• 제목/요약/키워드: elevated temperature wet

Search Result 28, Processing Time 0.021 seconds

An Experimental Study on the Strength of Two Serial Bolt-Fastened Composite Joints under Elevated Temperature and Humid Condition (고온다습 조건($82.2^{\circ}C$)에서 2열 볼트 체결 복합재 조인트의 강도에 관한 실험적 연구)

  • Kim, Hyo-Jin
    • Composites Research
    • /
    • v.22 no.5
    • /
    • pp.30-36
    • /
    • 2009
  • The failure strengths and modes in carbon fiber reinforced polymeric composites, with two serial bolt-fastened composite joints, were investigated to evaluate the typical joint configurations of composite components. The parametric studies were performed experimentally at room temperature dry and elevated temperature wet, $82.2^{\circ}C$ on several different laminate configurations. Based on the experimental data presented, two basic load-displacements curves are observed. Each failure mode has the characteristic curve. It is showed that the bearing failure mode occurs in elevated temperature wet condition. It is analysed that the strength of bearing failure mode is not highly depending on the effective modulus of specimen. The failure strength at elevated temperature wet is decreased by the cause of interfacial deterioration between fiber and matrix with moisture absorption.

Thermal behavior of groundwater-saturated Korean buffer under the elevated temperature conditions: In-situ synchrotron X-ray powder diffraction study for the montmorillonite in Korean bentonite

  • Park, Tae-Jin;Seoung, Donghoon
    • Nuclear Engineering and Technology
    • /
    • v.53 no.5
    • /
    • pp.1511-1518
    • /
    • 2021
  • In most countries, the thermal criteria for the engineered barrier system (EBS) is set to below 100 ℃ due to the possible illitization in the buffer, which will likely be detrimental to the performance and safety of the repository. On the other hand, if the thermal criteria for the EBS increases, the disposal density and the cost-effectiveness for the high-level radioactive wastes will dramatically increase. Thus, fundamentals on the thermal behavior of the buffer under the elevated temperatures is of crucial importance. Yet, the behaviors at the elevated temperatures of the bentonite under groundwater-saturated conditions have not been reported to-date. Here, we have developed an in-situ synchrotron-based method for the thermal behavior study of the buffer under the elevated temperatures (25-250 ℃), investigated dspacings of the montmorillonite in the Korean bentonite (i.e., Ca-type) at dry and KURT (KAERI Underground Research Tunnel) groundwater-saturated conditions (KJ-ii-dry and KJ-ii-wet), and compared the behaviors with that of MX-80 (i.e., Na-type, MX-80-wet). The hydration states analyzed show tri-, bi-, and mono-hydrated at 25, 120, and 250 ℃, respectively for KJ-ii-wet, whereas tri-, mono-, and de-hydrated at 25, 150, and 250 ℃, respectively for MX-80-wet. The Korean bentonite starts losing the interlayered water at lower temperatures; however, holds them better at higher temperatures as compared with MX-80.

Effect of Filled Hole on Strength Behavior of CFRP Composites at Cold Temperature Dry and Elevated Temperature Wet (저온건조($-55^{\circ}C$) 및 고온다습 조건($108.3^{\circ}C$)의 기계적 체결 홀이 탄소섬유강화 복합재의 강도 특성에 미치는 영향 연구)

  • Kim, Hyo-Jin
    • Composites Research
    • /
    • v.22 no.3
    • /
    • pp.82-88
    • /
    • 2009
  • The effect of open and filled holes on the strength behavior of carbon fiber reinforced polymeric (CFRP) composites was investigated. The strength was measured at room temperature dry, cold temperature dry, $-55^{\circ}C$, and elevated temperature wet, $108.3^{\circ}C$ on several different laminate configurations. Based on the experimental data presented, it is shown that the filled hole tensile strength is larger than that of open hole by reducing damage around the hole due to the constraint imposed by the fastener. The tensile strength at cold temperature dry, $-55^{\circ}C$ is increased with the brittleness by the thermal expansion coefficient of fiber and matrix. The compressive strength at elevated temperature wet, $108.3^{\circ}C$ is decreased by the cause of interfacial deterioration between fiber and matrix with moisture absorption.

