The Piezoelectric and Dielectric Properties of PZT-PMFW Piezoelectric Ceramics (PZT-PMFW 압전 세라믹의 압전 및 유전 특성)

  • 이종섭;이문주;이용희;정수현;임기조
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.689-692
    • /
    • 2001
  • In this paper, the pizoelectric and dielectric properties of 0.95Pb(ZrxTil-x)O$_3$- 0.05Pb(Mn$\_$0.2/Fe$\_$0.4/W$\_$0.4/)O$_3$piezoelectric ceramics is investigated as a function of Zr/Ti mole ratio. Also, MPB(Morphotropic Phase Boundary) and optimal sintering temperature is studied using XRD and SEM. As a results, when Zr/Ti mole ratio is 52/48, electromechanical coupling factor, k$\_$p/, is 58[%], permittivity, $\varepsilon$$\^$T/$\_$33//$\varepsilon$0, is 1360 and piezoelectric strain constant, d$\_$33/ is 265[pC/N] and the piezoelectric and dielectric properties become maximum. Phase transition temperature of its ternary piezoelectric system is about 350[$^{\circ}C$]. From the XRD analysis, when Zr/Ti mole ratio is 52/48, tetragonal phase transits to rhombohedral phase. Also, From measuring results of the sintering density, when sintering temperature is 1050[$^{\circ}C$], sintering density become maximum and is about 7930[kg/㎥], and average grain size is about 2-3[$\mu\textrm{m}$].

  • PDF

Dynamic Pyroelectric Properties and Their Frequency Dependences of $Pb(Zr_xTi_{1-x})O_3$ Ceramics with Various Compositions (성분에 따른 $Pb(Zr_xTi_{1-x})O_3$세라믹스의 Dynamic 초전 특성과 그 주파수 의존성)

  • 민경진;윤영섭
    • Proceedings of the IEEK Conference
    • /
    • 1998.10a
    • /
    • pp.609-612
    • /
    • 1998
  • Pyroelectric properties of rhombohedral $Pb(ZrxTi_1-x)O_3ceramics$ with various Zr/Ti ratios of 84/16, 87/13, 90/10, and 93/7 are investigated using dynamic method. The response characteristics of PZT samples are examined by considering frequency dispersion. Since the reorientation of the grain does not the influence on the increase of frequency at low frequency (2~200Hz), the maximum pyroelectric response can be obtained with the change of spontaneous polarization. However, the pyroelectric response of PZT samples could be reduced as the spontaneous polarization decreases due to the restrain of the reorientation of the grain with the increasing of requency at high frequency (200~2000Hz). We have obtained the good pyroelectric response in the PZT sample having 84/16 Zr/Ti ratio, then the pyroelectric coefficient (${\gamma}$) and the figure of merit (FV) were $17.3nC/\textrm{cm}^2K$ and 2.28$\times$10-11Ccm/J, respectively. The noise equivalent power (NEP), the detectivity (D*) were 1.21$\times$10-7W/Hz$\frac{1}{2}$ and 8.26$\times$106cmHz$\frac{1}{2}$/W, respectively.

  • PDF

Characterization of 0.5 % Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$ Thin Films Grown by RF Magnetron Sputtering Method (RF 마그네트론 스퍼터링법으로 성장시킨 0.5 % Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$(BCZT) 박막의 특성분석)

  • 최원석;박용섭;이준신;홍병유
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07a
    • /
    • pp.301-304
    • /
    • 2002
  • We investigated the structural and electrical properties of Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$(BCZT) thin films with a mole fraction of x=0.2 and a thickness about 100 nm. BCZT films were prepared on Pt/Ti/$SiO_2$/Si substrate by a RF magnetron sputtering system. We have measured the thickness profile with Ar/$O_2$ ratio and the surface roughness. It was observed that the oxygen gas, which introduced during the film deposition, have an influence on the roughness of the film and the film roughness was reduced by annealing from 2.33 nm to 2.02 m (RMS at $500^{\circ}C$, Ar:6 scrim, $O_2$:6 sccm). We have found that annealing procedure after top electrode deposit can reduce the dissipation factor.

