• Title/Summary/Keyword: Waste Ion Exchange Resin

Search Result 51, Processing Time 0.026 seconds

Treatment of Simulated Soil Decontamination Waste Solution by Ferrocyanide-Anion Exchange Resin Beads (Ferrocyanide-음이온 교환수지에 의한 모의 토양제염 폐액 처리)

  • Won Hui Jun;Kim Min Gil;Kim Gye Nam;Jung Chong Hun;Park Jin Ho;Oh Won Zin
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.3 no.1
    • /
    • pp.41-47
    • /
    • 2005
  • Preparation of ferrocyanide-anion exchange resin and adsorption test of the prepared resin on the Cs$^{+}$$ion were performed. Adsorption capability of the prepared resin on the Cs$^{+}$ion in the simulated citric acid based soil decontamination waste solution was 4 times greater than that of the commercial cation exchange resin. Adsorption equilibrium of the prepared resin on the Cs$^{+}$ion reached within 360 minutes. Adsorption capability on the Cs$^{+}$ion became to decrease above the necessary Co$^{2+}$ion concentration in the experimental range. Recycling test of the spent ion exchange resin by the successive application of hydrogen peroxide and hydrazine was also performed. It was found that desorption of Cs$^{+}$ion from the resin occurred to satisfy the electroneutrality condition without any degradation of the resin.

  • PDF

Recovery of Tin from Waste Tin Plating Solution by Ion Exchange Resin (주석도금폐액으로부터 이온교환수지를 이용한 주석 회수)

  • Shin, Gi-Wung;Kang, Yong-Ho;Ahn, Jae-Woo;Hyeon, Seung-Gyun
    • Resources Recycling
    • /
    • v.24 no.3
    • /
    • pp.51-58
    • /
    • 2015
  • In order to recover tin from the waste tin plating solution, we used the ion exchange method using three types of ion exchange resins. The ion exchange resin with tertiary functional group(Lewatit TP 272) has not adsorption ratio of tin. The ion exchange resin with iminodiacetic functional group(Lewatit TP 207) has high adsorption ratio of tin, but impurity content in the recovered tin solution was relatively high. Whereas, in case of the ion exchange resin with functional group of ethylhexyl-phosphate(Lewatit VP OC 1026), adsorption ratio of tin was less than that of Lewatit TP 207. However, it was possible to remove impurities in the recovered tin solution by controlling the pH of the solution. High purity tin solution can be recovered by removing the organic materials with water washing process.

Estimation of radionuclides leaching characteristics in different sized geopolymer waste forms with simulated spent ion-exchange resin

  • Younglim Shin;Byoungkwan Kim;Jaehyuk Kang;Hyun-min Ma;Wooyong Um
    • Nuclear Engineering and Technology
    • /
    • v.55 no.10
    • /
    • pp.3617-3627
    • /
    • 2023
  • This study presents a method to solidify spent ion-exchange resin (IER) in a metakaolin-based geopolymer and shows results of mechanical strength, immersion, leaching, irradiation, and thermal cycling tests for waste acceptance criteria (WAC) to repository. The geopolymer waste form with 20 wt% of simulated spent IER met the WAC in South Korea (ROK), and the leaching tests of various sized-waste forms up to 15.0 × 30.0 cm and waste loadings up to 20 wt% for 1-5 d and 1-90 d achieved a leachability index, Li > 6. In a leaching test for 5 d, the cumulative fraction leached (CFL) for Cs, which leached the most, was linearly correlated with the square root of leaching time for all waste forms, and Li increased as the size of the waste form increased. The CFL was also correlated with elapsed time in the 90 d leaching test. The correlations among CFL, time, and volume-to-surface area ratio of waste forms used to estimate the Li of Cs of a 200-L sized geopolymer with 15 wt% IER showed the Li values as 14.73 (5 d) and 17.71 (90 d), respectively, indicating that the large-sized geopolymer waste form met the WAC.

Recovery of High Purity Tin from Waste Solution of the Tin Plating by Ion-exchange and Cyclone-electrowinning (주석도금폐액으로부터 이온교환 및 사이클론 전해채취를 이용한 고순도 주석의 회수)

  • Kang, Yong-Ho;Shin, Gi-Wung;Ahn, Jae-Woo
    • Resources Recycling
    • /
    • v.25 no.4
    • /
    • pp.42-48
    • /
    • 2016
  • A research for the recovery of the metal with high purity from the waste tin plating solution was carried out. First, tin plating waste solution was tested to remove the organic substances and metallic impurities such as Fe, Zn, Na etc. using ion exchange resin having iminodiacetic functional groups (Lewatit TP 207). Second, the tin solution was purified to obtain the high purity tin solution using ion exchange resin having ethylhexyl-phosphate functional groups (Lewatit VPOC 1026). Finally, 99.98% of the high purity of tin metal can be recovered from the purified solution by cyclone type electrowinning method.

