• Title/Summary/Keyword: crack growth direction

Search Result 144, Processing Time 0.024 seconds

Double Punch Tensile Strength of Cylindrical Mortar with Steel Fibers aligned in Circumferential Direction by Electro-Magnetic Field (전자기장을 이용하여 강섬유를 원주방향으로 배열시킨 원통형 몰탈의 Double Punch 인장강도)

  • Shin, Sun-Chul;Mukharromah, Nur Indah;Moon, Do-Young;Park, Dae-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.1
    • /
    • pp.40-47
    • /
    • 2022
  • In this study, the direction of the steel fibers mixed in the normal mortar and the steel slag mortar was arranged in the circumferential direction by using an electromagnetic field, and a double punch test was performed to evaluate the effect of magnetic filed exposure on tensile strength and on fracture energy. As a result of the experiment, it was confirmed that it is possible to arrange the steel fibers in the circumferential direction. Tensile strength and displacement at failure were also increased according to the arrangement of steel fibers due to exposure to electromagnetic fields. On the other hand, the fracture energy hardly increased. It is considered that there was a limit in resisting crack growth because the area where the arrangement of steel fibers could be adjusted under the electromagnetic field was not deep to center of specimen and the end shape of the steel fibers were straight not hooked. Additional research is needed to address these issues.

Composition-control of Mn-Zn Ferrite Single Crystal Using a Phase Diagram (상평형도를 이용한 Mn-Zn 페라이트 단결정 조성 조절)

  • Je, Hae-June;Kim, In-Tae;Hong, Kug-Sun
    • Analytical Science and Technology
    • /
    • v.5 no.3
    • /
    • pp.327-332
    • /
    • 1992
  • Mn-Zn ferrite single crystals show some fluctuations in composition along the direction of growth by the conventional Bridgman method. The single crystal with a uniform composition was obtained by maintaining the liquid composition content. For example, two batches of powder were prepared : one is consisted of 52 mol% of $Fe_2O_3$, 30 mol% of MnO, and 18 mol% Zn(Composition A), and the other 53 mol% of $Fe_2O_3$, 28.5 mol% of MnO, and 18.5 mol% ZnO(Composition B). Crack-free single crystals with the uniform composition B were grown in a size of 60mm diameter, 300mm long by melting the pellets of composition A and followed by supplying the composition B as tablets. Initial permeabilities were obtained above 600 at 5 MHz in the region of 30~270 mm along the direction of growth.

  • PDF

Deposition of ZrO$_2$ and TiO$_2$ Thin Films Using RF Magnet ron Sputtering Method and Study on Their Structural Characteristics

  • Shin, Y.S.;Jeong, S.H.;Heo, C.H.;Bae, I.S.;Kwak, H.T.;Lee, S.B.;Boo, J.H.
    • Journal of Surface Science and Engineering
    • /
    • v.36 no.1
    • /
    • pp.14-21
    • /
    • 2003
  • Thin films of ZrO$_2$ and TiO$_2$ were deposited on Si(100) substrates using RF magnetron sputtering technique. To study an influence of the sputtering parameters, systematic experiments were carried out in this work. XRD data show that the $ZrO_2$ films were mainly grown in the [111] orientation at the annealing temperature between 800 and $1000^{\circ}C$ while the crystal growth direction was changed to be [012] at above $1000^{\circ}C$. FT-IR spectra show that the oxygen stretching peaks become strong due to $SiO_2$ layer formation between film layers and silicon surface after annealing, and proved that a diffusion caused by either oxygen atoms of $ZrO_2$ layers or air into the interface during annealing. Different crystal growth directions were observed with the various deposition parameters such as annealing temperature, RF power magnitude, and added $O_2$ amounts. The growth rate of $TiO_2$ thin films was increased with RF power magnitude up to 150 watt, and was then decreased due to a sputtering effect. The maximum growth rate observed at 150 watt was 1500 nm/hr. Highly oriented, crack-free, stoichiometric polycrystalline $TiO_2$<110> thin film with Rutile phase was obtained after annealing at $1000^{\circ}C$ for 1 hour.

