An Analysis on the Properties of Undispersed Underwater Mortar for Augered Pile with Fly-ash (플라이애쉬 치환율 변화에 따른 오거파일용 수중불분리 모르터의 특성 분석)

  • 이대주;이광설;유홍종;권지훈;한일영;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.04a
    • /
    • pp.261-266
    • /
    • 1998
  • The purpose of this study is to present the reference data on the development of undispersed underwater mortar for augered pile under various replacement ratio of fly-ash. According to the experimental results, when 10% of fly-ash is mixed under mix proportion of 1:1.5(c:s), as strength and shrinkage decrease slightly, whereas fluidity increase, high quality mortar for augered pile can be achieve in case above condition is applied.

  • PDF

Properties of Undispersed Underwater Mortar Using the Expansive Additives and Fly Ash (팽창재 및 플라이애쉬를 이용하는 수중불분리 모르터의 특성)

  • 한천구;이대주;이광설;한일영;권지훈;유홍종
    • Magazine of the Korea Concrete Institute
    • /
    • v.10 no.6
    • /
    • pp.223-231
    • /
    • 1998
  • Existing cast in place piles made by grouting cement mortar have many problems that cracks by autogeneous and drying shrinkage bring about the deterioration of force for piles, segregations by the submersion of ground water occur and also, high cement contents lead to rise the manufacturing cost. Therefore, this study is intended to investigate the mechanical properties of high performance mortar, incorporating expansive additives and fly ash. for cast in place piles. According to the experimental results, as the contents of expansive additives increase in mortar mixture, fluidity decrease and air contents shows inverse tendency. Setting time is delayed. Although compressive strength at 7days shows a decline tendency. compressive strength at 28days and 91days increase slightly with 5% of expansive additives. As fly ash increase in mortar mixture, high fluidity is shown, air contents increase and setting time is delayed at fresh state, and additives are, the larger length change is, whereas shrinkage decrease with the increase of fly ash.

An Analysis on the Properties of Undispersed Underwater Mortar for Augered Pile with Expansive Additives (팽창재 혼입율 변화에 따른 오거파일용 수중불분리 모르터의 특성 분석)

  • 이광설;이대주;유홍종;권지훈;한일영;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.04a
    • /
    • pp.255-260
    • /
    • 1998
  • As a part of the study on the development of augered pile method, this study is intended to investigate the properties of fresh and hardened mortar with the proportion of expansion additives. With the increase of proportion of expansion additives, the fluidity of mortar shows a decrease while air content increases and setting time gets retarded. It show the satisfactory property in strength at 5% of proportion, and shows more expansion with the increase of proportion of expansion additives and sand/cement ratio. In conclusion, both of strength and expansion reveal appropriate at 10% of proportion of expansion additives.

  • PDF