• 제목/요약/키워드: boron addition

검색결과 198건 처리시간 0.026초

육방정 질화붕소 나노입자 합성 및 열전도성 복합체 응용 (Synthesis of Hexagonal Boron Nitride Nanocrystals and Their Application to Thermally Conductive Composites)

  • 정재용;김양도;신평우;김영국
    • 한국분말재료학회지
    • /
    • 제23권6호
    • /
    • pp.414-419
    • /
    • 2016
  • Much attention has been paid to thermally conductive materials for efficient heat dissipation of electronic devices to maintain their functionality and to support lifetime span. Hexagonal boron nitride (h-BN), which has a high thermal conductivity, is one of the most suitable materials for thermally conductive composites. In this study, we synthesize h-BN nanocrystals by pyrolysis of cost-effective precursors, boric acid, and melamine. Through pyrolysis at $900^{\circ}C$ and subsequent annealing at $1500^{\circ}C$, h-BN nanoparticles with diameters of ~80 nm are synthesized. We demonstrate that the addition of small amounts of Eu-containing salts during the preparation of melamine borate precursors significantly enhanced the crystallinity of h-BN. In particular, addition of Eu assists the growth of h-BN nanoplatelets with diameters up to ~200 nm. Polymer composites containing both spherical $Al_2O_3$ (70 vol%) and Eu-doped h-BN nanoparticles (4 vol%) show an enhanced thermal conductivity (${\lambda}{\sim}1.72W/mK$), which is larger than the thermal conductivity of polymer composites containing spherical $Al_2O_3$ (70 vol%) as the sole fillers (${\lambda}{\sim}1.48W/mK$).

폐수처리용 붕소 도핑 다이아몬드 전극의 수명에 미치는 제조공정 변수의 영향 (Influence of Manufacturing Conditions for the Life Time of the Boron-Doped Diamond Electrode in Wastewater Treatment)

  • 최용선;이영기;김정열;김경민;이유기
    • 한국재료학회지
    • /
    • 제27권3호
    • /
    • pp.137-143
    • /
    • 2017
  • Boron-doped diamond (BDD) electrode has an extremely wide potential window in aqueous and non-aqueous electrolytes, very low and stable background current and high resistance to surface fouling due to weak adsorption. These features endow the BDD electrode with potentially wide electrochemical applications, in such areas as wastewater treatment, electrosynthesis and electrochemical sensors. In this study, the characteristics of the BDD electrode were examined by scanning electron microscopy (SEM) and evaluated by accelerated life test. The effects of manufacturing conditions on the BDD electrode were determined and remedies for negative effects were noted in order to improve the electrode lifetime in wastewater treatment. The lifetime of the BDD electrode was influenced by manufacturing conditions, such as surface roughness, seeding method and rate of introduction of gases into the reaction chamber. The results of this study showed that BDD electrodes manufactured using sanding media of different sizes resulted in the most effective electrode lifetime when the particle size of alumina used was from $75{\sim}106{\mu}m$ (#150). Ultrasonic treatment was found to be more effective than polishing treatment in the test of seeding processes. In addition to this, BDD electrodes manufactured by introducing gases at different rates resulted in the most effective electrode lifetime when the introduced gas had a composition of hydrogen gas 94.5 vol.% carbon source gas 1.6 vol.% and boron source gas 3.9 vol.%.

PECVD법에 의해 증착된 Ti-B-C코팅막 내의 보론함량과 증착온도에 따른 미세구조 및 기계적 물성의 변화 (The Effect of Boron Content and Deposition Temperature on the Microstructure and Mechanical Property of Ti-B-C Coating Prepared by Plasma-enhanced Chemical Vapor Deposition)

  • 옥정태;송풍근;김광호
    • 한국표면공학회지
    • /
    • 제38권3호
    • /
    • pp.106-111
    • /
    • 2005
  • Ternary Ti-B-C coatings were synthesized on WC-Co and Si wafers substrates by a PECVD technique using a gaseous mixture of $TiCl_4,\;BCl_3,\;CH_4,\;Ar,\;and\; H_2$. The effects of deposition variables such as substrate temperature, gas ratio, $R_x=[BCl_3/(CH_4+BCl_3)]$ on the microstructure and mechanical properties of Ti-B-C coatings were investigated. From our instrumental analyses, the synthesized Ti-B-C coatings was confirmed to be composites consisting of nanocrystallites TiC, quasi-amorphous TiB2, and amorphous carbon at low boron content, on the contrary, nanocrystallites $TiB_2$, quasi-amorphous TiC, and amorphous carbon at relatively high boron content. The microhardness of the Ti-B-C coatings increased from $\~23 GPa$ of TiC to $\~38 GPa$ of $Ti_{0.33}B_{0.55}C_{0.11}$ coatings with increasing the boron content. The $Ti_{0.33}B_{0.55}C_{0.11}$ coatings showed lower average friction coefficient of 0.45, in addition, it showed relatively better wear behavior compared to other binary coatings of $TiB_2$ and TiC. The microstruture and microhardness value of Ti-B-C coatings were largely depend on the deposition temperature.