  • PDF

Characterization of the Annealing Effect of 0.5 % Ce-doped Ba(Zr0.2Ti0.8)O3 Thin Films Grown by Rf Magnetron Sputtering Method (RF 마그네트론 스퍼터링법으로 성장시킨 0.5% Ce-doped Ba(Zr0.2Ti0.8)O3 (BCZT) 박막의 열처리 특성분석)

  • 최원석;박용섭;이준신;홍병유
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.5
    • /
    • pp.361-364
    • /
    • 2003
  • It was investigated that the structural and electrical Properties of Ce-doped Ba(Zr$_{x}$Ti$_{1-x}$ )O$_3$ (BCZT) thin films with a mole fraction of x=0.2 and a thickness about 100 nm. BCZT films were prepared on Pt/Ti/SiO$_2$/Si substrate by a RF magnetron sputtering system. We have measured the thickness profile with Ar/O$_2$ ratio and the surface roughness. It was observed that the oxygen gas, which introduced during the film deposition, have an influence on the roughness of the film and the film roughness was reduced by annealing from 2.33 nm to 2.02 nm (RMS at 500 $^{\circ}C$, Ar:6 sccm, $O_2$:6 sccm). It was found that annealing procedure after top electrode deposit can reduce the dissipation factor.

Effects of Ti, Hf and Zr Alloying Elements on Mechanical Properties and Fracture Behaviors of Fe-30Al-5Cr Alloys (Fe-30Al-5Cr 합금의 기계적 성질 및 파면양상에 미치는 Ti, Hf 및 Zr의 첨가효과)

  • Kim, Sung-Su;Joo, Sung-Min;Joo, Hyung-Gon;Lee, Doh-Jae;Choi, Dap-Chun
    • Journal of Korea Foundry Society
    • /
    • v.21 no.1
    • /
    • pp.24-32
    • /
    • 2001
  • Recently, iron aluminides based on Fe3Al and FeAl are ordered intermetallic alloys that offer good oxidation resistance, excellent sulfidation resistance, and potentially lower cost than many high-temperature structural materials. They have better strength, elasticity to weight ratio and high temperature strength, therefore, they can be cosidered as candidate heat resistance structural materials for automobiles, ships, airplanes and spaceships applications. The changes in the mechanical properties and fracture behavior were investigated for Fe-30at.%Al-5at.%Cr alloys when Ti, Hf and Zr were added respectively. For mechanical properties such as Rockwell hardness and yield strength at room temperature, those were decreased in the case of Fe-30at.%Al-5at.%Cr alloy then increased in the case of 5at.% and 10at.% addition of Ti alone. However, Rockwell hardness and yield strength decreased again at 15%Ti then increased dramatically due to the precipitation hardening of the second phase on the specimen at 20%Ti. For fracture modes, cleavage fracture showed in the case of Fe-30at.%Al and Fe-30at.%Al-5at.%Cr alloys. As the amount of Ti addition changed cleavage to transgranular fracture and to quasi-cleavage fracture at 20%Ti. When Hf, Zr and Hf+Zr were added respectively, transgranular, cleavage and quasi-cleavage fracture were coexisted.

  • PDF

Effect of Ti, B, Zr Elements on Grain Refinement and Castability of Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe Casting Alloy (주조용 Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe 합금의 결정립 미세화와 주조특성에 미치는 Ti, B, Zr 첨가원소의 영향)

  • Kim, Heon-Joo;Park, Su-Min
    • Journal of Korea Foundry Society
    • /
    • v.35 no.5
    • /
    • pp.120-127
    • /
    • 2015
  • The effects of Ti, B and Zr on grain refinement and castability were investigated in Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe alloy. Measurement of cooling curve and micro-structure observation were performed to analyze the effects of the addition of minor elements Ti, B and Zr during solidification. The prominence of effect on grain refinement was in increasing order for Ti, Zr and B element. Fine grain size and an increase of the crystallization temperature for ${\alpha}$-Al solution were evident as the amount of addition elements increased in this study. Addition of 0.15wt% Ti was most effective for grain refinement, and the resulting grain size of ${\alpha}$-Al solution for shell mold and steel mold were $72.3{\mu}m$ and $23.5{\mu}m$, respectively. Fluidity and shrinkage tests were perform to evaluate the castability of the alloy. Maximum fluidity length and minimum ratio of micro shrinkage were recorded for 0.15wt% Ti addition due to the effect of the finest grain size.

Physical properties of $PbZrO_3-PbTiO_3-Pb(Ni_{1/3}Nb_{2/3})O_3$ thin films by sol-gel method (Sol-gel법에 의한 $PbZrO_3-PbTiO_3-Pb(Ni_{1/3}Nb_{2/3})O_3$박막의 물리적 특성)

