지하매설 유체함입 강파이프의 감쇠특성 규명 (Attenuation Characteristics of the Buried Steel Water Pipes)

  • 박경조;강우석;김이곤
    • 동력기계공학회지
    • /
    • 제13권1호
    • /
    • pp.39-45
    • /
    • 2009
  • The attenuation of the fundamental non-torsional modes that propagate down buried steel water pipes has been studied. The mode shapes, mode attenuation due to leakage into the surrounding medium and the scattering of the modes as they interact with pipe joints and fittings have been investigated. In the low frequency region the mode predicted to dominate over significant propagation distances approximates a plane wave in the water within pipe. The established acoustic technique used to locate leaks in buried steel water pipes assumes that leak noise propagates as a single non-dispersive mode at a velocity related to the low frequency asymptote of this water borne mode.

  • PDF

토양매설 스테인리스강 상수도 배관의 부식원인 규명 (Elucidation of Corrosion and Failure of Stainless Steel Tubing buried in Soil for Potable Water)

  • 김영식;박수진;황보덕;신민철
    • Corrosion Science and Technology
    • /
    • 제11권1호
    • /
    • pp.20-28
    • /
    • 2012
  • Since buried pipes contact the soil directly, corrosion by the soil could be occurred. Recently, some stainless steel pipes after 8 years burial at G area were corroded and leaked. In order to elucidate highly corroded phenomena(its rate was about 0.175 mm/y) of these pipes, the investigation for corrosion environment, soil, stray current's effect, and chemical analysis on the pipes were performed. Most of investigated sites were close to traditional water-closet and showed high moisture and thus those areas could be highly corrosive. In the investigation by two kinds of soil evaluation methods, it was revealed that the soils at G areas were highly corrosive, and moreover the contents of sulfate reducing bacteria in the soils were high. Also, open circuit potentials of many pipes showed different values and its potentials were high positive. Therefore, it was considered that corrosion of buried pipes at G area could be affected by high corrosive soil's environment and stray current corrosion.

신설 파형강판 지중암거의 기존 콘크리트 박스 접합부 해석 (Connections of the Corrugated Steel Plate Culvert with the Concrete Box)

  • 조성민;변순주
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.373-378
    • /
    • 2000
  • Zinc galvanized steel plates(sections) of annular corrugations have been used in buried steel culverts. These structures are referred to by a variety of names such as flexible pipes, buried pipes, soil-steel bridges, corrugated steel culverts, and etc. Buried corrugated steel structures show flexible behaviour under the soil load. compared with concrete box structures. Finite element analysis was performed to suggest the reasonable connecting method between the flexible steel culverts and the rigid concrete box. It was predicted that perfectly constrained connections could induce the excessive stress in steel plates. Therefore elastic bearing connections that allow vertical displacement at the connecting point were applied.

  • PDF

온실 환경 하에서 20년 경과된 농업용 강관의 부식 및 강도변화 (Corrosion and Strength Changes of Agricultural Steel Pipes Elapsed 20 Years under the Greenhouse Environment)

  • 남상운;류희룡;최만권;신현호
    • 생물환경조절학회지
    • /
    • 제29권2호
    • /
    • pp.196-201
    • /
    • 2020
  • 파이프 골조 온실의 내구성 증대를 위하여 4가지의 부식방지 처리를 한 파이프를 실험온실 내부에 설치하여 20년경과 후 표면부식 상태와 강도 변화 실험을 실시하였다. 대기 중에 노출된 지상부위에서 무처리 파이프는 강도가 1.3%정도 줄었지만 다른 처리와의 차이는 거의 없는 것으로 나타났다. 지하 매설부위에서 중방식 처리한 파이프의 강도는 0.6%정도 줄어 거의 변화가 없었으나 무처리는 15.7% 감소하는 것으로 나타났다. 그리고 방청 페인트나 아스팔트 도포는 4.2~4.4%정도 감소하는 것으로 나타났다. 지상부위는 모든 시료에서 심한 부식상태를 보이지 않았다. 중방식 처리는 변화가 없었고, 방청페인트 처리도 녹은 발견되지 않고 약간의 변색만 있었다. 아스팔트 도포는 검게 변색되고 약간의 녹이 발견되었으며, 무처리는 표면의 20~30%정도가 녹슨 것으로 나타났다. 지하 매설부위 무처리 파이프의 경우에는 전체가 완전히 녹슬어 있었고, 아스팔트 도포한 파이프도 표면의 80~90%가 녹슬어 있었다. 방청페인트 처리는 20~30%정도 녹슬어 있었고, 중방식 처리는 거의 변화가 없었다. 중방식 처리는 지하 매설부위에서도 확실한 부식 방지 효과를 보이는 것을 확인할 수 있었고, 방청페인트 처리도 어느 정도 부식 방지 효과를 나타내고 있으므로 현장에 적용할 수 있을 것으로 판단된다.