보론 나이트라이드와 탄소나노튜브로 충전된 실리콘 고무의 열전도도 향상 (Improvement of Thermal Conductivity of Poly(dimethyl siloxane) Composites Filled with Boron Nitride and Carbon Nanotubes)

  • 하진욱;홍진호;김민재;최진규;박동화;심상은
    • 폴리머
    • /
    • 제37권6호
    • /
    • pp.722-729
    • /
    • 2013
  • Poly(dimethyl siloxane)(PDMS, 실리콘 고무)의 열전도도 향상을 위하여 보론 나이트라이드과 탄소나노튜브를 열전도성 충전제로 사용하였다. 보론 나이트라이드의 함량은 0에서 100 phr로 증가시켰으며, 탄소나노튜브의 함량은 보론 나이트라이드의 함량을 100 phr로 고정시킨 상태에서 0에서 4 phr로 증가시켰다. 실리콘 고무 복합재료의 열전도도는 보론 나이트라이드 함량의 증가에 따라 증가하였으나, 탄소나노튜브를 추가로 첨가하더라도 열전도도 향상에 대한 효과는 미미하였다. 100 phr 함량의 보론 나이트라이드 함량에 탄소나노튜브를 충전 시 복합재료의 열분해가 가속화되는 예상치 못한 결과를 얻었다. 이를 해석하기 위하여 Horowitz-Metzger 방법을 이용하여 열분해 활성화 에너지를 계산하였다. 또한 보론 나이트라이드/탄소나노튜브가 충전된 실리콘 고무 복합재료의 경화거동, 전기저항 및 기계적 물성을 연구하였다.

DMAB첨가량에 따른 연성회로기판을 위한 무전해 Ni 도금박막에 관한 연구 (DMAB Effects in Electroless Ni Plating for Flexible Printed Circuit Board)

  • 김형철;나사균;이연승
    • 한국재료학회지
    • /
    • 제24권11호
    • /
    • pp.632-638
    • /
    • 2014
  • We investigated the effects of DMAB (Borane dimethylamine complex, C2H10BN) in electroless Ni-B film with addition of DMAB as reducing agent for electroless Ni plating. The electroless Ni-B films were formed by electroless plating of near neutral pH (pH 6.5 and pH 7) at $50^{\circ}C$. The electroless plated Ni-B films were coated on screen printed Ag pattern/PET (polyethylene terephthalate). According to the increase of DMAB (from 0 to 1 mole), the deposition rate and the grain size of electroless Ni-B film increased and the boron (B) content also increased. In crystallinity of electroless Ni-B films, an amorphization reaction was enhanced in the formation of Ni-B film with an increasing content of DMAB; the Ni-B film with < 1 B at.% had a weak fcc structure with a nano crystalline size, and the Ni-B films with > 5 B at.% had an amorphous structure. In addition, the Ni-B film was selectively grown on the printed Ag paste layer without damage to the PET surface. From this result, we concluded that formation of electroless Ni-B film is possible by a neutral process (~green process) at a low temperature of $50^{\circ}C$.

Effect of Boron Additions on Glass Formation and Magnetic Properties of Fe-Co-Ti-Zr-B Amorphous Ribbons

  • Kim, Sumin;Han, Bo Kyeong;Choi-Yim, Haein
    • Journal of Magnetics
    • /
    • 제21권2호
    • /
    • pp.164-167
    • /
    • 2016
  • The effect of the B additions on glass formation and magnetic properties is reported for the $Fe_{(87-x-y)}Co_yTi_7Zr_6B_x$ (x = 2, 4, 6 and y = 35, 40) alloy system. The ribbon samples with the width of 2 mm for each composition were prepared by the melt spinning technique; furthermore, their phase information was obtained from X-ray diffraction. Glass formation and magnetic properties were measured using differential scanning calorimetry and vibrating sample magnetometer respectively. The $Fe_{45}Co_{40}Ti_7Zr_6B_2$ (x = 2 and y = 40) system has the nanocrystalline phase identified as ${\alpha}-Fe$, as well as the amorphous phase, whereas all other alloys are fully amorphous. It is associated with the role of B on the glass formation. The widest supercooled liquid region is obtained as 71 K at x = 4 (both y = 35 and 40). The saturation magnetization decreases with the increase of the amount of the B addition, and the highest value is 1.59 T as x = 2 and y = 35 for this alloy system.

