• Title/Summary/Keyword: laminate film

Search Result 38, Processing Time 0.025 seconds

Development of Edible Laminate-Composite Films Using Defatted Mustard Meal and Whey Protein Isolate (탈지겨자씨와 유청단백질을 재료로 사용한 가식성 적층필름의 개발)

  • Kim, Dayeon;Park, Ji Won;Noh, Bong-Soo;Min, Sea Cheol
    • Korean Journal of Food Science and Technology
    • /
    • v.44 no.6
    • /
    • pp.711-715
    • /
    • 2012
  • A laminate-composite film was developed using industry co-products of defatted mustard meal (DMM) and whey protein isolate (WPI). An individually prepared DMM-based film (DMM film) and a WPI-based film (WPI film) were thermally laminated at $130^{\circ}C$ at a rate of 30 cm/min. Microscopic images exhibited that the DMM film and the WPI film were continuously attached in the laminate without void spaces. The tensile strength, elongation at break, and water vapor permeability for the laminate were 0.7MPa, 4.0%, and $6.9g{\cdot}mm/kPa/h/m^2$, respectively. Stretchability and heat seal strength of the laminate were higher than those of the un-laminated DMM film. The film layers of the laminate were physically overlapped, not forming new biopolymer units induced by molecular interactions. The opportunity for DMM films to be used as food packaging materials for wrapping and sealing could be increased by thermal lamination with WPI films, which improves the stretchability and heat sealability of DMM films.

Low Temperature Cure Film Adhesive

  • Liang, Bin;Zhao, Shenglong
    • Journal of Adhesion and Interface
    • /
    • v.5 no.2
    • /
    • pp.1-7
    • /
    • 2004
  • A novel carboxyl terminated butadiene-acrylonitrile (CTBN) modified, low temperature cure epoxy film adhesive was developed in this paper. It can be cured at as low as $75^{\circ}C$ for 4 hours with a pressure of 0.1MPa. After post cure at $120^{\circ}C$ for 2 hours, the bonding strengths of Phosphoric Acid Anodizing(PAA) surface treated aluminum adherend were similar to those of structural film adhesives curing at $120^{\circ}C$. It is suitable to bond both metal/composite laminate-to-laminate and laminate to honeycomb structure.

  • PDF

Effect of Surface Film on Void Behavior in Composite Integrated Structure (표면접착필름이 복합재 일체형 구조물에서의 기공 거동에 미치는 영향)

  • Park, Dong-Cheol;Kim, Yun-Hae
    • Composites Research
    • /
    • v.33 no.3
    • /
    • pp.147-152
    • /
    • 2020
  • In this study, void behavior of composite laminate by local internal pressure gradient due to structural geometry and surface film application condition was experimentally evaluated through fabrication of spar/skin integrated structure specimens. Viscosity comparison and thermal analysis for both carbon fiber prepreg and surface film were conducted and cure characteristic and rate difference were analyzed. 2 types of spar/skin integrated structural specimens were prepared based on different application condition of surface film. Subsequently, those specimens were evaluated through visual surface inspection, non-destructive and destructive inspection. In a specimen #1 with full application of surface film, low pressurized area of composite laminate created by pressure gradient of structural geometry had voids. It exhibited that voids could not be evacuated and were locked in cured laminate by the influence of pre-cured surface film with relatively faster cure rate. In a specimen #2 without surface film, it revealed that all internal voids disappeared in the cured laminate. Therefore, it is verified that surface film acts as barrier film preventing void movement and evacuation during autoclave cure.

