• 제목/요약/키워드: fiber dimension

검색결과 110건 처리시간 0.024초

Toughness and microscopic pore structure analysis of pasture fiber recycled concrete

  • Hailong Wang;Lei Wang;Hong Yang
    • Advances in concrete construction
    • /
    • 제16권3호
    • /
    • pp.141-153
    • /
    • 2023
  • In order to develop and take full advantage of pasture fiber and waste concrete, this article studied how different amounts of pasture fiber influenced the toughness and pore structure of concrete with different replacement rates of recycled fine aggregate. Pasture fiber recycled concrete constitutive equations were established under idealized stiffness and toughness damage rate, based on fracture energy and damage mechanics theories. The relationship between pore structure and toughness was studied utilizing nuclear magnetic resonance and fractal theory. The toughness of text groups (0% (JZ), 10% (ZS10), 20% (ZS20)) first increased and then decreased with increasing amounts of pasture fiber, based on the damage rate of toughness. The toughness of concrete samples with recycled fine aggregate and pasture fiber is negatively correlated to the fractal dimension of small and medium-sized pores with a pore size of 0-500 nm. At a replacement rate of 10% of the recycled fine aggregate, the fractal dimension of the air voids (r: 500-9000 nm, i.e., Lg(r) ∈ [2.7, 3.9]) shows a gradual decrease with the increase of grass fiber dosage, indicating that with such a replacement rate of the recycled fine aggregate, the increase of pasture fiber can reduce the complexity of the pore structure of the air voids (500-9000 nm).

프랙탈 이론에 기초한 섬유보강시멘트 복합체의 균열패턴의 정량분석 (Quantitative Analysis of Crack Patterns of Fiber Reinforced Cement Composites based on Fractal)

  • 원종필;김성애
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.333-338
    • /
    • 2001
  • Fractal geometry is a non-Euclidean geometry which has been developed to quantitative analysis irregular or fractional shapes. Fractal dimension of irregular surface has fractal values ranging from 2 to 3 and of irregular line profile has fractal values ranging from 1 to 2. In this paper, quantitative analysis of crack growth patterns during the fracture processing of fiber-reinforced cement composites based on fractal geometry. The fracture behaviors of fiber reinforced mortar beams subjected to three-point loading in flexure. The beams all had a single notch depth, but varing volume fractions of polypropylene, cellulose fibers. The crack growth behaviors, as observed through the image processing system, and the box counting method was used to determine the fractal dimension, Df. The results showed that the linear correlation exists between fractal dimension and fracture energy of the fiber reinforced cement mortar.

  • PDF

심근경색 유발견에서 마취가 심초음파에 미치는 영향 (Effects of anesthesia on echocardiograms in myocardial infarcted dogs)

  • 윤정희;성재기
    • 대한수의학회지
    • /
    • 제37권3호
    • /
    • pp.669-685
    • /
    • 1997
  • The present study was performed to evaluate the effects of xylazine and tiletamine + zolazepam on echocardiograms before and after experimental myocardial infarctions in clinically normal dogs taken preliminary examinations related to cardiac function. The results are as follows. With xylazine administration, left ventricle end-diastolic dimension, left ventricle end-systolic dimension, left atrium/aorta, ejection time and velocity of circumferential fiber shortening increased and mitral valve CD slope, % delta D decreased(p<0.01). In tiletamine+zolazepam administered group, interventricular septum amplitude(p<0.01), mitral valve DE slope(p<0.05) and ejection time(p<0.01) decreased and left atrium/aorta, ejection time also decreased compared with xylazine group(p<0.01). In 48 hours after experimental myocardial infarction group, anterior aortic wall amplitude decreased compared with control, xylazine, tiletamine + zolazepam group, respectively(p<0.01). Posterior aortic wall amplitude decreased compared with control(p<0.01). Left ventricle end systolic dimension increased compared with control and tiletamine + zolazepam group, respectively(p<0.01). Left ventricular posterior wall end systolic dimension decreased compared with control(p<0.01). Left ventricular posterior wall amplitude decreased compared with control and tiletamine+zolazepam group(p<0.01). Left atrium/aorta decreased compared with xylazine group(p<0.01). % thickening left ventricular posterior wall decreased compared with control(p<0.05). % delta D decreased compared with control and tiletamine+zolazepam group(p<0.01). Ejection time decreased compared with xylazine(p<0.01). Velocity of circumferential fiber shortening increased compared with control and tiletamine + zolazepam group(p<0.01). With xylazine administration 48 hours after experimental myocardial infarction, anterior aortic wall amplitude, posterior aortic wall amplitude decreased compared with control(p<0.01). Left ventricle end-diastolic dimension increased compared with control(p<0.01). Left ventricle end-systolic dimension increased compared with control and tiletamine + zolazepam group, respectively(p<0.01). Left ventricular posterior wall end-systolic dimension and left ventricular posterior wall end-diastolic dimension decreased compared with control(p<0.01). Left atrium/aorta decreased compared with xylazine group(p<0.01). % thickening left ventricular posterior. wall(p<0.05) and % delta D(p<0.01) decreased compared with control. Velocity of circumferential fiber shortening increased compared with tiletamine + zolazepam group(p<0.01). With tiletamine + zolazepam administration 48 hours after experimental myocardial infarction, anterior aortic wall amplitude decreased compared with control, xylazine and tiletamine+zolazepam group, respectively(p<0.01). Posterior aortic wall amplitude decreased compared with control(p<0.01). Left ventricle end-systolic dimension increased compared with control and tiletamine+zolazepam group(p<0.01). Left ventricular posterior wall end-systolic dimension, left ventricular posterior wall end-diastolic dimension and interventricular septum amplitude decreased compared with control(p<0.01). Left atrium/aorta decreased compared with xylazine group(p<0.01). % delta D decreased compared with control and tiletamine + zolazepam group(p<0.01). Ejection time decreased compared with xylazine group and velocity of circumferential fiber shortening increased compared withtiletamine+zolazepam group(p<0.01). Conclusively, echocardiography was proved to be a useful, diagnostic, non-invasive and simple method for establishing the diagnosis of myocardial infarction and evaluating the effects of drug on cardiac function before and after myocardial infarction.

