Accuracy evaluation of metal copings fabricated by computer-aided milling and direct metal laser sintering systems

  • Park, Jong-Kyoung;Lee, Wan-Sun;Kim, Hae-Young;Kim, Woong-Chul;Kim, Ji-Hwan
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.2
    • /
    • pp.122-128
    • /
    • 2015
  • PURPOSE. To assess the marginal and internal gaps of the copings fabricated by computer-aided milling and direct metal laser sintering (DMLS) systems in comparison to casting method. MATERIALS AND METHODS. Ten metal copings were fabricated by casting, computer-aided milling, and DMLS. Seven mesiodistal and labiolingual positions were then measured, and each of these were divided into the categories; marginal gap (MG), cervical gap (CG), axial wall at internal gap (AG), and incisal edge at internal gap (IG). Evaluation was performed by a silicone replica technique. A digital microscope was used for measurement of silicone layer. Statistical analyses included one-way and repeated measure ANOVA to test the difference between the fabrication methods and categories of measured points (${\alpha}$=.05), respectively. RESULTS. The mean gap differed significantly with fabrication methods (P<.001). Casting produced the narrowest gap in each of the four measured positions, whereas CG, AG, and IG proved narrower in computer-aided milling than in DMLS. Thus, with the exception of MG, all positions exhibited a significant difference between computer-aided milling and DMLS (P<.05). CONCLUSION. Although the gap was found to vary with fabrication methods, the marginal and internal gaps of the copings fabricated by computer-aided milling and DMLS fell within the range of clinical acceptance (< $120{\mu}m$). However, the statistically significant difference to conventional casting indicates that the gaps in computer-aided milling and DMLS fabricated restorations still need to be further reduced.

Analysis of quality for fixed prostheses fabricated by dental CAD-CAM system (치과용 캐드캠 시스템으로 제작된 고정성 보철물의 품질 분석)

  • Kim, Won-Soo;Han, Man-So;Jung, Jae-Kwan;Kim, Ki-Baek
    • Journal of Technologic Dentistry
    • /
    • v.36 no.3
    • /
    • pp.159-164
    • /
    • 2014
  • Purpose: The purpose of this study was analysis of quality of fixed prostheses fabricated by dental CAD/CAM system. Methods: The ten same cases of stone models were manufactured by dental scannable model, and stone models were scanned using the dental scanner for changing digital model. Ten digital models were completed. The design of zirconia core for zirconia based all-ceramic crown was conducted by the dental CAD program. The samples were fabricated using the pre-sintered zirconia block by dental milling machine. Marginal gaps were analyzed using by silicone replica technique at the eight parts for quality analysis of samples. One-way ANOVA was used for statistical analysis(${\alpha}=0.05$). Results: The mean for marginal gaps were $93.2{\sim}99.1{\mu}m$ at the eight parts. One-was ANOVA didn't show significant differences(p=0.089). Conclusion: The fixed dental prostheses fabricated by dental CAD/CAM were within clinically acceptable range.

Evaluation of the marginal and internal fit of lithium disilicate crowns fabricated by different scanning methods (다른 스캐닝 방법으로 제작된 리튬 디실리케이트 단관의 변연 및 내면 적합도 평가)

  • Kim, Jae-Hong;Kim, Woong-Chul;Kim, Ji-Hwan
    • Journal of Technologic Dentistry
    • /
    • v.36 no.2
    • /
    • pp.75-81
    • /
    • 2014
  • Purpose: This study was to compare adaptations of lithium disilicate CAD/CAM crowns fabricated with different scanning systems. Methods: This study selected the mandibular right first molar as an abutment for experiments and produced 10 working models. Lithium disilicate crowns appropriate for each abutment were produced by using a CEREC$^{(R)}$ CAD/CAM system. The independent t-test was then used to compare and analyze the data obtained from the two groups(${\alpha}$=0.05). Results: Mean(SD) adaptation were $86.93(22.82){\mu}m$ for the InS group, $88.42(26.77){\mu}m$ for the ExS group. They were no statistically significant differences between groups for adaptation(p>0.05). Conclusion: Within the limitations of this study, the results suggest that the accuracy of all investigated optical scanner were satisfactory for clinical use. Further assessment and improvement of the lithium disilicate ceramic for the fabrication of FPDs is evidently still required.

Evaluation of fitness of metal-ceramic crown fabricated by cobalt-chrome alloy (코발트-크롬 합금으로 제작된 금속-도재관의 적합도 평가)

  • Kim, Jae-Hong;Kim, Won-Soo;Kim, Ki-Baek
    • Journal of Korean society of Dental Hygiene
    • /
    • v.13 no.2
    • /
    • pp.361-368
    • /
    • 2013
  • Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (${\alpha}$=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ${\mu}m$ for the cobalt-chrome alloy core group and 84.4(21.9) ${\mu}m$ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.

