방전플라즈마 소결법으로 제조된 Bismuth Antimony Telluride의 소결온도에 따른 열전특성 (Effect of Sintering Temperature on the Thermoelectric Properties of Bismuth Antimony Telluride Prepared by Spark Plasma Sintering)

  • 이경석;서성호;진상현;유봉영;정영근
    • 한국재료학회지
    • /
    • 제22권6호
    • /
    • pp.280-284
    • /
    • 2012
  • Bismuth antimony telluride (BiSbTe) thermoelectric materials were successfully prepared by a spark plasma sintering process. Crystalline BiSbTe ingots were crushed into small pieces and then attrition milled into fine powders of about 300 nm ~ 2${\mu}m$ size under argon gas. Spark plasma sintering was applied on the BiSbTe powders at 240, 320, and $380^{\circ}C$, respectively, under a pressure of 40 MPa in vacuum. The heating rate was $50^{\circ}C$/min and the holding time at the sintering temperature was 10 min. At all sintering temperatures, high density bulk BiSbTe was successfully obtained. The XRD patterns verify that all samples were well matched with the $Bi_{0.5}Sb_{1.5}Te_{3}$. Seebeck coefficient (S), electric conductivity (${\sigma}$) and thermal conductivity (k) were evaluated in a temperature range of $25{\sim}300^{\circ}C$. The thermoelectric properties of BiSbTe were evaluated by the thermoelectric figure of merit, ZT (ZT = $S^2{\sigma}T$/k). The grain size and electric conductivity of sintered BiSbTe increased as the sintering temperature increased but the thermal conductivity was similar at all sintering temperatures. Grain growth reduced the carrier concentration, because grain growth reduced the grain boundaries, which serve as acceptors. Meanwhile, the carrier mobility was greatly increased and the electric conductivity was also improved. Consequentially, the grains grew with increasing sintering temperature and the figure of merit was improved.

Chalcogenide계 열전재료

  • 김일호
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제24권7호
    • /
    • pp.10-17
    • /
    • 2011
  • 현재 개발 중인 Chalcogenide계 열전재료 중에서, 이방성 재료인 Thallium chalcogenide, Alkalimetal bismuth chalcogenide, Bismuth telluride와 등방성 재료인 Lead telluride, Silver antimony telluride, TAGS, LAST 및 SALT를 소개하였고, 이 재료들에 대한 연구 동향을 살펴보았다. Chalcogenide는 S, Se, Te 및 다른 원소와의 다양한 조합에 의해, 넓은 온도범위에서 열전재료로 응용하기 위한 밴드갭 에너지의 조절이 가능하다. 또한 합성공정에 따른 상변태, 석출 등 구조변화에 따른 열전특성의 변화를 기대할 수 있어 열전재료 개발 초기부터 활발한 연구가 진행되어 왔다. 과거의 전통적인 Chalcogenide계 열전재료뿐만 아니라, Chalcogenide계 열전 신소재에 대해서도 살펴보았다. Chalcogenide는 전자적, 광학적, 열적 성질 등 특성이 독특하고 변화가 무궁무진하여 아주 매력적이기 때문에, 앞으로도 계속 열전재료로서 각광받는 물질군으로 판단된다. 그림 11에 현재까지 ZT의 최댓값이 1이 넘는다고 보고된 열전재료의 성능지수를 요약하였다.

  • PDF

MOCVD를 이용한 $BiSbTe_3$ 박막성장 및 열전소자 제작

  • 권성도;윤석진;주병권;김진상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.425-425
    • /
    • 2008
  • Bismuth-antimony-telluride based thermoelectric thin film materials were prepared by metal organic vapor phase deposition using trimethylbismuth, triethylantimony and diisopropyltelluride as metal organic sources. A planar type thermoelectric device has been fabricated using p-type $Bi_{0.4}Sb_{1.6}Te_3$ and n-type $Bi_2Te_3$ thin films. Firstly, the p-type thermoelectric element was patterned after growth of $4{\mu}m$ thickness of $Bi_{0.4}Sb_{1.6}Te_3$ layer. Again n-type $Bi_2Te_3$ film was grown onto the patterned p-type thermoelectric film and n-type strips are formed by using selective chemical etchant for $Bi_2Te_3$. The top electrical connector was formed by thermally deposited metal film. The generator consists of 20 pairs of p- and n-type legs. We demonstrate complex structures of different conduction types of thermoelectric element on same substrate by two separate runs of MOCVD with etch-stop layer and selective etchant for n-type thermoelectric material. Device performance was evaluated on a number of thermoelectric devices. To demonstrate power generation, one side of the device was heated by heating block and the voltage output was measured. The highest estimated power of 1.3mW is obtained at the temperature difference of 45K. We provide a promising approach for fabricating thin film thermoelectric generators by using MOCVD grown thermoelectric materials which can employ nanostructures for high thermoelectric properties.

