MOCVD 법에 의해 제조된 YBCO 초전도 박막의 물성에 대한 완충층 템플릿의 영향 (Effect of the Buffered-template on the Property of YBCO Superconducting Film Deposited by MOCVD Method)

  • 전병혁;최준규;김찬중
    • Progress in Superconductivity
    • /
    • 제8권1호
    • /
    • pp.27-32
    • /
    • 2006
  • [$YBa_2Cu_3O_{7-x}$] thin films were deposited on various buffered-templates by a metal organic chemical vapor deposition(MOCVD). Three different templates of $CeO_2/YSZ/CeO_2/pure-Ni(CYC),\;CeO_2/YSZ/Y_2O_3/Ni-3at.%W(YYC)$ and $CeO_2/IBAD-YSZ$/stainless steel were used. The Ni and Ni-W alloy tapes were biaxially textured by cold rolling and annealing heat treatment. The dense YBCO films were grown on both the IBAD and YYC templates with no microcrack, while the YBCO films on the CYC templates were grown with the formation of microcracks and NiO. The YBCO film on the YYC template showed the higher $I_c$ than that on CYC template. Especially, the IBAD templates with a thin $CeO_2$(type I) and thick $CeO_2$(type II) top layer were used to compare the deposition nature of the YBCO on them. Comparing the current property of the YBCO films on IBAD templates, the YBCO film deposited on thick $CeO_2$ layer was better than the film on thin $CeO_2$ layer.

  • PDF

MOD-processed YBCO coated conductors on the $CeO_2$-buffered IBAD-MgO template

  • Shin, G.M.;Ko, R.K.;Oh, S.S.;Moon, S.H.;Yoo, S.I.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제11권4호
    • /
    • pp.20-24
    • /
    • 2009
  • YBCO coated conductors (CC) on the $CeO_2$-buffered IBAD-MgO template were fabricated by metal-organic deposition (MOD) Process with Ba-trifluoroacetate and fluorine-free Y and Cu precursor materials. The precursor solution was coated on $CeO_2$-buffered IBAD MgO templates using the multiple dip-coating method, decomposed into inorganic precursors by pyrolysis up to $400^{\circ}C$ within 3 h, and finally fired at $740{\sim}800^{\circ}C$ in a reduced oxygen atmosphere. Microstructure, texture, and superconducting properties of YBCO films were found highly sensitive to both the firing temperature and time. The high critical current density ($J_C$) of $1.15\;MA/cm^2$ at 77.3K in the self-field could be obtained from $1\;{\mu}m$ thick YBCO CC, fired at $740^{\circ}C$ for 3.5 h, implying that high performance YBCO CC is producible on IBAD MgO template. Further enhancement of $J_C$ values is expected by improving the in-plane texture of $CeO_2$-buffer layer and avoiding the metal substrate contamination.

나노임프린트 리소그래피를 이용한 곡면 기판 위에 정렬된 나노 볼 패턴 형성에 관한 연구 (Fabrication of High Ordered Nano-sphere Array on Curved Substrate by Nanoimprint Lithography)

  • 홍성훈;배병주;곽신웅;이헌
    • 한국표면공학회지
    • /
    • 제41권6호
    • /
    • pp.331-334
    • /
    • 2008
  • The replica of highly ordered nano-sphere array patterns were fabricated using hot embossing method. First, silica nano-sphere array on Si substrate was transferred to PVC film at $130^{\circ}C$ and 7 bar using hot embossing process. Then, silica nano-sphere array on PVC template was removed by soaking the PVC film in buffered oxide etcher. In order to form anti-stiction layer, the PVC template was coated with silicon dioxide layer and self-assembled monolayer. Through UV nanoimprint lithography with the fabricated flexible PVC template, highly ordered nano-sphere array pattern was imprinted on curved substrates with high fidelity.

Graphitic Mesostructured Carbon from an Aliphatic Hydrocarbon Precursor

  • Kim, Chy-Hyung;Oh, Teresa
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권9호
    • /
    • pp.1978-1980
    • /
    • 2009
  • A mesostructured form of carbon was fabricated from a template of mesostructured silica by using pentane, an aliphatic hydrocarbon precursor. To synthesize the mesostructured silica, a buffered (pH of 6.5) mixture of nonionic Pluronic P123 surfactant, sodium silicate, and acetic acid were used. The impregnated silica with Fe$(CO)_5$ (wt 5%) and pentane was placed in a quartz tube, treated with pentane vapor at 800 ${^{\circ}C}$ for two hours to synthesize the mesostructured carbon. The XRD patterns of the carbon replica in the low/wide angle regions, its TEM images, and nitrogen adsorption-desorption isotherm revealed that the long-range framework order of mesostructure with the pore size centered on 2.8 nm was maintained to some extent mainly due to some portions of mesophase carbon that work as a support to fix the hexagonal frameworks by anchoring on the pore surface with an improved graphitic character. The dc conductivity of the mesostructured carbon in pressed powder form at 6.0 MPa was 2.08 S/cm.