  • PDF

Fiber Morphology and Physical Characteristics of Gigantochloa atter at Three Different Ages and Heights of Culms for Better Utilization

  • Marsoem, Sri Nugroho;Setiaji, Fajar;Kim, Nam-Hum;Sulistyo, Joko;Irawati, Denny;Nugroho, Widyanto Dwi;Pertiwi, Yus Andini Bekti
    • Journal of the Korean Wood Science and Technology
    • /
    • 제43권2호
    • /
    • pp.145-155
    • /
    • 2015
  • Fiber morphology and basic characteristics of Legi bamboos (Gigantochloa atter) growing on Yogyakarta were studied considering their age and height positions in the culms. Culms of 4, 16, and 40 months were harvested, and their total lengths were measured. The length, diameter, and wall thickness of each internode were measured. All the sample culms were divided into three different parts along the height, and their fiber dimension and physical properties were observed. The data obtained were analyzed by analysis of variance. The results showed that the culms had a diameter of 5.8 to 10.8 cm. The lowest internodes always showed the shortest length and the thickest wall. The culms had an average fiber length of 2.41 mm and Runkel ratio of 0.61. Fiber length was affected by the height, while fiber diameter, lumen diameter, and fiber wall thickness were affected significantly by the age of the culms. The culms had high green moisture content (GMC) of 157.89%, and basic density (BD) of $456.67kg.m^{-3}$, a total longitudinal shrinkage of 0.35%, and relatively low R/T shrinkage ratio. The interactions between age and height were affected GMC and BD.

구조물 음향진동 모니터링을 위한 광섬유 센서 설계 (Fiber Optic Sensor Design for the Monitoring of Structural Sound and Vibration)

  • 이종길
    • 한국소음진동공학회:학술대회논문집
    • /
    • 한국소음진동공학회 2007년도 춘계학술대회논문집
    • /
    • pp.81-84
    • /
    • 2007
  • In this paper, fiber optic sound and vibration monitoring sensor which is latticed shape structure based on Sagnac interferometer is fabricated and tested in laboratory conditions. To detect external vibrations surface mounted fibers on the latticed steel wire fence with a dimension of 170cm by 180cm is used. To detect external sound frequency the tightened fiber optic itself wire netting fence with a dimension of 50cm by 50cm is used. Experiments for the detection of the excited vibration and sound signals were performed. A small vibrator induced external vibration signal and it is applied to the latticed structure in the range of 100Hz to several kHz. External sound signal applied to the fiber optic sensor net using non-directional sound speaker. The detected optical signals were compared and analyzed to the detected both accelerometer and microphone signals in the time and frequency domain. Based on the experimental results, distributed fiber optic sensor using Sagnac interferometer detected effectively external vibration and sound signal and had a good performance. This system can be expanded to the monitoring of a significant system and to the structural health monitoring system.

