• Title/Summary/Keyword: c-$Al_2O_3$

Search Result 2,887, Processing Time 0.035 seconds

A COMPARATIVE STUDY OF THE PHYSICOCHEMICAL PROPER TIES AND BOND STRENGTH TO METAL BETWEEN THE REGULAR OPAQUE POWDER AND CORE POWDER (도재소부전장금관용 Opaque 분말과 도재전장관용 core 분말의 물리화학적 성질 및 금속과의 결합력에 대한 비교연구)

  • Lim, Jang-Seop;Chung, Chang-Mo;Jeon, Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.35 no.1
    • /
    • pp.144-164
    • /
    • 1997
  • The purpose of this study were to investigate the chemical composition, mean particle size, linear thermal expansion coefficient and metal-bonding strength of the regular opaque powder and core powder. In this study, 4 types of ceramic powders, namely Duceram Jacket Opaque powder, Duceram Opaque powder, Vita Hi-Ceram powder, Vita VMK Paint On-88 powder were used. Chemical composition was evaluated by EDS(Energy Dispersive X-ray Spectrophotometer, Oxford QX-2000, England), particle size was measured by MALVERN Instruments(MALVERN Instruments SB. OC., U.S.A.. ad linear thermal expansion coefficient was measured by dilatometer(Motoyama, Japan). Bond strength was measured by the Universal tsting machine(Istron Co., Ltd., U.S.A.). The Results were as follows : 1. Through recognition of the relative difference in chemical composition between the core powder and the regular opaque powder, the difference in the proportion of $Al_2O_3$ in each type of material is demonstrated ; Duceram Jaket Opaque powder : 30.16%, Duceram Opaque powder : 16.60%, Vita Hi-Ceram : 63.64%, Vita VMK Paint-On 88 : 16.16%. 2. There was no significant difference in the proportion of metal-bonding materials between the core powder and the regular opaque powder. 3. In the regular opaque powder, alkaline materials were incoporated in order to increase the coefficient of thermal expansion. 4. In the particle size analysis, there was no significant difference in mean particle size or in the particle size distribution between the core powder and the regular opaque powder. 5. In the thermal expansion test for temperature range of $25-600^{\circ}C$, the regular opaque powder had higher coefficient of thermal expansion than that of core powder. 6. In the 4 point flexural bending test, there was no statistically significant difference in the mean bond strength between the core powder and the opaque powder among the Duceram products.

  • PDF

A Scientific Analysis of Dancheong Pigments at Yaksajeon Hall in Gwallyoungsa Temple (창녕 관룡사 약사전 단청안료의 과학적 분석)

  • Han, Min-su;Kim, Jin-hyoung;Lee, Jang-jon
    • Korean Journal of Heritage: History & Science
    • /
    • v.47 no.1
    • /
    • pp.18-31
    • /
    • 2014
  • This study aims at identifying of characteristics and types of the pigments used for Dancheong(surface decorative and protective pigments) of Yaksajeon Hall in Gwallyoungsa Temple using a Micro-XRF, XRD, SEM-EDS and thereafter, comparing it with the pigments of the wall painting in the same building and with Dancheong pigments of Daeungjeon Hall. The results can be briefly summarized as two points. First, different types of pigments for red, green and white colours had been applied based on different parts of the building and more than two different pigments had been mixed to produce various colours in so me parts. Second, scientific analysis has confirmed that raw minerals for each colour groups are: Cinnabar, minium and Hematite for red; white clay and oyster shell white($Al_2O_3{\cdot}SiO_2{\cdot}4H_2O$) for white; Atacamite and Celadonite for green; carbon(C) for black; Yellow Ocher for yellow; and Lazulite for blue. Comparative analysis of such result with that of the wall paintings and of Dancheong of Daeungjeon Hall has revealed that similar minerals had been used in overall except that several different pigments had been added or removed for making green, white and yellow colour groups in some parts. In conclusion, the result has displayed that painters had used different ways of producing pigments by a type of painting or a building within the same period or for the buildings in the same buddhist temple compound.