MOD-processed YBCO coated conductor on the IBAD-MgO template

  • Shin, Geo-Myung;Ko, Rock-Kil;Song, Kyu-Jeong;Yoo, Jai-Moo;Oh, Sang-Soo;Moon, Seung-Hyun;Yoo, Sang-Im
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제9권4호
    • /
    • pp.16-18
    • /
    • 2007
  • We report the results of MOD-processed YBCO coated conductors on the IBAD-MgO template. The precursor solution was coated on the $CeO_2-buffered$ IBAD-MgO template using a slot-die coating method, calcined at a temperature of $550^{\circ}C$, and fired at high temperatures for 2.5 h in a reduced oxygen atmosphere. The $J_C$ value of YBCO coated conductors was found to be very sensitive to the microstructure, and thus higher $J_C$ value could be achieved when the in-plane texture was higher and the difference in $T_{C,zero}$. was negligible. Optimally processed YBCO coated conductor exhibited $J_C$ value of $0.75MA/cm^2$ at 77 K in self-field, which might be due to somewhat depressed $T_{C,zero}$ of 87.3 K caused by possible $Sm^{3+}$ substitution on the $Ba^{2+}$ site.

$BaHfO_3$ 완충층을 사용한 IBAD MgO 기판 위에 제조된 고임계전류밀도의 $GdBa_2Cu_3O_y$ 박막 (High-$J_c$ $GdBa_2Cu_3O_y$ films on $BaHfO_3$ buffered IBAD MgO template)

  • 고경필;이정우;고락길;문승현;오상수;유상임
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제13권1호
    • /
    • pp.6-11
    • /
    • 2011
  • The $BaHfO_3$ (BHO) buffer layer on the IBAD MgO template was turned to be effective for a successful fabrication of $GdBa_2Cu_3O_{7-{\delta}}$ (GdBCO) films with high critical current density ($J_c$). Both the BHO buffer layers and GdBCO films were prepared by pulsed laser deposition (PLD). The effects of the PLD conditions, including substrate temperature ($T_s$), oxygen partial pressure ($PO_2$), and deposition time on the in-plane texture, surface roughness, and microstructures of the BHO buffer layers on the IBAD MgO template were systematically studied for processing optimization. The c-axis oriented growth of BHO layers was insensitive to the deposition temperature and the film thickness, while the in-plane texture and surface roughness of those were improved with increasing $T_s$ from 700 to $800^{\circ}C$. On the optimally processed BHO buffer layer, the highest $J_c$ value (77 K, self-field) of 3.68 $MA/cm^2$ could be obtained from GdBCO film deposited at $780^{\circ}C$, representing that BHO is a strong candidate for the buffer layer on the IBAD MgO template.

STRATEGIC RESEARCH AT ORNL EOR THE DEVELOPMENT OF ADVANCED COATED CONDUCTORS: PART - II

  • Paranthama, M. Parans;Aytug, T.;Sathyamurthy, S.;Zhai, H.Y.;Christen, H.M.;Martin, P.M.;Goyal, A.;Christen, D.K.;Kroeger, D.M.
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2002년도 학술대회 논문집
    • /
    • pp.340-340
    • /
    • 2002
  • In an effort to develop alternative single buffer layer technology for YBa$_2$Cu$_3$O$_{7-{\delta}}$ (YBCO) coated conductors, we have investigated both LaMnO$_3$, (LMO) and La$_2$Zr$_2$O$_{7}$ (LZO) as potential buffer layers. High-quality LMO films were grown directly on textured Ni and Ni-W (3%) substrates using rf magnetron sputtering. Highly textured LZO buffers were grown on textured Ni substrates using sol-gel alkoxide processing route. YBCO films were then grown on both LMO and LZO buffers using pulsed laser deposition. Detailed X-ray studies have shown that YBCO films were grown on both LMO and LZO layers with a single epitaxial orientation. A high J$_{c}$ of over 1 MA/cm$^2$ at 77 K and self-field was obtained on YBCO films grown on both LMO-buffered Ni or Ni-W substrates, and also on LZO-buffered Ni substrates. We have identified LaMnO$_3$ as a good diffusion barrier layer for Ni and it also provides a good template for growing high current density YBCO films. Similarly we have also demonstrated the growth of high J$_{c}$ YBCO films on all solution buffers. We will discuss in detail about our buffer deposition processes. processes.s.s.s.s.