Comparison the fit of three-unit metal framework fabricated by wax milling method and digital light projection method (왁스 밀링 방법 및 디지털 광 프로젝션 방법으로 제작된 3본 금속 구조물의 적합도 비교)

  • Lee, Jung-Hwan;Ahn, Jae-Seok
    • Journal of Technologic Dentistry
    • /
    • v.41 no.1
    • /
    • pp.9-19
    • /
    • 2019
  • Purpose: This study was conducted to comparative evaluate the marginal and internal gap of three-unit metal frameworks(Co-Cr) fabricated by wax milling method and digital light projection method of CAD/CAM systems. Methods: All the specimens were fabricated by three different fabrication methods: conventional wax up with casting(CWC), milled wax block with casting(MWC), digital light projection with casting(DLPC) (n=10 each). The marginal and internal fits of specimens were examined using a replica technique. The light-body silicone thickness was measured at 8 reference points(each abutment: 16 measurements). All measurements were conducted by a stereomicroscope. Digital photo were taken at $150{\times}$ magnification and then analyzed using a measurement software. The Mann-Whitney test was used for analyzing the results. Results: Statistically significant differences were found between the fabrication methods(p<0.001). The mean(SD) is ${\mu}m$ for fabrication methods, the mean marginal fit were recorded respectively, CWC 63(38), MWC group 50(33), DLPC 103(54) and the mean internal fit CWC 96(47), MWC group 116(41), DLPC 138(66). Conclusion : The marginal and internal fit were statistically different according to the fabrication methods(p<0.001). In all fabrication methods, the greatest misfit was found the occlusal area of all specimens.

Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing

  • Kang, Seen-Young;Lee, Ha-Na;Kim, Ji-Hwan;Kim, Woong-Chul
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.5
    • /
    • pp.347-353
    • /
    • 2018
  • PURPOSE. The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS. The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers using a microstereolithography apparatus (AM group), ten veneers using a five-axis milling machine (SM group), and ten veneers using a traditional free-hand wax technique (TW group) were prepared according to the respective manufacturing method. The ceramic veneers were also fabricated using a heat-press technique, and a silicone replica was used to measure their marginal discrepancy. The marginal discrepancies were measured using a digital microscope (${\times}160$ magnification). The data were analyzed using a nonparametric Kruskal-Wallis H test. Finally, post-hoc comparisons were conducted using Bonferroni-corrected Mann-Whitney U tests (${\alpha}=.05$). RESULTS. The $mean{\pm}SD$ of the total marginal discrepancy was $99.68{\pm}28.01{\mu}m$ for the AM group, $76.60{\pm}28.76{\mu}m$ for the SM group, and $83.08{\pm}39.74{\mu}m$ for the TW group. There were significant differences in the total marginal discrepancies of the ceramic veneers (P<.05). CONCLUSION. The SM group showed a better fit than the AM and TW groups. However, all values were within the clinical tolerance. Therefore, CAD/CAM manufacturing methods can replace the traditional free-hand wax technique.

Marginal fit evaluation of 3 unit fixed dental prostheses fabricated by rapid prototyping method (쾌속 조형 기술을 이용하여 제작된 3본 고정성 보철물의 적합도 평가)

  • Kim, Ki-Baek;Kim, Jae-Hong;Kim, Woong-Chul;Kim, Hae-Young;Kim, Ji-Hwan
    • Journal of Technologic Dentistry
    • /
    • v.34 no.2
    • /
    • pp.105-111
    • /
    • 2012
  • Purpose: The purpose this study was to evaluate the marginal fitness of metal copings fabricated using rapid prototyping method and to compare the fitness with copings by conventional method. Then clinical availability of fixed dental prostheses (FDPs) fabricated using rapid prototyping method shall be confirmed based on marginal fitness. Methods: Ten same cases of3 unit FDPs epoxy models (abutment teeth 14 and 16) were manufactured. Each of ten epoxy models were scanned by 3shape D-700 scanner to be designed by experienced technician, and photopolymer 3 unit FDPs were fabricated using rapid prototyping methodand fabricated using Lost wax technique (LW) with same models. Marginal fitness of 3 unit FDPs were measured by silicone replica technique. T-test of independent sample for statistical analysis was executed with SPSS 12.0K for Windows. (${\alpha}$=.05) Results: Significantly higher mean (SD) marginal fitness (P<.000) were observed in the RP group $(95.9(18.0){\mu}m$ compared to the conventionally LW group $(80.1(13.8){\mu}m$. Conclusion: Marginal fitness of LW group showed excellent rather than RP group. However marginal fitness of 3 unit FDPs fabricated by RP method did not get out of clinical allowance value range significantly to allow clinical application.

