Synthesis of Semiconducting $KTaO_3$ Thin films

  • Bae, Hyung-Jin;Ku, Jayl;Ahn, Tae-Won;Lee, Won-Seok
    • Proceedings of the IEEK Conference
    • /
    • 2005.11a
    • /
    • pp.1265-1268
    • /
    • 2005
  • In this study, the synthesis and semiconducting properties of cation and defect-doped $KTaO_3$ film is reported. $KTaO_3$ is an important material for optoelectronic and tunable microwave applications. It is an incipient ferroelectric with a cubic structure that becomes ferroelectric when doped with Nb. While numerous studies have investigated the thin-film growth of semiconducting perovskites, little is reported about semiconducting $KTaO_3$ thin films. In this work, the films were grown on (001) MgO single crystal substrates using pulsed-laser deposition. Semiconducting behavior is achieved by inducing oxygen vacancies in the $KTaO_3$ lattice via growth in a hydrogen atmosphere. The resistivity of semiconducting $KTaO_3:Ca$ films was as low as 10cm, and n-type semiconducting behavior was indicated. Hall mobility and carrier concentration were $0.27cm^2/Vs$ and $3.21018cm^{-3}$, respectively. Crystallinity and microstructure of the $KTaO_3:Ca$ films were examined using X-ray diffraction and field-emission scanning microscopy.

  • PDF

Fabrication of MFISFET Compatible with CMOS Process Using $SrBi_2Ta_2O_9$(SBT) Materials

  • You, In-Kyu;Lee, Won-Jae;Yang, Il-Suk;Yu, Byoung-Gon;Cho, Kyoung-Ik
    • Transactions on Electrical and Electronic Materials
    • /
    • v.1 no.1
    • /
    • pp.40-44
    • /
    • 2000
  • Metal-ferroelectric-insulator-semoiconductor field effect transistor (MFISFETs) were fabricated using CMOS processes. The Pt/SBT/NO combined layers were etched for forming a conformal gate by using Ti/Cr metal masks and a two step etching method, By the method, we were able to fabricate a small-sized gate with the dimension of $16/4{\mu}textrm{m}$ in the width/length of gate. It has been chosen the non-self aligned source and drain implantation process, We have deposited inter-layer dielectrics(ILD) by low pressure chemical vapor deposition(LPCVD) at $380^{circ}C$ after etching the gate structure and the threshold voltage of p-channel MFISFETs were about 1.0 and -2.1V, respectively. It was also observed that the current difference between the $I_{ON}$(on current) and $I_{OFF}$(off current) that is very important in sensing margin, is more that 100 times in $I_{D}-V_{G}$ hysteresis curve.

  • PDF

Variations of ferroelectric properties with the addition of Yttrium acetate in the $Pb(Zr_{0.65}Ti_{0.35})O_3$ thin films prepared by Sol-Gel processing (Sol-Ge법에 의한 $Pb(Zr_{0.65}Ti_{0.35})O_3$박막의 Yttrium acetate 첨가에 따른 강유전 특성의 변화)

  • 김준한;이규선;이두희;박창엽
    • Electrical & Electronic Materials
    • /
    • v.8 no.3
    • /
    • pp.261-266
    • /
    • 1995
  • In this study, PZT solutions added impurities of Yttrium acetate were prepared by sol-gel processing and were deposited on Pt/ $SiO_{2}$/Si substrates at 5000 rpm for 20 sec. using spin-coating method. Coated films were annealed at 700-750.deg. C for 30 min. using conventional furnace method. Variations of the crystallographic structure and microstructure of PZT thin films with adding impurities were observed using XRD and SEM, and the electrical properties, such as relative permittivity, tan .delta., hysteresis curves and leakage currents, were measured. As the yttrium contents were increased, the remanent polarization and coercive field were decreased. Variations of remanent polarizations and coercive fields of pure and yttrium doped specimens according to polarization reversal cycles were observed using hysteresis measurement. PZT thin films added $Y^{3+}$ ions were completely crystallized at 750.deg. C. $Y^{3+}$ ions, as donor impurity, substituted Pb.sup 2+/ ions located at A-site of perovskite structure. By substitution of $Y^{3+}$ ions, leakage currents became less by decreasing the space charges. Degradation of remanent polarizations of Yttrium added specimens after fatigue was not observed and coercive fields increased more than those of pure PZT thin films.