The Effect of Oxide Compound on Electrical Resistivity and Oxidation Stability in High-temperature for Ferritic P/M Stainless Steel (산화물 혼합상이 페라이트계 P/M스테인리스강의 고온산화 및 전기저항 안정성에 미치는 영향)

  • Park, Jin-Woo;Ko, Byung-Hyun;Jung, Woo-young;Park, Dong-Kyu;Ahn, In-Shup
    • Journal of Powder Materials
    • /
    • v.23 no.3
    • /
    • pp.240-246
    • /
    • 2016
  • In order to improve the high-temperature oxidation stability, sintered 434L stainless steel is studied, focusing on the effect of the addition of metallic oxides to form stable oxide films on the inner particle surface. The green compacts of Fecralloy powder or amorphous silica are added on STS434L and oxidized at $950^{\circ}C$ up to 210 h. The weight change ratio of 434L with amorphous silica is higher than that of 434L mixed with Fecralloy, and the weight increase follows a parabolic law, which implies that the oxide film grows according to oxide diffusion through the densely formed oxide film. In the case of 434L mixed with Fecralloy, the elements in the matrix diffuse through the grain boundaries and form $Al_2O_3$ and Fe-Cr oxides. Stable high temperature corrosion resistance and electrical resistivity are obtained for STS434L mixed with Fecralloy.

Lamination of Dielectric Layers by High Pressure Spray Coating for LTCC (고압 스프레이 코팅법에 의한 저온동시소성세라믹(LTCC) 유전체 층의 적층방법)

  • Lee, Jee-Hee;Kim, Young-Jin
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.13 no.3 s.40
    • /
    • pp.33-38
    • /
    • 2006
  • Aerosol slurry composed of dielectric materials, distilled water, and deflocculants was sprayed on the substrates, through a high-pressure spray gun as an aerosol. The coated layers were cofired together with $Al_{2}O_{3}$ substrates and green sheets on which the inner connectors were printed. Although the coating rate of coated layers strongly depended on slurry viscosity, spray shape, and the pressure of the spray gun, the coated density was not changed. Buried conductors were maintained as printed by high pressure spray coating method, because the pressing process was not used. At the optimum condition of air controller step 3-4 and slurry viscosity c.p 2000-4000, dense and uniform layers could be achieved. Comparing with conventional lamination process using green sheets, spray coating method enabled thin dielectric layers of $20{\sim}50{\mu}m$.

  • PDF

Size and Shape Effect of Metal Oxides on Hydrocarbon Selective Catalytic Reduction of Nitrogen Oxides (금속 산화물 촉매의 크기와 형태에 따른 질소산화물의 탄화수소 선택적 촉매환원 특성)

  • Ihm, Tae-Heon;Jo, Jin-Oh;Hyun, Young Jin;Mok, Young Sun
    • Journal of the Korean Institute of Gas
    • /
    • v.19 no.5
    • /
    • pp.20-28
    • /
    • 2015
  • This work investigated the size and shape effect of ${\gamma}$-alumina-supported metal oxides on the hydrocarbon selective catalytic reduction of nitrogen oxides. Several metal oxides including Ag, Cu and Ru were used as the catalysts, and n-heptane as the reducing agent. For the Ag/${\gamma}$-alumina catalyst, the $NO_x$ reduction efficiency in the range of $250{\sim}400^{\circ}C$ increased as the size of Ag decreased (20 nm>50 nm>80 nm). The shape effect of metal oxides on the $NO_x$ reduction was examined with spherical- and wire-shape nanoparticles. Under identical condition, higher catalytic activity for $NO_x$ reduction was observed with Ag and Cu wires than with the spheres, while spherical- and wire-shape Ru exhibited similar $NO_x$ reduction efficiency to each other. Among the metal oxides examined, the best catalytic activity for $NO_x$ reduction was obtained with Ag wire, showing almost complete $NO_x$ removal at a temperature of $300^{\circ}C$. For Cu and Ru catalysts, considerable amount of NO was oxidized to $NO_2$, rather than reduced to $N_2$, leading to lower $NO_x$ reduction efficiency.