비닐하우스용 아연도강관의 강도경년변화 시험(농업시설) (A Secular Change of Strength for Galvanized Steel Pipes for Vinyl Housing)

  • 남상운;김문기;권혁진
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 2000년도 학술발표회 발표논문집
    • /
    • pp.296-301
    • /
    • 2000
  • Bend test for metallic materials was conducted on samples of galvanized steel pipes being used in greenhouse farms. A secular change of yield strength for galvanized steel pipes was analyzed with the part of buried in the ground and exposed in the atmosphere. From those experimental results and corrosion rate of galvanized film, the standard durable years for pipe framed greenhouses are estimated that the small sized pipe houses of movable type is 7∼8 years and the large sized pipe houses of fixed type is 14∼15 years.

  • PDF

REAL-TIME CORROSION CONTROL SYSTEM FOR CATHODIC PROTECTION OF BURIED PIPES FOR NUCLEAR POWER PLANT

  • Kim, Ki Tae;Kim, Hae Woong;Kim, Young Sik;Chang, Hyun Young;Lim, Bu Taek;Park, Heung Bae
    • Corrosion Science and Technology
    • /
    • 제14권1호
    • /
    • pp.12-18
    • /
    • 2015
  • Since the operation period of nuclear power plants has increased, the degradation of buried pipes gradually increases and recently it seems to be one of the emerging issues. Maintenance on buried pipes needs high quality of management system because outer surface of buried pipe contacts the various soils but inner surface reacts with various electrolytes of fluid. In the USA, USNRC and EPRI have tried to manage the degradation of buried pipes. However, there is little knowledge about the inspection procedure, test and manage program in the domestic nuclear power plants. This paper focuses on the development and build-up of real-time monitoring and control system of buried pipes. Pipes to be tested are tape-coated carbon steel pipe for primary component cooling water system, asphalt-coated cast iron pipe for fire protection system, and pre-stressed concrete cylinder pipe for sea water cooling system. A control system for cathodic protection was installed on each test pipe which has been monitored and controlled. For the calculation of protection range and optimization, computer simulation was performed using COMSOL Multiphysics (Altsoft co.).

구조해석을 통한 도시가스 매설배관의 지진 영향 분석 (Seismic Impact Analysis of Buried Citygas Pipes through Structural Analysis)

  • 조윤호;최마리아;양주안;전상일;전지훈
    • 한국가스학회지
    • /
    • 제27권4호
    • /
    • pp.19-26
    • /
    • 2023
  • 지진은 지하 구조물에 영향을 미치는 가장 중요한 재해 중 하나이다. 도시가스 지하 매설 배관은 지진 발생 시 구조물의 안전성 문제가 발생할 수 있다. 우리나라는 디지털 관측을 시작한 이래로 지진 발생 횟수가 꾸준히 증가하고 있다. 도시가스배관의 내진 설계 기준은 2008년에 KGS GC204 가스배관 내진설계 기준이 제정되었지만 이는 배관 설치 시 기준으로 지진 발생 시 배관의 영향을 추정하기는 어렵다. 본 연구에서는 국내에서 매설배관으로 주로 사용하고 있는 PE(폴리에틸렌관)배관과 PLP(폴리에틸렌 피복강관) 배관을 대상으로 지진 발생 시 환경 및 배관의 변수에 따른 구조해석을 수행하였다. 본 연구는 CAE(Computer Aided Engineering)를 통해 배관을 모델링하고 지반에 변위를 발생시켜 가장 취약한 매설배관의 변수를 찾고자하였다. 이 연구를 통해 토양은 탄성계수가 클 수록, 매설심도는 깊을 수록, 관경은 작을 수록, 압력은 높을 수록, PE 보다 PLP 배관이 더 지진에 영향을 많이 받는 것을 확인할 수 있었다. 이 결과를 토대로 매설 도시가스배관의 취약지점을 유추하여 지진발생 시 매설배관의 특별점검에 활용하고자한다.[1]