CO2 Laser Scribing Process of Soda Lime Glass (소다석회유리의 CO2 레이저 스크라이빙 가공)

  • Kang, Seung-Gu;Shin, Joong-Han
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.18 no.5
    • /
    • pp.74-81
    • /
    • 2019
  • This study reports the CW $CO_2$ laser scribing of soda lime glass. In this study, scribing experiments are carried out at different laser powers, scan speeds, and focal positions to investigate the effect of the process parameters on the interaction characteristics between a laser beam and glass. In particular, the interaction characteristics are analyzed and described with the input laser energy per unit length. According to the experimental results, the damage threshold for the glass surface was found to exist between 0.072 and 0.08 J/mm. The input laser energy in this region induced partial melting of the surface and grain-shaped cracks. These cracks tended to increase as the input laser energy increased. At the laser input energy larger than 1 J/mm, a huge crack propagating along the scan direction was produced, and the volume below the scribed area was fully melted. The growth of this crack finally resulted in the complete cutting of the glass at the input laser energy above 8 J/mm. It was found that both the width and depth of the scribed line increased with increasing input laser energy. For the beam focusing at the rear surface, the width of the scribed line varied irregularly. This could be ascribed to the increased asymmetry of the beam intensity distribution when the laser beam was focused at the rear surface. Under this condition, a large burr was only produced on one side of the scribed line.

Case Study on the Firing Pin Fatigue Destruction of the Korean Rifle by Repeated Impact (반복충격에 의한 한국형 소총의 공이 피로파괴 사례 연구)

  • Lee, Ho-Jun;Choi, Si-Young;Shin, Tae-Sung;Seo, Hyun-Su
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.5
    • /
    • pp.648-655
    • /
    • 2020
  • The firing pin of modern automatic rifles detonates the primer of loaded ammunition via a hammer. During this process, the firing pin receives an impact load and repetitive force throughout the life of the rifle. An endurance test of a rifle showed that the firing pin breaks prematurely at 96.26% of life. Accordingly, a case study was conducted through cause analysis and a reconstruction test. Optical microscopy and scanning electron microscopy of the broken surface of the firing pin showed that a crack began in the circumferential direction of the surface, resulting in a fatigue crack to the core after repeated impact. Crack growth and fatigue destruction occurred at the end due to the repetitive impact and was estimated using a notch. For verification, a sample that produced a 0.03mm circumferential notch was broken at 64.25% of life in the reconstruction test. A test of breakage according to the notch types showed that a 0.3mm and a 0.5mm one-side notch were broken at 66.53% and 50.76%, respectively, and a 0.03mm six-point notch was broken at 85.65%. The endurance life of a sample firing pin with a rough surface and tool mark was examined, but an approximately 381 ㎛ internal crack formed. Through this study, failure for each notch type was considered. These results show that quality control of the notch and surface roughness is essential for ensuring the reliability of a component subjected to repeated impact.

Microproperties and Fracture Behavior of Galvannealed Coating Layer of Automobiles (자동차용 합금화 용융아연도금강판의 도금층 미소물성 및 파괴 거동)

  • Park, Chun-Dal;Ko, Dae-Cheol;Kim, Byung-Min
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.24 no.3 s.192
    • /
    • pp.91-99
    • /
    • 2007
  • Fractures of galvannealed coating layer during actual press forming in automotive applications were observed by scanning electron microscopy in order to understand fracture mechanism. Fracture behaviors of galvannealed coating layer in extra deep drawing quality steels and high strength steels have been studied by performing the tests describing the representative plastic deformation in sheet metal forming such as uni-axial tensile test, compression test, bi-axial test and plane strain test. Growth and direction of cracks were deeply related to the plastic deformation modes and history. The material properties of galvannealed coating layer were investigated by nano-indentation test equipped with Berkovich diamond indentor for the specimens. Hardness and elastic modulus of the coating layer were higher than bared steels and that was the reason for crack of coating layer. Flat friction test and drawbead friction test were performed to observe the effect of the surface morphology on the frictional characteristics. The micro-plasto hydrodynamic lubrication were appeared and played an important role in reducing the coefficient of friction.

Assessment of Notch Effect on Fracture Plane Control (노치 발파공에 의한 파단면 제어 효과에 관한 연구)

  • Kim, Kwang-Yeom;Kim, Dong-Gyou;Jeong, Dong-Ho;Cho, Sang-Ho
    • Explosives and Blasting
    • /
    • v.26 no.1
    • /
    • pp.57-66
    • /
    • 2008
  • It has been proven that the pre-cracking notches in a blasting hole are applicable to control crack growth along specific direction. This study compared the roughnesses of the fracture plane resulting from test blasts using a regular charge hole and notched charge hole to investigate the effect of the notches of charge hole on the formation of fracture plane. A notch bit system was used to drill the notched hole in the rock specimens. The surfaces of the fracture planes were reconstructed as Digital Elevation Model (DEM) using digital photogrammetric method and the roughnesses of the surfaces were estimated with Surface Roughness Profile Index (SRp).