Metamorphism of the Gyeonggi Massif in the Gapyeong-Cheongpyeong area (가평-청평 지역 경기육괴의 변성작용)

  • Lee Kwang Jin;Cho Moonsup
    • The Journal of the Petrological Society of Korea
    • /
    • v.1 no.1
    • /
    • pp.1-24
    • /
    • 1992
  • Precambrian metamorphic rocks of the Gapyeong-Cheongpyeong area consist of banded gneiss, augen gneiss, leucocratic gneiss, quartz schist and quartzite, together with minor intercalations of serpentinite, amphibolite and marble. Mineral assemblages of meta-sedimentary rocks are classified into three types: sillimanite-free; sillimanite-bearing; and sillimanite+K-feldspar-bearing assemblages. Compositions of metamorphic phases depend on the type of mineral assemblages. In particular, the Ca contents of plagioclase and garnet are high in sillimanite-free assemblges. Kyanite occurs in three samples, and coexists with sillimanite in one sample. The presence of kyanite indicates that metamorphic rocks of the study area have experienced the Barrovian type metamorphism. Peak metamorphic conditions estimated from various geothermobarometers and phase equilibria are 618-674$^{\circ}C$ and 6.5${\pm}$2.0 kbar for sillimanite-free assemblages, and 701-740$^{\circ}C$ and 4.4${\pm}$0.8 kbar for sillimanite-bearing assemblages, respectively. Furthermore, a clockwise P-T-time path is deduced for the study area, based on the following observations: (1) the polymorphic transition of kyanite to sillimanite, (2) the occurrence of sillimanite and K-feldspar belonging to the upper amphibolite facies, and finally (3) the retrograde metamorphism characterized by muscovite-, chlorite-, and actinolite-bearing assemblages.

  • PDF

A Case of Interstitial Pneumonitis developed by Interferon-${\alpha}$ Treatment for Chronic Hepatitis C (만성 C형 간염 환자에서 Interferon-${\alpha}$를 투여중 발생한 간질성 폐렴 1예)

  • Yoon, Jong Goo;Ahn, Joong Hyun;Ko, Seung Hyeon;Lee, Hyun Seoung;Kwon, Soon Seog;Kim, Young Kyoon;Moon, Hwa Sik;Park, Sung Hak;Song, Jeong Sup
    • Tuberculosis and Respiratory Diseases
    • /
    • v.43 no.4
    • /
    • pp.637-644
    • /
    • 1996
  • Interstitial pneumonitis associated with interferon alpha therapy for chronic hepatitis C was first describe6 in 1994 by Kazoo et al In Japan. The mechanism of interstitial pneumonitis developed by interferon alpha was still unknown but immunologic, allergic of direct lung toxicity were suggested. We experienced a case of interstitial pneumonitis developed during interferon alpha therapy for chronic hepatitis C in a 52-year-old male patient. He was treated with 6 million units of interferon alpha intramuscularly 3 times per week for 4 weeks and noted progressive dyspnea and cough. These symptoms were subsided after 6 weeks' discontinuation of interferon alpha therapy. And so, he was retreated with 3 million units of interferon alpha 3 times per week for 8 weeks and felt dyspnea again. He was admitted to our hospital for further evaluation of progressive dyspnea. Arterial blood gas(ABG) values were $PaO_2$ 90.7 mmHg and $PaCO_2$ 31.9 mmHg, and antinuclear antibody(ANA) was negative. A chest X-ray film revealed diffuse reticulo-nodular shadows in bilateral lung fields, suggesting a diagnosis of interstitial pneumonitis. A marked increase in lymphocyte count and suppressor T cell were observed in bronchoalveolar lavage(BAL) fluid. Lymphocyte stimulation test with interferon alpha was positive. Interstitial pneumonitis was confirmed by transbronchial lung biopsy. After discontinuation of interferon alpha, we gave oral steroid in the condition that clinical symptoms were being improved gradually.