Thin Film Encapsulation with Organic-Inorganic Nano Laminate using Molecular Layer Deposition and Atomic Layer Deposition

  • Yun, Gwan-Hyeok;Jo, Bo-Ram;Bang, Ji-Hong;Seong, Myeong-Mo
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.270-270
    • /
    • 2016
  • We fabricated an organic-inorganic nano laminated encapsulation layer using molecular layer deposition (MLD) combined with atomic layer deposition (ALD). The $Al_2O_3$ inorganic layers as an effective single encapsulation layer were deposited at 80 degree C using ALD with alternating surface-saturation reactions of TMA and $H_2O$. A self-assembled organic layers (SAOLs) were fabricated at the same temperature using MLD. MLD and ALD deposition process were performed in the same reaction chamber. The prepared SAOL-$Al_2O_3$ organic-inorganic nano laminate films exhibited good mechanical stability and excellent encapsulation property. The measurement of water vapor transmission rate (WVTR) was performed with Ca test. We controlled thickness-ratio of organic and inorganic layer, and specific ratio showed a lowest WVTR value. Also this encapsulation layer contained very few pin-holes or defects which were linked in whole area by defect test. To apply into real OLEDs panels, we controlled a film stress from tensile to compressive and flexibility defined as an elastic modulus with organic-inorganic ratio. It has shown that OLEDs panel encapsulated with nano laminate layer exhibits better properties than single layer encapsulated in acceleration conditions. These results indicate that the organic-inorganic nano laminate thin films have high potential for flexible display applications.

  • PDF

Effect of Poly(vinyl alcohol) Adhesives on the Dimensional Stability of LCD Polarizer (폴리(비닐 알코올) 접착제가 LCD 편광판의 치수안정성에 미치는 영향)

  • Suh, Ju-Hee;Shin, Jung-Woo;Kim, Hyo-Kap;Kim, Han-Sung;Kim, Yong-Won;Kang, Ho-Jong
    • Polymer(Korea)
    • /
    • v.34 no.6
    • /
    • pp.560-564
    • /
    • 2010
  • Dimensional stability of LCD polarization film consisted of triacetyl cellulose (TAC) and poly(vinyl alcohol) (PVA) film has been studied and especially, the effect of PVA adhesive on the dimensional stability has been considered as function of deacetylation and molecular weight of PVA adhesive. The maximum adhesion strength between TAC and PVA film was obtained in the laminate using PVA adhesive with 70% of OH content and the effect of molecular weight on the adhesion strength was only pronounced in the laminate using PVA adhesive with OH content above 70%. It was found that the optimum dimensional stability of TAC/PVA/TAC laminate (polarizing film) was obtained when applied PVA adhesive has low molecular weight and it was more dependent upon the OH content than the adhesion strength between TAC and PVA films.

Improvement of wear resistance of laminate flooring by liquid overlay decorative laminate system (Liquid overlay를 이용한 강화마루의 내마모도 향상)

  • Kim, Su-Min;Lee, Jeong-Hun;Yoon, Dong-Won
    • Journal of the Korea Furniture Society
    • /
    • v.21 no.2
    • /
    • pp.126-132
    • /
    • 2010
  • High wear resistances are obtained with an additional coating of the surface of the decor film in the same operation of impregnating with low viscosity melamine resin by liquid overlay system. The cellulosic fibers have a good adhesion to the corundum particles and keep them sufficiently homogeneous in the blend with the resin. The amount of these fibers in nearly as big as it is in a common overlay in relation to the resin. Therefore these fibers keep the resin inside during the press process and consequently very the surface of the decor print of the film. That means that the corundum particles are equally dissipated throughout the entire layer over the decor. The change of the color of the print is nearly not visible as the particles are almost equally dissipated. Looking to the flooring purposes of liquid overlay one can see that by the lesser exposure of the corundum particles on the very surface, there is no longer an abrasive surface but a feeling like a normal melamine surface.

  • PDF

Comparison of Energy Harvesting Characteristics in Trapezoidal Piezoelectric Cantilever Generator with PZT Laminate Film by Longitudinal (3-3) Mode and Transverse (3-1) Mode (PZT 라미네이트 Trapezoidal Piezoelectric Cantilever Generator의 모드(3-1, 3-3)별 에너지 하베스팅 특성 비교)