Metal Copper Clad Laminate (MCCL)의 고방열 특성을 위한 Epoxy/BN 복합체 개발 (Development of Epoxy/Boron Nitride Composites for High Heat Dissipation of Metal Copper Clad Laminate (MCCL))

  • 최호경;최재현;최봉구;윤도영;최중소
    • Korean Chemical Engineering Research
    • /
    • 제58권1호
    • /
    • pp.64-68
    • /
    • 2020
  • 본 연구에서는, 열 전도성 충진제로 충진 된 에폭시복합체를 사용하여 금속 구리판에 이를 코팅한 기판이 제조되었다. 에폭시 복합체의 열전도도를 향상시키기 위해서는 에폭시 매트릭스에 있는 전도성 필러의 최적 분산을 통한 전도성 네트워크를 형성하게 하고, 인접한 필러 입자들 사이에서 열 저항 접합의 수를 감소시키는 것이 중요한 요소이다. 이는 에폭시는 열전도도가 0.2~0.3 W 밖에 안되기 때문에 높은 열전도도를 유지하기 위해선 열전도성 필러가 서로 연결되어 입자간에 갭이 적어야 열저항을 감소시킬수 있기 때문이다. 본 연구의 목적은 에폭시 수지에 Al2O3와 Boron Nitride (BN) 충진제를 균일하게 분산시켜 고방열 에폭시 복합체를 개발하는 데 있다. 그 결과, Al2O3와 Boron nitride Filler가 에폭시 수지 매트릭스에 서로 연결되어 에폭시 수지와 알루미나/Boron nitride 하이브리드 필러 간에 계면 공극 없이 분산되어 열전도도 특성 향상을 확인 할 수 있었고, 표면 처리한 s-BN 필러가 에폭시 수지의 매트릭스의 계면접착력을 향상시켰으며, 계면 공극을 최소화함에 따라 높은 열전도도 특성을 확보 할 수 있었다.

카본 및 보론 첨가가 탄화규소 열간 가압 소결거동 및 기계적 특성에 미치는 영향 (Effect of carbon and boron addition on sintering behavior and mechanical properties of hot-pressed SiC)

  • 안종필;채재홍;김경훈;박주석;김대근;김형순
    • 한국결정성장학회지
    • /
    • 제18권1호
    • /
    • pp.15-21
    • /
    • 2008
  • 탄화규소(SiC)는 산화저항성, 내식성, 고온 강도 및 열전도 특성 등의 기계적 특성이 매우 우수한 재료로 알려져 있지만, 강한 공유결합성으로 인하여 그 소결이 매우 어려운 재료이다. 본 연구에서는 치밀한 탄화규소 소결체를 제조하기 위하여 카본 및 보론을 소결 첨가제로하여 열간 가압 소결법을 적용하여 탄화규소 소결체를 제작하여 그 특성을 평가하였다. 카본의 첨가는 탄화규소의 소결을 촉진하는 역할을 하여 비정상 입성장을 억제하기 때문에 미세하고 균일한 미세구조를 형성하였기 때문에 탄화규소 소결체의 기계적 특성을 향상시키는 것을 확인 할 수 있었다. 또한 차본의 첨가는 소결 중 보론의 첨가에 의해 발생하는 탄화규소의 6H 구조에서 4H 구조로의 상전이를 억제함을 알 수 있었다.

Effects of Hafnium, Boron and Zirconium on the Ductility of Ni$_3$(Al, Fe) Intermetallic Compounds

  • Lim, S.H.;No, J.Y.;No, K.S.;Wee, D.M.
    • 한국재료학회지
    • /
    • 제2권4호
    • /
    • pp.306-310
    • /
    • 1992
  • Effects of hafnium, boron and zirconium on the ductility of Ni$_3$(Al, Fe) intermetallic compounds were studied using tensile test and SIMS analysis. Ni$_3$(Al, Fe) alloy with 0.1 at.% Hf, 0.05 at.% B and 0.1 at.% Zr additions showed maximum elongations of about 30% at 300K, 10% at 300K and 14% at 473K, respectively. The fracture mode of the alloy without the additive was the mixture of intergranular and transgranular fractures, but the addition of Hf, Zr or B changed the fracture mode to transgranular only. SIMS analysis showed that the beneficial effects of Hf, Zr or B segregation on the grain boundary strength are consistent with the grain boundary cohesion theory.

  • PDF