  • PDF

Effect of DyFeO3 Addition on Crystal Structure and Ferrcelectricity of the BiFeO3-PbTiO3 System

  • Kim, Seong-Seog;Kwon, Jong-Uk;Cheon, Chae Il
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.5 s.276
    • /
    • pp.299-303
    • /
    • 2005
  • The crystal structure and ferroelectricity of the $(1-x)BiFeO_3\;(BF)-xPbTiO_3$ (PT) ceramic system with the addition of $DyFeO_3$ (DF) have been investigated for attaining a high temperature piezoelectric material. This study is focused on the relation between crystal structure and ferroelectric property with the addition of DF over the phase boundary in the (1-x)BF-xPT system. Hysteresis curves of polarization-electric field at room temperature have been measured. The X-ray and neutron diffraction data were analyzed by the rietveld refinement method. The addition of 0.1 mole DF into BF-PT system greatly increases the ferroelectric remanant polarization Pr values, e.g. 17 ${\mu}C/cm^2$ in 0.6BF-yDF-(0.4-y)PT and 31${\mu}C/cm^2$ in 0.5BF-yDF-(0.5.y)PT, respectively. The improved Pr value has been discussed in relation with crystal structure and electrical property.

Preparation and Characterization of Small Sized PZT Powders: A Sol-Gel Modified Approach

  • Choi, Kyu-Man;Lee, Hae-Chun
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.1 no.2
    • /
    • pp.27-32
    • /
    • 2008
  • A current research basically diverted towards an increase in the operational output with the minimization of the materials used, which ultimately scaled down the dimensions of ceramic electronic components. In this direction the nano-technology pave the revolutionary changes in particular the electronic industries. The applications of nano-sized particles or nano-sized materials are hence, playing a significant role for various purposes. The PZT(lead, zirconium, titanium) based ceramics which, are reported to be ferroelectric materials have their important applications in the areas of surface acoustic waves (SAW), filters, infrared detectors, actuators, ferroelectric random access memory, speakers, electronic switches etc. Moreover, these PZT materials possess the large electro mechanical coupling factor, large spontaneous polarization, low dielectric loss and low internal stress etc. Hence, keeping in view the unique properties of PZT piezoelectric ceramics we also tried to synthesize indigenously the small sized PZT ceramic powder in the laboratory by using the modified sol-gel approach. In this paper, propyl alcohol based sol-gel method was used for preparation of PZT piezoelectric ceramic. The powder obtained by this sol-gel process was calcined and sintering to reach a pyrochlore-free crystal phase. The characterization of synthesized material was carried out by the XRD analysis and the surface morphology was determined by high resolution scanning electron microscopy.

  • PDF

Characteristics of the SrBi2Nb2O9 Thin Films Deposited by RF Magnetron Sputtering with Controlling of Bi Contents (RF마그네트론 스퍼터링 법에 의해 증착된 SrBi2Nb2O9 박막의 Bi 량의 조절에 따른 특성분석)

  • Lee, Jong-Han;Choi, Hoon-Sang;Sung, Hyun-Ju;Lim, Geun-Sik;Kwon, Young-Suk;Choi, In-Hoon;Son, Chang-Sik
    • Korean Journal of Materials Research
    • /
    • v.12 no.12
    • /
    • pp.962-966
    • /
    • 2002
  • The $SrBi_2$$Nb_2$$O_{9}$ (SBN) thin films were deposited with $SrNb_2$$O_{6}$ / (SNO) and $Bi_2$$O_3$ targets by co-sputtering method. For the growth of SBN thin films, we adopted the various power ratios of two targets; the power ratios of the SNO target to $Bi_2$$O_3$ target were 100 W : 20 W, 100 W : 25 W, and 100 W : 30 W during sputtering the SBN films. We found that the electrical properties of SBN films were greatly dependent on Bi content in films. The $Bi_2$Pt and $Bi_2$$O_3$ phase as second phases occurred at the films with excess Bi content greater than 2.4, resulting in poor ferroelectric properties. The best growth condition of the SBN films was obtained at the power ratio of 100 W : 25 W for the two targets. At this condition, the crystallinity and electrical properties of the films were improved at even low annealing temperature as $700^{\circ}C$ for 1h in oxygen ambient and the Sr, Bi and Nb component in the SBN films were about 0.9, 2.4, and 1.8 respectively. From the P-E and I-V curves for the specimen, the remnant polarization value ($2P_{r}$) of the SBN films was obtained about 6 $\mu$C/c $m^2$ at 250 kV/cm and the leakage current density of this thin film was $2.45$\times$10^{-7}$ $A/cm^2$ at an applied voltage of 3 V.V.