Fatigue Strength Improvement of Pressure Vessel Steel by Lasler Beam Radiation (레이저빔 조사에 의한 압력용기용 강의 피로강도 향상방법 개발)

  • 권재도;진영준;김상태;최선호
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.18 no.2
    • /
    • pp.519-528
    • /
    • 1994
  • Degradation problem due to long term service in machine or structure is now one of important problems in whole industrial field. In this study, pressure vessel steel, Cr-Mo steel, which was used more than 60,000 hours, was surface-modified by laser beam radiation for the improvement of fatigue strength. To find out optimum radiation condition, hardness, residual stress measurement and fatigue tests were carried out with the specimen of different radiation conditions. Experimental results show that micro-hardness values on the surface of the radiated specimens were approximately 2.2 times higher than those of un-radiated ones. In the depth direction of the specimen, hardness on the surface showed maximum value and was decreased at the inside the specimen. Different hardness values are due to the energy density Q which was absorbed by the specimen. Fatigue tests show that fatigue life was improved by the compressive residual stress after laser beam radiation. However, some specimens with differednt conditions show the shorter fatigue life. It means that laser beam radiation with optimum parameter can improve thae fatigue strength.

Remaining Life Assessment of High Temperature Steam Piping (고온 증기 파이프의 잔여수명 평가)

  • 윤기봉
    • Journal of Welding and Joining
    • /
    • v.13 no.2
    • /
    • pp.12-24
    • /
    • 1995
  • Recently, more researches have been actively performed for the assessment of material degradation and residual-life of elevated temperature plant components, as some of domestic fossil power plants become older than 30 years. In this paper, results of on_site residual life assessment are reported for main steam pipes of Youngwol power station #2 which have operated since 1965. For critical weld locations such as butt welds branch welds, Y_sections and a T-section, replication technique and hardness measurement technique were employed for life_assessment. When cracks were detected by conventional NDT tests, crack growth life was calculated using a computer code. On the other hand, for matrix of pipes, residual life was quantitatively estimated by an analytic method and material degradation was estimated qualitatively using diameter measurement data and grain-boundary etching method. Also, direction in further improvement of on-site life assessment techniques are proposed.

  • PDF

$TiO_2$ Thin Film Patterning on Modified Silicon Surfaces by MOCVD and Microcontact Printing Method

  • 강병창;이종현;정덕영;이순보;부진효
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2000.02a
    • /
    • pp.77-77
    • /
    • 2000
  • Titanium oxide (TiO2) thin films have valuable properties such as a high refractive index, excellent transmittance in the visible and near-IR frequency, and high chemical stability. Therefore it is extensively used in anti-reflection coating, sensor, and photocatalysis as electrical and optical applications. Specially, TiO2 have a high dielectric constant of 180 along the c axis and 90 along the a axis, so it is highlighted in fabricating dielectric capacitors in micro electronic devices. A variety of methods have been used to produce patterned self-assembled monolayers (SAMs), including microcontact printing ($\mu$CP), UV-photolithotgraphy, e-beam lithography, scanned-probe based micro-machining, and atom-lithography. Above all, thin film fabrication on $\mu$CP modified surface is a potentially low-cost, high-throughput method, because it does not require expensive photolithographic equipment, and it produce micrometer scale patterns in thin film materials. The patterned SAMs were used as thin resists, to transfer patterns onto thin films either by chemical etching or by selective deposition. In this study, we deposited TiO2 thin films on Si (1000 substrateds using titanium (IV) isopropoxide ([Ti(O(C3H7)4)] ; TIP as a single molecular precursor at deposition temperature in the range of 300-$700^{\circ}C$ without any carrier and bubbler gas. Crack-free, highly oriented TiO2 polycrystalline thin films with anatase phase and stoichimetric ratio of Ti and O were successfully deposited on Si(100) at temperature as low as 50$0^{\circ}C$. XRD and TED data showed that below 50$0^{\circ}C$, the TiO2 thin films were dominantly grown on Si(100) surfaces in the [211] direction, whereas with increasing the deposition temperature to $700^{\circ}C$, the main films growth direction was changed to be [200]. Two distinct growth behaviors were observed from the Arhenius plots. In addition to deposition of THe TiO2 thin films on Si(100) substrates, patterning of TiO2 thin films was also performed at grown temperature in the range of 300-50$0^{\circ}C$ by MOCVD onto the Si(100) substrates of which surface was modified by organic thin film template. The organic thin film of SAm is obtained by the $\mu$CP method. Alpha-step profile and optical microscope images showed that the boundaries between SAMs areas and selectively deposited TiO2 thin film areas are very definite and sharp. Capacitance - Voltage measurements made on TiO2 films gave a dielectric constant of 29, suggesting a possibility of electronic material applications.

  • PDF