  • Lee, Min-seon;Kim, Chang-il;Yun, Ji-sun;Park, Woon-ik;Hong, Youn-woo;Paik, Jong-hoo;Cho, Jeong-ho;Park, Yong-ho;Jeong, Young-hun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.12
    • /
    • pp.768-775
    • /
    • 2017
  • Energy harvesting characteristics of trapezoidal piezoelectric cantilever generator, which has a lead zirconate titanate (PZT) laminate film, were compared by longitudinal (3-3) and transverse (3-1) modes. The PZT laminate film, fabricated by a conventional tape casting process, was cofired with Ag electrode at $850^{\circ}C$ for 2 h. A multi-layered Ag electrode by a planar pattern and an interdigitated pattern was applied to the PZT laminate to implement the 3-3 and 3-1 modes, respectively. The energy harvesting performance of the 3-3 mode trapezoidal piezoelectric cantilever generator was better than that of the 3-1 mode. An extremely high output power density of $26.7mW/cm^3$ for the 3-3 mode was obtained at a resonant frequency of 145 Hz under a load resistance of $50{\Omega}$ and acceleration of 1.3 G, which is ~3-times higher than that for the 3-1 mode. Therefore, the 3-3 mode is considered significantly efficient for application to high-performance piezoelectric cantilever generator.

Viscoelastic Analysis of Osmotic Blistering Behavior of Coating Film

  • Lee, Sang Soon;Park, Myung Kyu
    • Corrosion Science and Technology
    • /
    • v.8 no.1
    • /
    • pp.11-14
    • /
    • 2009
  • The osmotic blistering behavior of polymeric coating film which is in contact with an aqueous environment has been investigated. In this study, the coating film has been assumed to be linearly viscoelastic. Interfacial stresses induced in a laminate model consisting of the viscoelastic film and the elastic substrate as the film absorbs moisture from the ambient environment have been investigated using the time-domain boundary element method. The overall stress intensity factor for interfacial cracks subjected to a uniform osmotic pressure has been computed using the tractions at the crack tip node. The magnitude of stress intensity factors decreases with time due to viscoelastic relaxation, but remains constant at large times.

Carbon Fiber Tow Spreading Technology and Mechanical Properties of Laminate Composites (탄소섬유 펼침 기술 및 이를 적용한 적층 복합재료의 기계적 특성)

  • Park, Sung Min;Kim, Myung Soon;Choi, Yoon Sung;Lee, Eun Soo;Yoo, Ho Wook;Chon, Jin Sung
    • Composites Research
    • /
    • v.28 no.5
    • /
    • pp.249-253
    • /
    • 2015
  • This paper reports a study on a method for achieving lightweight thermoplastic laminate composites referred to as tow spreading technology. Thickness of an unspread 12 K carbon fiber tow is reduced by increasing the tow width from 7 mm to 20 mm. The polypropylene (PP) film was used to stabilize and impregnate the spread tow, covering it into a partially consolidated prepreg: 12 K carbon fiber spread tow/PP. Laminates were fabricated from the spread tow prepreg and control laminate composites were produced from unspread tow prepreg consisting of 12 K carbon fiber and PP. The void content, tensile and flexural properties of the composite laminates were investigated. Consequently, the spread tow laminate composite exhibited lower void content and improved mechanical properties.

Effect of Microstructure of hBN Thin Films on the Nucleation of cBN Phase Deposited by RF UBM Sputtering System (RF UBM Sputtering에 의해 증착된 hBN 박막의 미세구조가 cBN 상의 핵형성에 미치는 영향)

  • Lee Eun-Ok;Park Jong-Keuk;Lim Dae-Soon;Baik Young-Joon
    • Journal of the Korean Vacuum Society
    • /
    • v.13 no.4
    • /
    • pp.150-156
    • /
    • 2004
  • Boron nitride thin films were deposited on Si(100) substrate by RF (Radio-frequency) UBM (Unbalanced Magnetron) sputtering system. The effect of working pressure and substrate bias voltage on microstructure and compressive stress of boron nitride thin films has been investigated. In high working pressure, the alignment of hBN laminates increased with substrate bias voltage, in low working pressure, however, it was high in low substrate bias voltage. Compressive stress evolution and surface morphology of deposited BN films are closely related with the alignment of hBN laminates. The cBN phase without high compressive stress could be nucleated on hBN thin film by controlling the alignment of hBN laminates.