  • PDF

Meter-long coated conductor by R2R PVD methods on RABiTS template

  • Ko, Rock-Kil;Kim, Ho-Sup;Ha, Hong-Soo;Chung, Jun-Ki;Yang, Joo-Saing;Park, Yu-Mi;Shi, Dong-Qi;Song, Kyu-Jeong;Park, Chan;Yoo, Sang-Im;Moon, Seung-Hyun;Kim, Young-Cheol
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권4호
    • /
    • pp.13-16
    • /
    • 2004
  • Three film deposition systems (pulsed laser deposition, sputtering, and evaporation) equipped with reel-to-reel metal tape moving apparatus were installed and used to make meter-long coated conductor. Buffer architecture of $CeO_2/YSZ/Y_2O_3$ was deposited on Ni alloy using sputtering, evaporation, and PLD. YBCO superconducting layer was continuously deposited on buffered metal tape by PLD. End-to-end critical current ($I_c$) of 107 A at 77 K, self-field has been achieved in 1 em-wide tape (thickness 0.6∼1.0${\mu}{\textrm}{m}$, tape moving speed 54∼72 cm/hr) over 1 meter length.

PCR Diagnosis of Entamoeba histolytica Cysts in Stool Samples

  • Moon, Joung-Ho;Cho, Shin-Hyeong;Yu, Jae-Ran;Lee, Won-Ja;Cheun, Hyeng-Il
    • Parasites, Hosts and Diseases
    • /
    • 제49권3호
    • /
    • pp.281-284
    • /
    • 2011
  • Amebiasis is a protozoan disease caused by Entamoeba histolytica and a potential health threat in areas where sanitation and hygiene are inappropriate. Highly sensitive PCR methods for detection of E. histolytica in clinical and environmental samples are extremely useful to control amebiasis and to promote public health. The present study compared several primer sets for small subunit (SSU) rDNA and histone genes of E. histolytica cysts. A 246 bp of the SSU rDNA gene of pure cysts contained in phosphate-buffered saline (PBS) and in stool samples was successfully amplified by nested PCR, using the 1,147-246 bp primer set, of the primary PCR products which were pre-amplified using the 1,147 bp primer as the template. The detection limit of the nested PCR using the 1,147-246 primer set was 10 cysts in both groups (PBS and stool samples). The PCR to detect histone gene showed negative results. We propose that the nested PCR technique to detect SSU rDNA can be used as a highly sensitive genetic method to detect E. histolytica cysts in stool samples.

후막 SmBCO/IBAD-MgO 초전도 박막선재의 제조 (Fabrication of Thick SmBCO/IBAD-MgO coated conductor)

  • 이정훈;강득균;하홍수;고락길;오상수;김호경;양주생;정승욱;문승현;염도준;김철진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 춘계학술대회 논문집
    • /
    • pp.9-9
    • /
    • 2009
  • Coated conductor is required to have good critical current property for high efficiency of electric power applications. Until now, long coated conductor does not show high Jc over 3 MA/$cm^2$ in thick superconducting layer because of texture degradation by thick superconducting layer. In this study, in order to overcome this issue, thicker superconducting layer was deposited with optimized conditions to reduce the degradation of critical current density. SmBCO superconducting coated conductor was deposited with 1~3 um of thickness at $750\sim850^{\circ}C$ under 15~20 mTorr of oxygen partial pressure using batch type EDDC( evaporation using drum in dual chamber). The buffered substrate for superconducting layer deposition was used IBAD-MgO template with the architecture of $LaMnO_3/MgO/Y_2O_3/Al_2O_3$/Hastelloy. After fabrication of coated conductor, critical current was measured by 4-prove method under self-magnetic field and 77K. In addition, surface morphology and texture were analyzed by SEM and XRD, respectively. 3 um thick SmBCO coated conductor shows highest $I_C$ values of 638A/cm-w in 1 m long in the world.

  • PDF