Effect of Cold Temperature Dry and Elevated Temperature Wet on Mechanical Properties of CFRP Composites (냉각($-55^{\circ}C$) 및 고온다습 조건($82.2^{\circ}C$)이 탄소섬유강화 복합재의 기계적 특성에 미치는 영향 연구)

  • Kim, Hyo-Jin;Lee, Sih-Joong;Han, Sang-Ho;Kim, Sang-Kuk;Park, Seong-Jun
    • Composites Research
    • /
    • v.22 no.3
    • /
    • pp.60-65
    • /
    • 2009
  • The mechanical behavior of carbon fiber reinforced polymeric (CFRP) composites was investigated. Both strength and modulus were measured at room temperature dry, cold temperature dry, $-55^{\circ}C$, and elevated temperature wet, $82.2^{\circ}C$ on seven different laminate configurations consisting of $[0_6]_T$, $[90_{12}]_T$, $[0_{16}]_T$ and $[90_{16}]_T$ unidirectional laminates, $[{\pm}45]_{5S}$ angle-ply laminate, $[0/90_{12}/0]_T$ cross-ply laminate, a 36-ply laminate $[0/45/-45/45/-45/0]_{3S}$. Based on the experimental data presented, it is shown that the strength at cold temperature dry, $-55^{\circ}C$ is increased with the brittleness of fiber or matrix. Moreover, it is shown that both shear strength and modulus at elevated temperature wet, $82.2^{\circ}C$ are decreased by the cause of interfacial deterioration between fiber and matrix with moisture absorption.

Effect of Elevated Steeping Temperature on Properties of Wet-milled Rice Flour (가온 수침처리가 습식제분 쌀가루의 특성에 미치는 영향)

  • Kim, Sang-Sook;Kang, Kyung-A;Choi, So-Yeon;Lee, Young-Tack
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • v.34 no.3
    • /
    • pp.414-419
    • /
    • 2005
  • Newly harvested milled rice and stored milled rice for 2 years were steeped at the elevated temperatures of 40, 50, and 60℃ for 2hr, and physicochemical properties of the wet-milled rice flour were investigated. The lightness of rice flour was slightly higher in the newly harvested milled-rice, while yellowness was higher in the stored milled rice. For both newly harvested and stored milled rice, WAI, WSI, and gel consistency increased as steeping temperature increased. The amylograph pasting properties indicated that increasing steeping temperature increased peak viscosity. The differential scanning calorimetry (DSC) results of the rice flour showed that increasing steeping temperature increased onset and peak temperatures, with reduced gelatinization enthalphy, suggesting partial annealing occured. Particle size of rice flour from newly harvested milled rice was larger than that from stored milled rice.

Comparison of Etching Rate Uniformity of $SiO_2$ Film Using Various Wet Etching Method ($SiO_2$막의 습식식각 방법별 균일도 비교)

  • Ahn, Young-Ki;Kim, Hyun-Jong;Sung, Bo-Ram-Chan;Koo, Kyo-Woog;Cho, Jung-Keun
    • Journal of the Semiconductor & Display Technology
    • /
    • v.5 no.2 s.15
    • /
    • pp.41-46
    • /
    • 2006
  • Wet etching process in recent semiconductor manufacturing is devided into batch and single wafer type. Batch type wet etching process provides more throughput with poor etching uniformity compared to single wafer type process. Single wafer process achieves better etching uniformity by boom-swing injected chemical on rotating wafer. In this study, etching characteristics of $SiO_2$ layer at room and elevated temperature is evaluated and compared. The difference in etching rate and uniformity of each condition is identified, and the temperature profile of injected chemical is theoretically calculated and compared to that of experimental result. Better etching uniformity is observed with single wafer tool with boom-swing injection compared to single wafer process without boom-swing or batch type tool.

  • PDF

Effect of Adhesive Shear Strength of CFRP/Ni-Cr Alloy Under Severe Environmental Condition (가혹 환경이 복합재/Ni-Cr 합금 접착전단강도에 미치는 영향 연구)

  • Cho, Hyeon-Tae;Park, Seong-Min;Kim, Min-Jun;Hoang, Van-Tho;Kim, Hak-Inn;Son, Myung-Sook;Ahn, Jong-Kee;An, Ji-Min;Choi, Jin-Ho;Nam, Young-Woo;Kweon, Jin-Hwe
    • Composites Research
    • /
    • v.33 no.5
    • /
    • pp.275-281
    • /
    • 2020
  • The mechanical property related to lap shear strength of the joint structure between carbon fiber reinforced polymer (CFRP) composite and metal (Ni-Cr Alloy) under varying environmental conditions (temperature and humidity) was studied in order to apply to the aircraft fan blade. Room temperature dry (RTD), elevated temperature wet (ETW), and cold temperature dry (CTD) environmental conditions were chosen for investigation based on the flight conditions of aircraft. Lap shear strength tests were conducted according to ASTM Standard D3528 to evaluate the shear strength. The microstructure characteristic of failure zone was analyzed by SEM images to check the adhesive shear strength with the three environmental conditions. In comparison with shear strength for the RTD condition, the shear strength in the ETW condition was reduced by 72.8% while those for the CTD condition increased by 56.5%. The moisture absorption and high temperature in ETW condition strongly had an affect on mechanical property of adhesive, while cold temperature could enhance the adhesive shear strength due to the higher brittleness.

