institute Conference
/
1997.10a
/
pp.190-195
/
1997
The purpose of this study was to use daily waste incinerated ash, which was reclaimed worthlessly, as substitutes of fine aggregates in concrete. Various kinds of admixture was utilized to strengthen the cement mortar mixed with waste incinerated ash, and altered the curing condition to diminish the rate of expansion. By the results of this experiment, it was possible to produce the lightweight concrete, charactered with the gravity below 1.5 and over 160kg/$\textrm{cm}^2$ compressive strength by replacing all fine aggregates with waste incinerated ash. It was also observed that the low temperature curing condition, lessoned gas exhausts, was effective to increase the strength of cement mortar.
Direct shear tests were carried out on the rock joints and artificial discontinuities to investigate the influence of joint roughness on the shear strength and deformation behaviour. Single direct shear testing apparatus used in experiment was designed and manufactured. Its capacity is 200 tons of shear load, 20 tons of normal load and 50$\textrm{cm}^2$ of maximum shear area. Test samples were cement mortar with artificial discontinuity and sandstone with natural joint. Peak shear strength was increased as joint roughness or normal stress was increased, especially, linearly increased with roughness angle in cement mortar. If joint roughness angle was constant at low normal stress, shear strength was not affected by width and height of joint roughness in cement mortar. Peak shear strengths obtained from tests were larger than the values calculated by Barton's equation, and shear stiffness was increased with joint roughness coefficient.
Journal of the Korea Institute of Building Construction
/
v.2
no.4
/
pp.113-122
/
2002
In this study we intended to investigate properties of cement mortar with recycled PET fiber, PE fiber. and PP fiber such as slump flow, compressive strength, tensile strength, and flexural strength. At results of experiment. several properties of specimen with recycled PET fiber were little low comparing those of specimen with PE fiber and PP fiber. But if we see from point of economy and recycle of industrial wastes, it has enough reason to be used. Compressive strength of specimen with recycled PET fiber at 55 days was about 10% higher. but tensile strength and flexural strength were lower than that of no-fiber.
The present study aims to understand the behaviour of low-strength masonry prisms constructed with locally-produced low-strength hollow concrete blocks. Compression tests were conducted on masonry prisms constructed with three different mortar grades of cement-sand ratios of 1:3, 1:4.5 and 1:6 representing strong, moderately strong and weak mortar. Stress-strain curves were generated from the test results for the masonry prisms. The hollow concrete masonry units employed in this study are some of the weakest as compared to other masonry units employed by other researchers. The compressive strengths for masonry prisms with mortar grades 1:3, 1:4.5 and 1:6 are 2.21 MPa, 2.19 MPa and 2.25 MPa respectively. The results indicate that the masonry compressive strength of such low-strength hollow concrete block masonry prisms is not influenced by the mortar strength. Simple relationships to estimate the modulus of elasticity and compressive strength of masonry prisms is also proposed.
Proceedings of the Korean Institute of Building Construction Conference
/
2011.11a
/
pp.245-246
/
2011
In recent research in this emerging and latent heat storage material features an innovative temperature - controlled Phase Change Materials to evaluate the superior thermal performance would like to calculate the thermal conductivity. Specified in KS F 4040 test specimen dimensions were equivalent in specifications, test methods according to KS L 9016 was an experiment in progress. As a result, the thermal conductivity of plain cement mortar mixed with more PCM came out with low thermal conductivity of mortar, thermal performance was excellent.
Lee, Kang Jin;Kim, Jin Hyoung;Park, Ki Bong;Lee, Han Seung
KIEAE Journal
/
v.12
no.3
/
pp.115-122
/
2012
Based on previous research and existing literature, this study examines the development of admixture, which increases the early concrete strength (1 and 3 day) by mixing blast furnace slag cement and concrete stimulant. The research on early strength development of concrete is necessary in dealing with the drawbacks of slow early strength concrete on site and to shorten the construction time. The study confirmed that when a high alkaline mortar mixture is mixed with blast furnace slag, the early strength of admixture exceeds that of ordinary portland cement (OPC). The use of calcium chloride ($CaCl_2$) promotes hydration of cement at low temperature and show similar strength as the blast furnace slag admixture. Although calcium chloride seems economically advantageous, it causes steel corrosion and its use in concrete should be further studied in-depth.
Proceedings of the Korean Institute of Building Construction Conference
/
2023.05a
/
pp.309-310
/
2023
Slag and ash generally have a higher powder degree than portland cement, so workability may deteriorate under the same unit quantity condition, and strength and durability decrease when the unit quantity is increased. At this time, if an aggregate having a low water absorption and an appropriate particle size is used to recover the loss of strength, it can contribute to reducing the unit quantity of the binder. Therefore, for the purpose of improving the workability and strength of non-sintered cement mortar using slag and ash, ferro nikel slag whose particle size was adjusted was used as an aggregate and its applicability was identified. In this experimental condition, it was confirmed that non-sintered cement mortar tends to improve workability and secure strength when ferro nikel slag having various particle size distributions is used as an aggregate. This can be analyzed as the effect of ferro nikel slag material properties including glassy properties and mixing conditions with a wide particle size distribution.
Journal of the Korean Recycled Construction Resources Institute
/
v.10
no.2
/
pp.176-183
/
2022
High-purity waste CNTs were mixed into cement mortar to manufacture heat-generating concrete that can use low voltage power, and carbon fiber and waste cathode materials were also used improve the conductivity of the mortar. The waste CNTs were analyzed to have a high concentration of multi-walled CNTs, and substituted liquid type waste CNTs were used during mortar mixing in order to increase dispersibility. The temperature change of the mortar with CNT was evaluated when using electric power below DC 24 V in order to utilize a small self-generation facility such as small solar power module when the mortar heats up and to minimize electromagnetic waves. When liquid-type waste CNTs were applied and a voltage of DC 24 V was introduced, it rose to 60 ℃ in a 200 × 100 × 50 mm mortar block specimen. The field applicability of self heating mortar with waste CNT was sufficient and also the amount of change in heat energy in mortar with liquid type waste CNT, carbon fiber and waste cathode materials is more effective compared to it of other variables.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.