Viscoplastic response and collapse of 316L stainless steel tubes under cyclic bending

  • Chang, Kao-Hua;Hsu, Chien-Min;Sheu, Shane-Rong;Pan, Wen-Fung
    • Steel and Composite Structures
    • /
    • 제5권5호
    • /
    • pp.359-374
    • /
    • 2005
  • This paper presents the experimental and theoretical results of the viscoplastic response and collapse of 316L stainless steel tubes subjected to cyclic bending. The tube bending machine and curvature-ovalization measurement apparatus, which was designed by Pan et al. (1998), were used for conducting the cyclic curvature-controlled experiment. Three different curvature-rates were controlled to highlight the characteristic of viscoplastic response and collapse. Next, the endochronic theory and the principle of virtual work were used to simulate the viscoplastic response of 316L stainless steel tubes under cyclic bending. In addition, a proposed theoretical formulation (Lee and Pan 2001) was used to simulate the relationship between the controlled cyclic curvature and the number of cycles to produce buckling under cyclic bending at different curvature-rates (viscoplastic collapse). It has been shown that the theoretical simulations of the response and collapse correlate well with the experimental data.

온도변화에 따른 AISI 304SS의 틈내 전위강하에 관한 연구 (A Study on the IR Drop in Crevice of AISI 304 Stainless Steel by Temperature Variation)

  • 나은영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제27권7호
    • /
    • pp.872-878
    • /
    • 2003
  • As the results of recent industrial development, many industrial plants and marine structures are exposed to severe corrosion environment than before. Especially, under the wet environment, crevice corrosion damage problems necessarily occur and encourage many interests to prevent them. In this study, the electrochemical polarization test was carried out to study characteristics of crevice corrosion for AISI 304 stainless steel in various solution temperatures. The results are as follows ; 1) as the solution temperature increased in IN $\textrm{H}_2\textrm{SO}_4$, the passive current density and critical current density were increased, whereas corrosion potential and break down potential were nearly constant, 2) as the solution temperature increased. the induced time for initiation of crevice corrosion was shortened. 3) The potential range in the crevice was -220mV/SCE to -380mV/SCE according to the distance from the crevice opening, which is lower than that of external surface of -200mV/SCE.

오스테나이트계 스테인레스 강관에서의 손상해석에 관한 연구 (Failure Analysis of Austenitic Stainless Steel Pipe)

  • 이상율;이종오;이주석;조경식;조종춘;이보영
    • Journal of Welding and Joining
    • /
    • 제11권1호
    • /
    • pp.21-32
    • /
    • 1993
  • A cracking failure of a austenitic stainless steel elbow in a naphtha cracking line in a petrochenmical plant occurred, resulting in leakage of organic compound flowing inside the elbow. Due to the failure, emergency shutdown of the plant was enforced to repair the troubled part of the line. The repair cost as well as production loss during the unscheduled plant shutdown has cost the company a great amount of financial loss. In this studies, a failure analysis of the cracked elbow was performed using NDT, chemical analysis, microstructural analysis including optical microscopy as well as scanning electron microscopy with EPMA, mechanical testings such as tensile testing, hardness testing and Charphy impact test fractography. The results indicated that several problems such as a welding defect and presence of a detrimental phase which was found to be relate to improper postforming heat treatment process was identified and the failure was concluded to be due to a low temperature embrittlement of the defect-containing elbows.

  • PDF

Micro Capillary Tube 방법을 이용한 430 스테인레스강 틈의 폭변화에 따른 틈부식의 전기화학적 평가 (An Electrochemical Evaluation on the Crevice Corrosion of 430 Stainless Steel with Variation of Crevice Wide by Micro Capillary Tubing Method)

  • 나은영
    • 전기화학회지
    • /
    • 제6권4호
    • /
    • pp.250-254
    • /
    • 2003
  • 본 연구는 전기화학적 실험측정으로 페라이트계 430스테인레스강 시험편에 인위적으로 틈을 형성시켰다. 부식용액은 IN $H_2SO_4+0.1N\;NaCl$ 전해액을 사용하였고, 각 시험편의 틈의 크기를 달리하였다. 전기화학적 평가방법은 -600mV/5CE에서 정방향으로 +1,200mV/SCE까지 주사속도 600mV/hr로 동전위 분극시험을 실시하여 부식전위, 부동태 전류밀도 등의 부식거동을 분석하였다. 그리고 정전위 분극시험을 실시하여 부동태 구간 전위 -200mV/SCE를 일정하게 인가 한 후, 틈내에 부동태 전류밀도와 틈부식 발생시간을 계측하였다 실험방법에 있어 Microcapillary tube(MCT)를 이용한 방법으로 틈내 각 지점의 전위를 틈 깊이에 따른 틈내부의 전위강하(IR Drop)에 주목하고, 575 430 스테인레스강 금속에 대한 분극특성과 연계하므로써 틈부식의 발생 원인을 '전위의 이동'의 관점에서 규명 하였다.

슬러지 연마입자를 이용한 이음매 없는 스테인리스강 튜브내면의 자기연마 (Magnetic Abrasive Polishing for Internal Face of Seamless Stainless Steel Tube Using Sludge Abrasive Grain)

  • 김희남;윤여권;김상백;최희성
    • 한국자동차공학회논문집
    • /
    • 제12권6호
    • /
    • pp.151-157
    • /
    • 2004
  • In this paper deals with behavior of the magnetic abrasive using sludge on polishing characteristics in a new internal finishing of seamless stainless steel tube applying magnetic abrasive polishing. The magnetic abrasive using sludge-abrasive grain WA and GC used to resin bond fabricated low temperature. And sludge of magnetic abrasive powder fabricated that sludge was crused into 200 mesh. The previous research have made an experiment in the static state the movement of magnetic abrasive grain is nevertheless in the dynamic state. In this paper, We could have investigated into the changes of the movement of magnetic abrasive grain. In reference to this result, we could have made the experiment which is set under the condition of the magnetic flux density, polishing velocity according to the form of magnetic brush.

