• Title/Summary/Keyword: Wire Forming

검색결과 83건 처리시간 0.024초

Hydrostatic Press Forming of Microparts

  • Na K. H.;Kim S. S.;Park H. J.;Yoon D. J.;Choi T. H.;Lee S.;Kim E. Z.
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 The 8th Asian Symposium on Precision Forging ASPF
    • /
    • pp.167-174
    • /
    • 2003
  • Microforming technology becomes crucial in variety of industries as up-to-date machinery products and parts are miniaturized Therefore research on micro forming processes are actively conducted because of its high productivity, high precision and efficienct material usage. Since friction during microforming has greater influence than macroforming, hydrostatic pressing is much more efficient. In this paper minimization of bur during fine sheet shear forming and hydrostatic process of multi-filament extrusion to obtain fine wire of micro-order have been conducted.

  • PDF

유한요소 해석을 이용한 동피복 복합선재의 인발 공정 해석 (Analysis of Copper clad steel wire in the drawing process using FE method)

  • 김현수;조훈;조형호;김대근;김병민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.27-30
    • /
    • 2004
  • Clad wire , which has the advantages of the high strength of a steel core and the electro-conductivity, corrosion resistance of a copper layer, is widely being used the telecommunications, electric-electronic and military technology industries, among others. It is important to obtain uniform coated rate when producing clad wires. Clad wire drawing process can be influenced on damage and coated rate of core and sleeve by process variables as semi-die angle and reduction in area. Therefore, in this study, the finite-element results established in previous study is used to analyze the effect of the various forming parameters, which included the semi-die angle, reduction in area etc. The coated rate will be predicted with observation copper coated rate variation according to total reduction in area and the optimal pass schedule will be set up through proper reduction in area and semi-die angle variation.

  • PDF

제재공장내 슬라임 발생원의 분리와 동정 (Isolation and Identification of the Origins Causing the Slime Found in Pulp and Paper Making Processes)

  • 오정수;조병묵;김은희
    • Journal of the Korean Wood Science and Technology
    • /
    • 제25권3호
    • /
    • pp.50-57
    • /
    • 1997
  • The presence of slime in paper mills is practically universal. Many researches have been performed for many years to resolve the problem caused by the slime in pulp and paper mill. Many papers have been published to show the bacteria is a major cause of paper mill slime. Now that the recycling of the water has been increased and the regulations of a toxic chemical dosage have become more strengthen, the importance of the control of slime in pulp and paper mill recently has been more recognized. Therefore, to produce quality products at the lowest economic and environmental costs, a through study of the microbial ecology and the indentification of troublesome slime-forming bacteria is a quite necessary. The purpose of this paper is to indentify slime~forming bacteria isolated from the papermaking process. The samples were taken from four parts of making fine paper : machine chest, head box, wire part, white water tank. Machine chest showed the most numbers of bacteria, numbering $2.55{\times}10^7$. The different colony types were taken from the 105 dilution plate. Nine bacteria were identified u sing the Biolog system and the vitek system: 6 gram-negative bacteria, 3 gram-positive bacteria. They are Pseudomonas paucimobilis B., Staphylococcus sp., Acinetobacter calcoaceticus., Pseudomonas cepacia, Actinobaci1lus capsulatus, Acidovorax sp., Flavobacterium sp., and Staphylococcus auricularis in addition to one unidentified sp., Among them. Pseudomonas paucimobillis was found in all places where the samples were taken. And, each parts had the different predominant bacteria in it : Pseudomonas paucimobilis B. in machine chest, Acinetobactor calcoaceticus. in Wire Part and Staphylococcus sp. in head box.

  • PDF

산화아연과 탄소나노튜브의 선형 층상 복합체의 일산화질소 가스 감지특성 (NO Gas Sensing Characteristics of Wire-Like Layered Composites Between Zinc Oxide and Carbon Nanotube)

  • 김옥길;김효진;김도진
    • 한국재료학회지
    • /
    • 제22권5호
    • /
    • pp.237-242
    • /
    • 2012
  • We report on the NO gas sensing properties of Al-doped zinc oxide-carbon nanotube (ZnO-CNT) wire-like layered composites fabricated by coaxially coating Al-doped ZnO thin films on randomly oriented single-walled carbon nanotubes. We were able to wrap thin ZnO layers around the CNTs using the pulsed laser deposition method, forming wire-like nanostructures of ZnO-CNT. Microstructural observations revealed an ultrathin wire-like structure with a diameter of several tens of nm. Gas sensors based on ZnO-CNT wire-like layered composites were found to exhibit a novel sensing capability that originated from the genuine characteristics of the composites. Specifically, it was observed by measured gas sensing characteristics that the gas sensors based on ZnO-CNT layered composites showed a very high sensitivity of above 1,500% for NO gas in dry air at an optimal operating temperature of $200^{\circ}C$; the sensors also showed a low NO gas detection limit at a sub-ppm level in dry air. The enhanced gas sensing properties of the ZnO-CNT wire-like layered composites are ascribed to a catalytic effect of Al elements on the surface reaction and an increase in the effective surface reaction area of the active ZnO layer due to the coating of CNT templates with a higher surface-to-volume ratio structure. These results suggest that ZnO-CNT composites made of ultrathin Al-doped ZnO layers uniformly coated around carbon nanotubes can be promising materials for use in practical high-performance NO gas sensors.