  • PDF

Effects of particle size on processing variables and green microstructure in gelcast alumina green bodies (겔-케스팅한 알루미나 성형체에서 출발입도가 공정변수 및 성형 미세구조에 미치는 영향)

  • Ha, Chang-Gi;Kim, Jae-Won;Jo, Chang-Yong;Baek, Un-Gyu;Jeong, Yeon-Gil
    • Korean Journal of Materials Research
    • /
    • v.11 no.10
    • /
    • pp.869-878
    • /
    • 2001
  • Alumina $(Al_2O_3)$ green bodies were fabricated by gel-casting using three kinds of alumina with different particle size (mean particle size: 4.6 $\mu\textrm{m}$, 0.32 $\mu\textrm{m}$, 10nm). The effects of particle size on gel-casting process and green microstructure were investigated. The optimum dispersion conditions using ammonium salt (D-3019) as dispersant were 0.2 wt% (4.63 $\mu\textrm{m}$), 0.5 wt% (0.32 $\mu\textrm{m}$), and 5.0 wt% (10 nm), in high solid loading. The optimum solid loading of each starting material for gel-casting was obtained as 59 vol% (4.63 $\mu\textrm{m}$), 57 vol% (0.32 $\mu\textrm{m}$), 15 vol% (10 nm), depending on particle size, indicating that nano-size particle (10 nm) represent lower solid loading as high specific surface area than those of other two starting materials. The drying at ambient conditions (humidity; $\thickapprox$90%) was performed more than 48hrs to enable ejection of the part from the mold and then at $120^{\circ}C$ for 2hrs in an air oven, showing no crack and flaw in the dried green bodies. The pore size and distribution of the gelcast green bodies showed the significant decrease with decreasing particle size. Green microstructure was dependent on the pore size and distribution due to the particle size, and on the deairing step. The green density maximum obtained was 58.9% (4.63 $\mu\textrm{m}$), 60% (0.32 $\mu\textrm{m}$), 47% (10 nm) theoretical density (TD), and the deairing step applied before gel-casting did not affect green density.

  • PDF

Characteristic and Economic evaluation of low cost TiO2 photocatalyst made by TiCl4 (TiCl4로 제조된 저비용 이산화티타늄 광촉매의 특성 및 경제성 평가)

  • Kim, Jong Kyu
    • Proceedings of the Korea Water Resources Association Conference
    • /
    • 2019.05a
    • /
    • pp.197-197
    • /
    • 2019
  • 총인처리시설에서는 응집제를 주입하여 인이나 오염물질을 침전시켜 처리하고 있으며 PAC(poly aluminum chloride)나 $FeCl_3$, $Al_2(SO_4)_3$, 등 다양한 종류의 응집제가 사용되어지고 있다. 하지만 기존에 사용되어 지고 있는 알루미늄계열의 응집제는 처리수에 잔류이온이 존재하게 되어 인체에 축적돼 알츠하이머 병 등 신체질환을 유발할 수 있는 단점이 있다. 따라서 이러한 단점을 사전에 예방하기 위해 $TiCl_4$와 같은 티타늄계열 응집제에 대한 연구가 진행되고 있다. $TiCl_4$ 응집제는 인 제거에 효과적으로 적용할 수 있으며 수중에 잔류이온을 유발하지 않으며 Ti이온은 치과임플란트나 의료장비로 사용될 만큼 인체에 무해하다고 알려져 있다. 응집제 사용에 따라 생성된 응집슬러지의 처리방안에 있어서 기존 응집제의 경우 생성된 슬러지의 대부분은 하수슬러지 위탁처리업체를 통해 소각 및 매립, 재활용 되고 있으나, $TiCl_4$를 응집제로 사용할 경우 생성된 슬러지를 인발하여 건조 및 소성을 통해 이산화티타늄으로 재활용할 수 있어 슬러지를 친환경적으로 처리가 가능해 기존 슬러지 처리방안의 경제적, 환경적 부담을 줄일 수 있는 장점이 있다. 따라서 본 연구에서는 $TiCl_4$를 하수처리장 방류수에 주입하여 수중의 총인(T-P)을 처리한 후 생성된 슬러지를 인발하여 건조와 소성과정을 거쳐 이산화티타늄을 제조하였다. 방류수를 취수해 2.5mg/L의 초기 총인 농도를 가진 원수를 제조하였으며 제조된 원수에 $TiCl_4$를 0.6mL 주입하였을 때 99.93%의 총인제거효율을 얻을 수 있었다. 응집 실험 후 생성된 슬러지를 인발하여 건조 후 $300{\sim}1000^{\circ}C$의 각각 다른 온도조건에서 소성하여 이산화티타늄을 제조하였으며, SEM과 XRD를 통해 제조된 이산화티타늄의 표면특성과 결정성 분석을 실시하였다. 제조된 이산화티타늄은 $500{\sim}800^{\circ}C$에서는 아나타제, $900{\sim}1000^{\circ}C$에서는 루타일 결정구조가 나타났다. 또한, $TiCl_4$ 주입량에 따른 이산화티타늄의 최종 생산량과 제조 시 사용되는 건조로 및 소성로의 경제적 비용 등을 고려하여 이산화티타늄 1Ton을 제조하기 위해 필요한 단가를 산출하였다. 본 연구에서 제조된 이산화티타늄 1kg의 생산단가는 약 5,400원으로 나타났으며, 가장 많이 사용되는 P-25 광촉매 보다 저렴한 가격으로 제조 및 판매를 기대할 수 있다. 따라서 하수처리장에 적용 시 기존 응집제 보다 비싼 $TiCl_4$ 비용을 보완하고 친환경적인 슬러지 처리로 제조된 이산화티타늄의 유통 및 현장적용을 통해 경제적, 환경적으로 우수하다고 판단된다.