A STUDY ON ADSORPTION AND DESORPTION BEHAVIORS OF 14C FROM A MIXED BED RESIN

  • Park, Seung-Chul;Cho, Hang-Rae;Lee, Ji-Hoon;Yang, Ho-Yeon;Yang, O-Bong
    • Nuclear Engineering and Technology
    • /
    • v.46 no.6
    • /
    • pp.847-856
    • /
    • 2014
  • Spent resin waste containing a high concentration of $^{14}C$ radionuclide cannot be disposed of directly. A fundamental study on selective $^{14}C$ stripping, especially from the IRN-150 mixed bed resin, was carried out. In single ion-exchange equilibrium isotherm experiments, the ion adsorption capacity of the fresh resin for non-radioactive $HCO_3{^-}$ ion, as the chemical form of $^{14}C$, was evaluated as 11mg-C/g-resin. Adsorption affinity of anions to the resin was derived in order of $NO_3{^-}$ > $HCO_3{^-}{\geq}H_2PO_4{^-}$. Thus the competitive adsorption affinity of $NO_3{^-}$ ion in binary systems appeared far higher than that of $HCO_3{^-}$ or $H_2PO_4{^-}$, and the selective desorption of $HCO_3{^-}$ from the resin was very effective. On one hand, the affinity of $Co^{2+}$ and $Cs^+$ for the resin remained relatively higher than that of other cations in the same stripping solution. Desorption of $Cs^+$ was minimized when the summation of the metal ions in the spent resin and the other cations in solution was near saturation and the pH value was maintained above 4.5. Among the various solutions tested, from the view-point of the simple second waste process, $NH_4H_2PO_4$ solution was preferable for the stripping of $^{14}C$ from the spent resin.

Preparation and Properties of Heterogeneous Cation Exchange Membrane for Recovery of Ammonium Ion from Waste Water (폐수중 암모늄 이온 회수를 위한 불균질 양이온교환막의 제조 및 특성)

  • Jeong, Boo-Young;Song, Sang-Hun;Baek, Ki-Wan;Cho, In-Hee;Hwang, Taek-Sung
    • Polymer(Korea)
    • /
    • v.30 no.6
    • /
    • pp.486-491
    • /
    • 2006
  • Heterogeneous membranes were prepared by compression molding for the recovery of ammonium ion from waste water. Degree of sulfonation for sulfonated ion exchange resin increased with increasing amount of chlorosulfonic acid. It was 3.32 meq/g at 10 vol%. The tensile strength and elongation of the heterogeneous membrane was decreased with increasing contents of ion exchange resin. The tensile strength for LLDPE matrix membrane was the highest and also the elongation for EVA matrix membranes were the highest. The water content of heterogeneous membrane was increased with increasing contents of ion exchange resin. The maximum value of transport number for PE matrix membrane was 0.973. The electrical resistance of LLDPE matrix membrane was the lowest. It was value of $10.36{\Omega}/cm^2$ at 70 wt% resins.

Preparation and Characterization of Heterogeneous Anion Exchange Membrane for Recovery of Sulfate Ion from Waste Water (폐수 중 황산이온 회수를 위한 불균질 음이온교환막의 제조 및 특성)

  • Choi, Kuk-Jong;Choi, Jae-Hwan;Hwang, Eui-Hwan;Rhee, Young-Woo;Hwang, Taek-Sung
    • Polymer(Korea)
    • /
    • v.31 no.3
    • /
    • pp.247-254
    • /
    • 2007
  • Heterogeneous anion exchange membranes were prepared by compression molding for the recovery of sulfate ion from waste water. The swelling ratio, transport number, and ion exchange capacity of the heterogeneous anion exchange membranes were increased and their electrical resistances were decreased as the amount of ion exchange resin content in the matrix was raised. The tensile strength of the heterogeneous anion exchange membrane was decreased with increasing the amount of ion exchange resin in the LLDPE. The tensile strength for the LDPE heterogeneous membrane containing 30 wt% anion exchange resin showed the highest value. The water content increased with increasing amount of ion exchange resin in the membrane. Moreover the highest transport number of the membrane was 0.86. The electrical resistance of LDPE matrix membrane with 50 wt% resin showed $46.5{\Omega}{\cdot}cm^2$. Current efficiency of electrodialysis for sulfate ion showed the highest value at the current density of $125 mA/cm^2$ in 0.5 mol/L sulfuric acids solution.

Ion Exchange Behavior of $^{137}Cs,\;^{60}Co$ on Diphosil, a new ion exchange resin (Diphosil 이온교환수지에 의한 $^{137}Cs,\;^{60}Co$의 이온교환 거동)

  • Kim, Su-Jeong;Lee, Sang-Jin;Yang, Ho-Yeon;Shin, Sang-Woon
    • Journal of Radiation Protection and Research
    • /
    • v.29 no.1
    • /
    • pp.1-8
    • /
    • 2004
  • Diphosil, a new version of the organic-inorganic composite resin developed by ANL has a structure of the chelating diphosphonic acid groups grafted to a silica support. To apply Diphosil for the treatment of liquid radioactive waste from nuclear power plants, the adsorption equilibrium and column experiments were carried out for the main radionuclides, $^{137}Cs\;and\;^{60}Co$, in the liquid radwaste stream. Through the adsorption equilibrium experiments, the removal efficiencies of $^{137}Cs\;and\;^{60}Co$, and the effects of non-radioactive ions on the removal efficiency have been measured in various conditions using radiotracers. The breakthrough curves for the tested tracers were obtained from the laboratory scale column tests using the simulated liquid radioactive waste. In addition, the removal capacity of Diphosil is compared with that of Amberlite IRN 77 resin, generally used in nuclear power plants.