Contribution of the Interface Energies to the Growth Process of Cemented Carbides WC-Co

  • Lay, Sabine;Missiaen, Jean-Michel;Allibert, Colette H
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.332-333
    • /
    • 2006
  • The driving forces and the probable processes of WC-Co grain growth are reanalysed from recent data of interface energy and microstructure. Grain growth is driven by the disappearing of the high energy WC/WC and WC/Co interfaces with habit planes different from {0001}, ${10\bar{1}0}$ and ${11\bar{2}0}$ facets and by the area decrease of the WC/WC and WC/Co interfaces with {0001} and ${10\bar{1}0}$ habit planes. Grain growth mainly results of dissolution-precipitation. Abnormal grains are likely formed by defects assisted nucleation.

  • PDF

Hybrid Composite Nano-sized WC-Co Cemented Carbide

  • Park, Sun-Yong;Lee, Wan-Jae
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.640-641
    • /
    • 2006
  • To improve the mechanical properties of WC-Co cemented carbides, the dual composite was studied. The compositions of granule and matrix were nano-sized WC-6 wt% Co(granule) and normal sized WC-20 wt% Co(matrix), respectively. The granules were grouped 50, 100 and $150\;{\mu}m$ and mixed with WC and Co powders as the volume fractions of granule to matrix were 50 to 50, 40 to 60 and 30 to 70. These compacts were sintered at $1380^{\circ}C$ for 10 minutes in vacuum. The microstructure, transverse rupture strength and wear resistance were investigated.

  • PDF

Microstructure and Flexural Strength of Hardmetals

  • Hayashi, Koji
    • 한국분말재료학회지
    • /
    • 제1권2호
    • /
    • pp.119-198
    • /
    • 1994
  • The characteristics of various important microstructural factors of WC-base hard- metals (cemented carbides) such as the amount of Co metal binder phase, the carbide grain size, the microstructural defects acting as a fracture source, the solid solubility of tungsten in the binder phase affected by the carbon content, the precipitation of $Co_3W$, the domain size of binder phase, the formation of ${\beta}-free$ layer or Co-rich layer and CVD or PVD coated layer, and the effects of these factors on the flexural strength of the hardmetals are reviewed.

  • PDF

Machining Characteristics of Cemented Carbides in Micro Cutting within SEM

  • Heo, Sung-Jung
    • International Journal of Precision Engineering and Manufacturing
    • /
    • 제5권3호
    • /
    • pp.35-42
    • /
    • 2004
  • This research describes that the cutting characteristics and tool wear behavior in the micro cutting of three kinds of wear resistant cemented carbides (WC-Co; V40, V50 and V60) using PCD (Poly Crystalline Diamond) and PCBN (Poly crystalline Cubic Boron Nitride) cutting tools by use of the SEM (Scanning Electron Microscope) direct observation method. The purpose of this research is to present reasonable cutting conditions from the viewpoint of high efficient cutting refer to a precise finished surface and tool wear. Summary of the results is as follows: (1) The cutting forces tend to increase as the increase of the weight percentage of WC particles, and the thrust forces was larger than the principal forces in the cutting of WC-Co. These phenomena were different from the ordinary cutting such as cutting of steel or cast iron. (2) The cutting speed hardly influenced the thrust force, because of the frictional force between the cutting tool edge and small WC particles at low cutting speed region such as 2$\mu\textrm{m}$/s. It seemed that the thrust cutting force occurred by the contact between the flank face and work material near the cutting edge. (3) The wear mechanism for PCD tools is abrasion by hard WC particles of the work materials, which leads diamond grain to be detached from the bond. (4) From the SEM direct observation in cutting the WC-Co, it seems that WC particles are broken and come into contact with the tool edge directly. This causes tool wear, resulting in severe tool damage. (5) In the orthogonal micro cutting of WC-Co, the tool wear in the flank face was formed bigger than that in the rake face on orthogonal micro cutting. And the machining surface integrity on the side of the cutting tool with a negative rake angle was better than that with a positive one, as well as burr in the case of using the cutting tool with a negative rake angle was formed very little compared to the that with a positive one.

계장화 샬피충격시험을 이용한 WC-Co 초경합금의 동적 균열개시인성치 결정 (Determination of Dynamic Crack Initiation Toughness Using Instrumented Charpy Impact Test in WC-Co Alloy)

  • 이억섭;박원구;홍성경;윤경수
    • 대한기계학회논문집
    • /
    • 제19권3호
    • /
    • pp.688-696
    • /
    • 1995
  • Cemented carbides, best known for their superior mechanical properties such as high strength, high hardness and high wear resistance, have a wide range of industrial applications including metal working tools, mining tools, and wear resistance components. The cobalt has been used as a binder in the WC-based hard composites due to its outstanding wetting and adhesion characteristics even though its expensiveness. Therefore many studies attempted to find a better substitute for cobalt as binder to decrease production costs. This investigation is a pre-step to study dynamic fracture characteristic evaluation of a WC-Co hardmetal were evaluated by using the instrumented Charpy impact testing procedures. It was found that the dynamic characteristics of used strain amplifier were very important experimental factors to extract valid dynamic fracturing data in WC-Co specimens. It was suggested by showing some experimental examples that when we wished to evaluate dynamic fracture toughness for cemented carbide composites by using the instrumented Charpy impact testing procedure, a careful attention must be given to obtain valid results.