Preparation and Characterization of Multiferroic $0.7BiFeO_3-0.3BaTiO_3$ Thin Films by Pulsed Laser Deposition (펄스 레이저 증착법으로 제작된 다강체 $0.7BiFeO_3-0.3BaTiO_3$ 박막의 특성 연구)

  • Kim, Kyung-Man;Yang, Pan;Zhu, Jinsong;Joh, Young-Gull;Lee, Hee-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.88-88
    • /
    • 2009
  • $BiFeO_3$(BFO), when forming a solid solution with $BaTiO_3$(BTO), shows structural transformations over the entire compositional range, which not only gives a way to increase structural stability and electrical resistivity but also applies a means to have better ferromagnetic ordering. In this respect, we have prepared and studied 0.7BFO-0.3BTO thin films on $Pt(111)/TiO_2/SiO_2/Si$ substrates by pulsed laser deposition. Various deposition parameters, such as deposition temperature and oxygen pressure, have been optimized to get better quality films. Based on the X-ray diffraction results, thin films were successfully deposited at the temperature of $600^{\circ}C$ and an oxygen partial pressure of 10mTorr. The dielectric, ferroelectric, and magnetic properties have then been characterized. It was found that the films deposited under lower oxygen pressure corresponded to lower leakage current. Magnetism measurement showed an induced ferromagnetism. The microstructures associated with. the magnetic and dielectric properties of this mixed-perovskite solid solutions were observed by transmission electron. microscopy, which revealed the existence of complicated ferroelectric domains, suggested that the weak spontaneous magnetization was closely associated with the decrease in the extent of rhombohedral distortion by a partial substitution of $BaTiO_3$ for $BiFeO_3$.

  • PDF

Effect of the Hydrogen Annealing on the Pb(Zr0.52Ti0.48)O3 Film using (Pb0.72La0.28)Ti0.94O3 Buffers ((Pb0.72La0.28)Ti0.94O3 Buffer를 사용한 Pb(Zr0.52Ti0.48)O3 박막의 수소 후열처리 효과)

  • Lee, Eun-Sun;Li, Dong-Hua;Chung, Hyun-Woo;Lim, Sung-Hoon;Lee, Sang-Yeol
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.4
    • /
    • pp.327-329
    • /
    • 2005
  • Pb(Zr/sub 0.52/Ti/sub 0.48/)O₃(PZT) thin films were deposited by using a pulsed laser deposition method on a Pt/Ti/SiO₂/Si substrate with (Pb/sub 0.72/La/sub 0.28/)Ti/sub 0.93/O₃ (PLT) buffer and on a Pt/Ti/SiO₂/Si substrate without buffer. These films were annealed in H₂-contained ambient for 30 minutes at the substrate temperature of 400。C to evaluate the forming gas annealing effects. The comparative studies on the ferroelectric properties of these two films were carried out, which are shown that ferroelectric properties, such as remanent polarization didn't change in the case of PLT buffered PZT film while remanent polarization value of PZT film degraded from 20.8 C/㎠ to 7.3 C/㎠. The leakage current became higher in both cases, but that of the more-oriented PZT film had the moderate value of the 10/sup -6/ order of A/㎠. This is mainly because the hydrogen atoms which make the degradation of PZT films cannot infiltrate into the more -oriented PZT film as well as the less-oriented PZT film.

Effect Of Variation Of Laser Wavelength OH Properties of ($Pb_{0.72}La_{0.28}$)$Ti_{0.93}O_{3}$Thin Films Fabricated by Pulsed Laser Deposition (펄스레이저 증착법으로 제작된 ($Pb_{0.72}La_{0.28}$)$Ti_{0.93}O_{3}$박막의 레이저 파장 변화에 따른 특성 연구)

  • 한경보;허창회;이상렬
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.170-173
    • /
    • 2001
  • Thin films of phase-pure perovskite (P $b_{0.72}$L $a_{0.28}$) $Ti_{0.93}$ $O_3$(PLT) were deposited in-situ onto Pt/Ti/ $SiO_2$/Si substrates by pulsed laser deposition. We have systematically investigated the variation of grain sizes depending on the process condition. Both in-situ annealing and ex-situ annealing treatments have been compared depending on the annealing time. Two-step process to grow (P $b_{0.72}$L $a_{0.28}$) $Ti_{0.93}$ $O_3$(PLT) films was adopted and verified to be useful to enlarge the grain size of the film and to enhance the leakage current characteristics. The grain sizes of PLT thin films were successfully controlled 260 to 350 nm by changing process parameters. Electrical properties including dielectric constant, ferroelectric characteristics, crystallization and leakage current of PLT thin films were shown to be strongly inf1uenced by grain size. Also PLT thin films on p-type(100) Si substrate will be fabricated by pulsed laser deposition technique using a Nd:YAG laser with different wavelengths of 355, 532 and 1064 nm. Effect of the variation of laser wavelength on dielectric properties will be discussed. Microstructural and electrical properties of the film were investigated by C-V measurement leakage current measurement and SEM.ent and SEM.

  • PDF