알루미늄 폼으로 충진된 스테인레스 관의 3 점 굽힘 특성에 관한 수치적 연구 (A Numerical Study on The Three Point Bending Behavior of Aluminum Foam Filled Stainless Steel Tube)

  • 하산;김엄기;전성식;이창훈;이효진;조성석
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.388-393
    • /
    • 2004
  • A comprehensive numerical study on the three point bending behavior of Aluminum foam-filled stainless steel tube has been performed. Aluminium alloy foams with various densities were produced and their mechanical properites were evaluated. Finite element(FE) analysis of three point bending test was performed to evaluate bending behavior of foam filled cylindrical structures. Results showed that foam filling offered remarkable increase of bending resistance and enhanced the crashworthiness of the structure. It turned out to prevent the inward fold formation at the compression flange, resulted into the multiple propagating folds and increased the load carrying capacity.

  • PDF

Magnetic Abrasive Polishing for Internal Face of Seamless Stainless Steel Tube using Sludge Abrasive Grain

  • Kim, Hee-Nam
    • 동굴
    • /
    • 제78호
    • /
    • pp.23-27
    • /
    • 2007
  • In this paper, we have investigated the characteristics of the magnetic abrasive using sludge on polishing of internal finishing of seamless stainless steel tube applying magnetic abrasive polishing. Either white alumina grain was used to resin sludge at a low temperature, and the sludge of magnetic abrasive powder was synthesized and crushed into 200 meshes. Surface roughness was measured before and after polishing, and more than 40% of improvement of surface roughness was achieved when grain was used under a specific condition. Even though some degree of surface roughness due to deeper scratches still exist, but the result showed a prospective magnetic abrasive polishing using sludge with white alumina grains.

SDSS (Super Duplex Stainless Steel) 강관의 미세조직 및 부식특성에 미치는 열처리 온도의 영향 (The Influence of Heat Treatment Temperature on Microstructure and Corrosion Behavior of SDSS Tube)

  • 이인섭;천창석;임태홍;한윤호;이면학
    • 한국표면공학회지
    • /
    • 제48권6호
    • /
    • pp.329-334
    • /
    • 2015
  • The aim of this paper is to determine the proper heat treatment temperature for SDSS tube production without ${\sigma}$-phase precipitation. When Mother steel tube was heat treated at $800^{\circ}C$ temperature, relatively a large amount of ${\sigma}$-phase precipitated and grain refinement of ferrite phase occurred simultaneously. However, in Pilgered and Drawn steel tubes, grain refinement of the ferrite phase did not occur and a small amount of ${\sigma}$-phase precipitated. For all three types of steel tubes, the pitting potential was reduced to 2/5 or less compared with the untreated one and corrosion also occurred in the salt spray test due to the precipitation of ${\sigma}$-phase. When heat treatment temperature was $900^{\circ}C$, grain refinement of the ferrite phase occurred and very little ${\sigma}$-phase precipitated in Pilgered and Drawn steel tubes. But when heat treatment was done at $1,000^{\circ}C$ temperature, all three types of steel tubes had a similar corrosion properties of that of untreated one and also corrosion did not occur in the salt spray test, as ${\sigma}$-phase did not precipitate. Therefore, the optimum heat treatment temperature range is determined to be more than $1000^{\circ}C$ for the SDSS at which corrosion does not occur.

AL계 희생양극에 의한 2종스테인리스 강축의 음극방식 실용화 연구 (Study of Practical Cathodic Protection of 2nd Class Stainless Steel Shaft by means of Al Sacrificial Anode)

  • 손영태;이명훈;이희준
    • 선박안전
    • /
    • 통권22호
    • /
    • pp.34-53
    • /
    • 2007
  • In the case of hull material. large sized merchant ships are made of steel, on the other hand FRP or wood are used for small sized fishing boats. At present in Korea approximately 88,500 fishing boats are in operation of which 70% are made of FRP In the meantime, stainless steel is frequently used as shaft materials of the small-size FRP fishing boat. Namely, the kinds of shaft materials are STS 304(18Cr-8Ni), STS 316(18Cr-12Ni-2.5Mo steel) and STS 630(17Cr-Ni-Nb steel)etc. Among these things, STS 304 which is the cheapest and having ordinary corrosion resistance is most widely used as 2nd class shaft material. But, using STS 304 for shaft system material of the small-size FRP fishing boat on seawater environments entails a severe corrosion which causes shaft system troubles. Particularly, the corrosions tend to be concentrated of the stern and bow side, propeller shaft surface of inside of stern tube and the boat having no stern cooling pipe line system. As a solution for those problems, research on the ways to mitigate corrosion on the part of 2nd class stainless steel shaft have been undertaken. In the result, not only clarification for the reason of corrosion of the part of stainless steel shaft used mainly for the small-size FRP fishing boat was done, but also most optimal corrosion protection system was developed by experimenting shaft's protection simulation based of the electrochemical cathodic protection principle. In addition, verification through the field test on the optimal cathodic corrosion protection method by means of aluminum sacrificial anode was carried out. In this study, effective and economical shaft's protection system is suggested to the small-size FRP fishing boat operator by substantiating the results obtained from the research on the optimal cathodic protection.

  • PDF