피스톤 링 제조용 선재의 다단 형상 압연공정 설계 (Process Design of Multi-Pass Shape Rolling for Manufacturing Piston Ring Wire)

  • 김남진;이경훈;임상혁;이제문;김병민
    • 소성∙가공
    • /
    • 제26권1호
    • /
    • pp.28-34
    • /
    • 2017
  • Multi-pass shape rolling is performed to produce long products of arbitrary cross-sectional shapes. In the past, the multi-pass shape rolling process has been designed by the trial and error method or the experience of experts based on the empirical approach. Particularly, the design of roll caliber in shape rolling is important to improve product quality and dimensional accuracy. In this paper, the caliber design and pass schedule of multi-pass shape rolling were proposed for manufacturing piston ring wire. In order to design roll caliber, major shape parameter and dimension was determined by analysis of various caliber design. FE-simulation was conducted to verify effectiveness of proposed process design. At first, forming simulation was performed to predict shape of the product. Then, fracture of the wire was evaluated by critical damage value using normalized Cockcroft-Latham criteria. The experiment was carried out and the results are within the allowable tolerance.

셀프실드용접 와이어의 Al 첨가량에 따른 용접금속 인성 및 기공형성 변화 (Variation of Toughness and Porosity Formation in Weld Metal with Al Content in Self-Shielded Arc Welding Wire)

  • 방국수;박찬;길웅;장웅성
    • Journal of Welding and Joining
    • /
    • 제29권1호
    • /
    • pp.74-79
    • /
    • 2011
  • Three different welding wires were used to study the effects of Al content on weld metal toughness and porosity formation in self-shielded arc welding. Weld metal microstructure showed that while wire with 1.3% Al content contains coarse $\delta$-ferrite, wires with less than 0.5% Al content showed no such phase. In addition to the microstructural differences, cleanliness in weld metal was also different among wires. It showed that weld metal toughness was influenced by the $\delta$-ferrite formation, cleanliness and Ni addition. Even though wires with less than 0.5% Al content showed higher weld metal toughness, they showed relatively poor workability, forming porosities in weld bead in lower arc voltages.

포물선형상의 성형성에 관한 유한요소해석 (Finite Element Analysis on Formability of Parabolic Shape)

  • 정상원;이경원
    • 한국생산제조학회지
    • /
    • 제21권4호
    • /
    • pp.677-682
    • /
    • 2012
  • For the product with small diameter, long column, and parabolic shape, the forging formability of the high-carbon steel wire rod was investigated in this study. By using the three-dimensional finite element method, the formability of wire was reviewed by forming analysis for the desired parabolic shape of local part. Analysis results due to forging direction, forging velocity, friction coefficient and constraint location were also investigated. On the basis of these results, it is noted that the forging direction has the big influence when the product with long column is forged. As the forging velocity increases, buckling tends to be limited and formability of parabolic shape is improved. By constraining the lower parabolic shape part to suppress plastic strain, the effect depending on friction coefficient is not almost appeared. And good parabolic shape is obtained at the region of the forging velocity of more than 0.5 m/s.

광삼각법을 이용한 고반사 BGA 볼의 정밀 높이 측정 방법 (3D Accuracy Enhancement of BGA Shiny Round Ball Using Optical Triangulation Method)

  • 주병권;조택동
    • 한국정밀공학회지
    • /
    • 제32권9호
    • /
    • pp.799-805
    • /
    • 2015
  • The further development of information, communication and digital media technologies requires the use of advanced, miniaturized semiconductor chips that operate at a high frequency. Die bonding and wire bonding methods for semiconductor packaging have been replaced by direct attachment to the substrate after forming a bump on the chip. However, the height of the bump or ball is an important factor for defects during assembly. This paper proposes an algorithm to measure the height of the bumps or balls in semiconductor packaging with greater accuracy. The performance of the proposed algorithm is experimentally validated. Non-contact 3D measurements of a shiny round ball is quite difficult, and it is not easy to obtain accurate data. This paper thus proposes an optical method and technique to improve the measurement accuracy.

Interaction of Tip Vortices Generated by a Split Wing

  • Youn, Won Suk;Han, Yong Oun;Lee, Dong Yeon
    • International Journal of Aeronautical and Space Sciences
    • /
    • 제2권2호
    • /
    • pp.39-45
    • /
    • 2001
  • To reduce the strength of tip vortex of the fixed wing, a horizontal wing-let splitted into two parts was utilized, and the interaction between vortices generated by these wing-lets was investigated by the hot-wire anemometry. The process of vortex forming and merging was clarified by measurements of velocity vectors and their contours at five downstream cross-sections; 0.05C(chord length), 0.2C, 0.5C, 1.0C and 2.0C. Both vortex-lets formed by each wing-lets rotate counterclockwise and merge into a larger single vortex within a short downstream distance, 0.5C in this case. The strength of the merged tip vortex turned out to become smaller than that of the plain wing tip near the vortex core.

  • PDF

신선 가공된 열처리 생략강의 냉간 성형성에 대한 연구 (Study on the Cold Formability of Drawn Non-heat Treated Steels)

  • 박경수;박용규;이덕락;이종수
    • 소성∙가공
    • /
    • 제12권4호
    • /
    • pp.364-369
    • /
    • 2003
  • Non-heat treated steels are attractive in the steel-wire industry since the spheroidization and quenching-tempering treatment are not involved during the processing. However, non-heat treated steels should satisfy high strength and good formability without performing heat treatment. Therefore, it is important to investigate optimum materials showing a good combination of strength and formability after the drawing process. In this study, three different steels such as dual phase steel, low-Si steel, and ultra low carbon bainitic steel were used to study their mechanical properties and the cold formability. The cold formability of three steels was investigated by estimating the deformation resistance and the forming limit. The deformation resistance was estimated by calculating the deformation energy, and the forming limit was evaluated by measuring the critical strain revealing crack initiation at the notch tip of the specimens. The results showed that deformation resistance was the lowest in the low-Si steel, and the forming limit strains of ultra low carbon bainitic steel and low-Si steel were higher than that of commercial SWRCH45F steel.