Study on methodology for the assessment of internal and marginal adaptation on fixed dental prosthesis (고정성 보철물의 내면 및 변연적합도를 평가하는 방법에 대한 고찰)

  • Pyo, Se-Wook;Lee, Jun-Jae;Han, Jung-Suk;Lim, Young-Jun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.32 no.3
    • /
    • pp.158-168
    • /
    • 2016
  • This article is to review various methods used to investigate internal and marginal adaptation of fixed dental prostheses, and to summarize a merit, worth, and limitation of each method, using some results of previous studies. The methods of measuring internal and marginal gap are divided into two categories in this study; in vivo and in vitro. In vivo methods are clinical evaluations, including exploration, radiography, and impression technique. In vitro methods are laboratory evaluations such as direct view, cross-sectioning, and silicone replica technique using microscope. Measuring by micro computed tomography (CT) or profilometer is also in vitro methods. In recent years, the development of scanning systems is able to analyze 3-dimensional internal and marginal space in detail. As measuring and analyzing technology become more advanced, the ability to thoroughly examine crown adaptation is becoming both simpler and more efficient.

Evaluation of Marginal Gap of Fixed Dental Prostheses Fabricated by Soft Metal Material Using Dental CAD/CAM (치과용 캐드캠을 이용하여 연질금속 재료로 제작한 고정성 보철물의 변연 간격 평가)

  • Kim, Jae-Hong;Kim, Won-Soo;Kim, Ki-Baek
    • Journal of dental hygiene science
    • /
    • v.14 no.3
    • /
    • pp.349-355
    • /
    • 2014
  • The purpose of this study was to evaluate marginal gap of fixed dental prostheses (FDPs) fabricated by soft metal material with using dental computer aided design/computer aided manufacturing (CAD/CAM) system and to compare gap of its by a conventional method. Ten same cases of study models were manufactured and scanned for digital models fabricating. Ten FDPs were fabricated by soft metal material using dental CAD/CAM (SMB group). Then, ten FDPs were fabricated by cast metal using lost wax technique and casting method (LWC group). Marginal gap was measured by silicone replica technique. Gap was measured by digital microscope (${\times}160$). Mann-Whitney test for statistical analysis was executed (${\alpha}=0.05$). The mean (standard deviations) of marginal gap was $76.5{\mu}m$ (35.2) for the SMB group, and $82.9{\mu}m$ (22.1) for the LWC group. Statistically significant differences were not found between SMB and LWC. As results, FDPs fabricated by soft metal material were clinically acceptable range.

Evaluation of marginal and internal gaps of Ni-Cr and Co-Cr alloy copings manufactured by microstereolithography

  • Kim, Dong-Yeon;Kim, Chong-Myeong;Kim, Ji-Hwan;Kim, Hae-Young;Kim, Woong-Chul
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.3
    • /
    • pp.176-181
    • /
    • 2017
  • PURPOSE. The purpose of this study was to evaluate the marginal and internal gaps of Ni-Cr and Co-Cr copings, fabricated using the dental ${\mu}-SLA$ system. MATERIALS AND METHODS. Ten study dies were made using a two-step silicone impression with a dental stone (type IV) from the master die of a tooth. Ni-Cr (NC group) and Co-Cr (CC group) alloy copings were designed using a dental scanner, CAD software, resin coping, and casting process. In addition, 10 Ni-Cr alloy copings were manufactured using the lost-wax technique (LW group). The marginal and internal gaps in the 3 groups were measured using a digital microscope ($160{\times}$) with the silicone replica technique, and the obtained data were analyzed using the non-parametric Kruskal-Wallis H test. Post-hoc comparisons were performed using Bonferroni-corrected Mann-Whitney U tests (${\alpha}=.05$). RESULTS. The mean (${\pm}$ standard deviation) values of the marginal, chamfer, axial wall, and occlusal gaps in the 3 groups were as follows: $81.5{\pm}73.8$, $98.1{\pm}76.1$, $87.1{\pm}44.8$, and $146.8{\pm}78.7{\mu}m$ in the LW group; $76.8{\pm}48.0$, $141.7{\pm}57.1$, $80.7{\pm}47.5$, and $194.69{\pm}63.8{\mu}m$ in the NC group; and $124.2{\pm}52.0$, $199.5{\pm}71.0$, $67.1{\pm}37.6$, and $244.5{\pm}58.9{\mu}m$ in the CC group. CONCLUSION. The marginal gap in the LW and NC groups were clinically acceptable. Further improvement is needed for CC group to be used clinical practice.