  • PDF

Characteristics of Pyrophyllite Powder Molding Material by High-Speed, High-Pressure Dynamic Compression Technology (고속고압 동적 압축 기술에 의한 연납석 분말 성형 재료 특성)

  • Jeongdu Noh;Sangyeon Ban;Taeyoon Oh;Jangbok Wi;Seong-Seung Kang
    • The Journal of Engineering Geology
    • /
    • v.34 no.3
    • /
    • pp.403-413
    • /
    • 2024
  • This study aims to investigate the material properties of specimens made from pyrophyllite and pyrophyllite-aluminum mixed powders using high-speed, high-pressure dynamic compression technology. The aluminum powder exhibited a highly uniform particle size distribution ranging from 10 to 100 ㎛, whereas the pyrophyllite powder displayed four distinct particle size distributions: 0.1~1 ㎛, 1~10 ㎛, 80~100 ㎛, and 200~1,000 ㎛. Using high-speed, high-pressure dynamic compression technology with a drop time of approximately 0.34~0.4 seconds and a dynamic load of about 207 tonf, it was possible to fabricate pyrophyllite and pyrophyllite-aluminum mixed powder specimens with a volume of about 548 mm2. The Shore hardness measurement results showed that specimen BG100 had an average of 43.7, BG90 had an average of 33.2, and BG85, BG80, BG75, and BG70 had an average of 31.0, indicating that the specimen with the least aluminum content exhibited the highest Shore hardness value. The thermogravimetric analysis revealed mass losses at two points: the first mass loss occurred at around 270℃ with a loss of approximately 1.45%, and the second mass loss occurred at around 600℃, where BG70 and BG80 showed a mass loss of about 2.53%, and BG75, BG85, and BG90 showed a mass loss of about 3.43%. Scanning electron microscopy analysis indicated that the microstructure of the specimens was similar regardless of the mixing ratio, with three elements-O, Si, and Al-being detected in all specimens. The mapping analysis of BG90 revealed an oxygen weight ratio of 50.80%, silicon weight ratio of 37.36%, and aluminum weight ratio of 11.85%. In the case of BG85, the results were 43.09% oxygen, 43.50% silicon, and 13.41% aluminum; for BG80, the results were 44.83% oxygen, 40.30% silicon, and 14.87% aluminum; for BG75, the results were 44.71% oxygen, 35.49% silicon, and 19.80% aluminum; and for BG70, the results were 34.95% oxygen, 35.73% silicon, and 29.32% aluminum.