• Title/Summary/Keyword: Silicon thin

검색결과 1,697건 처리시간 0.037초

고감도 박막형 스트레인 게이지의 제작 (Fabrication of High-sensitivity Thin-film Type Strain-guges)

  • 정귀상;서정환
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 영호남학술대회 논문집
    • /
    • pp.135-141
    • /
    • 2000
  • The physical, electrical and piezoresitive characteristics of CrN(chromiun nitride) thin-films on silicon substrates have been investigated for use as strain gauges. The thin-film depositions have been carried out by OC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-(5~25 %)$N_2$). The deposited CrN thin-films with thickness of $3500{\AA}$ and annealing conditions($300^{\circ}C$, 48 hr) in Ar-10 % $N_2$ deposition atmosphere have been selected as the ideal piezoresistive material for the strain gauges. Under optimum conditions, the CrN thin-films for the strain gauges is obtained a high electrical resistivity, $\rho=1147.65\;{\mu}{\Omega}cm$, a low temperature coefficient of resistance, TCR=-186 ppm/$^{\circ}C$ and a high temporal stability with a good longitudinal gauge factor, GF=11.17.

  • PDF

Epitaxial Growth of $\beta$-SiC Thin Films on Si(100) Substrate without a Carburized Buffer Layer

  • Wook Bahng;Kim, Hyeong-Joon
    • The Korean Journal of Ceramics
    • /
    • 제3권3호
    • /
    • pp.163-168
    • /
    • 1997
  • Most of heteroepitaxial $\beta$-SiC thin films have been successfully grown on Si(100) adapting a carburizing process, by which a few atomic layers of substrate surface is chemically converted to very thin SiC layer using hydrocarbon gas sources. Using an organo-silicon precursor, bis-trimethylsilymethane (BTMSM, [$C_7H_{20}Si_2$]), heteropitaxial $\beta$-SiC thin films were successfully grown directy on Si substrate without a carburized buffer layer. The defect density of the $\beta$-SiC thin films deposited without a carburized layer was as low as that of $\beta$-SiC films deposited on carburized buffer layer. In addition, void density was also reduced by the formation of self-buffer layer using BTMSM instead of carburized buffer layer. It seems to be mainly due to the characteristic bonding structure of BTMSM, in which Si-C was bonded alternately and tetrahedrally (SiC$_4$).

  • PDF

스핀코터 회전속도에 따른 탄탈륨 박막두께의 선형모델에 관한 연구 (The Research via Linear of Tantalum Thin Film Thickness Depending on Revolution Velocity of Spin Coater)

  • 김승욱
    • 반도체디스플레이기술학회지
    • /
    • 제19권1호
    • /
    • pp.17-22
    • /
    • 2020
  • Recently, the decrease in thin film thickness has been actively studied by changing several physical elements such as the increase in revolution velocity of lower substrate equipped with AC or DC motor. In this paper, we propose a novel spin coater control system that changes AC or DC motor and common use software with limitation of velocity and position control into step motor and LABVIEW software based on GUI to control revolution velocity and position more precisely. By determining six input values of rotation velocity 1, 5, 10, 25, 50, 100 PPS, we fabricated six samples using coating target, TA(tantalum) on silicon substrate and measured their thin film thickness by SEM. Hence, this research can be applied to inferring thin film thickness of tantalum regarding any value of revolution velocity without additional experiments and for linear reference model via property analysis of thin film thickness using other thin-film materials.

Luminescence Characteristics of Red Light Emitting (YVO4:Eu Thin-Film Phosphors Deposited on Si Substrate Using Pulsed Laser Deposition

  • Kim, Dong-Kuk;Kang, Wee-Kyung
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권12호
    • /
    • pp.1859-1862
    • /
    • 2004
  • Europium doped yttrium vanadate ($YVO_4$:Eu) phosphor thin films were grown using a pulsed laser deposition (PLD) technique on silicon substrate. The structural characterization carried out on a series of ($YVO_4$:Eu films at post annealing temperature in the range of 550 $^{\circ}C$-1150 $^{\circ}C$ indicating that films were preferentially (200) oriented at post annealing temperature above 950 $^{\circ}C.$ Photoluminescence of thin film increased with the increase of post annealing temperature and ambient oxygen pressure though the thin film has the powder-like surface morphology at oxygen pressure above 200 mTorr. Photoluminescence decay from $^5D_1$ level of $Eu^{3+}$ show the great concentration dependency, which can be used as a good parameter to control the composition of ($YVO_4$:Eu thin film.