방전플라즈마 소결 공정 적용 전이금속 카바이드 서멧의 소결 및 기계적 특성 (Sintering Behavior and Mechanical Property of Transition Metal Carbide-Based Cermets by Spark Plasma Sintering)

  • 이정한;박현국;홍성길
    • 한국재료학회지
    • /
    • 제32권1호
    • /
    • pp.44-50
    • /
    • 2022
  • Transition metal carbides (TMCs) are used to process difficult-to-cut materials due to the trend of requiring superior wear and corrosion properties compared to those of cemented carbides used in the cutting industry. In this study, TMC (TiC, TaC, Mo2C, and NbC)-based cermets were consolidated by spark plasma sintering at 1,300 ℃ (60 ℃min) with a pressure of 60 MPa with Co addition. The sintering behavior of TMCs depended exponentially on the function of the sintering exponent. The Mo2C-6Co cermet was fully densified, with a relative density of 100.0 %. The Co-binder penetrated the hard phase (carbides) by dissolving and re-precipitating, which completely densified the material. The mechanical properties of the TMCs were determined according to their grain size and elastic modulus: TiC-6Co showed the highest hardness of 1,872.9 MPa, while NbC-6Co showed the highest fracture toughness of 10.6 MPa*m1/2. The strengthened grain boundaries due to high interfacial energy could cause a high elastic modules; therefore, TiC-6Co showed a value of 452 ± 12 GPa.

방전플라즈마소결법을 이용한 WC-3 wt%Co 소결체 제조 및 평가 (Fabrication and Evaluation of WC-3 wt%Co Compacts Fabricated by Spark Plasma Sintering)

  • 최정철;장세훈;차용훈;오익현
    • 한국재료학회지
    • /
    • 제18권7호
    • /
    • pp.357-361
    • /
    • 2008
  • Microstructure and mechanical properties of WC-3 wt% Co cemented carbides, fabricated by a spark plasma sintering (SPS) process, were investigated in this study. The WC-3 wt%Co powders were sintered at $900{\sim}1100^{\circ}C$ for 5min under 40MPa in high vacuum. The density and hardness were increased as the sintering temperature increased. WC-3 wt%Co compacts with a relative density of 97.1% were successfully fabricated at $1100^{\circ}C$. The fracture toughness and hardness of a compact sintered at $1100^{\circ}C$ were $21.6 MPa{\cdot}m^{1/2}$ and 4279 Hv, respectively.

호닝 가공에 사용되는 다이아몬드 공구의 성능평가에 관한 연구 (A Study on the Performance Evaluation of the Diamond Tool in Honing)

  • 김민주;이승수;전언찬
    • 한국공작기계학회논문집
    • /
    • 제11권1호
    • /
    • pp.10-16
    • /
    • 2002
  • This study is to evaluate the tool performance in honing using diamond reamer and present grounds whether the localized products are sufficiently competitive comparing with the existing imported ones. The heads of the tool performance evaluation are roundness, roughness, tool life of the workpiece and so on. When evaluating the tool performance, cutting process is divided by three areas which are rough semi-finish and finish cut. cloning improves the accuracy such as boring and reaming after manufacturing the inside diameter, and finishing directly by honing is a recent trend. This honing is used greatly In hard cutting materials like cemented carbides and it is the CBN and diamond that is used in hard cutting materials. Both of them are expensive and most oi them are imported.

유리섬유 강화 플라스틱(GERP) 절삭시의 공구마멸 특성 (Characteristics of tool wear in cutting glass fiber reinforced plastics : the effect of physical properties of tool materials)

  • 이원평;강명순
    • 오토저널
    • /
    • 제10권1호
    • /
    • pp.33-41
    • /
    • 1988
  • A turning (facing) test on Glass Fiber Reinforced Plastics was performed with several tool materials, e.g., cemented carbides, cermet and ceramic, and the wear patterns and wear rate were analyzed to clarify the relation between physical(mechanical) properties and flank wear of cutting tool. The main results are obtained as follows: (1) When cutting speed is increased, the flank wear in every tool material grows the abnormal wear in the shape of triangle at a certain speed, i.e., a critical speed. (2) When cutting speed is increased, the wear rate in experimental tool material starts to increase remarkably at a critical speed. (3) The thermal conductivity among the properties of the tool material and the thermal crack coefficient of it are almost in proportion to the critical speed. (4) The order of performance in tool materials for cutting GFRP is K 10, M10, P20, TiC, CB.

  • PDF

초경합금재의 절삭에 관한 연구 -선반절삭에 있어서 공구의 마멸과 절삭저항-

  • 허성중
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2004년도 춘계학술대회 논문요약집
    • /
    • pp.248-248
    • /
    • 2004
  • 초경합금재 (cemented carbides)는 WC(텅스텐 카바이드, 탄화텅스텐)과 Co(코발트)를 주성분으로 한 복합재료로서 저온경도와 고온경도가 뛰어 나며, 압축강도와 강성이 높은 것 등, 제반 물리적 성질이 안정되어 있다 이와 같은 우수한 특징을 이용하여, 초경합금재는 다양한 분야에 이용되고 있는데, 크게 나누어 절삭 공구용으로 뿐만 아니라 IT 관련, 환경 관련 산업용, 광산용 공구, 건설 공구, 철강의 압연 롤러 등의 내마멸, 내충격용 재료에도 많이 사용된다. 이들 가운데, 내마멸, 내충격용으로 사용되는 것은 절삭 공구용 초경합금재에 비해 결합제인 코발트를 많이 함유하며 경질 성분의 텅스텐 카바이드의 입자 지름도 거칠고 크다.(중략)