Development of Structural CFRP according to BMS Certification Standard (BMS 인증기준에 따른 구조용 CFRP 개발)

  • Kang, Byong-Yun;Son, Chang-Suk;Moon, Chang-Kwon;Nam, Ki-Woo;Kim, Yoon-Hae
    • Journal of Ocean Engineering and Technology
    • /
    • v.23 no.2
    • /
    • pp.92-97
    • /
    • 2009
  • In order to export aircraft components or substructures, it is necessary to get a certification from the main company for the components or an airworthiness certification from the FAA. In Korea, those processes are performed by a small number of private companies for aircraft components. However, airworthiness certification has never been done in the company. To export an assembled aircraft, whether small or large, it is obligatory to get a certification for the aircraft being exported. Currently, the Korean government is trying to get BASA agreement in a few years. For a mid-size company, it is easier to get the NADCAP audit process for the supply of aircraft components to the main company. In this paper, the overall process of aircraft certification is discussed and airworthiness certification is treated for export aircraft. Moreover, the NADCAP audit process is described in detail by introducing example parts made of composite material. This detailed process would be very helpful to a small or mid-size company that wants to develop and deliver aircraft components to foreign companies.

Strength of sandwich-to-laminate single-lap bonded joints in elevated temperature and wet condition (샌드위치와 적층판을 접착한 단일겹침 체결부의 고온습도 강도특성 연구)

  • Choi, Bae-Hyun;Kweon, Jin-Hwe;Choi, Jin-Ho;Shin, Sang-Jun;Song, Min-Hwan
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.38 no.11
    • /
    • pp.1115-1122
    • /
    • 2010
  • The main objective of this study is to experimentally investigate the effect of adhesive thickness and environmental conditions on the failure and strength of sandwich-to-laminate bonded joints. Three different adhesive thicknesses (t=0.2, 2 and 4 mm) and two different environmental conditions were considered. Environmental conditions include the RTD(room temperature and dry condition) and ETW(elevated temperature and wet condition). Test results show as the adhesive thickness increases from 0.2 mm to 2 and 4 mm, the joint strength decreases 16 and 30%, respectively. Regarding the effect of environmental conditions, except for one case, the joint strength in the ETW conditions turned out to be 12% higher than those in the RTD conditions. In the joints with adhesive thickness of 0.2 mm, remarkable difference from RTD condition was not found.

Properties of Starch Isolated from Wet-milled Rice after Steeping at Elevated Temperatures for Annealing Effect (Annealing 수침처리에 따른 습식제분 쌀가루의 전분 특성)

  • Lee, Young-Tack;Yoo, Moon-Sik;Lee, Bo-Ram;Park, Jong-Hyun;Chang, Hak-Gil
    • Korean Journal of Food Science and Technology
    • /
    • v.36 no.3
    • /
    • pp.393-397
    • /
    • 2004
  • Rice was steeped at elevated temperatures of $40,\;50,\;or\;60^{\circ}C$ for 2 hr, and physicochemical properties of starches isolated from wet-milled rice flour were investigated. Steeping at elevated temperatures slightly decreased lightness of rice starch, while increased yellowness and redness. Average granule size of rice starch was decreased by steeping treatment. Swelling power and solubility increased as temperature increased. Starch from rice steeped at $40^{\circ}C$ displayed highest swelling power and solubility. Differential scanning calorimetry data of starch obtained from steeped rice at $60^{\circ}C$ showed increased onset and peak temperatures, with narrower gelatinization temperature range, suggesting partial annealing effect. Pasting properties of starch measured by Rapid Visco-Analyzer indicated increased peak viscosity due to rice steeping at $40^{\circ}C$. Peak and breakdown viscosities decreased at $50\;and\;60^{\circ}C$, whereas setback and final viscosities increased.