  • PDF

유리섬유 단열재 제조업 근로자의 공기중 유리섬유 폭로 특성 및 평가 방법에 관한 연구 (Characterization and Evaluation of Worker s Exposure to Airborne Glass Fibers in Glass Wool Manufacturing Industry)

  • 신용철;이광용;박천재;이나루;정동인;오세민
    • 한국환경보건학회지
    • /
    • 제22권2호
    • /
    • pp.43-57
    • /
    • 1996
  • To characterize worker's exposure to glass fibers, to find the correlation between airborne total dust concentrations and fiber concentrations and to recommend an appropriate evaluation method for worker's exposure to fibrous dusts in glass wool industry, we carried out this study. Average respirable fiber levels at five factories were 0.013-0.056 f/cc, and fairly below the OSHA PEL, 1 f/cc. A factory showed the lowest airborne fiber level, 0.013 f/cc, which was different significantly from those of other factories of which average fiber concentration was 0.046 f/cc. The cutting and grinding operations of insulation products resulted in higher airborne fiber cocentrations than any other processes(p<0.05). To characterize airborne fiber dimension, fiber length and diamter were determined using phase contrast microscope. The geometric means of airborne fiber lengths were $42-105 \mu m$. One factory had airborne fibers whose length distribution(GM = $105 \mu m$) was different from those of other factories(GM = $42-50 \mu m$). The percentages of respirable fibers less thinner than 3 gm were 38.9-90.9% at four factories, and two factories of them had the higher percentages than others. The findings explain for variation of airborne fiber diameters between factories. On the other hand, between the processes were the difference of fiber-length distributions observed. The cutting and grinding operations showed shorter fiber-length distributions than the fiber forming one. However, fiber-diameter distributions or respirable fiber contents were similar in all processes. The airborne fiber concentrations and the dust concentrations had relatively weak correlation(r=0.25), thus number of fibers couldn't be expected reliably from dust amount. Fiber count is appropriate for assessing accurate exposures and health effects caused by fibrous dusts including glass fibers. Ministry of Labor have established occupational exposure limit to glass fibers as nuisiance dust, but should establish it on the basis of respirable fiber concentration to provide adequate protection for worker's health

  • PDF

NITE-SiC 복합재료의 미세구조 특성에 미치는 섬유배열방향 영향 (Effects of Fiber Arrangement Direction on Microstructure Characteristics of NITE-SiC Composites)

  • 이영주;윤한기;박준수
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2006년 창립20주년기념 정기학술대회 및 국제워크샵
    • /
    • pp.158-161
    • /
    • 2006
  • SiC materials have been extensively studied for high temperature components in advanced energy conversion system and advanced gas turbine. However, the brittle characteristics of SiC such as law fracture toughness and law strain-to fracture impose a severe limitation on the practical applications of SiC materials. SiC/SiC composites can be considered as a promising candidate in various structural materials, because of their good fracture toughness. In this composite system, the direction of SiC fiber will give an effect to the mechanical properties. It is therefore important to control a properdirection of SiC fiber for the fabrication of high performance SiC/SiC composites. In this study, unidirection and two dimension woven structures of SiC/SiC composites were prepared starting from Tyranno SA fiber. SiC matrix was obtained by nano-powder infiltration and transient eutectoid (NITE) process. Effect of microstructure and density on the sintering temperature in NITE-SiC/SiC composites are described and discussed with the fiber direction of unidirection and two dimension woven structures.

  • PDF

Rheo-compocasting 및 Hot Pressing에 의하여 제조한 $Al-Si-Mg/Al_2O_3$ 단섬유강화 복합재료의 조직 및 인장특성 (Microstructures and Tensile Properties of $A_2O_3$ Short Fiber/Al-Si-Mg Alloy Composites Fabricated by Rheo-compocasting and Hot Pressing)

  • 곽현만;이학주
    • 한국주조공학회지
    • /
    • 제13권6호
    • /
    • pp.547-554
    • /
    • 1993
  • Aluminum alloy matrix composites reinforced with various amounts of $Al_2O_3$ short fibers have been produced by rheo-compocasting accompanied by hot pressing. When composites reinforced with fibers are produced by rheo-compocasting, S-L process is the most effective method for homogeneous dispersion of fibers. A sound composites with the improved orientation(3 dimension${\rightarrow}$2 dimension) of the fibers and increased volume fraction of them have been fabricated through the hot pressing of the casted composites. Fibers are broken down when rheo-compocasting, hot pressing, and $T_6$ treating. Among them fibers are broken down most heavily in the hot pressing. And even in the case of the composite reinforced with 30 vol% fibers, which showed the hardest fiber break down, aspect ratio(11.6) is higher than critical aspect ratio(10.7). The fiber strengthening effect in the composites has showed upto 573K. As the test temperature increases to the range of 573K, the effect has been higher. The fracture of composites is controlled by fiber from room temperature to 473K, but the fracture of composites is controlled by interface between fiber and matrix alloy above 473K.