  • 임무열;구경완;김성일;유영각
    • Electrical & Electronic Materials
    • /
    • v.9 no.10
    • /
    • pp.991-1000
    • /
    • 1996
  • PbTiO$_{3}$-PbZrO$_{3}$-Pb(Ni$_{1}$3/Nb$_{2}$3/O$_{3}$) (PZT-PNN) thin films were prepared from corresponding metal organics partially stabilized with diethanolamine by the sol-gel spin coating method. Each mol ratio of PT:PZ:PNN solutions were #1(50:40:10), #2(50:30:20), #3(45:35:20), #4(40:40:20), #5(40:50:10), #6(35:45:20) and #7(30:50:20) respectively. The spin-coated PZT-PNN films were heat-treated at 350.deg. C for decomposition of residual organics, and were sintered from 450.deg. C to 750.deg. C for crystallization. The substrates, such as Pt and Pt/TiN/Ti/TiN/Si were used for the spin coating of PZT PNN films. The perovskite phase was observed in the PZT-PNN films heat-treated at 500.deg. C. The crystalline of the PZT-PNN films was optimized at the sintering of 700.deg. C. By the result of AES analysis, It is confirmed that the films of TiN/Ti/TiN was a good diffusion barrier and that co-diffusion into the each films was not observed.

  • PDF

Pulse electric field-excited electron emission from Pb$(Zr_xTi_{1-x})O_3$ ceramics prepared by conventional solid state reaction (고상 반응법에 의해 제조된 Pb$(Zr_xTi_{1-x})O_3$ 세라믹스에서 펄스 전계에 의한 전자 방출)

  • Kwak, Sang-Hee;Kim, Tae-Heui;Park, Kyung-Bong;Kim, Chang-Soo
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1867-1869
    • /
    • 1999
  • Pulse electric field induced electron emission from ferroelectrics has been studied with Pb$(Zr_xTi_{1-x})O_3$ ceramics with varying Zr/Ti ratio from 35/65 to 65/35, Electron emission was proved to be concentrated on the electrode edge by emission profile test and emission capture photographs. The 65/35 composition showed largest emission charge in lowest field and lowest emission threshold field. The emission characteristics are closely dependent on their ferroelectric properties in hysteresis curve. Electron emission charge increases with the polarization charge and emission threshold voltage is dependent on coercive field regardless of their composition. But dielectric constant has little relation with emission property. Electron emission charge increases exponentially with pulse electric field irrespective of composition. On the assumption that the surface potential is linear with the pulse electric field, electron emission can be regarded as a field emission at the electrode edge using Fowler-Nordheim plot of ln$(Q_e/E_{fe})$ to $1/E_{fe}$.

  • PDF

Electrical properties of Low Fired Pb(Mg,Te,Mn,Nb)$O_3-Pb(Zr,Ti)O_3$ Ceramics (저온에서 소결한 Pb(Mg,Te,Mn,Nb)$O_3-Pb(Zr,Ti)O_3$세라믹스의 전기적 특성)

  • 정수태;조상희
    • Electrical & Electronic Materials
    • /
    • v.9 no.7
    • /
    • pp.652-659
    • /
    • 1996
  • Sintering characteristics and electrical properties of xPb(Mg$_{1}$8/Te$_{1}$8/Mn$_{1}$4/Nb$_{1}$2/) $O_{3}$-(1-x) Pb (Zr$_{1}$2/ $Ti_{1}$2/) $O_{3}$ (x=0.075, 0.1, 0.125) ceramics are investigated. A sintering temperature of ceramics could be reduced to 950.deg. C by a reaction between PbO and B site compound material. The physical properties of 0.1Pb(Mg, Te, Mn, Nb) $O_{3}$ - 0.9Pb(Zr, Ti) $O_{3}$ bulk ceramic with 3wt% glass frit(0.857PbO-0.143W $O_{3}$) were following : den = 7.95 g/cm$^{3}$, T$_{c}$=340.deg. C, .epsilon.$_{33}$= 754, k$_{31}$=0.3 and Q.=1780. The 3-layer piezoelectric transformer by using a tape casting method showed a good monolithic structure, and its voltage setup ratio was 2.5 times higher than that of a single device by using bulk ceramics.s.s.

  • PDF

Dielectric and Piezoelectric Properties of BNT-PNN-PZT system Ceramics (BNT-PNN-PZT계 세라믹스의 유전 및 압전특성에 관한 연구)

  • 유주현;홍재일;임인호;정희승;윤현상;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1995.11a
    • /
    • pp.44-47
    • /
    • 1995
  • In this study, dielectric and piezoelectric properties of 0.4[0.1Bi(Ni$\_$1/2/Ti$\_$1/2/)O$_3$0.9Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$]-0.6(PbZr$\_$y/Ti$\_$1-y/)O$_3$ceramics with Zr/Ti ratio were observed. As a results, structure of the ceramics with ZrO$_2$(y) 0.425 and 0.45 was MPB. Electromechanical coupling coefficients k$\_$p/, k$\_$31/ of the BN$\_$162/ specimen were 57.2%, 35.6% and piezoelectric constants d$\_$33/, d$\_$31/ were 720, 298[x10$\_$-12/C/N).