  • PDF

MOCVD를 이용한 BiSbTe3 박막성장 및 열전소자 제작 (Properties of BiSbTe3 Thin Film Prepared by MOCVD and Fabrication of Thermoelectric Devices)

  • 권성도;윤석진;주병권;김진상
    • 한국전기전자재료학회논문지
    • /
    • 제22권5호
    • /
    • pp.443-447
    • /
    • 2009
  • Bismuth-antimony-telluride based thermoelectric thin film materials were prepared by metal organic vapor phase deposition using trimethylbismuth, triethylantimony and diisopropyltelluride as metal organic sources. A planar type thermoelectric device has been fabricated using p-type $Bi_{0.4}Sb_{1.6}Te_3$ and n-type $Bi_{2}Te_{3}$ thin films. Firstly, the p-type thermoelectric element was patterned after growth of $5{\mu}m$ thickness of $Bi_{0.4}Sb_{1.6}Te_3$ layer. Again n-type $Bi_{2}Te_{3}$ film was grown onto the patterned p-type thermoelectric film and n-type strips are formed by using selective chemical etchant for $Bi_{2}Te_{3}$. The top electrical connector was formed by thermally deposited metal film. The generator consists of 20 pairs of p- and n-type legs. We demonstrate complex structures of different conduction types of thermoelectric element on same substrate by two separate runs of MOCVD with etch-stop layer and selective etchant for n-type thermoelectric material. Device performance was evaluated on a number of thermoelectric devices. To demonstrate power generation, one side of the device was heated by heating block and the voltage output was measured. The highest estimated power of 1.3 ${\mu}m$ is obtained at the temperature difference of 45 K.

Flexible Thermoelectric Device Using Thick Films for Energy Harvesting from the Human Body

  • Cho, Han Ki;Kim, Da Hye;Sin, Hye Sun;Cho, Churl-Hee;Han, Seungwoo
    • 한국세라믹학회지
    • /
    • 제54권6호
    • /
    • pp.518-524
    • /
    • 2017
  • A flexible thermoelectric device using body heat has drawn attention as a power source for wearable devices. In this study, thermoelectric thick films were fabricated by cold pressing method using p-type antimony telluride and n-type bismuth telluride powders in accordance with specific loads. Thermoelectric thick films were denser and improved the electrical and thermoelectric properties while increasing the load of the cold pressing. The thickness of the specimen can be controlled by the amount of material; specimens were approximately 700 um in thickness. Flexible thermoelectric devices were manufactured by using the thermoelectric thick films on PI (Polyimide) substrate. The process is cheap, efficient, easy and scalable. Evaluation of power generation performance and flexibility on the fabricated flexible thermoelectric device was carried out. The flexible thermoelectric device has great flexibility and good performance and can be applied to wearable electronics as a power source.

플라즈마 아크 방전법에 의한 Bi-Sb-Te 나노 열전분말 제조 (Synthesis of Bi-Sb-Te Thermoelectric Nanopowder by the Plasma Arc Discharge Process)

  • 이길근;이동열;하국현
    • 한국분말재료학회지
    • /
    • 제15권5호
    • /
    • pp.352-358
    • /
    • 2008
  • The present study focused on the synthesis of a bismuth-antimony-tellurium-based thermoelectric nanopowders using plasma arc discharge process. The chemical composition, phase structure, particle size of the synthesized powders under various synthesis conditions were analyzed using XRF, XRD and SEM. The powders as synthesized were sintered by the plasma activated sintering. The thermoelectric properties of sintered body were analyzed by measuring Seebeck coefficient, specific electric resistivity and thermal conductivity. The chemical composition of the synthesized Bi-Sb-Te-based powders approached that of the raw material with an increasing DC current of the are plasma. The synthesized Bi-Sb-Te-based powder consist of a mixed phase structure of the $Bi_{0.5}Sb_{1.5}Te_{3}$, $Bi_{2}Te_{3}$ and $Sb_{2}Te_{3}$ phases. This powder has homogeneous mixing state of two different particles in an average particle size; about 100nm and about 500nm. The figure of merit of the sintered body of the synthesized 18.75 wt.%Bi-24.68 wt.%Sb-56.57 wt.%Te nanopowder showed higher value than one of the sintered body of the mechanically milled 12.64 wt.%Bi-29.47 wt.%Sb-57.89 wt.%Te powder.

가압소결온도에 따른 p형 (Bi0.2Sb0.8)2Te3 가압소결체의 열전특성 (Thermoelectric Properties of the p-type (Bi0.2Sb0.8)2Te3 with Variation of the Hot-Pressing Temperature)

  • 최정열;오태성
    • 마이크로전자및패키징학회지
    • /
    • 제18권4호
    • /
    • pp.33-38
    • /
    • 2011
  • p형 $(Bi_{0.2}Sb_{0.8})_2Te_3$ 분말을 기계적 합금화 공정으로 제조하여 가압소결 후 가압소결온도에 따른 열전특성을 분석하였다. 가압소결온도를 $350^{\circ}C$에서 $550^{\circ}C$로 증가시킴에 따라 상온에서 측정한 Seebeck 계수가 237 ${\mu}V/K$에서 210 ${\mu}V/K$로 감소하고 전기비저항이 2.25 $m{\Omega}-cm$에서 1.34 $m{\Omega}-cm$로 감소하였으며, power factor가 $25.0{\times}10^{-4}W/m-K^2$에서 $32.9{\times}10^{-4}W/m-K^2$로 증가하였다. $350{\sim}550^{\circ}C$의 온도범위에서 가압소결한 시편들 중에서, $500^{\circ}C$에서 가압소결한 $(Bi_{0.2}Sb_{0.8})_2Te_3$ 가압소결체가 상온에서 1.09 및 $75^{\circ}C$에서 1.2의 가장 높은 무차원 성능지수를 나타내었다.