RF magnetron sputtering으로 증착한 IGZO 박막의 RF power에 따른 구조적, 광학적 및 전기적 특성 연구 (The Structures, Optical and Electrical Properties of IGZO Thin Films by RF Magnetron Sputtering According to RF Power)

  • 연제호;김홍배
    • 반도체디스플레이기술학회지
    • /
    • 제15권3호
    • /
    • pp.57-61
    • /
    • 2016
  • We have studied the structural, optical and electrical properties of IGZO thin films. The IGZO thin films were deposited on the silicon wafer by RF magnetron sputtering method. The RF power in sputtering process was varied as 15W, 30W, 45W, 60W, 75W, respectively. All of the thin films transmittance in the visible range was above 85%. XRD analysis showed that amorphous structure of the thin films without any peak. The Hall measurements in the low RF power is the high mobility above $10cm^2/V{\cdot}s$ and the low resistvity are obtained in the IGZO thin films.

Interfaces of Stacking $TiO_2$ Thin Layers Affected on Photocatalytic Activities

  • 주동우;부진효
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.189.1-189.1
    • /
    • 2013
  • Titanium dioxide (TiO2) is a wide bandgap semiconductor possessing photochemical stability and thus widely used for photocatalysis. However, enhancing photocatalytic efficiency is still a challenging issue. In general, the efficiency is affected by physio-chemical properties such as crystalline phase, crystallinity, exposed crystal facets, crystallite size, porosity, and surface/bulk defects. Here we propose an alternative approach to enhance the efficiency by studying interfaces between thin TiO2 layers to be stacked; that is, the interfacial phenomena influencing on the formation of porous structures, controlling crystallite sizes and crystallinity. To do so, multi-layered TiO2 thin films were fabricated by using a sol-gel method. Specifically, a single TiO2 thin layer with a thickness range of 20~40 nm was deposited on a silicon wafer and annealed at $600^{\circ}C$. The processing step was repeated up to 6 times. The resulting structures were characterized by conventional electron microscopes, and followed by carrying out photocatalytic performances. The multi-layered TiO2 thin films with enhancing photocatalytic efficiency can be readily applied for bio- and gas sensing devices.

  • PDF

Structural, Morphological and Electrical Properties of TiO2 Thin Films Deposited by ALD Method

  • Seung-Yeon Oh;Jae-Min Shin;Gyeong-Hun Na;Min-Seok Kwon;Sang-Jeen Hong;Bumsuk Jung
    • 반도체디스플레이기술학회지
    • /
    • 제22권2호
    • /
    • pp.87-95
    • /
    • 2023
  • TiO2 thin films were grown using the Atomic Layer Deposition (ALD) and their structural and electrical properties were investigated. The crystal structure, dielectric constant, and surface roughness of the TiO2 thin films grown by the ALD deposition method were studied. The grown TiO2 thin films showed an anatase crystal structure, and their properties varied with temperature. In particular, the properties of the TiO2 thin films were confirmed by changing the process temperature. The electrical properties of Metal-Insulator-Silicon (MIS) capacitor structures were analyzed using a probe station. The performance improvement of capacitors using TiO2 as a dielectric was confirmed by measuring capacitance through Capacitance-Voltage (C-V) curves.

  • PDF

RF Sputtering 공정 법을 이용해 증착한 Te 기반 박막 및 박막 트랜지스터의 공정 변수에 따른 전기적 특성 평가 (Effect of Working Pressure Conditions during Sputtering on the Electrical Performance in Te Thin-Film Transistors)

  • 이규리;김현석
    • 한국전기전자재료학회논문지
    • /
    • 제35권2호
    • /
    • pp.190-193
    • /
    • 2022
  • In this work, the effect of sputtering working pressure for the tellurium film and its thin-film transistor was investigated. The transfer characteristics of tellurium thin-film transistors were improved by increasing the working pressure during sputtering process. As increasing working pressure, physical and optical properties of Te films such as crystallinity, transmittance, and surface roughness were improved. Therefore, the improved transfer characteristics of Te thin-film transistors may originate from both improved interface properties between the silicon oxide gate dielectric layer and the tellurium active layer with an improved quality of Te film. In conclusion, the control of working pressure during sputtering would be important for obtaining high-performance tellurium-based thin film transistor