원자력발전소 적용 고밀도 폴리에틸렌 배관의 맞대기 융착절차 및 검증절차 분석 (Butt-fusing Procedures and Qualifications of High Density Polyethylene Pipe for Nuclear Power Plant Application)

  • 오영진;박흥배;신호상
    • Journal of Welding and Joining
    • /
    • 제31권6호
    • /
    • pp.1-7
    • /
    • 2013
  • In nuclear power plants, lined carbon steel pipes or PCCPs (pre-stressed concrete cylinder pipes) have been widely used for sea water transport systems. However, de-bonding of linings and oxidation of PCCP could make problems in aged NPPs (nuclear power plants). Recently at several NPPs in the United States, the PCCPs or lined carbon steel pipes of the sea water or raw water system have been replaced with HDPE (high density polyethylene) pipes, which have outstanding resistance to oxidation and seismic loading. ASME B&PV Code committee developed Code Case N-755, which describes rules for the construction of buried Safety Class 3 polyethylene pressure piping systems. Although US NRC permitted HDPE materials for Class 3 buried piping, their permission was limited to only 10-year operation because of several concerns including the quality of fusion zone of HDPE. In this study, various requirements for fusion qualification test of HDPE and some regulatory issues raised during HDPE application review in foreign NPPs are introduced.

각종 매설관의 동적거동에 관한 연구 (A Study on the Dynamic Behavior of a Various Buried Pipeline)

  • 정진호;임창규;정두회;국승규
    • 한국지진공학회논문집
    • /
    • 제10권4호
    • /
    • pp.15-24
    • /
    • 2006
  • 본 연구는 각종 매설관의 경계조건에 따른 동적 거동에 대한 연구이다. 축방향 및 축직각방향에 대한 거동을 조사하였다. 매설관은 탄성기초 위에 놓인 보요소로 모형화하였고, 지진파는 정현파 형태의 지반 변위로 적용하였다. 매설관의 고유진동수와 모드 형태 그리고 매개변수의 영향을 조사하기 위해 자유 진동에 대한 해석을 수행했다. 그리고 지반진동에 대한 거동을 조사하기 위해 자유진동 해석을 통해 얻어진 고유진동수와 모드 형태를 이용하여 강제 진동에 대한수식을 유도하였다. 자유 진동시 매설관의 고유진동수에 가장 큰 영향을 미치는 것은 지반 강성과 매설관의 길이였다. 지반진동의 전파방향과 전파속도 그리고 진동수에 대한 콘크리트관, 강관, FRP관의 동적거동을 연구하였고 그 결과를 비교하였으며 다양한 단부경계조건에 대한 동적거동해석을 통해 매설관의 종류와 단부경계조건에 따른 최대 변형률 발생지점을 산정하였다.

주변 흙의 특성이 물이 찬 매립된 배관에서 전파되는 기본 유도 종파 모드 감쇠에 미치는 영향 (Effect of Surrounding Soil Properties on the Attenuation of the First Guided Longitudinal Wave Mode Propagating in Water-filled, Buried Pipes)

  • 이주원;나원배;신성우;김재민
    • 한국해양공학회지
    • /
    • 제24권4호
    • /
    • pp.32-37
    • /
    • 2010
  • This study presents the attenuation characteristics of the first guided longitudinal wave mode propagating in water-filled, buried steel pipes in order to investigate the effects of soil saturation and compaction on the attenuation patterns. For numerical calculation of attenuation, 10 different combinations of S-wave velocity, P-wave velocity, and soil densities were considered. From the attenuation dispersion curves, which were obtained using Disperse software, we determined that the attenuation decreases as saturation increases, whereas it increases as compaction increases. Over the frequency range from 0.2 to 0.4 MHz, the first longitudinal wave mode has attenuations that are relatively lower than for other ranges, is faster than the first flexural wave mode, and is sensitive to defects aligned in the axial direction. Hence, the first longitudinal wave mode over the mentioned frequency range would be the proper choice for long-range buried pipelines that transport water.